PLD법으로 제작된 xPb(Al0.5Nb0.5)O3-(1-x)Pb(Zr0.52Ti0.48)O3박막의 유전 및 압전 특성 (Dielectric and Piezoelectric Properties of xPb(Al0.5Nb0.5)O3-(1-x)Pb(Zr0.52Ti0.48)O3 Thin films Prepared by PLD)

  • 김민철;박용욱;최지원;강종윤;안병국;김현재;윤석진
    • 한국전기전자재료학회논문지
    • /
    • 제16권9호
    • /
    • pp.795-800
    • /
    • 2003
  • The dielectric and piezoelectric properties of the xPb(A $l_{0.5}$N $b_{0.5}$) $O_3$-(1-x)Pb(Z $r_{0.52}$ $Ti_{0.48}$) $O_3$ [xPAN-(1-x)PZT] thin films by pulsed laser deposition (PLD) were investigated as a function of PAN contents. The effect of texture on dielectric and piezoelectric properties of the 0.05PAN-0.95PZT thin films having the highest piezoelectric constant( $d_{33}$) was studied more precisely. For 0$\leq$x$\leq$0.15 compositions in xPAN-(1-x)PZT thin films, the well-developed perovskite phase with (111) preferred orientation was obtained at the deposition temperature of 50$0^{\circ}C$. With increasing PAN content, remanent polarization and coercive field decreased. The dielectric constant increased with an increase of PAN content until it reached 1450 at $\chi$= 0.05, and then decreased for higher PAN content. The maximum points of dielectric constant coincides with the maximum points of the piezoelectric constant $d_{33}$.33/.33/././.

펄스 레이저 증착(PLD)법에 의한 ZnO 박막 성장과 열처리 효과 (Growth and Effect of Thermal Annealing for ZnO Thin Film by Pulsed Laser Deposition)

  • 홍광준
    • 한국전기전자재료학회논문지
    • /
    • 제17권5호
    • /
    • pp.467-475
    • /
    • 2004
  • ZnO epilayer were synthesized by the pulsed laser deposition(PLD) process on $Al_2$ $O_3$substrate after irradiating the surface of the ZnO sintered pellet by the ArF(193 nm) excimer laser. The epilayers of ZnO were achieved on sapphire(A $l_2$ $O_3$) substrate at a temperature of 400 $^{\circ}C$. The crystalline structure of epilayer was investigated by the photoluminescence and double crystal X-ray diffraction(DCXD). The carrier density and mobility of ZnO epilayer measured with Hall effect by van der Pauw method are 8.27${\times}$$10^{16}$$cm^{-3}$ and 299 $\textrm{cm}^2$/Vㆍs at 293 K, respectively. The temperature dependence of the energy band gap of the ZnO obtained from the absorption spectra was well described by the Varshni's relation, $E_{g}$(T)= 3.3973 eV - (2.69 ${\times}$ 10$_{-4}$ eV/K) $T^2$(T+463k). After the as-grown ZnO epilayer was annealed in Zn atmospheres, oxygen and vaccum the origin of point defects of ZnO atmospheres has been investigated by the photoluminescence(PL) at 10 K. The native defects of $V_{Zn}$ , $V_{o}$ , Z $n_{int}$, and $O_{int}$ obtained by PL measurements were classified as a donors or accepters type. In addition, we concluded that the heat-treatment in the oxygen atmosphere converted ZnO thin films to an optical p-type. Also, we confirmed that vacuum in ZnO/A $l_2$ $O_3$did not form the native defects because vacuum in ZnO thin films existed in the form of stable bonds.s.s.s.

Amorphous Silicon Carbon Nitride Films Grown by the Pulsed Laser Deposition of a SiC-$Si_3N_4$ Mixed Target

  • Park, Nae-Man;Kim, Sang-Hyeob;Sung, Gun-Yong
    • ETRI Journal
    • /
    • 제26권3호
    • /
    • pp.257-261
    • /
    • 2004
  • We grew amorphous SiCN films by pulsed laser deposition using mixed targets. The targets were fabricated by compacting a mixture of SiC and $SiC-{Si_3}{N_4}$ powders. We controlled the film stoichiometry by varying the mixing ratio of the target and the target-to-substrate distance. The mixing ratio of the target had a dominant effect on the film composition. We consider the structures of the SiCN films deposited using 30~70 wt.% SiC in the target to be an intermediate phase of SiC and $SiN_x$. This provides the possibility of growing homogeneous SiCN films with a mixed target at a moderate target-to-substrate distance.

  • PDF

Pulsed Laser Deposition of $CuIn_{1-x}M_xO_2$(M=Ca, Mg, or Ti) Thin Films for Transparent Conducting Oxide

  • 이종철;엄세영;허영우;이준형;김정주
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2007년도 추계학술대회 논문집
    • /
    • pp.103-104
    • /
    • 2007
  • $CuInO_2$ 단일상은 합성조건이 매우 까다롭기 때문에 일반적인 고상법으로 얻기 힘든 것으로 알려저 있다. 투명전도성 $CuInO_2$ 박막을 증착하기 위하여 일반적인 고상법으로 Cu와 In의 비율이 1:1인 $Cu_2O-In_2O_3$ composite target 및 In 대신 Ca, Mg, Ti가 각각 1mol% 도핑된 target을 제작하였다. 제작된 각각의 composite target을 이용하여 pulsed laser deposition(PLD) 공정으로 투명전도성 $CuInO_2$ 박막을 증착하였다. Cu와 In이 1:1 인 $Cu_2O-In_2O_3$ composite target을 사용한 경우, 증착된 박막이 Cu와 In의 비율이 1:1인 c-axis 배향된 단일상의 $CuInO_2$ 박막임을 확인하였다.

  • PDF

PLD법에 의한 OLED 제작 공정 개발 (Development of OLED manufacturing process using PLD method)

  • 김창교;노일호;장석원;홍진수;양성준
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2004년도 추계학술대회 논문집 Vol.17
    • /
    • pp.598-602
    • /
    • 2004
  • Organic light entitling diode panel was fabricated using pulsed laser deposition (PLD) method Nd-YAG laser with Q-Switched and 355 nm pulse was used for the PLD. While TPD(N,N'-Di-[naphthaleny]-N, N'-diphenyl-benzidine) was used as a HTL(Hole transport layer), $Alq_3$(8-Hydroxyquinoline, Aluminum Salt) was used as EML/ETL(Emitting Layer/Electron Transport Layer) Organic pellet was fabricated and employed for the PLD method. The absorbances of the organic films were investigated and the measured absorbance values of TPD and $Alq_3$ films was 362 nm and 399 nm, respectively. The turn-on voltage of the OLED panel was 7.5 V and its luminance was $90\;cd/m^2$

  • PDF

Intermediate band solar cells with ZnTe:Cr thin films grown on p-Si substrate by pulsed laser deposition

  • Lee, Kyoung Su;Oh, Gyujin;Kim, Eun Kyu
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2016년도 제50회 동계 정기학술대회 초록집
    • /
    • pp.247.1-247.1
    • /
    • 2016
  • Low-cost, high efficiency solar cells are tremendous interests for the realization of a renewable and clean energy source. ZnTe based solar cells have a possibility of high efficiency with formation of an intermediated energy band structure by impurity doping. In this work, ZnO/ZnTe:Cr and ZnO/i-ZnTe structures were fabricated by pulsed laser deposition (PLD) technique. A pulsed (10 Hz) Nd:YAG laser operating at a wavelength of 266 nm was used to produce a plasma plume from an ablated a ZnTe target, whose density of laser energy was 10 J/cm2. The base pressure of the chamber was kept at approximately $4{\times}10-7Torr$. ZnTe:Cr and i-ZnTe thin films with thickness of 210 nm were grown on p-Si substrate, respectively, and then ZnO thin films with thickness of 150 nm were grown on ZnTe:Cr layer under oxygen partial pressure of 3 mTorr. Growth temperature of all the films was set to $250^{\circ}C$. For fabricating ZnO/i-ZnTe and ZnO/ZnTe:Cr solar cells, indium metal and Ti/Au grid patterns were deposited on back and front side of the solar cells by using thermal evaporator, respectively. From the fabricated ZnO/ZnTe:Cr and ZnO/i-ZnTe solar cell, dark currents were measured by using Keithley 2600. Solar cell parameters were obtained under Air Mass 1.5 Global solar simulator with an irradiation intensity of 100 mW/cm2, and then the photoelectric conversion efficiency values of ZnO/ZnTe:Cr and ZnO/i-ZnTe solar cells were measured at 1.5 % and 0.3 %, respectively.

  • PDF

펄스 레이저 증착법으로 성장된 투명 TFTs 채널층을 위한 ZnO 박막 분석 (Characterization of ZnO Thin Films Grown by Pulsed Laser Deposition for Channel Layer of Transparent TFTs)

  • 이원용;김지홍;노지형;조대형;문병무;구상모
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.77-78
    • /
    • 2008
  • ZnO thin films were deposited on glass substrates by pulsed laser deposition (PLD) at various oxygen pressures. We observed structural, electrical and optical properties of ZnO films. Structural properties were analysed by XRD and FE-SEM. Electrical properties for applications of transparent thin film transistors (TTFTs) were measured by hall measurement using van der pauw methods at room temperature. In order to apply in transparent devices, we measured transmittance, and optical bandgap energy was calculated by Tauc's equation. The results showed that ZnO films deposited at 200mTorr oxygen pressure were applicable to channel layers of transparent TFTs. It had high hall mobilities ($52.92cm^2$/V-s) and suitable transmittance at visible wavelength region (above 80%).

  • PDF

초전도 필터의 중심 주파수 변화 (Shift of center frequency of superconducting microwave liker)

  • 송석천;박정호;이상렬
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 하계학술대회 논문집
    • /
    • pp.787-789
    • /
    • 2000
  • High temperature superconducting YBCO films have been grown on MgO substrates by pulsed laser deposition (PLD) with Nd:YAG laser Superconducting microwave filter was fabricated by conventional photolithography method. We have designed filter with the center frequency of 14 GHz. We have measured the center frequency of filter at 77 K and its critical temperature 89K. Also we have designed another filter to compare frequency responses. The measured frequency responses will be presented.

  • PDF

레이저 어블레이션에 의한 (Pb,La)$TiO_3$박막의 제작조건에 따른 특성 (CHaracteristics of (Pb,La)T$TiO_3$ Thin Film by Deposition Condition of Pulsed Laser Ablation)

  • 박정흠;박용욱;마석범
    • 한국전기전자재료학회논문지
    • /
    • 제14권12호
    • /
    • pp.1001-1007
    • /
    • 2001
  • In this study, high dielectric materials, (Pb,La)Ti $O_3$ thin films were fabricated by PLD (Pulsed Laser Deposition) method and investigated in terms of structural and electrical characteristics in order to develope the dielectric materials for the use of new capacitor layers of Giga bit-level DRAM. The deposition conditions were examined in order to fabricate uniform thin films through systematic changes of oxygen pressures and substrate temperature. The uniform thickness and smooth morphology of (P $b_{0.72}$L $a_{0.28}$)Ti $O_3$ thin films were obtained at the conditions of substrate-target distance 5.5[cm], laser energy density 2.1[J/$\textrm{cm}^2$], oxygen pressure 200[mTorr] and substrate temperature 500[$^{\circ}C$]. After the (P $b_{0.72}$L $a_{0.28}$)Ti $O_3$ thin films were fabricated under the above conditions, they were post-annealed by RTA process in order to increase the dielectric constant. The film thickness of 1200 [$\AA$] had dielectric constant 821. Assuming that operating voltage is 2V, leakage current density of (P $b_{0.72}$L $a_{0.28}$)Ti $O_3$ thin films would result into 10$^{-7}$ [A/$\textrm{cm}^2$] and satisfied the specification of 256M DRAM planar capacitor, 4$\times$10$^{-7}$ [A/$\textrm{cm}^2$]m}^2$]

  • PDF

광흡수층 적용을 위한 PLD용 $Cu_2ZnSnSe_4$ 타겟 제조와 증착 박막의 특성 (Characteristics of $Cu_2ZnSnSe_4$ Thin Film Solar Absorber Prepared by PLD using Solid Target)

  • 정운화;라흐멧 아드히 위보우;김규호
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2009년도 춘계학술대회 논문집
    • /
    • pp.130-133
    • /
    • 2009
  • $Cu_2ZnSnSe_4$(CZTSe) is one of the promising materials for the solar cell due to its abundant availability in the nature. In this study, we report the fabrication of CZTSe thin film by Pulsed Laser Deposition(PLD) method using quaternary compound target on sodalime glass substrate. The quaternary CZTSe compound target was synthesized by solid state reaction method using elemental powders of Cu, Zn, Sn and Se. Powders were milled in high purity ethanol using zirconia ball with mixed size of 1 and 3 mm at the same proportions for 72 hours milling time. The structural, chemical and mechanical properties of the synthesized CZTSe powders were investigated prior to the deposition process. The CZTSe compound powder, and $500^{\circ}C$ of sintering temperature shows the best properties for PLD target. Results show that the as-deposited CZTSe thin films with the precursors by PLD have a composition near-stoichiometric.

  • PDF