Preparation of Electrically Conductive Composites Filled with Nickel Powder and MWCNT Fillers (다중벽 탄소나노튜브와 니켈 분말을 포함하는 전도성 복합체 제조)

  • Kim, Sunghoon;Park, Seonghwan;Kwon, Jaebeom;Ha, KiRyong
    • Korean Chemical Engineering Research
    • /
    • v.54 no.3
    • /
    • pp.410-418
    • /
    • 2016
  • In this study, we prepared electrically conducting composites using epoxy resin of diglycidyl ether of bisphenol A (DGEBA) as a matrix, triethylenetetramine (TETA) as a hardener and nickel powder or multi-walled carbon nanotubes (MWCNTs) grafted with $-NH_2$ groups (MWCNT-$NH_2$) as electrically conducting fillers. Electrical conductivity of composite films were measured by coating on the slide glass with a doctor blade. We measured modification reactions of MWCNT and reaction of MWCNT-$NH_2$ with DGEBA epoxy resin by fourier transform infrared spectrometer (FTIR), thermogravimetric analyzer (TGA) and elemental analyzer (EA). Morphology of composites was investigated by scanning electron microscope (SEM) and sheet resistances of composites were measured by 4-point probe. We found $(9.87{\pm}1.09){\times}10^4{\Omega}/sq$ of sheet resistance for epoxy composite containing both 40 wt% nickel powder and 0.5 wt% of MWCNT-$NH_2$ as fillers, equivalent to epoxy composite containing 53.3 wt% nickel powder only as a filler.

Effect of processing parameters on TiO2 film by room temperature granule spray in vacuum (상온진공과립분사에 의한 TiO2 코팅층에 미치는 공정변수의 영향)

  • Kim, Han-Gil;Park, Yoon-Soo;Bang, Kook-Soo;Park, Dong-Soo;Park, Chan
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.27 no.1
    • /
    • pp.22-27
    • /
    • 2017
  • $TiO_2$ films, thickness of $1{\sim}30{\mu}m$ were deposited on glass substrate at room temperature by room temperature granule spray in vacuum. The starting powder was calcinated at $600^{\circ}C$ for 4 h using $Al_2O_3$ crucible in the furnace. The particle size of the $TiO_2$, $1.5{\mu}m$ was measured by a particle size analyzer. The effect of different process parameters such as number of pass, gas flow rate and feeder voltage was studied. As the number of passes increased, the film thickness increased proportionally due to adequate kinetic energy conserved. The effect of three different flow rates (i.e. 15, 25, and 35 LPM) on deposited film was investigated. As gas flow rate increased, the film thickness increased up to 25 LPM and then decreased. Higher feeder voltage with low flow rate of 15 LPM resulted in unsufficient coating thickness due to insufficient kinetic energy. Microstructure of $TiO_2$ films was investigated by scanning electron microscope and high resolution tramission electron microscope.