• Title/Summary/Keyword: quasi-nonvolatile memory

Search Result 2, Processing Time 0.017 seconds

Quasi-nonvolatile Memory Characteristics of Silicon Nanosheet Feedback Field-effect Transistors (실리콘 나노시트 피드백 전계효과 트랜지스터의 준비휘발성 메모리 특성 연구)

  • Seungho Ryu;Hyojoo Heo;Kyoungah Cho;Sangsig Kim
    • Journal of IKEEE
    • /
    • v.27 no.4
    • /
    • pp.386-390
    • /
    • 2023
  • In this study, we examined the quasi-nonvolatile memory characteristics of silicon nanosheet (SiNS) feedback field-effect transistors (FBFETs) fabricated using a complementary metal-oxide-semiconductor process. The SiNS channel layers fabricated by photoresist overexposure method had a width of approximately 180 nm and a height of 70 nm. The SiNS FBFETs operated in a positive feedback loop mechanism and exhibited an extremely low subthreshold swing of 1.1 mV/dec and a high ON/OFF current ratio of 2.4×107. Moreover, SiNS FBFETs represented long retention time of 50 seconds, indicating the quasi-nonvolatile memory characteristics.

A study on the fabrication and characteristics of the scaled MONOS nonvolatile memory devices for low voltage EEPROMs (저전압 EEPROM을 위한 Scaled MONOS 비휘발성 기억소자의 제작 및 특성에 관한 연구)

  • 이상배;이상은;서광열
    • Electrical & Electronic Materials
    • /
    • v.8 no.6
    • /
    • pp.727-736
    • /
    • 1995
  • This paper examines the characteristics and physical properties of the scaled MONOS nonvolatile memory device for low programming voltage EEPROM. The capacitor-type MONOS memory devices with the nitride thicknesses ranging from 41.angs. to 600.angs. have been fabricated. As a result, the 5V-programmable MONOS device has been obtained with a 20ms programming time by scaling the nitride thickness to 57.angs. with a tunneling oxide thickness of 19.angs. and a blocking oxide thickness of 20.angs.. Measurement results of the quasi-static C-V curves indicate, after 10$\^$6/ write/erase cycles, that the devices are degraded due to the increase of the silicon-tunneling oxide interface traps. The 10-year retention is impossible for the device with a nitride less than 129.angs.. However, the MONOS memory device with 10-year retentivity has been obtained by increasing the blocking oxide thickness to 47.angs.. Also, the memory traps such as the nitride bulk trap and the blocking oxide-nitride interface trap have been investigated by measuring the maximum flatband voltage shift and analyzing through the best fitting method.

  • PDF