열처리한 $CaO-SiO_2-H_2O$계의 수열반응과 이의 응용에 관한 연구 (Re-hydration of Heat-treated $CaO-SiO_2-H_2O$ System and Their Application under Hydrothermal Condition)

  • 윤철현;송태웅
    • 한국세라믹학회지
    • /
    • 제31권11호
    • /
    • pp.1387-1395
    • /
    • 1994
  • Re-hydration properties of heated and ground CaO-SiO2-H2O system were studied under hydrothermal condition in order to examine the possibility of recycling ALC waste as raw materials of ALC. Powder of calcium silicate hydrates and ALC waste without heat treatment did not show further hydration while those of heat-treated at proper temperature showed re-hydration properties under hydrothermal condition. The lath-like shape of initially synthesized tobermorite was gradually turned into small debris during heating and plate-like tobermorite was crystallized during re-hydration of the heated powders. Heated and ground ALC waste could be added to natural raw mix for ALC at the ammount up to 20% with increased compressive strength and up to 30% with slightly decreased compressive strength. The optimum heating temperature of ALC for recycling was about 50$0^{\circ}C$.

  • PDF

Recover of gypsum from waste plaster board and the refining process

  • Song, Young-Jun;Hiroki Yotsumoto
    • 대한전자공학회:학술대회논문집
    • /
    • 대한전자공학회 2001년도 The 6th International Symposium of East Asian Resources Recycling Technology
    • /
    • pp.342-348
    • /
    • 2001
  • This study was conducted to obtain granular crystalline gypsum that can be used as raw material for plaster boards or cements from waste Plaster board. We could disintegrate preferentially gypsum to gypsum needle in 10${\mu}{\textrm}{m}$ or less size among the contents of waste plaster board (gypsum, paper, fiber, and inorganic material .etc.) by hydration afterwards the dehydration of crushed waste plaster board. In this case, the optimum conditions for minimizing the size of gypsum were dehydration rate of 75%~ 85%, hydration concentration of 10~20%, agitation speed of 250~400rpm, crushing size of 2cm or less. Gypsum of 98.21% grade was recovered with 99.0% yield from under screenings of 325mesh wet screening which followed by the dehydration-hydration process performed in the conditions of dehydration rate of 80%, hydration concentration of 15%, agitation speed of 300rpm, crushing size of 2cm or less. Subsequently, Plate-like Crystalline gypsum of is 151${\mu}{\textrm}{m}$ size and the grade of 99.49% with the Yield of 98.0% from the upper screenings of 270mesh wet screening carried out after the re-crystallization of the recovered gypsum needle slurry.

  • PDF

한국인 주요 단백질 급원식품 10종에 대한 동결건조 전후의 특성 연구 (Study on Major Korean Protein Sources Before and After Freeze Drying Processing)

  • 손양주;최수영;이금양;황영;유경미;황인경
    • 한국식품조리과학회지
    • /
    • 제30권1호
    • /
    • pp.64-75
    • /
    • 2014
  • Freeze-drying process was used for 10 major protein foods referred by the Korea Health Statistics 2011 as follows; chicken, pork, beef, eggs, tofu, squid, soybean, mackerel, anchovy, and pollack/frozen pollack. Boiled samples and re-hydrated samples after freeze-drying were prepared for analysis. The weight variation, the chromaticity, the mechanical texture and sensory properties by eight trained panelists were measured. In the ratio of re-hydration, the anchovy showed the highest value(89.40%), followed by eggs, and squid showed the lowest value(35.51%). Changes of Hunter color value were observed among all samples. For rates on changes of hardness, every sample was increased except for eggs(p<.05). Among the 9 samples, except for eggs, chicken showed the lowest rate of increase in hardness(125.44%) while squid showed the highest rate of increase in hardness(1335.1%). Except for eggs and pork, eight samples represented differences in sensory properties, especially in juiciness and tenderness(p<.05). As a result, we found that egg is the most suitable for freeze-drying among 10 protein sources followed by pork and chicken.

재유화형 폴리머를 첨가한 폴리머시멘트 모르타르의 특성 (Properties of Polymer Modified Mortars Substitution Re-dispersible Polymer Powders)

  • 장건영;류동우;전찬수
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2018년도 춘계 학술논문 발표대회
    • /
    • pp.19-20
    • /
    • 2018
  • For this study, a test was conducted on the basic polymer property depending on the replacement amount of polymer. The result showed that the flow of slump was increased with the increase of polymer replacement amount and an amount of air entraining. In addition, with a decrease of unit W/B, an amount of bleeding was reduced, and the first and final time for 6% replacement amount was found to be the fastest. This implies that replacement of more than 6% may affect the hydration of cement.

  • PDF

각질층 환경변화에 따른 얼굴과 하박내측 피부의 탄력 특성 비교연구 (Study on Skin Elasticity Property between Face and Forearm according to the Environmental Change of Stratum Corneum)

  • 장민열
    • 대한화장품학회지
    • /
    • 제44권4호
    • /
    • pp.455-463
    • /
    • 2018
  • 피부의 탄성은 주로 콜라겐, 탄력섬유 등이 풍부한 진피의 영향을 받는다. 하지만, 피부의 가장 바깥층인 각질층의 변화가 피부의 기계적인 특성에 어떠한 영향을 미치는지에 대해선 아직 명확하게 밝혀지지 않고 있다. 이에 본 연구에서는 새롭게 디자인한 시험방법을 통해 피부 깊이별 탄성 특성과 수화과정을 통한 각질층 변화가 피부 탄성 특성에 어떻게 영향을 주는지를 알아보았다. 또한 이 방법을 이용해 얼굴피부와 하박내측 피부의 특성을 비교 평가하였다. 25-40세 연령의 건강한 성인 10명을 대상으로, 피부 깊이별 탄성 특성을 연구하기 위해 $Cutometer^{(R)}$의 음압을 다양하게 설정하여 얼굴피부와 하박내측 피부의 탄성 특성을 측정하여 비교 평가하였다. 음압은 100, 200, 300, 450 mbar로 구분하여 측정하였다. 또한 충분한 수화과정을 통해 각질층의 변화를 유도하고, 다양한 음압 조건에서 피부 탄성 특성을 측정하였다. 그 결과, 음압 조건을 달리함에 따라 피부 깊이에 따른 탄성 특성 측정이 가능함을 확인하였다. 그리고 하박내측 피부의 R7 값은 모든 음압조건에서 얼굴피부보다 통계적으로 유의하게 높았다(p < 0.05). 또한 수화과정에 의한 각질층의 변화는 피부탄성 특성에 영향을 줄 수 있음을 확인하였다. 특히 얼굴피부의 R7 값은 300 mbar 음압조건에서 수화전 상태의 피부에 비해 통계적으로 유의하게 변화하였다(p < 0.05). 그리고 전체적으로 얼굴피부가 하박내측 피부보다 수화과정에 더 크게 영향을 받고 있음을 알 수 있었다. 이러한 결과는 다양한 음압조건과 피부 수화 과정을 활용한다면, 각질층 및 표피층의 변화를 고려한 피부탄력특성을 평가할 수 있는 유용한 시험법이 될 것으로 사료된다.

Freeze-dried bovine amniotic membrane as a cell delivery scaffold in a porcine model of radiation-induced chronic wounds

  • Oh, Daemyung;Son, Daegu;Kim, Jinhee;Kwon, Sun-Young
    • Archives of Plastic Surgery
    • /
    • 제48권4호
    • /
    • pp.448-456
    • /
    • 2021
  • Background Locoregional stem cell delivery is very important for increasing the efficiency of cell therapy. Amnisite BA (Amnisite) is a freeze-dried amniotic membrane harvested from bovine placenta. The objective of this study was to investigate the retention of cells of the stromal vascular fraction (SVF) on Amnisite and to determine the effects of cell-loaded Amnisite in a porcine radiation-induced chronic wound model. Methods Initially, experiments were conducted to find the most suitable hydration and incubation conditions for the attachment of SVF cells extracted from pig fat to Amnisite. Before seeding, SVFs were labeled with PKH67. The SVF cell-loaded Amnisite (group S), Amnisite only (group A), and polyurethane foam (group C) were applied to treat radiation-induced chronic wounds in a porcine model. Biopsy was performed at 10, 14, and 21 days post-operation for histological analysis. Results Retaining the SVF on Amnisite required 30 minutes for hydration and 1 hour for incubation. A PKH67 fluorescence study showed that Amnisite successfully delivered the SVF to the wounds. In histological analysis, group S showed increased re-epithelialization and revascularization with decreased inflammation at 10 days post-operation. Conclusions SVFs had acceptable adherence on hydrated Amnisite, with successful cell delivery to a radiation-induced chronic wound model.

Bonding of nano-modified concrete with steel under freezing temperatures using different protection methods

  • Yasien, A.M.;Bassuoni, M.T.
    • Computers and Concrete
    • /
    • 제26권3호
    • /
    • pp.257-273
    • /
    • 2020
  • Concrete bond strength with steel re-bars depends on multiple factors including concrete-steel interface and mechanical properties of concrete. However, the hydration development of cementitious paste, and in turn the mechanical properties of concrete, are negatively affected by cold weather. This study aimed at exploring the concrete-steel bonding behavior in concrete cast and cured under freezing temperatures. Three concrete mixtures were cast and cured at -10 and -20℃. The mixtures were protected using conventional insulation blankets and a hybrid system consisting of insulation blankets and phase change materials. The mixtures comprised General Use cement, fly ash (20%), nano-silica (6%) and calcium nitrate-nitrite as a cold weather admixture system. The mixtures were tested in terms of internal temperature, compressive, tensile strengths, and modulus of elasticity. In addition, the bond strength between concrete and steel re-bars were evaluated by a pull-out test, while the quality of the interface between concrete and steel was assessed by thermal and microscopy studies. In addition, the internal heat evolution and force-slip relationship were modeled based on energy conservation and stress-strain relationships, respectively using three-dimensional (3D) finite-element software. The results showed the reliability of the proposed models to accurately predict concrete heat evolution as well as bond strength relative to experimental data. The hybrid protection system and nano-modified concrete mixtures produced good quality concrete-steel interface with adequate bond strength, without need for heating operations before casting and during curing under freezing temperatures down to -20℃.

결합재 종류에 따른 콘크리트의 단열온도상승특성 및 단열온도상승에 따른 압축강도특성에 관한 연구 (Properties of Adiabatic Temperature Rise of Concrete Using Different Types of Binder and Effects of Adiabatic Temperature on the Compressive Strength)

  • 하재담;김태홍;이종열;김진근
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2001년도 봄 학술발표회 논문집
    • /
    • pp.527-532
    • /
    • 2001
  • The crack of concrete induced by a temperature rise in early age concrete due to the heat of ration of cement is a serious problem for massive or high strength concrete structures. However, re is still no reasonable equations for the prediction of the temperature rising. On this study, the prediction equations of the heat of hydration of different types of binder are pained from the adiabatic temperature rise test, and compared with the results from different nations to obtain the best approximated equation. The strengths of concrete of which specimens were placed in the same chamber for the adiabatic to were compared with those under standard curing.

  • PDF

황산나트륨 용액에서 인산부생석고의 결정성장 특성 (Crystal growth of phospho-gypsum in Na2SO4 solution)

  • 이계승;이정미;송영준;신강호;김윤채;윤시내;장윤호;이성룡
    • 한국결정성장학회지
    • /
    • 제21권1호
    • /
    • pp.6-14
    • /
    • 2011
  • 이수석고 상태로 존재하는 인산부생석고를 ${\beta}$형 반수석고가 되도록 탈수한 다음 급격히 수화시켜 석고성분 만을 미립의 침상결정이 되도록 하여 불순물과 분리하는 공정과 여기서 회수된 침상의 이수석고 슬러리에 무수황산나트륨 ($Na_2SO_4$)을 첨가하여 용해시키고 적당한 조건에서 탈수와 결정성장 조작을 행하여 고순도 이수석고 결정을 회수하는 공정을 제안하였다. 본 고에서는 상온에서의 미립 이수석고의 결정성장속도, 전체 공정 단계별 수용액 내 $Ca^{2+}$의 농도 변화, 결정질 석고의 입도와 회수율에 미치는 수중탈수 시간, 결정성장 온도, 강온속도의 영향에 대하여 조사하였다.

폐콘크리트 미분말을 이용한 재생시멘트 모르터의 중성화 특성 (Carbonation Properties of Recycled Cement Mortar made of Cementitious Powder from Concrete Waste)

  • 김진양;박차원;안재철;강병희
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2005년도 춘계 학술기술논문발표대회 논문집
    • /
    • pp.61-64
    • /
    • 2005
  • Recently, there have been many studies about recycling cementitious powder from concrete waste(hereinafter referred to as waste powder), generated after recycle aggregate production. Previous studies showed that when the heating process of waste powder at $700^{\circ}C,\;Ca(OH)_2$ in paste is dehydrated making possible the restoration of hydraulic properties. Recycled cement with hydraulic properties restored is thought to be re-hydrated through the mechanism of hydration, which is almost similar in Portland cement. This clearly suggests that the hydrate of recycled cement is alkali in type. Like in general concrete, if recycled cement is used as a structural material, resistance performance against carbonation or neutralization by $CaCO_3$ in air probably would be most influential to the life of steel-reinforced concrete structure. Thus the purpose of this study is to make an experimental review on chemical properties of recycled cement, manufactured with concrete waste as base material, and investigate the durability of concrete using recycled cement through evaluating the cement s performance of resistance to carbonation in accordance with its accelerating age. Based on its results, further, the study seeks to provide basic information about ways of utilizing recycled cement.

  • PDF