Wood Properties of Actinodaphne lancifolia Meisn. (육박나무의 목재성질)

  • 정성호;정두진;박병수;이도식;조성택;서준원
    • Journal of the Korea Furniture Society
    • /
    • v.13 no.2
    • /
    • pp.19-28
    • /
    • 2002
  • This study was carried out to investigate the wood properties for efficient utilization of warm temperate tree species. The tested species were Actinodaphne lancifolia Meisn. grown in Korea. Fundamental wood properties such as anatomical, physical and mechanical properties and chemical components were examined. This species was diffuse porous, straight grained and fine textured wood. The heartwoods of this species was not distinguished clearly to the sapwoods. This species had moderate specific gravity, shrinkage, and mechanical properties. And this species had high content of the extractives by organic solvent.

  • PDF

A Review of tissue changes caused by joint immobilization and classification of contracture (관절고정에 의한 조직변화와 구축의 분류에 대한 고찰)

  • Yoon, Sang-Jib;Lee, Joon-Hee
    • Journal of Korean Physical Therapy Science
    • /
    • v.8 no.1
    • /
    • pp.727-734
    • /
    • 2001
  • Contracture is defined as the lack of full passive range of motion resulting from pint, muscle or soft tissue limitationprolonged Pint immobilization will result in stress and stretch deprivation and gradual development of contracture. the tissue changes caused by immobilization may be categorized as cellular modeling, ground substance and collagen response, and tissue response. contracture can be divided into three categories according to the anatomical location of pathological changes :arthrogenic, myogenic, soft tissue contractures Therapeutic approach of contracture is thermal or cold agents application, stretch or restoration of length, traction, manipulation, mobilization positioning and restoration of function. The purpose of this article is to review current concepts of mechanical properties and synthesis of collagen tissue and the underlying pathomechanics as it relates to evaluation and treatment of contracture.

  • PDF

Characterization of Artificial Graphite Electrodes

  • Park, Sei-Min;Han, Sang-Moo;Oh, Seh-Min
    • Carbon letters
    • /
    • v.1 no.2
    • /
    • pp.76-81
    • /
    • 2000
  • Physical properties of artificial graphite electrodes were evaluated along three different directions; circumferential (X), radial (Y), and axial (Z) directions. Four kinds of commercial electrode products were used in this study for the evaluation; pole (AP) and nipple (AN) of manufacturer A, pole (BP) and nipple (BN) of manufacturer B. The mechanical, electrical, and thermal properties in X and Y directions were very similar to each other. In Z direction, however, the mechanical properties, including flexural strength and compressive strength, were higher, and electric resistance and thermal expansion were much lower than those in the other directions. The microstructures observed by optical microscope and scanning electron microscope revealed that the differences in properties by the measuring direction were caused by the preferential alignment of needle cokes along the Z direction. When comparing the properties of the electrode samples in the same direction, the mechanical properties mainly depended on the bulk density or porosity of the samples as well as preferential alignment of needle cokes.

  • PDF

The Study on the Properties of EPDM/NR Blends (EPDM/NR 블랜드의 물성에 관한 연구)

  • Go, Jin-Hwan;Park, Sung-Soo
    • Elastomers and Composites
    • /
    • v.29 no.2
    • /
    • pp.121-130
    • /
    • 1994
  • The physical properties of rubber blend between natural rubber(NR) and ethylene propylene diene terpolymer(EPDM) were investigated as a study of EPDM composite materials. For EPDM/NR blends, the effects of ethylene and diene contents in EPDM, blend ratio, dicumyl peroxide(DCP) curing system on the physical properties, interfacial adhesion force and dynamic crack growth etc. were studied. EPDM/NR blends loaded with carbon black were prepared by mechanical mixing and cured by plate heating cure press. Crosslinking density was measured by swelling method with toluene. The physical properties of all blends were measured with Instron, fatigue to failure(FTF), Demattia flex cracking tester(DMFC), scanning electron microscopy (SEM), etc. As the ethylene and diene contents in EPDM increased, the physical properties, such as dynamic crack growth, adhesion to other component were increased too. Interfacial adhesion force of EPDM/NR blends to dissimilar layer was improved by the use of optimum peroxide curing system.

  • PDF

Relations between Physical and Mechanical Properties of Core Samples from the Bukpyeong and Pohang Basins (북평분지와 포항분지 시추코어의 물리적 성질과 역학적 성질간의 관계)

  • Kim, Hyunjin;Song, Insun;Chang, Chandong;Lee, Hikweon;Kim, Taehee
    • The Journal of Engineering Geology
    • /
    • v.23 no.4
    • /
    • pp.329-340
    • /
    • 2013
  • A geologic survey of the Bukpyeong and Pohang basins, as candidate basins for the geological storage of $CO_2$, was performed to evaluate storage capacity and security. To analyze the mechanical stability of the storage reservoir and cap rocks, we measured the porosity, seismic velocity, uniaxial strength, internal frictional angle, and Young's modulus of core samples recovered from the two basins. It is costly and sometimes impossible to conduct tests over the entire range of drill holes, and continuous logging data do not yield the mechanical parameters directly. In this study, to derive the mechanical properties of geologic formations from the geophysical logging data, we determined the empirical relations between the physical properties (seismic velocity, porosity, and dynamic modulus) and the mechanical properties (uniaxial strength, internal friction angle) of the core samples. From the comparison with our core test data, the best fits to the two basins were selected from the relations suggested in previous studies. The relations between uniaxial strength, Young's modulus, and porosity of samples from the Bukpyeong and Pohang basins are more consistent with certain rock types than with the locality of the basins. The relations between the physical and mechanical properties were used to estimate the mechanical rock properties of geologic formations from seismic logging data. We expect that the mechanical properties could also be used as input data for a modeling study to understand the mechanical instability of rock formations prior to $CO_2$ injection.

Effect of Transition Metal Oxides Addition on Yttria - stabilized Zirconia for improving Physical and Mechanical Properties

  • Park, Jaesung;Lee, Yeongshin
    • Journal of Korea Society of Digital Industry and Information Management
    • /
    • v.12 no.3
    • /
    • pp.25-31
    • /
    • 2016
  • Mechanical properties of Y2O3-containing tetragonal ZrO2 polycrystals(Y-TZP) were investigated. Several additives were used to modify the hardness and fracture toughness of Y-TZP. The effects of these individual additives were discussed and their interactions were also analysed. Each additive, such as CoO, Fe2O3, MnO2 was found to deteriorate the mechanical properties of Y-TZP when it was used singly. But the fracture toughness of Y-TZP was significantly improved when these additives and Al2O3 were added in combination at a certain ratio. The addition of CoO, Fe2O3 and MnO2 into Y-TZP resulted in the more complex behavior of fracture toughness and hardness. The specimen with 1.5 wt%-Fe2O3, 3.0 wt% -Al2O3 and 1.5 wt%-CoO showed the monoclinic to tetragonal phase ratio of 18% and the highest toughness of $10.8MPa{\cdot}m1/2$ with Vickers hardness of 1201 kgf/mm2. However, the toughness decreased as the ratio increased and macrocracks developed beyond the ratio of 25%. Sample No. 16 is improved high Physical and Mechanical Properties.

Studies on the new manufacturing process and physical, mechanical properties of barkboard (수피(樹皮)보드의 새로운 제조방법(製造方法)과 그 물리기계적(物理機械的) 성질(性質)에 관(關)한 연구(硏究))

  • Lee, Hwa-Hyoung
    • Journal of the Korean Wood Science and Technology
    • /
    • v.17 no.4
    • /
    • pp.26-34
    • /
    • 1989
  • This study was carried out to manufacture bark board from oak bark by new processes and to examine the physical and mechanical properties of the board. This process with no addition of adhesive used higher pressure and temperature than the conventional one and was applied with or without paraformaldehyde. The results are as follows: 1. The new manufacturing process allowed a good bark board with high absorption coefficient. 2. The best manufacturing process for the mechanical properties of bark board was paraformaldehyde 10%-$250^{\circ}C$-100kg/$cm^2$-3 minutes, (bending strength 40kg/$cm^2$, internal bonding strength 2kg/$cm^2$) and the best manufacturing process for both the mechanical properties of bark board and economic point of view was $250^{\circ}C$-100kg/$cm^2$-3 minutes (bending strength 28kg/$cm^2$, internal bonding strength 1.52kg/$cm^2$). 3. Bark board showed specific gravities from 0.94 to 1.03 and air dried moisture content 9.2% to 11.7%, but Bark board needed paraffin wax emusion treatment. 4. The absorption coefficient of bark boards had two peaks along with frequency; one in 200-400 cps, the other 1200-2000 cps. The former was low but the latter great.

  • PDF

Mechanical Properties of Rice Husk Flour-Wood Particleboard by Urea-Formaldehyde Resin

  • Lee, Young-Kyu;Kim, Sumin;Yang, Han-Seung;Kim, Hyun-Joong
    • Journal of the Korean Wood Science and Technology
    • /
    • v.31 no.3
    • /
    • pp.42-49
    • /
    • 2003
  • The objective of this research was to investigate the possibility of using rice husk flour as a partial substitute for the wood particles used as the raw material for manufacturing particleboards, by examining the physical and mechanical properties of the rice husk flour-wood particleboard as a function of the type of urea-formaldehyde resin used. Commercial wood particles and two types of rice husk flours (A type (30 ㎛), B type (300 ㎛)) were used. E1 and E2 class urea-formaldehyde resin was used as the composite binder, combined with 10 wt.% NH4Cl solution as a hardener. Rice husk flour-wood particleboards with dimensions of 27×27×0.7 (cm) were manufactured at a specific gravity of 0.7 with rice husk flour contents of 0, 5, 10, and 15 (wt.%). We examined the physical properties (specific gravity and moisture content), mechanical properties (three point bending strength and internal bonding) of the composite. In general, it can be concluded that composites made from rice husk flours are of somewhat poorer quality than those made from wood; however, blending in small amounts of rice husk flour (e.g., 5% to 10% by weight) may have no significant impact on quality.

Influence of Dilauroyl Peroxide on Mechanical and Thermal Properties of Different Polypropylene Matrices (Dilauroyl Peroxide의 PP에 대한 기계적, 열적 성질 변화)

  • Sirin, Kamil;Yavuz, Mesut;Canli, Murat
    • Polymer(Korea)
    • /
    • v.39 no.2
    • /
    • pp.200-209
    • /
    • 2015
  • In this study, the influence of dilauroyl peroxide on mechanical and thermal properties of different polypropylene (PP) matrices was investigated. Polypropylene matrices, different molecular weight isotactic PP containing 0.01, 0.02, 0.04, 0.06, 0.08, and 0.1 wt% of dilauroyl peroxide (DLP) were prepared by using a single-screw extruder. The effect of the visbreaking agent (DLP) on mechanical, physical, thermal and morphological properties of different molecular weight PP had been studied. Mechanical properties (tensile strength at break point, at yield and elongation at break point), melt flow index (MFI), scanning electron microscope (SEM) and differential scanning calorimetric (DSC) analyses of these matrices were examined. Melting ($T_m$) and crystallization ($T_c$) temperatures, crystallinity ratio (%) and enthalpies were determined. The microstructure of isotactic polypropylene matrix was investigated by scanning electron microscopy (SEM). From SEM analysis, it was observed that the surface disorder increased by the increasing amount of DLP. As a result of DSC analyses, the crystallinity ratio of the PP matrices has varied between 1.64-7.27%. Mechanical properties of the matrices have been improved. Particularly, the mechanical tests of PP have given interesting results when compounded with 0.06-0.08 wt% dilauroyl peroxide (DLP). Mechanical properties and thermal decomposition processes were all changed by increasing the amount of DLP in the matrix structure.

Comprehending Polymer-Clay Nanocomposites and Their Future Works (고분자-점토 나노복합체 이해와 향후 연구 방향)

  • Choi, Yeong Suk;Chung, In Jae
    • Korean Chemical Engineering Research
    • /
    • v.46 no.1
    • /
    • pp.23-36
    • /
    • 2008
  • Polymer-clay nanocomposites, a novel organic-inorganic hybrid, attract much attention from both scientific fields and engineering fields due to their balanced improvements in mechanical properties as well as diffusion behaviors, including flame-retarding and barrier properties, with small amounts of clay. Preparation of polymer-clay nanocomposites, summarized as a process for uniform dispersion of hydrophilic layered clays in hydrophobic polymer matrixes, includes several technologies and scientific phenomena, such as surface-modifications of clay layers, physical properties of clays in liquids and dried states, polymer synthesis, polymer rheology, behaviors of polymer solutions/or monomers in the confined geometry, mechanical properties of polymers and clays. To comprehend complicated physical/chemical phenomena involved in the fabrication of nanocomposites, we reviewed physical properties of clays, structures of clays in nanocomposites, characterization of nanocomposites, the relation between morphology and physical property of nanocomposites, surveyed recent research trends, and then suggested a few strategies or methods for fabrication of nanocomposites reflecting future research directions.