• 제목/요약/키워드: pin-on-disc test

검색결과 50건 처리시간 0.02초

레이저 표면 딤플 패턴된 PMMA 소재 표면의 식염수 윤활 하에서의 미끄럼 마찰특성 (Sliding Friction Properties of Laser Surface Dimple Patterned on PMMA under Saline Lubricated)

  • 현동호;채영훈;정다이
    • Tribology and Lubricants
    • /
    • 제39권4호
    • /
    • pp.148-153
    • /
    • 2023
  • Laser surface dimple patterning is a method of laser surface texturing to reduce lubrication sliding friction. The dimple pattern improves friction properties by reserving lubricant and trapping worn particles. This surface texturing technology can reduce coefficients of friction and extend the service life by applying a uniform load to the surface of the material. This study investigates the friction properties using PMMA, a highly compatible polymer material, as a specimen. We observe the friction properties of untextured specimens by processing specimens with dimple pattern densities of 5 and 10 on the surface area using laser. Dimple pattern density affects the coefficient of friction. We present the following friction property results using a pin-on-disc sliding friction test under saline lubrication. The coefficients of friction for the dimple patterned specimens are lower than those for the untextured specimens. As the normal load and sliding speed increase, the coefficients of friction of the dimple pattern specimens decrease differently from those of the untextured specimens. The specimen with a dimple pattern density of 5 at a normal load of 24.5 N and a sliding speed of 0.22 m/s has the best friction properties. Notably, different friction properties are exhibited depending on the dimple pattern densities.

SCM440강에 대한 마찰 마멸의 기본적 거동해석 (Fundamental Behavior Analysis of SCM440 Steel on Friction and Wear)

  • 변재영;이창주;장준수;최원식
    • 한국기계가공학회지
    • /
    • 제15권1호
    • /
    • pp.74-80
    • /
    • 2016
  • Due to the increased use of power caused by industrial development, the importance of improving wear and friction in the contact region has emerged. Except for some parts, such as brakes or clutches and friction, seals and precision mechanical parts (e.g., pistons, bearings, valves, and cams) are important engine components that require low friction characteristics. In this study, the experimental method used to determine the friction characteristics was based on the type of rpm with the pin-on-disc test device, the element analysis program ANSYS was used to analyze the surfaces of the two metals rubbing together, and physical formation FEM models were used to study the properties and wear. The friction coefficient of variation was unsafe, but at the start of wear, it converged to a stable friction coefficient that increased after a certain slip away.

미끄럼 접촉을 하는 탄소강의 경도차 조합에 따른 마모특성변화 연구 (The Change of Sliding wear properties of Carbon Steel against several hardened steels)

  • 이한영;김근영
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2003년도 학술대회지
    • /
    • pp.85-90
    • /
    • 2003
  • Although wear resistance of material improves with increasing its hardness, it is known that the wear resistance of steel is varied with hardness of counter material. In this context, wear properties of steel must be depended on the difference of hardness between the testpiece and the counter material. In this study, using the pin-on-disc type wear machine, annealed carbon steels were tested against ahoy tool steels with various levels of hardness. Then the changes of wear properties of carbon steel according to the hardness of counter material were investigated and the morphology of worn surface after test were evaluated. The results indicate that if there are no remarkable difference of hardness between them, wear resistance of carbon steel in running-in wear decreases with increasing the hardness of counter material. However, its wear properties at the range of high sliding speed have no relation with hardness of counter material. It is clear that wear properties is influenced by the formation of oxide of steel on their worn surface during wear.

  • PDF

상대재의 거칠기에 따른 실리카 입자강화 나노 복합재료의 마찰 및 마모에 관한 실험적 연구 (An experimental study of the friction and wear on counterpart roughness of silica particle reinforced nano composites)

  • 김형진;이정규;고성위
    • 수산해양기술연구
    • /
    • 제50권2호
    • /
    • pp.162-168
    • /
    • 2014
  • The friction and wear characteristics of the rubber matrix composites filled with nano sized silica particles were investigated at ambient temperature by pin-on-disc friction test. The volume fraction of silica particles was 19%. The cumulative wear volume and wear rate of these materials on counterpart roughness were determined experimentally. The major failure mechanisms were lapping layers, deformation of matrix, ploughing, debonding of particles, fracture of particles and microcracking by scanning electric microscopy photograph of the tested surface. The cumulative wear volume showed a tendency to increase with increase of sliding distance. The wear rate of these composites tested indicated low value as increasing the sliding distance.

입자지름의 변화에 따른 실리카 복합재료의 마찰 및 마모 특성 (Friction and Wear Characteristics of Silica/Epoxy Composites for various Particle Size)

  • 고성위;김형진;김재동;김창수
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2006년 창립20주년기념 정기학술대회 및 국제워크샵
    • /
    • pp.141-144
    • /
    • 2006
  • In this study, the friction and wear characteristics of pure epoxy and silica-filled epoxy resin composites with average silica particle diameter of $6-33{\mu}m$ were investigated at ambient temperature by pin-on-disc friction test. The cumulative wear volume, friction coefficient and wear rate of these materials against SiC abrasive paper were determined experimentally. The cumulative wear volume tended to increase nonlinearly with increase of sliding distance and depended on diameter of the silica particle for all these composites. The sliding wear tests of the materials demonstrated that the friction coefficient and the wear rate of silica filled epoxy composites were lower than those of the pure epoxy. silica filled epoxy.

  • PDF

그리스 윤활하에서 레이저 표면 텍스쳐링된 그루브 빗살무늬 패턴의 사잇각에 따른 미끄럼 마찰특성 평가 (Dependence of Sliding Friction Properties on the Angle of Laser Surface Texturing for a Grooved Crosshatch Pattern Under Grease Lubrication)

  • 공민선;채영훈
    • Tribology and Lubricants
    • /
    • 제38권6호
    • /
    • pp.261-266
    • /
    • 2022
  • Notably, laser surface patterning facilitates tribological applications under lubricated sliding contacts. Consequently, a special pattern that can reduce the coefficient of friction under contact is considered necessary for improved machine efficiency. However, inappropriate pattern designs produce higher friction coefficients and cannot reduce friction. In this study, we use cast iron pins as specimens to investigate their friction and wear characteristics. Moreover, we experimentally investigate the correlation between the friction reduction effect and the design of groove crosshatch patterns fabricated with various angles and widths. We conduct a friction test using a pin-on-disc type tribometer under grease lubrication to study the friction reduction effect of the specimens, and we observe that the average coefficient of friction changes with the crosshatch angle and width. The experiment reveals that grooved crosshatch specimens with a crosshatch angle of 135°maximize friction reduction. The coefficient of friction of the groove specimens with a width of 120 ㎛ is lower than that of the specimens with a width of 200?. The friction reduction effect of the width of the groove is attributed to the density of the groove pattern. Thus, grooved crosshatch patterns can be designed to maximize friction reduction, and the friction property of a grooved crosshatch pattern is found to be related to its width and angle.

에폭시 기지 나노복합재료의 마모 특성 (Wear Properties of Epoxy Matrix Nanocomposites)

  • 김재동;김형진;고성위;김영식
    • 동력기계공학회지
    • /
    • 제14권6호
    • /
    • pp.83-88
    • /
    • 2010
  • The wear behavior of epoxy matrix composites filled with nano sized silica particles is discussed in this paper. Especially, the variation of the coefficient of friction and the wear resistance according to the change of apply load and sliding velocity were investigated for these materials. Wear tests of pin-on-disc mode were carried out and the wear test results exhibited as following ; The epoxy matrix composites showed lower coefficient of friction compared to the neat epoxy through the whole sliding distance. As increasing the sliding velocity the epoxy matrix composites indicated lower coefficient of friction, whereas the neat epoxy showed higher coefficient of friction as increasing the sliding velocity. The specific friction work of both materials were increased with apply load. In case of the epoxy matrix composites, the running in periods of friction were reduced as increase in apply load. The epoxy matrix composites were improved the wear resistance by adding the nano silica particles remarkably. It is expected that the load carrying capacity of the epoxy matrix composites will be improved by increase of Pv factor.

구상흑연주철의 고압하 마멸특성에 미치는 합금원소의 영향 I-Cu, Mn (Effects of Alloying Elements on the High Pressure Wear Characteristics of Ductile Cast Iron I-Cu, Mn)

  • 방웅호;강춘식;박재현;권영각
    • 한국주조공학회지
    • /
    • 제20권4호
    • /
    • pp.230-239
    • /
    • 2000
  • High pressure wear characteristics of DCI(Ductile Cast Iron) were investigated through unlubricated pin-on-disc wear test. Wear test were carried out at speed of 23m/min, under pressure of 3MPa and 3.3 MPa. Cu and/or Mn were added to examine the effect of alloying elements on the high pressure wear characteristics of DCI. To investigate the relationship between wear characteristics and mechanical properties of DCI, Brinell hardness and V-notched Charpy impact energy were tested. Wear surface of each specimen was observed by SEM to determine the wear mechanism of DCI under high pressure wear condition. In the mild wear region, wear characteristics of alloyed DCI specimens were very similar to that of unalloyed DCI. But mild-severe wear transition was occurred at different wear distance and wear rate of DCI specimens were changed by alloying elements. In severe wear condition, wear rate of DCI was dramatically increased by the addition of Mn. Although the addition of Cu 0.46wt% did not decrease the wear rate of DCI in the severe wear region, but it delayed the mild-severe wear transition. Under high pressure wear condition, wear rate and mild-severe wear transition were not concerned with hardness of DCI specimens, but they were deeply associated with impact energy changed by alloying elements.

  • PDF

구상흑연주철의 고압하 마멸특성에 미치는 합금원소의 영향 II-Si, Mo (Effects of Alloying Elements on the High Pressure Wear Characteristics of Ductile Cast Iron II - Silicon and Molybdenum)

  • 방웅호;강춘식;박재현;권영각
    • 한국주조공학회지
    • /
    • 제20권4호
    • /
    • pp.240-246
    • /
    • 2000
  • Surface layer properties such as composition, phase, hardness, and oxide layer condition are very important if the main failure mechanism of metals is wear. Generally, stable and dense oxide layers are known to decrease the wear rate of metals by prohibition of metallic junction occurred between bare metals. Addition of Si above 4 wt% to DCI(Ductile Cast Iron) is reported to enhance the significant oxidation resistance by forming the silicon-rich surface layer which inhibits further oxidation. And addition of up to 2 wt% Mo to high Si ductile iron produces significant increases in high temperature tensile strength, creep strength, thermal fatigue resistance and oxidation resistance. High pressure wear characteristics of unalloyed DCI(Ductile cast Iron), 4.46 wt% Si ductile iron, 4.3 wt% Si-0.52 wt% Mo ductile iron were investigated through unlubricated pin-on-disc wear test. Wear test was carried out at speed of 23m/min, under pressure of 3 MPa and 3.3 MPa. Wear surfaces of each specimen were observed by SEM to determine the wear mechanism under high pressure wear condition. Addition of Si 4.46 wt% severely deteriorated wear property of ductile iron compared to unalloyed DCI. But combined addition of Si 4.3 wt%andMo0.52wt%decreasedthefrictioncoefficient(${\mu}$)ofductileironsandremarkablydelayedthemild-severeweartransition.

  • PDF

연소합성 코팅된 NiAl 금속간화합물의 화학양론이 미끄럼 마모특성에 미치는 영향 (Effects of Stoichiometry on Properties of NiAl Intermetallics coated on Carbon Steel through Combustion Synthesis)

  • 이한영;이재성
    • Tribology and Lubricants
    • /
    • 제36권3호
    • /
    • pp.124-132
    • /
    • 2020
  • The effect of the stoichiometry on the sliding wear properties of NiAl coatings has been investigated. Three different powder mixtures with the compositions of Ni-50at%Al, Ni-54at%Al and Ni-42at%Al were diepressed respectively, and which were subsequently coated on mild steel through combustion synthesis in an induction heating system. Sliding wear behavior of the coatings was examined against an alloyed tool steel using a pin-on-disc type sliding wear test machine. As results, it could be seen that powder mixture(Ni-54at%Al) with displaying Al-rich deviations from the stoichiometry of NiAl(Ni-50at%Al) was promoted the most the synthetic reactivity. The microstructure of the coating layer with the compositions of Ni-54at%Al exhibits the porous NiAl single phase structure. However, the microstructure of the coating layer of the compositions of Ni-42at%Al exhibits the denser multi-phase structure containing several intermediate phases in addition to NiAl. Densification of the coating layer was enhanced by increasing the reacting temperature. On the other hand, the wear properties of the coating layers showed that the wear mode at speeds of around 1 m/s was severe wear, regardless of the stoichiometry and reacting temperature. However, wear properties of coating layer with the compositions of Ni-42at%Al were superior to those of coating layer with the compositions of Ni-54at%Al. This would be attributed by the fact that coating layer with the compositions of Ni-42at%Al develops little void and much intermediate phases with high strength.