Nanostructures, with a diversity of shapes, built on substrates have been developed within many research areas. Lithography is one powerful, but complex, technique to make structures at the nanometer scale, such as platinum nanowires for studying CO catalytic reactions [1], or aluminum nanodisks for studying the plasmon effect [2]. In this work, we approach a facile method to construct nanostructures using noble metals on a titania thin film by using self-assembled structures as a pattern. Here, a large-scale silica monolayer is transferred to the titania thin film substrates using a Langmuir-Blodgett trough, followed by the deposition of a thin transition metal layer. Owing to the hexagonal close-packed structure of the silica monolayer, we would obtain a metal nanostructure that includes separated metallic triangles (islands) after removing the patterning silica beads. This nanostructure can be employed to investigate the role of metal-oxide interfaces in CO catalytic reactions by changing the patterning silica particles with different sizes or by replacing the oxide support. The morphology and chemical composition of the structure can be characterized by scanning electron microscopy, atomic force microscopy and X-ray photoelectron spectroscopy. In addition, we modify these islands to a connected island structure by reducing the silica size of the patterning monolayer, which is utilized to generating hot electron flow based on the localized surface plasmon resonance effect of the metal nanostructures.
Core/shell ($\pm$)PS/(-)silica nanocomposite particles were synthesized by dispersion polymerization using an amphoteric initiator, 2,2'-azobis [N-(2-carboxyethyl)-2,2-methylpropionamidine] ($HOOC(CH_2)_2HN$(HN=) $C(CH_3)_2CN$=NC $(CH_3)_2C$(=NH)NH $(CH_2)_2COOH$), VA-057. Negatively charged (-6.9 mV) silica was used as the stabilizer. The effects of silica addition time and silica and initiator concentrations were investigated in terms of polymerization kinetics, ultimate particle morphology, and size/size distribution. Uniform hybrid microspheres with a well-defined, core-shell structure were obtained at the following conditions: silica content = 10-15 wt% to styrene, VA-057 content=above 2 wt% to styrene and silica addition time=0 min after initiation. The delay in silica addition time retarded the polymerization kinetics and broadened the particle size distribution. The rate of polymerization was strongly affected by the silica content: it increased up to 15 wt% silica but then decreased with further increase in silica content. However, the particle size was only marginally influenced by the silica content. The zeta potential of the composite particles slightly decreased with increasing silica content. With increasing VA-057 concentration, the PS microspheres were entirely coated with silica sol above 1.0 wt% initiator.
The impact of major surface chemical properties of silica sols on the retention and drainage performance of the silica based micrparticle system, Compozil was investigated using four different silica sols. And the effect of silica properties on the interactions with cationic starch and cationic plyacrylamide has also been identified. The surface charge density and the stability over pH of silica sols were increased by introducing aluminosilicate anions at surface. It was found that the charge density of silica sols determined the addition level necessary to attain the maximum retention and drainage. When silica sols were combined with cationic starch, the change density of the product was the critical properties and the degree of microagregation was of minor importance. In the cationic polyacrylamide system the degree of colloid structure appeared to be a more critcial property than the charge density of silica sols.
Tetraethyl orthosilicate (TEOS)로부터 유도된 동결건조 실리카 젤의 기공구조에 미치는 하소온도의 영향이 질소 등온흡착 및 수은압입법에 의하여 조사되었다. 동결건조물은 다소간의 마이크로기공을 함유하고 있었으나 주로 4~6nm 크기의 매크로기공 및 7~20$\mu\textrm{m}$ 크기의 매크로기공으로 구성되어 있었다. 하소온도의 증가에 따른 기공구조변화는 치밀화 정도에 의존하였다.
The synthesis behavior of nanoporous silica aerogel in the macroporous ceramic structure was observed using TEOS as a source material and glycerol as a DCCA(dry control chemical additive). Silica aerogel in the macroporous ceramic structure were synthesized through a sono-gel process. The wet gel in the macroporous ceramic structure were aged in ethanol for 72 h at $50^{\circ}C$. The aged wet gel was dried under supercritical drying condition. The addition of glycerol has a role of giving the uniform pore size distribution. The reproducibility of aerogel in the macroporous ceramic was improved in the glycerol(0.05 mol%) added to the silica sol and TEOS : $H_2O$=1 : 12.
The synthesis behavior of nanoporous silica aerogel in the macroporous ceramic structure was observed using TEOS as a source material and glycerol as a dry control chemical additive (DCCA). Silica aerogel in the macroporous ceramic structure was synthesized via sono-gel process using hexamethyldiazane (HMDS) as a modification agent and n-hexane as a main solvent. The wet gel with a modified surface was dried at $105^{\circ}C$ under ambient pressure. The addition of glycerol appears to give the wet gel a more homogeneous microstructure. However, glycerol also retarded the rate of surface modification and solvent exchange. Silica aerogel completely filled the macroporous ceramic structure without defect in the condition of surface modification (20% HMDS/nhexane at 36hr).
Sugar-based gelator p-dodecanoyl-aminophenyl- ${\beta}$-D-aldopyranosides (1-3) have been shown to self-assemble in the presence of p-aminophenyl aldopyranosides. The hydrogel 1+4 showed the double-helical structure with 3-25 nm outer diameters, which is quite different from that of 1. The gel 2+5 revealed twisted ribbon structure with 30-50 nm in widths and a few micrometers of length whereas the gel 3+4 revealed the single and the bundled fiber structures. The difference in these gel supramolecular structures has successfully been transcribed into silica structures by sol-gel polymerization of tetraethoxysilane (TEOS), resulting in the doublehelical, the twisted-ribbon, the single and the multiple (lotus-shaped) hollow fiber structures. These results indicate that novel silica structures can be created by transcription of various superstructures formed in binary gels through the hydrogen-bonding interaction, and the amino group of the p-aminophenyl aldopyranosides acts as an efficient driving force to create novel silica nanotubes. Furthermore, electron energy-loss spectroscopy (ELLS) provided strong evidence for the inner hollow structure of the double-helical silica nanotube. This is a novel and successful example that a variety of new silica structures can be created using a library of carbohydrate gel fibers as their templates.
Mesoporous silica was prepared from hydrothermal synthesis using gel mixture of tetraethylorthosilcate (TEOS) as silica source and cetyltrimethylammonium bromide (CTMABr) as a surfactant. In the optimum synthesis cause, molar ratio of template and silica changed. The surface and structure properties of mesoporous silica were determined by XRD, SEM, TEM and BET. Also, surface potential of mesoporous silica was measured using zeta potential. $N_2$ adsorption isotherm characteristics, including the specific surface area ($S_{BET}$), total pore volume $V_T$), and average pore diameter ($D_{BJH}$), were determined by BET. As a result, SBET of $100m^2/g{\sim}1500m^2/g$ was determined from the $N_2$ adsorption isotherm. Also, the average pore diameter was 2 nm∼4 nm. Mesoporous silica's surface potential of minus charge was determined from zeta potential.
[ $BaMgAl_{10}O_{19}:Mn^{2+}$ ](BAM:Mn) phosphor particles with spherical shape were prepared by spray pyrolysis from colloidal solution with silica. The phosphor particles prepared by spray pyrolysis from aqueous solution had irregular morphology after high temperature post-treatment. On the other hand, the phosphor particles prepared from spray solution with colloidal silica had spherical shape after post-treatment. Colloidal silica used as additive improved the spherical shape and filled morphology of the precursor particles prepared by spray pyrolysis. The precursor particles with filled structure produced the BAM:Mn phosphor particles with spherical shape and non-aggregation characteristics after post-treatment at $1400^{\circ}C$ under reducing atmosphere. The phosphor particles prepared from colloidal solutions formed the crystal structure of BAM:Mn phosphor irrespective of the silica contents. The BAM:Mn phosphor particles prepared from aqueous and colloidal solutions had similar photoluminescence intensities under vacuum ultraviolet.
Sanghoon Song;Junhwan Jeong;Donghyuk Kim;Kiwon Hwang;Sungwook Chung;Wonho Kim
Elastomers and Composites
/
제59권1호
/
pp.8-16
/
2024
As regulations on greenhouse gas emission have strengthened globally, the demand for improved fuel efficiency in automobiles continues to rise. In response, the tire industry is actively conducting research to improve fuel efficiency by enhancing tire performance. In this study, silica-filled epoxidized natural rubber (ENR)/butadiene rubber (BR) blend compounds were manufactured according to ENR types and silica contents, and their physical properties and vulcanizate structure were evaluated. ENR-50, which has a higher epoxide content than ENR-25, exhibited stronger filler-rubber interaction, resulting in superior abrasion resistance. In addition, because of its high glass transition temperature (Tg), the wet grip performance of ENR-50 improved, even though the rolling resistance increased. Increasing the amount of silica had little effect on the abrasion resistance due to the increase in filler-rubber interaction and decrease in toughness. In addition, ENR-50 exhibited better wet grip performance; however, the rolling resistance increased. The results indicated that truck bus radial (TBR) tire tread compounds can be designed by applying ENR-50 to improve wear resistance and wet grip performance. In addition, by applying ENR-25 and reducing the silica contents improve fuel efficiency.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.