This study is investigated the various properties and drying shrinkage of concrete according to water content under the condition proper fluidity is adjusted, in order to suggest the method for reduction of crack by drying shrinkage. According to the results, though water content varies, slump and air content are satisfied to the planed values, but shear slump and separation happen at water content of 120 and 140kg/$m^3$ due to the overuse of superplasticizer(SP). As water content is diminished, setting time is retarded by an increase of the using amount of SP, and compressive and tensile strength increase in the range of 160-180kg/㎥ of water content, but decrease significantly at 120 and 140kg/$m^3$. Length change by drying shrinkage decrease with a decrease of water content. Therefore, considering not only drying shrinkage but also fluidity, setting time and strength, it proves that the most appropriate water content of concrete is 160kg/$m^3$ in the condition of this experiment.
Asad Ullah Qazi;Ali Murtaza Rasool;Iftikhar Ahmad;Muhammad Ali;Fawad S. Niazi
Structural Engineering and Mechanics
/
v.89
no.4
/
pp.335-347
/
2024
This study pioneers the exploration of creep and shrinkage behavior in ambient-cured geopolymer concrete (GPC), a vital yet under-researched area in concrete technology. Focusing on the influence of sodium hydroxide (NaOH) solution concentration, the research utilizes low calcium fly ash (Class-F) and alkaline solutions to prepare two sets of GPC. The results show distinct patterns in compressive strength development and dry shrinkage reduction, with a 14 M NaOH solution demonstrating a 26.5% lower dry shrinkage than the 16 M solution. The creep behavior indicated a high initial strain within the first 7 days, significantly influenced by curing conditions and NaOH concentration. This study contributes to the existing knowledge by providing a deeper understanding of the time-dependent properties of GPC, which is crucial for optimizing its performance in structural applications.
Lee, Chang Soo;Park, Jong Hyok;Jung, Bong Jo;Choi, Young Jun
KSCE Journal of Civil and Environmental Engineering Research
/
v.29
no.4A
/
pp.385-393
/
2009
This study grasped the relationship between relative humidity in concrete and concrete shrinkage followed by pre-absorbed water of porous lightweight aggregates through measurements of concrete shrinkage and humidity and comparisons with established research results. It was showed that shrinkage reduction effect of lightweight concrete is 36% at 7 days early ages and 25% at 180 days long-term ages when water-binder ratio is 0.3. It also showed that shrinkage reduction effect is 19% at 7 days and 16% at 180 days when water-binder ratio is 0.4 and 37%, 32% when water-binder ratio is 0.5. The moisture supply effect of lightweight aggregates was remarkable at early age within 7~10 days irrespective of water-binder ratio. In case of waterbinder ratio is 0.3, the relationship between shrinkage and internal humidity of concrete has been underestimated regardless of applied existing model type and in case of water-binder ratio is 0.4, 0.5, measurement values are relatively similar with existing model equations. Finally this study did regression analyses about the relation among the humidity change and the shrinkage strain as a high-degree polynomial and derived parameters that can connect moisture movement analysis with differential shrinkage analysis in case of considering relative humidity at the time by moisture movement analysis of concrete.
Journal of the Korea Academia-Industrial cooperation Society
/
v.20
no.11
/
pp.416-424
/
2019
In Korea, press concrete in basements is mainly applied using plain concrete. This system has undesirable defects such as cracks caused by plastic shrinkage and irregular temperature distribution. To solve this problem, metal lath and fibers have been used in the past. However, they have not been effective in controlling cracks. This study analyzed the reduction of plastic shrinkage cracking for press concrete using various admixtures in a basement has been. In the air contents test, the specimens with various admixtures showed air contents similar to plain concrete (4.5±1.5%). The specimens using silica fume, super plasticizer agent, and SBR showed higher compressive strength by about 10-15% than plain concrete. Cracking decreased when the MC, super plasticizer, and SBR were added. When MC was used in the concrete, the plastic shrinkage did not occur.
The purpose of this study was to present a making method of jeans pattern with high fitness after deriving the appropriate shrinkage rate by material and washing process. Research Method of jeans pattern was presented after applying the optimized shrinkage rate. According to the result of the exterior evaluation of test jeans, all 6 jeans were rated high with scores close to 3.5. Following the evaluation of satisfaction of usage by physical movement, the highest ranking was in the order of walking with normal steps, back bending $90^{\circ}$, chair sitting, climbing stairs, and squatting. The shrinkage rate by physical area showed the highest score in the order of pants length, waist circumference, thigh circumference, knee circumference, hem circumference, hips circumference. In addition, the shrinkage rate was higher in warp direction than weft direction after washing finishing. As for the result of addition and reduction of pattern measurements by parts of jeans, waist circumference was $2.5{\sim}5.2cm$, hips circumference was $-1.8{\sim}2.8cm$, thigh circumference was $-1.3{\sim}2.0cm$ and knee circumference was $-1.0{\sim}1.7cm$. Also, hem circumference was $-1.0{\sim}1.8cm$ and pants length was $2.9{\sim}6.2cm$. That is, this results showed a wide range of addition and reduction according to material and washing finishing.
Jacquard floor covering could be prepared from low-melting/regular sheath-core hybrid polyester, where the fiber is dyed in yarn state. With regard that the expected high shrinkage of the hybrid polyester in water makes problems in yarn dyeing, low-temperature dyeing properties of the hybrid polyester were studied. The rate of shrinkage of low-melting hybrid polyester exceeds 9% in hot water above $90^{\circ}C$, at such condition, cheese yarn dyeing is very difficult. Although disperse dyes exhaust in a relatively high speed on low-melting hybrid polyester, diffusion of these dyes to the core regular polyester was extremely slow under $90^{\circ}C$. Foron Blue E-BL 150, an anthraquinone E-type disperse dye, showed appreciable diffusion after 48hrs dyeing at $90^{\circ}C$. The fastness to rubbing and drycleaning were improved by one grade after reduction cleaning.
It has been well appreciated that reducing weld-induced deformation as law as possible is important during fabrication for a more efficient production of blocks. The weld-induced deformation is more serious in thin plates than in thick plates because heat affect zone of thin plates is wider than that of thick plates and in addition internal and external constraints much more influence upon weld-induced deformation of thin plates. This paper deals with the application of the mechanical tensioning method to butt weld of thin plates to reduce the weld-induced deformation. In order to investigate the quantitative effect of tensioning method upon the reduction of angular deformation and shrinkage in longitudinal and transverse direction of weld line, butt welding test have been carried out for several thin plate specimens with varying plate thickness and magnitude of tensile load. From the present experimental study, it has been found that the tensioning method is very effective on reduction of weld-induced residual stress as well as weld-induced deformation.
Han Cheon-Goo;Kim Sung-Wook;Koh Kyoung-Taek;Cheol Han-Min
Journal of the Korea Concrete Institute
/
v.16
no.5
s.83
/
pp.605-612
/
2004
This study investigated the fundamental properties and shrinkage properties of high performance concrete with water/binder ratio of 0, 30 and with combination of expansive additive and shrinkage reducing agent. According to the results, the fluidity of high performance concrete showed lower the using method in combination with expansive additive and shrinkage reducing agent than the separately using method of that, so the amount of superplasticizer increased when the adding ratio of expansive additive and shrinkage reducing agent increased. However the air content of concrete increased when used in combination with expansive additive and shrinkage reducing agent, so the amount of AR agent decreased. The compressive strength showed the highest at $5\%$ of expansive additive, and decreased with an increase of the amount of shrinkage reducing agent. Furthermore, in order to reduce the shrinkage of high performance concrete, it was found that the using method in combination with expansive additive and shrinkage reducing agent was more effective than separately using method of that. Therefore, it analyzed that the combination of expansive additive of $5\%$ and shrinkage reduction agent of $1\%$ was the most suitable mixture, considering to the fluidity, strength and shrinkage under the condition of this experiment.
Proceedings of the Korea Concrete Institute Conference
/
2008.11a
/
pp.919-922
/
2008
This paper reports the physical and shrinkage properties of concrete using expansive additive(E) and three shrinkage reducing admixtures(SRA1, 2, 3) in order to reduce shrinkage of concrete. For the properties of fresh concrete, the use of SRA1, 2, 3 results in a increase in fluidity and decrease in the dosage of super plasticizer as much as 0.05$\sim$0.1%. And For the properties of hardened concrete, the use of SRA1, 2, 3 results in a decrease in compressive, tensile and flexural strength slightly. For drying shrinkage properties, the use of SRA3 is the most effective for reduction of shrinkage, and the next best way to reduce shrinkage is combination with expansive additive(E) and shrinkage reducing admixture(SRA) or the using of expansive additive(E).
Park, Jung-Jun;Moon, Jae-Heum;Park, Jun-Hyoung;Lee, Jang-Hwa;Kim, Sung-Wook
Journal of the Korea institute for structural maintenance and inspection
/
v.18
no.5
/
pp.34-40
/
2014
High-performance fiber-reinforced cement composite (HPFRCC) shows very high autogenous shrinkage, because it contains a low water-to-binder ratio (W/B) of 0.2 and high fineness admixture without coarse aggregate. Thus, it needs a method to decrease the cracking potential. Accordingly, in this study, to effectively reduce the shrinkage of HPFRCC, a total of five different ratios of SRA (1% and 2%), EA (5% and 7.5%), and a combination of SRA and EA (1% and 7.5%) were considered. According to the test results of ring-test, a combination of SRA and EA (1% and 7.5%) showed best performance regarding restrained shrinkage behavior without significant deterioration of compressive and tensile strengths. This was also verified by performing modified drying shrinkage crack test.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.