STUDY ON THE ENHANCING MICRO-ROUGHNESS OF POROUS SURFACED DENIAL IMPLANT THROUGH ANODIZATION (양극산화처리를 통한 다공성 임플랜트 표면의 표면거칠기 증대에 대한 연구)

  • Yoon, Tae-Ho;Song, Kwang-Yeob
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.44 no.5
    • /
    • pp.617-627
    • /
    • 2006
  • Statement of problem: HA has been used as a coating material on Ti implants to improve osteoconductivity. However. it is difficult to form uniform HA coatings on implants with complex surface geometries using a plasma spraying technique. Purpose : To determine if Ti6Al4V sintered porous-surfaced implants coated with HA sol-gel coated and hydrothermal treated would accelerate osseointegration. Materials and Methods : Porous implants which were made by electric discharge were used in this study. Implants were anodized and hydrothermal treatment or HA sol-gel coating was performed. Hydrothermal treatment was conducted by high pressure steam at $300^{\circ}C$ for 2 hours using a autoclave. To make a HA sol, triethyl phosphite and calcium nitrate were diluted and dissolved in anhydrous ethanol and mixed. Then anodized implant were spin-coated with the prepared HA sols and heat treated. Samples were soaked in the Hanks solution with pH 7.4 at $37^{\circ}C$ for 6 weeks. The microstructure of the specimens was observed with a scanning electron microscope (SEM), and the composition of the surface layer was analyzed with an energy dispersive spectroscope (EDS). Results : The scanning electron micrographs of HA sol-gel coated and hydrothermal treated surface did not show any significant change in the size or shape of the pores. After immersion in Hanks' solution the precipitated HA crystals covered macro- and micro-pores The precipitated Ca and P increased in Hanks' solution that surface treatment caused increased activity. Conclusion : This study shows that sol-gel coated HA and hydrothermal treatment significantly enhance the rate of HA formation due to the altered surface chemistry.

Effects of Powder Melting Degree on Microstructural Features of Plasma Sprayed Y2O3 Coating (플라즈마 제트에서의 분말 용융특성에 따른 Y2O3 코팅층의 미세조직 형성거동)

  • Kang, Sang-Woon;Baik, Kyeong-Ho
    • Korean Journal of Materials Research
    • /
    • v.26 no.5
    • /
    • pp.229-234
    • /
    • 2016
  • In this study, the degree of particle melting in $Y_2O_3$ plasma spraying and its effects on coating characteristics have been investigated in terms of microstructural features, microhardness and scratch resistance. Plasma sprayed $Y_2O_3$ coatings were formed using two different powder feeding systems: a system in which the powder is fed inside the plasma gun and a system in which the powder is fed externally. The internal powder spraying method generated a well-defined lamellae structure that was characterized by a thin porous layer at the splat boundary and microcracks within individual splats. Such micro-defects were generated by the large thermal contraction of splats from fully-molten droplets. The external powder spraying method formed a relatively dense coating with a particulate deposition mode, and the deposition of a higher fraction of partially-melted droplets led to a much reduced number of inter-splat pores and intra-splat microcracks. The microhardness and scratch resistance of the $Y_2O_3$ coatings were improved by external powder spraying; this result was mainly attributed to the reduced number of micro-defects.

Plasma-Sprayed $Al_2O_3-SiO_2$ Multi-Oxide Films on Stainless Steel Substrate

  • Korobova, N.;Soh, Deawha
    • Proceedings of the Korean Institute of Navigation and Port Research Conference
    • /
    • 2000.11a
    • /
    • pp.116-119
    • /
    • 2000
  • The advantage of plasma-sprayed coating is their good resistance against thermal shock due to the porous state of the coated layer with a consequently low Youngs modulus. However, the existence of many pores with a bimodal distribution and a laminar structure in the coating reduces coating strength and oxidation protection of the base metals. In order to counteract these problems, there have been many efforts to obtain dense coatings by spraying under low pressure or vacuum and by controlling particle size and morphology of the spraying materials. The aim of the present study is to survey the effects of the HIP treatment between 1100 and 130$0^{\circ}C$ on plasma-sprayed oxide coating of A1$_2$O$_3$, A1$_2$O$_3$-SiO$_2$on the metal substrate (type C18N10T stainless steel). These effects were characterized by phase identification, Vickers hardness measurement, and tensile test before and after HIPing. These results show that high-pressure treatment has an advantage for improving adhesive strength and Vickers hardness of plasma-sprayed coatings.

  • PDF

Plasma-Sprayed $Al_{2}O_{3}-SiO_{2}$ Multi-Oxide Films on Stainless Steel Substrate

  • Korobova, N.;Soh, Deawha
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.11a
    • /
    • pp.116-119
    • /
    • 2000
  • The advantage of plasma-sprayed coating is their good resistance against thermal shock due to the porous state of the coated layer with a consequently low Youngs modules. However, the existence of many pores with a bimodal distribution and a laminar structure in the coating reduces coating strength and oxidation protection of the base metals. In order to counteract these problems, there have been many efforts to obtain dense coatings by spraying under low pressure or vacuum and by controlling particle size and morphology of the spraying materials. The aim of the present study is to survey the effects of the HIP treatment between 1100 and 130$0^{\circ}C$ on plasma-sprayed oxide coating of A1$_2$O$_3$, A1$_2$O$_3$-SiO$_2$ on the metal substrate (type C18N10T stainless steel). These effects were characterized by phase identification, Vickers hardness measurement, and tensile test before and after HIPing, These results show that high-pressure treatment has an advantage for improving adhesive strength and Vickers hardness of plasma- sprayed coatings.

  • PDF

Effect of Fe(NO3)2 Concentration on Electrochemical Behavior of SCM430 in Zinc Phosphate Conversion Coating Solution (아연계 인산염 피막용액에서 Fe(NO3)2 농도가 SCM430 합금의 전기화학적 거동에 미치는 영향)

  • Kwon, Duyoung;Song, Pung-Keun;Moon, Sungmo
    • Journal of the Korean institute of surface engineering
    • /
    • v.52 no.4
    • /
    • pp.233-238
    • /
    • 2019
  • The formation behavior of zinc phosphate conversion coating (ZPCC) on SCM430 alloy was investigated in 25 vol.% of 1M ZnO + 170 ml/L solution containing various $Fe(NO_3)_2$ concentrations, using open-circuit potential(OCP), electrochemical impedance spectroscopy(EIS), cyclic polarization(CP) curve and tape peel test. OCP of SCM430 alloy and corrosion current density increased with increasing $Fe(NO_3)_3$ concentration. Resistance of films formed on SCM430 alloy by chemical conversion treatment decreased with increasing $Fe(NO_3)_3$ concentration. Color and adhesion of chemical conversion coatings became darker and worse, respectively, with increasing $Fe(NO_3)_3$ concentration. It is concluded that addition of $Fe(NO_3)_3$ into a zinc phosphating bath leads to faster reaction to form porous surface coatings with poor adhesion and corrosion resistance.

Characteristics and oxidation behavior of the hybrid-HVOF sprayed $Cr_3C_2$-7wt%(NiCr) coatings depending on $H_2/O_2$ ratio ($H_2/O_2$ 비에 따른 Hybrid HVOF 용사된 $Cr_3C_2$-7wt%(NiCr) 용사층의 특성 및 산화거동)

  • 김병희;서동수
    • Journal of Welding and Joining
    • /
    • v.15 no.4
    • /
    • pp.126-135
    • /
    • 1997
  • $H_2/O_2$ 비에 따른 Hybrid HVOF 용사된 $Cr_3C_2$-7wt%(NiCr) 용사층의 특성 및 산화거동 This study was performed to investigate the influence of fuel/oxygen ratio (F/O=3.2, 3.0, 2.8) on the characteristics and the oxidation behavior of the hybrid-HVOF sprayed $Cr_3C_2$-7wt%NiCr coatings. Decomposition and the oxidation of the $Cr_3C_2$was occured during spraying. The degree of transformation from $Cr_3C_2$to $Cr_7C_3$ was increased with decreasing the F/O ratio. The microstructural differences of the as sprayed coating with F/O ratio can not be distinguished, However, large pores were diminished and then the coatings became dense by heat treatment. Microhardness of the as-sprayed specimen which sprayed with F/O=3.0 condition was hightest ($Hv_{300}$=1140) and the hardness was increased to 1500 after heat treatment at $600^{\circ}C$ for 50hrs in air. It was supposed that hardness was increased due to the formation of $Cr_2O_3$ within $Cr_3C_2$/$Cr_7C_3$matrix and the densification of coating layer during heat treatment. Apparent activation energy for oxidation was varied from 21.2 kcal$mol^{-1}K^{-1}$ to 23.8 kcal$mol^{-1}K^{-1}$ with respect to the F/O ratio. The surface morphology was changed to porous and oxide chusters were grown after oxidation $1000^{\circ}C$ for 50 hours by the aggressive evolution of gas phase ($CrO_3$ and$CO_2$). The oxide cluster was composed of Ni and Cr.

  • PDF

Corrosion Behavior of Ti-6Al-4V Alloy after Plasma Electrolytic Oxidation in Solutions Containing Ca, P and Zn

  • Hwang, In-Jo;Choe, Han-Cheol
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2016.11a
    • /
    • pp.120-120
    • /
    • 2016
  • Ti-6Al-4V alloy have been used for dental implant because of its excellent biocompatibility, corrosion resistance, and mechanical properties. However, the integration of such implant in bone was not in good condition to achieve improved osseointergraiton. For solving this problem, calcium phosphate (CaP) has been applied as coating materials on Ti alloy implants for hard tissue applications because its chemical similarity to the inorganic component of human bone, capability of conducting bone formation and strong affinity to the surrounding bone tissue. Various metallic elements, such as strontium (Sr), magnesium (Mg), zinc (Zn), sodium (Na), silicon (Si), silver (Ag), and yttrium (Y) are known to play an important role in the bone formation and also affect bone mineral characteristics, such as crystallinity, degradation behavior, and mechanical properties. Especially, Zn is essential for the growth of the human and Zn coating has a major impact on the improvement of corrosion resistance. Plasma electrolytic oxidation (PEO) is a promising technology to produce porous and firmly adherent inorganic Zn containing $TiO_2(Zn-TiO_2)$coatings on Ti surface, and the a mount of Zn introduced in to the coatings can be optimized by altering the electrolyte composition. In this study, corrosion behavior of Ti-6Al-4V alloy after plasma electrolytic oxidation in solutions containing Ca, P and Zn were studied by scanning electron microscopy (SEM), AC impedance, and potentiodynamic polarization test. A series of $Zn-TiO_2$ coatings are produced on Ti dental implant using PEO, with the substitution degree, respectively, at 0, 5, 10 and 20%. The potentiodynamic polarization and AC impedance tests for corrosion behaviors were carried out in 0.9% NaCl solution at similar body temperature using a potentiostat with a scan rate of 1.67mV/s and potential range from -1500mV to +2000mV. Also, AC impedance was performed at frequencies ranging from 10MHz to 100kHz for corrosion resistance.

  • PDF

Electrochemical Characteristics of Zn and Si Ion-doped HA Films on Ti-6Al-4V by PEO Treatment

  • Lim, Sang-Gyu;Hwang, In-Jo;Choe, Han-Cheol
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2016.11a
    • /
    • pp.199-199
    • /
    • 2016
  • Commercially pure titanium (cp-Ti) and Ti alloys (typically Ti-6Al-4V) display excellent corrosion resistance and biocompatibility. Although the chemical composition and topography are considered important, the mechanical properties of the material and the loading conditions in the host have, conventionally. Ti and its alloys are not bioactive. Therefore, they do not chemically bond to the bone, whereas they physically bond with bone tissue. The electrochemical deposition process provides an effective surface for biocompatibility because large surface area can be served to cell proliferation. Electrochemical deposition method is an attractive technique for the deposition of hydroxyapatite (HAp). However, the adhesions of these coatings to the Ti surface needs to be improved for clinical used. Plasma electrolyte oxidation (PEO) enables control in the chemical com position, porous structure, and thickness of the $TiO_2$ layer on Ti surface. In addition, previous studies h ave concluded that the presence of $Ca^{+2}$ and ${PO_4}^{3-}$ ion coating on porous $TiO_2$ surface induced adhesion strength between HAp and Ti surface during electrochemical deposition. Silicon (Si) in particular has been found to be essential for normal bone and cartilage growth and development. Zinc (Zn) plays very important roles in bone formation and immune system regulation, and is also the most abundant trace element in bone. The objective of this work was to study electrochemical characteristcs of Zn and Si coating on Ti-6Al-4V by PEO treatment. The coating process involves two steps: 1) formation of porous $TiO_2$ on Ti-6Al-4V at high potential. A pulsed DC power supply was employed. 2) Electrochemical tests were carried out using potentiodynamic and AC impedance methoeds. The morphology, the chemical composition, and the micro-structure an alysis of the sample were examined using FE-SEM, EDS, and XRD. The enhancements of the HAp forming ability arise from $Si/Zn-TiO_2$ surface, which has formed the reduction of the Si/Zn ions. The promising results successfully demonstrate the immense potential of $Si/Zn-TiO_2$ coatings in dental and biomaterials applications.

  • PDF

Development of New Surfaces and Materials for Separation Science

  • Linford, Matthew R.
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2015.08a
    • /
    • pp.59.1-59.1
    • /
    • 2015
  • In the Linford group at Brigham Young University we have recently developed three new sets of materials for three different areas of separations science: thin layer chromatography (TLC), high performance liquid chromatography (HPLC), and solid phase microextraction (SPME). First, via microfabrication we have grown patterned carbon nanotube (CNT) forests on planar substrates that we have infiltrated with inorganic materials such as silicon nitride. The coatings on the CNTs are conformal and typically deposited in a process like low pressure chemical vapor deposition. The resulting materials have high surface areas, are porous, and function as effective separation devices, where separations on our new TLC plates are typically significantly faster than on conventional devices. Second, we used the layer-by-layer (electrostatically driven) deposition of poly (allylamine) and nanodiamond onto carbonized poly (divinylbenzene) microspheres to create superficially porous particles for HPLC. Many interesting classes of molecules have been separated with these particles, including various cannabinoids, pesticides, tricyclic antidepressants, etc. Third, we have developed new materials for SPME by sputtering silicon onto cylindrical fiber substrates in a way that creates shadowing of the incoming flux so that materials with high porosity are obtained. These materials are currently outperforming their commercial counterparts. Throughout this work, the new materials we have made have been characterized by X-ray photoelectron spectroscopy, time-of-flight secondary ion mass spectrometry, scanning electron microscopy, transmission electron microscopy, etc.

  • PDF

A study of hydroxyapatite coating on Ti-6Al-4V alloy with different surface treatments using a sol-gel derived precursor

  • Balakrishnan Avinash;Kim Yun-Jong;Lee Seung-Woo;Kim Taik-Nam
    • The Journal of Engineering Research
    • /
    • v.6 no.1
    • /
    • pp.161-168
    • /
    • 2004
  • In the present study, a simple method was successfully used for hydroxyapatite coatings on Ti-6AL-4V substrates deposited by using a sol-gel derived precursor. Prior to hydroxyapatite coating the samples were micropolished (0.1 micron) and divided into three sets. The first set, were the micropolished samples kept as such. The second set were coated with titania sol and the third set was treated with 5M NaOH. After three repetitions of hydroxyapatite coating procedures on each set and heat treatment at $600^{\circ}C$, the formation of hydroxyapatite has been confirmed by XRD analyses and the substrate material was found to be oxidized with negligible amount of CaO in the coating. The SEM studies revealed surface morphology. Hydroxyapatite, calcined at $600^{\circ}C$, displaying a porous structure arisen from heating of the bulk