Sapstain and Mold Control on Radiata Pine Lumber: Laboratory and Field Tests of Selected Fungicides

  • Kim, Jae-Jin;Ra, Jong-Bum;Kim, Hyung-Jun;Kim, Gyu-Hyeok
    • Mycobiology
    • /
    • v.30 no.1
    • /
    • pp.37-40
    • /
    • 2002
  • The susceptibility of radiata pine sapwood to fungal attack and the ability of selected fungicides to control colonization of sapstain and mold fungi on green radiata pine sapwood were evaluated. Radiata pine sapwood was highly susceptible to fungal staining, suggesting that prompt application of fungicides after sawing is essential for preventing fungal colonization. The ability of commercial fungicides to prevent fungal discoloration on radiata pine sapwood was assessed using an accelerated 6-week test on small samples in the laboratory, and in field tests using bulk-piled boards exposed outdoors for 6 weeks during summer rainy season. In laboratory tests, Hylite extra provided excellent protection against fungal discoloration even at the lowest concentrations. Hylite clear, Britewood S, and NP-1 Plus provided good short-term protection(2 to 4 weeks), but higher chemical loadings were, required for long-term protection(6 weeks). Woodguard produced little or no protection over the test periods. In field tests, Kathon 893 provided markedly superior protection at the concentration of 0.5 percent or higher. NP-1 Plus provided relatively good protection at all concentrations evaluated. Hylite extra was effective only for short-term protection(2 to 4 weeks) at all concentrations tested, but higher solution strengths were needed for longterm protection.

The Mechanical Properties of New Zealand-grown Radiata Pine (뉴질랜드산(産) 라디에타 소나무의 기계적(機械的) 성질(性質)에 관(關)한 연구(硏究))

  • Oh, Seung-Won
    • Journal of the Korean Wood Science and Technology
    • /
    • v.24 no.3
    • /
    • pp.12-17
    • /
    • 1996
  • This study was carried out to investigate some mechanical properties for wood rational utilization of heartwood and sapwood in radiata pine according to basic density, ring width and proportion of latewood which were grown in New Zealand. This result were summarized as follow: Heartwood showed 35.78(MPa) of the compression strength parallel to the grain while sapwood showed 42.08(MPa). The modulus of rupture in static bending was higher in sapwood showing 86.12(MPa) than in heartwood 72.99(MPa) Heartwood had 7.38(GPa) for the modulus of elasticity in static bending and sapwood 8.17(GPa). As the basic density and proportion of latewood increased: compression strength parallel to the grain, MOR and MOE in static bending had a tendency to increase. As ring width increased, the mechanical properties decreased.

  • PDF

Effect of Heat Treatment on the Dimensional Stability and the Bending Properties of Radiata Pine Sapwood

  • Yun, Ki-Eon;Kim, Gyu-Hyeok;Kim, Jae-Jin
    • Journal of the Korean Wood Science and Technology
    • /
    • v.27 no.4
    • /
    • pp.30-37
    • /
    • 1999
  • The effects of heat treatment on the dimensional stability and bending properties of radiata pine sapwood were investigated. The dimensional stability was almost achieved by heat treatment though the loss of strength was accompanied as a negative effect. The improvement in dimensional stability of wood and the resultant reduction in bending properties were closely related to treatment temperature and duration. The optimum treatment conditions, which could be used to achieve a desired improvement in dimensional stability with resultant losses in modulus of rupture were proposed based on the results obtained in this study.

  • PDF

Moisture Movement in Softwood and its Activation Energy (침엽수재(針葉樹材) 내부수분이동(內部水分移動)과 확산활성화(擴散活性化)에너지)

  • Kang, Ho-Yang
    • Journal of the Korean Wood Science and Technology
    • /
    • v.19 no.4
    • /
    • pp.27-33
    • /
    • 1991
  • Three kinds of specimens(radiata pine sapwood, radiata pine heartwood and whemlock heartwood) were dried at four temperature levels (30, 40, 50 and $60^{\circ}C$) in an emvironmental chamber. Unsteady-state diffusion coefficients were calculated from obtained drying fates by using infinite slab equation for first half of sorption and interval diffusion equation for second half of sorption. Activation energies for moisture diffusion in wood were calculated from the diffusion coefficients obtained at four temperatures. In most cases diffusion coefficients for radial movement were higher than those for tangential movement. Activation energy differences between sapwood and heartwood weren't significant for radial movement, but were significant for tangential movement. Most activation energies calculated from drying rates were lower than heat of water condensation(about 11,000cal/mole). Specially the avenge activation energy for sapwood tangential movement was only 5,000cal/mole.

  • PDF

Removing Sapstain of Radiata Pine by Bleaching (표백에 의한 라디에타소나무의 청변 제거)

  • Kim, Gyu-Hyeok;Kim, Hyung-Jun;Ra, Jong-Bum;Kim, Jae-Jin
    • Journal of the Korean Wood Science and Technology
    • /
    • v.31 no.1
    • /
    • pp.46-51
    • /
    • 2003
  • The feasibility of using bleaching treatments for removing fungal stain was evaluated on heavily stained raiadta pine sapwood. Sodium chlorite and sodium hypochlorite appeared to destain fungal discoloration by providing proper treatment conditions (chemical concentration, treatment temperature, and treatment time), while hydrogen peroxide did not remove fungal stain under the bleaching regimes evaluated. The addition of sodium silicate and sodium hydroxide in the hydrogen peroxide solution as a buffer could remove fungal discoloration completely; however, the color of wood surface turned faint green after bleaching, thereby reducing the lightness of bleached samples. The results suggest that hydrogen peroxide bleaching could be a feasible method for removing fungal discoloration of stained radiata pine sapwood, although further research is needed to solve the problem of color change after bleaching. Also, further tests under field conditions are recommended.

Prevention of Mold Growth on CCA-treated Radiata Pine Lumber by Incorporation of Moldicide into the CCA Solution

  • Kang, Sun-Mi;Kim, Gyu-Hyeok
    • Journal of the Korean Wood Science and Technology
    • /
    • v.35 no.2
    • /
    • pp.79-84
    • /
    • 2007
  • Surface mold fungi growing on CCA-treated wood could be inhibited effectively by the incorporation of moldicide into treating solution. In this study, moldicides compatible with the CCA solutions from various commercial moldicides were screened, and then their optimum concentrations for controlling surface mold on CCA-treated radiata pine sapwood were examined through both the laboratory and the field trials. Among nine commercial moldicdes tested, two substituted isothiazolinones, moldicide A containing 2-n-octyl-4-isothiazoline-3-one and moldicide B containing 5-chloro-2-methyl-4-isothiazolin-3-one and 2-methyl-4-isothiazolin-3-one, were chemically compatible with CCA solution. The optimum concentration to be incorporated into 2% CCA treating solution was determined to be 0.001% for moldicide A and 0.003% for moldicide B.

A Study on Internal Moisture Gradients of Wood (목재(木材) 건조중(乾燥中) 내부수분경사(內部水分傾斜)에 관(關)한 연구(硏究))

  • Kang, Ho-Yang
    • Journal of the Korean Wood Science and Technology
    • /
    • v.19 no.2
    • /
    • pp.30-39
    • /
    • 1991
  • Internal moisture gradients of 3cm-thick radiata pine (Pinus radiata) sapwood and meranti(Shorea spp.) heartwood were determined by using slicing method during drying and were predicted by Hart's Sorption Simulation. The shapes of internal moisture gradients. moisture contents and drying rates, which were obtained by the slicing method. were compared with those predicted by Sorption Simulation. After the 2nd fitting attempts. the differences between the gravimetric drying rates and the drying rates predicted by Sorption Simulation were less than 0.021%/hr for radiata pine and 0.043%/hr for meranti. The shapes of the internal moisture gradients predicted by Sorption Simulation were in good agreement with those obtained by the slicing method. It could be concluded that Sorption Simulation be an excellent tool to predict internal moisture gradients of wood.

  • PDF

A Comparison of Chromium and Copper-Containing Waterborne Wood Preservatives for Fixing and Leaching Characteristics (크롬-구리 화합물계(化合物系) 목재방부제(木材防腐劑)의 정착(定着) 및 용탈특성(溶脫特性) 비교(比較))

  • Ra, Jong-Bum;Kim, Gyu-Hyeok
    • Journal of the Korean Wood Science and Technology
    • /
    • v.23 no.3
    • /
    • pp.66-72
    • /
    • 1995
  • The rate of fixation of the components were evaluated in CCA-Type B and CCFZ-treated radiata pine sapwood by quantitative analysis of solution expressed from the treated wood. The leaching characteristics of radiata pine blocks treated with CCA-Type B and CCFZ were also evaluated by the AWPA standard leaching test. Both fixation and leaching charactersistics of CCA-Type B were compared with CCA-Type C treated wood samples. The rate of CCA-Type B fixation was a little faster than that of CCFZ. However, significant amounts of arsenic was unfixed in the CCA-Type B treated samples and consequently leached. These significant quantities of arsenic liberated from the CCA-Type B treated wood during service may pose some environmental concerns. Arsenic was no longer detectable from CCA-Type C treated samples when fixation was complete, even though the fixation of CCA-Type C was slower in some degree than CCA-Type B. In summary, it could be said that CCFZ was much safer preservative than CCA-Type B by the criterion based on the relative hazard assessed by absolute amount of unfixed element present in the treated wood. Also the decision that CCA preservative has to move from Type B to Type C should be made sooner or later for continuous use of CCA preservative in the future.

  • PDF

Fungi Colonizing Sapwood of Japanese Red Pine Logs in Storage

  • Kim, Jae-Jin;Ra, Jong-Bum;Son, Dae-Sun;Kim, Gyu-Hyeok
    • Mycobiology
    • /
    • v.29 no.4
    • /
    • pp.205-209
    • /
    • 2001
  • The Korean sawmills have recently recognized the importance of prevention of fungal discoloration due to increased losses in revenue. Before establishing integrated control strategies of fungal discoloration, more complete knowledge about causal organisms is needed. As a first step, we initiated a through survey of fungi colonizing commercially important softwood(Pinus dens flora, Pinus koraiensis, and Pinus radiata) logs and lumber in Korea. In this paper we report results obtained from Japanese red pine(Pinus densiflora) log study. In summer 2000, fungi were isolated from Japanese red pine logs in storage, and identified based on their cultural and morphological characteristics. A total of 595 fungi were isolated, representing 21 genera and 30 species. Mold fungi, mostly Trichoderma species, were the most frequently isolating fungi, representing more than half of all isolates. Dematiaceous fungi represented approximately one fifth of the isolates, and Rhinocladiella atorvirens was the most abundant in all samples. Opiostoma species represented 7% of all isolates from cores planted on malt extract agar(MEA) and the incidence of these species doubled with the addition of streptomycin and cycloheximide to MEA. The results indicate that Japanese red pine sapwood is susceptible to colonization by a variety of fungal species. As a result, control strategies that concentrate on one fungus may have limited success because of interference from competing flora.

  • PDF

Reduction in Mechanical Properties of Radiata Pine Wood Associated with Incipient Brown-Rot Decay (초기(初期) 갈색부후(褐色腐朽)에 따른 라디에타소나무의 역학적(力學的) 성질(性質) 감소(減少))

  • Kim, Gyu-Hyeok;Jee, Woo-Kuen;Ra, Jong-Bum
    • Journal of the Korean Wood Science and Technology
    • /
    • v.24 no.1
    • /
    • pp.81-86
    • /
    • 1996
  • This study was performed to evaluate the reduction in bending properties of radiata pine sapwood associated with incipient brown-rot decay. Decayed bending specimens by Tyromyces palustris and Gloeophyllum trabeum for varoious periods were tested destructively. Brown-rot decay by T. palustris and G. trabeum caused serious reduction in bending properties at very early stages of decay, with about 30 percent decrease in bending strength observed for only 1~2 percent weight loss. In general, the reduction in bending properties caused by T. palustris was somewhat greater than that by G. trabeum. Work to maximum load was reduced most severely and rapidly from the onset of decay, while modulus of elasticity showed a much more moderate rate of reduction. Modulus of rupture was affected by decay to a greater extent than was modulus of elasticity. Since a relatively strong correlation between weight loss and bending strength was observed, the residual strength of decayed wood can be predicted by weight loss due to decay. The results of this study indicate that very early stages of brown-rot decay reduce the bending strength significantly. Thus, it is recommended that all load-bearing members in wooden structures, especially those that are periodically wetted, should be inspected regularly to prevent a sudden failure even though there are no definite signs of decay.