• Title/Summary/Keyword: rubber asphalt

Search Result 85, Processing Time 0.029 seconds

The Study on the Pressure-Sensitive Adhesion Property of Waste FKM Powder and SBS Modified Asphalt (폐불소고무 분말과 SBS로 개질된 아스팔트의 점착 특성에 관한 연구)

  • Chung, Kyung-Ho;Kang, Min-Kyu;Han, Kyung-A
    • Elastomers and Composites
    • /
    • v.44 no.3
    • /
    • pp.282-289
    • /
    • 2009
  • The pressure-sensitive adhesive(PSA) tapes are widely used as floor-sealing material in Korean constructive industry. However, the general PSA tapes can not seal the apertures completely. This is one of main reasons to cause imperfect finishing. In order to solve the problems, the asphalts were modified by FKM powder and SBS in this study. The physical properties of modified asphalts were examined by measuring the softening point, viscosity, tensile strength and adhesion strength of FKM and SBS modified asphalt. The softening point of SBS modified asphalt was increased greatly due to the formation of network structure in asphalt. Also, the change of adhesion strength of SBS modified asphalt with temperature was not so great comparing to those of pure asphalt and FKM modified asphalt. The best results of pressure-sensitive adhesion could be obtained by the SBS(linear) modified asphalt containing 6 wt.% of linear type SBS.

Analyses on Environment-friendliness of Waterproof Materials Based on Fish Toxicity Test (어독성 실험에 따른 방수재 친환경 특성 분석)

  • Kim, Sung-Kyun;Woo, Ji-Keun;Lee, Im-Gyu;Yoo, Hy-Ein;Jeong, Jae-Wook
    • Journal of the Korean Society of Environmental Restoration Technology
    • /
    • v.13 no.1
    • /
    • pp.57-68
    • /
    • 2010
  • The purpose of this study is to analyze the characteristics of environment-friendliness of waterproof materials based on comprehensive experiments on waterproofness in terms of coefficients of permeability, harmfulness of waterproof materials and fish toxicity of Oryzias latipes mortality to verify eco-toxicity of each method of construction and waterproof material, which are to be applied by taking eco-toxicity into account when building ecological flows in upper areas on natural and artificial grounds. As a result, the following conclusions have been reached in this study: 1. In regard of the harmfulness analyzed, each material showed a different result of analytical value in each lab tank. Compared to input water, pH, COD, SS, T-P, and T-N values increased a little, but DO value decreased. The value of turbidity analyzed independent of the water quality standard of aquatic ecosystem set forth by the Ministry of Environment increased a little compared to the value in input water. 2. In the experiment of fish toxicity, compacted quicklime, cement fluid waterproof material, cement mortar waterproof material and bentonite powder were found to have 100% of fish mortality, respectively, and membrane waterproof material showed 83.3% of mortality, indicating strong fish toxicity. Improved asphalt sheet (63.3%) and synthetic rubber sheet (53.3%) were analyzed to have medium fish toxicity, while bentonite sheet (6.7%), Hwang-toh (6.7%) and clay (3.3%) showed relatively lower mortality and fish toxicity. 3. Regarding the analysis on waterproofness in terms of the coefficient of permeability of each waterproof material, improved asphalt sheet, synthetic rubber sheet, membrane waterproof material, cement fluid and mortar waterproof material and bentonite sheet were found impervious in case no leakage takes place in construction. Bentonite powder was found practically impervious based on the analytical results from the experiment done in compliance with weight ratios. So were the clay and Hwang-toh from the experimental results. To sum up such results as found in the experiment mentioned so far, the values of harmfulness and waterproofness analyzed were different in each lab tank, but there was absolutely little correlation with the mortality gained from the experiment on fish toxicity. In the experiment of fish toxicity, environment-friendly waterproof materials were analyzed, and it was found that clay, Hwang-toh and bentonite sheet are highly environment-friendly. In contrast, synthetic rubber and improved asphalt sheets were found to have medium-level environment-friendliness. Also, membrane water-proof materials, compacted quicklime, cement fluid and mortar waterproof material and bentonite powder were analyzed to have low environment-friendliness.

A Study on the Safety and Comfort of Pedestrians according to the Type of Sidewalk Pavement (보도포장의 종류에 따른 보행자의 안전성 및 쾌적감에 대한 연구)

  • Choi, Jae Jin
    • Journal of the Korean Society of Safety
    • /
    • v.30 no.1
    • /
    • pp.66-71
    • /
    • 2015
  • Safety, resilience and comfort of pedestrian were assessed by the British Pendulum Test and SB/GB factor test at 8 kinds of sidewalk pavement. Sidewalk paving materials were normal concrete, porous concrete, concrete block, soil concrete, asphalt, rubber chip/resin mixture, wood chip/resin mixture and floor tile. In addition, a survey was conducted to investigate the perception of pedestrians on the sidewalk paving material. As a result, while the skid resistance value was measured in the most 60BPN above, the floor tile showed a low value of about 30BPN. The ratios of SB factor to GB factor of the elastic pavements(rubber/resin mixture and wood chip/resin mixture) appeared to be relatively large when compared with those of the conventional sidewalks. The survey showed that respondents perceived as more safe and comfortable elastic pavements compared to conventional pavements. Approximately 50% of respondents answered that hardened soil pavement was the most environmentally friendly.

Analytical Method for Determination of the Content of Tire Wear Particle in Tire and Road Wear Particles

  • Son, Chae Eun;Choi, Sung-Seen
    • Elastomers and Composites
    • /
    • v.56 no.1
    • /
    • pp.1-5
    • /
    • 2021
  • Tire and road wear particles (TRWPs) were collected from road dust and thermogravimetric analysis (TGA) was performed to measure the content of tire wear particles (TWPs) in the TRWPs. The TGA thermograms of TRWPs showed two weight loss steps associated with polymer decomposition including weight loss after 480℃ which may be due to road wear particles. Different samples gave different TGA thermograms because the types and contents of the road wear particles attached to the TWPs should be different from each other, and each TWP might have different composition. The TGA results of the model asphalt pavement wear particles, with (volatile organics + polymers + carbon black) : ash = 33.5 : 66.5, was applied to the TRWP results, and the TWP contents of TRWPs were found to be 50-65%. The zinc oxide content in the rubber compound was negligible.

Evaluation of Color Coating Method for Color Maintenance of Color Asphalt Pavement (칼라 아스팔트 포장의 색채 표면보수를 위한 칼라코팅 공법 성능평가)

  • Park, Tae-Soon
    • International Journal of Highway Engineering
    • /
    • v.13 no.4
    • /
    • pp.93-101
    • /
    • 2011
  • The evaluation of various color coating methods for color maintenance of color asphalt pavement is conducted using the laboratory and field tests on the bus lane. The surface of color asphalt constructed on the bus lane is deteriorated such as changing color and decoloration and abrasion due to the passing of the traffic and time. The total of 9 coating methods were evaluated in this study. The laboratory tests included Ultra violet test, adhesion test and Taber abrasion test and the field tests were british pendulum test and visual survey. The results of tests showed that the different methods showed the their own engineering characteristics and it is dependant upon the main material used. The rubber epoxy material for the main material showed the satisfactory result among the methods tested. However, the performance of the coating methods after 100days are not satisfactory, decoloration, abrasion and peeling up are investigated and need to be studied for the further application in the field.

Evaluation of Hot Mix Asphalt Properties using Complex Modifiers (복합개질제를 이용한 아스팔트 혼합물의 물성 평가)

  • Lee, Kwan-Ho;Kim, Seong-Kyum
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.19 no.5
    • /
    • pp.146-152
    • /
    • 2018
  • In this study, to improve the performance of asphalt mixtures for plastic deformation occurring mainly in Korea, complex modifiers were prepared by mixing powders and liquid type modifiers. The main constituents were powdery diatomaceous earth, mica and carbon black, and liquid type solid 70% SBR latex. The tensile strength ratios for the two asphalt mixtures used in the test were above 0.80 for the Ministry of Land Transportation (2017) asphalt mixture production and construction guidelines. The effects of increasing the tensile strength in the dry state was more than 14% when the composite modifier was added. The deformation rate per minute by the wheel tracking test load was an average of 0.07 to 0.147 for each mixture. The strain rate per minute was improved by the modifier, and the dynamic stability was improved by almost 100% from 295 to 590. In addition, the final settling was reduced from 11.38 mm to 9.57 mm. A plastic deformation test using the triaxial compression test showed that the amount of deformation entering the plastic deformation failure zone at the end of the second stage section and in the third stage plastic deformation section was 1.76 mm for the conventional mixture and 1.50 mm for the complex modifier mixture. The average slope of the complex modifier asphalt mixture mixed with the multi-functional modifier was 0.005 mm/sec. The plastic deformation rate is relatively small in the section where the road pavement exhibits stable common performance, i.e. the traffic load.

Characteristics in Densities and Shapes of Various Particles Produced by Friction between Tire Tread and Road Surface

  • Jung, Uiyeong;Choi, Sung-Seen
    • Elastomers and Composites
    • /
    • v.57 no.3
    • /
    • pp.92-99
    • /
    • 2022
  • A large amount of particles on the roads is produced by friction between the vehicles and the road surface and by inflow from outside. The type of these particles affects the abrasion behavior of tire tread. In this study, road dust collected at a bus stop was separated by size, and the particles with sizes of 106-212 mm were analyzed. The particles were separated by density using NaI and NaBr aqueous solutions with densities in the range of 1.10-1.80 g/cm3 with the 0.10 g/cm3 interval. In the road dust sample, the following particle types were found: tire-road wear particles (TRWPs), asphalt pavement wear particles (APWPs), plant-related particles (PRPs), road paint wear particles (RPWPs), and plastic particles (PPs). The densities of TRWPs, APWPs, PRPs, and RPWPs were 1.20-1.80, >1.60, >1.10, and >1.40 g/cm3, respectively, while PPs were found in all density ranges. Additionally, many small mineral particles were observed on the particles. Order of the relative content of the particles was PRP > TRWP > APWP ~ RPWP > PP. APWPs that were stuck to TRWP could be removed by chloroform treatment. The shapes of the particles were characterized using their magnified images.

Reliability Evaluation of Rubber Wheel and Steel Wheel for Wheel Tracking Test of Bituminous Concretes (역청 콘크리트 반복주행시험에서 고무바퀴와 강재바퀴의 신뢰성 비교 연구)

  • Hong, Joon-Pyo;Doh, Young-Soo;Kim, Kwang-Woo
    • International Journal of Highway Engineering
    • /
    • v.7 no.2 s.24
    • /
    • pp.97-107
    • /
    • 2005
  • Since the purpose of wheel tracking test is to find out relative difference of mixture's rut resistance, the wheel is an important part in the test for obtaining a consistent output. This study is performed to examine efficiency of different wheel material, rubber and steel in wheel tracking test. The rubber was inserted as a ring on the outer face of the steel wheel, and thickness of rubber ring was 15mm and 7.5mm and 0mm (steel wheel without rubber), making the total outer diameter 200mm. The objective of this study was to select reliable wheel material type in wheel tracking test at $60^{\circ}C$ based on variance in output (rut depth and dynamic stability) and correlation with SD (deformation strength). The result of regression analysis of rut depth with Sd showed that $R^2$ values of wheel rubber thickness of 15mm, 7.5mm and 0mm were 0.7, 0.8 and over 0.9, respectively. In a case of steel wheel (0mm), the highest $R^2$ value was 0.9569. Therefore, the wheel without rubber ring was the best in output consistency level and coefficient of determination $(R^2)$ with deformation strength. Therefore, the steel wheel without rubber ring is suggested as the best choice for wheel tracking test of asphalt concrete.

  • PDF

Geotechnical properties of tire-sand mixtures as backfill material for buried pipe installations

  • Terzi, Niyazi U.;Erenson, C.;Selcuk, Murat E.
    • Geomechanics and Engineering
    • /
    • v.9 no.4
    • /
    • pp.447-464
    • /
    • 2015
  • Millions of scrap tires are discarded annually in Turkey. The bulk of which are currently landfilled or stockpiled. These tires consume valuable landfill space or if improperly disposed, create a fire hazard and provide a prolific breeding ground for rats and mosquitoes. Used tires pose both a serious public and environmental health problem which means that economically feasible alternatives for scrap tire disposal must be found. Some of the current uses of scrap tires are tire-derived fuel, creating barrier reefs and as an asphalt additive in the form of crumb rubber. However, there is a much need for the development of additional uses for scrap tires. One development the creation of shreds from scrap tires that are coarse grained, free draining and have a low compacted density thus offering significant advantages for use as lightweight subgrade fill and backfill material. This paper reports a comprehensive laboratory study that was performed to evaluate the use of a shredded tire-sand mixture as a backfill material in trench conditions. A steel frame test tank with glass walls was created to replicate a classical trench section in field conditions. The results of the test demonstrated that shredded tires mixed with sand have a definite potential to be effectively used as backfill material for buried pipe installations.

A Safety Evaluation on Structure of Panel for Railway (철도용 보판의 구조안전성 평가)

  • 윤성철;정종덕;김원경;박기준
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2003.06a
    • /
    • pp.1553-1556
    • /
    • 2003
  • As the public use part of the railway and the road, the railway crossing is important to work properly by two transportation means. Also, It is important to provide the good face of friction on the railway crossing in aspect of protecting the railway crossing accident. Lately, the material of railway crossing panel is the wood. the asphalt, and the steel. As they have a various fault, it was studied to analyze the structural action of the new material. rubber panel. This paper analyzed eigenvalue, stress and displacement by truck passing weight and thermal stress using the FEM model.

  • PDF