To investigate the strong and effective sericin fixing agents and conditions, raw silk fibers were treated with the mixtures of urea-formalin, thiourea-formalin and melamine-formalin as sericin fixing agents, respectively. And the treated raw silk fibers were degummed by the degumming liquors of alkaline detergent and sodium carbonate to confirm the hardness of sericin fixation. The weight of raw silk fibers was decreased in the process of sericin fixation treating at 80$^{\circ}C$ for 60min. The effective sericin fixation was obtained by treating at $60{\sim}80^{\circ}C$ for 15min with the mixture of melamine and formalin. The mixture of melamine and formalin showed an outstanding ability of sericin fixation because the three amino groups of melamine were able to cross-link the hydroxy amino acids of sericin such as serine with the assistance of formalin.
Journal of the Korea Academia-Industrial cooperation Society
/
v.10
no.2
/
pp.412-417
/
2009
In order to investigate the effective sericin fixation of raw silk fibers the influence of various additives added to the melamine and formalin mixtures on sericin fixation was studied. When raw silk fibers were treated with wetting agent but without subsequent washing before sericin fixation, the strong sericin fixation was obtained by fixing sericin. Adding hydrogen peroxide to the melamine and formalin mixture made sericin fixation worse, resulting weaken the sericin hardness of fixed raw silk fibers and tight bonding of the fibers. On the other hand, it was confirmed that adding sodium hydrosulfite to the melamine and formalin mixtures gave better sericin hardness of fixed raw silk fibers without the bonding of fibers. Supplying additional melamine with he low concentration of sodium hydroxide to the melamine and formalin mixture(melamine:formalin= 1:6) resulted in very good sericin fixation. But adding hydrochloric acid or methanol to the same mixture had no effect on the sericin fixation, and adding magnesium chloride to it made the hardness of sericin fixation even worse.
The sericin fixation of raw silk by formalin and glutaraldehyde mixed solutions was done and the effect of sericin fixtion by various conditions on degumming ratio, whiteness and physical properties was investigated and discusse. The obtained results were summarized as follows ; The sericin fixation by 1% formalin solution and upward, regardlles the concentration of glutaraldehyde solution, improved the whitenes of raw silk to 96% level of non fixed raw silk. The decrease of whiteness by degumming was prevented effectively by treatment of formalin and glutaraldehyde mixed solutions. The complete sericin fixation was obtained by the treatment of mixed solution including above 0.5% formalin solution. The proper treatment of sericin fixation can make increase the values of tenacity and elongation of silk.
Lee Ki Hoon;Kang Gyung Don;Shin Bong Seob;Park Young Hwan
Fibers and Polymers
/
v.6
no.1
/
pp.1-5
/
2005
In this study, we attempted to evaluate a novel use of sericin-fixed silk fiber (SFx) as an immobilization support of enzyme. Sericin was fixed on the silk fiber using glutaraldehyde as a fixation reagent. After 6 hours of fixation, the degree of fixation increases linearly with linear decrease of the amount of bound $\alpha$-chymotrypsin (CT). This suggests that the increase of the degree of fixation is due to the further crosslinking of free aldehyde groups on the surface of sericin-fixed silk fiber (SFx). Even though perfect fixation was not achieved, sericin did not dissolve seriously and could be removed by further washing. The specific activity did not differ significantly after 6 hours of fixation. The activity of immobilized CT on SFx decreased to its half after 6 hours of incubation at 50$^{\circ}C$. However, it retained $78\%$ of initial activity even after 1 hour of treatment with $100\%$ ethanol. As a result, the SFx could be used as an immobilization support of enzyme in non-aqueous media at ambient temperature.
The sericin fixation of raw silk by glutaraldehyde solutions with catalyst(serifix B) was done and the effect of sericin fixation by catalyst on reaction mechanism, whiteness and physical properties were investigated and discussed. The obtained results were summarized as follows; 1) The complete sericin fixation were obtained by glutaraldyhyde solution regardless the concentration of catalyst. 2) The tenacities of sericin fixed silk increased in comparison with that of nontreated silk. 3) There were not constant tendency in elongation of sericin fixed silk in comparison with nontreated silk. 4) The whiteness of sericin fixed silk treated glutaral-silk in comparison with nontreated silk. 5) FT-IR spectra were quite different from sericin fixed reagent and catalyst.
The sericin fixation of silk fabrics by epoxy resins was studied in the presence of aqueous salt solution in different solvents at the indicated temperature for the desired time. Heavy weight gains were obtained in the reaction with glycerol diglycidyl ether (EX-313) and ethylene glycol diglycidyl ether (EX-810) catalyzed by potassium thiocyanate in such solvents as carbon tetrachloride and p-chloroethylene. The obtained results were summarized as follows; 1) The tested resins were found similar in reaction behavior to silk fabric. The effect of fixation and weight gains was higher in EX-810 than EX-313. 2) The weight gains were increased with reaction time and temperature, and degumming ratio reached a constant value in 90 min at 70$^{\circ}C$. 3) The weight gains and the degumming ratio reached an equilibrium at 3-5% of epoxy concentration. 4) The weight gains were remarkably influenced and increased by the concentration of salt solution. The degumming ratio reached an equilibrium over 0.5N concentration of salt. 5) The weight gains were increased with the dipping time in gently-sloping. The degumming ratio reached an equilibrium over 15 min dipping. 6) The effect of sericin fixation of hydrophobic solvents, such as Carbon Tetrachloride, p-Chloroeth-ylene, Cyclohexane, Xylene and Toluene, was found suitable. 7) The effect of drying temperature was not remarkable on the weight gains and the degumming ratio. 8) There was a slight decrease in the moisture regain of sericin-fixed silk and it may be possible to maintain the moisture regain in the sericin-fixed silk by the epoxy resins. 9) The results on testing physical properties of sericin-fixed silk fabric were as follows; The crease recovery was almost not different from undegummed fabric, but inferior to degummed fabric. The tensile strength was improving in accordance with the effect of sericin fixation, either the elongation did.
Cerium (IV) ion-initiated graft copolymerizations of acrylonitrile to raw silk were investigated in an effort to carry out sericine-fixation. The change in ceric ammonium nitrate concentration exhibited a maximum in percentage of grafting at 0.003M. Also observed was that the change in nitric acid content in reaction media gave a maximum in percentage of grafting at 0.1M. Percentage of grafting was increased generally with increase in acrylonitrile concentration, reaction time and reaction temperature. Raw silk sericin grafted with acrylonitrile was not de gummed by boiling off test and optimum graft percentage was considered at 20%.
Journal of the Korea Academia-Industrial cooperation Society
/
v.18
no.5
/
pp.93-98
/
2017
The fixing behaviors of raw silk yarns treated with melamine and formaldehyde at a molar ratio of 1:3 for trimethylolmelamine were investigated. Sericin was fixed during the fixing process, but a part of sericin I was removed simultaneously by hot water. The weight losses by fixing and the degumming losses by degumming greatly decreased with increasing concentrations of melamine and formaldehyde. The silk yarns fixed with 0.011 M melamine and 0.033M formaldehyde were significantly degummed due to the insufficient fixation of sericin and the alkaline hydrolysis of sericin by sodium carbonate during the degumming process. On the other hand, the silk yarns fixed with 0.055M melamine and 0.165M formaldehyde were degummed slightly (the degumming losses of 3-8%) due to the strong fixation of sericin, which might result from the many cross-linkages between the sericin I molecules, which were formed by trimethylolmelamine. Those fixed with the fixing solution containing 15% owf softener showed the lowest weight and degumming losses because under the condition of 15% owf softener, the cation of the softener can effectively form ionic bonds with the negatively charged side chain of aspartic acid in sericin. In addition, van der Waals' forces may be also formed between the hydrophobic tail of the softener and the hydrophobic region of sericin, which may help inhibit the removal of sericin I.
This has been carried out how the sericin insoluble fixations of raw silk should be with potassium alum. This is learned from the leather tanning technique which the process works with collagen, a kind of proteins. Former reports had shown such works, however, they did not consider the moisture absorbability after their process reports by using chromium alum, formalin or vinyl acetate grafting. This report, however, paid attention to protect such absorbability as well as sericin fixation, so far it may be useful for plactical use of silk. In order to clear how the sericin is fixed with such chemicals, fundermental mechanism of weding process and chemical reaction against proteins were also discussed. The obtained results of the report are as followings. 1. Alum should not be treated for raw silk with high temperature bath like other reports because such treat induces raw silk to be stiffly after the treat. 2. It is recommended that raw silk should be treated with alum solution at room temperature for more than three hours. Even in this case, the use of only alum with raw silk could to fix sericin some how, but it increased the water proofness of the silk. 3. 1% of alum solution was found to be able to fix the sericin of raw silk. 4. In case we consider only sericin fixations, a combination treat of 1% alum for three hours and 0.5% NaOH for ten minutes method showed the best result. 5. In case we consider sericin insoluble fixation and moisture absorbility, the reversive combination of the above process was found to be the best results. 6. Sericin fixing evidence was shown with drying feature curves of wed each treated silk where we could to analyze how the chemical nature is changed after each treat. 7. Deguming ratio may be obtained up to 4.3% after the alum combination treat with regular raw silk. Such ratio was considered to be good enough for the purpose when the textile is washed with warm soap water. 8. Moisture absorbability of the combination treat of alum and NaOH was found to be good enough as well as non treated silk. 9. The tenacity and elongation of the treated silk did not change even after three month. 10. Above all, this method is considered to be better process than other coloured fixing (tannin method. Cr-alum method) or smell fixing (formalin method. vinyl acetate method).
Sericin 정착은 친수성 단백질인 세리신을 화학처리에 의하여 소수성으로 변화시켜 fibroin 에 밀착, 응고시켜 생사를 양모와 유사한 섬유로 변화시켜 제품의 다양화를 기할 목적으로 많이 행하여졌으며 이에 따른 증량효과도 크게 기대되어진다. 종래의 세리신 정착방법들은 생사의 제리신 정착외에 공업적으로 그 가치가 크게 인정되었던 견사, 생사 층 등에도 광범위하게 응용되어 많은 특허가 있는데 이들 정착방법을 대별하면 (1) Aldehyde 처리에 의한 세리신 정착 (2) Cr 감류처리에 의한 세리신 정착 (3) Epoxy 화합물의 처리에 의한 세리신 정착 (4) 합성수지 처리에 의한 세리신 정착등을 들 수 있겠으며 그 중에서도 특히 Aldehyde 에 의한 정착 (주로 formaldehyde 사용) 과 Cr 감류에 의한 정착이 가장 많이 행해진 경향을 보인다. (중략)
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.