• 제목/요약/키워드: over thickness

검색결과 1,822건 처리시간 0.026초

PREFERRED ORIENTATION OF TIN FILM STUDIED BT A REAL TIME SYNCHROTRON X-RAY SCATTERING

  • Je, J.H.;Noh, D.Y.
    • 한국표면공학회지
    • /
    • 제29권5호
    • /
    • pp.399-406
    • /
    • 1996
  • The orientational cross-over phenomena in an RF sputtering growth of TiN films were studied in an in-situ, real-time synchrotron x-ray scattering experiment. For the films grown with pure Ar sputtering gas, the cross-over from the more strained (002)-oriented grains to the less strained (111)-oriented grains occurred as the film thickness was increased. As the sputtering power was increased, the cross-over thickness, at which the growth orientation changes from the <002> to the <111> direction, was decreased. The addition of $N_2$ besides Ar as sputtering gas suppressed the cross-over, and consequently resulted in the (002) preferred orientation without exhibiting the cross-over. We attribute the observed cross-over phenomena to the competition between the surface and the strain energy. The x-ray powder diffraction, the x-ray reflectivity, and the ex-situ AFM surface topology study consistently suggest that the microscopic growth front was in fact always the (002) planes. In the initial stage of growth, the (002) planes were aligned to the substrate surface to minimize the surface energy. At later stages, however, the (002) growth front tilted away from the surface by about $60^{\circ}$ to relax the strain, which caused the cross-over of the preferred growth direction to the <111> direction.

  • PDF

투명단열 축열벽 시스템의 열성능 평가 실험 연구 (Thermal Performance Evaluation Monitoring Study of Transparent Insulation Wall System)

  • 김병수;윤종호;윤용진;백남춘;이진숙
    • 한국태양에너지학회 논문집
    • /
    • 제23권1호
    • /
    • pp.1-8
    • /
    • 2003
  • Various efforts to combine new high-tech materials with solar system have been progressed nowadays in order to improve the performance of the existing passive solar system. TIM(Transparent Insulation Material) replacing the conventional outer building envelope glazing as well as the wall is good example for this trend. TI integrated wall is a thermal mass wall with a special shaped TIM instead of using typical envelope materials The tested TIM type is a small(diameter 4mm and thickness 50mm) capillary tube of Okalux model and cement brick(density 1500kg/m3). The purpose of this study was to analyze the thermal performance through the actual measurements performed in a test cell. This study was carried out to justify the following issues. 1) the impact of Tl-wall over the temperature variations 2) the impact of mass wall surface absorptance over the transient thermal behavior and 3) the impact of thermal mass wall thickness over the temperature variations. Finally, as results indicated that the peak time of room temperature was shifted about one hour early when absorptance of thermal mass wall changed from 60% to 95% for the 190mm thickness thermal mass wall test case. the temperature difference of both surfaces of thermal mass wall surface showed about $23^{\circ}C$ during a day of March for the 380mm thickness thermal mass wall case. However, the thermal mass wall was over-heated by outside temperature and solar radiation in a day of May the temperature difference of both surfaces of thermal mass wall surface was indicated $10^{\circ}C$ and inside temperature was observed more than average 22C.

Abdominal skin subcutaneous fat thickness over the gestational period in Korean pregnant women: a descriptive observational study

  • Hwang, Moon Sook
    • 여성건강간호학회지
    • /
    • 제27권4호
    • /
    • pp.318-325
    • /
    • 2021
  • Purpose: Although insulin is usually injected into the abdominal subcutaneous fat, in pregnancy women tend to avoid abdominal injections due to concern about fetal damage. Prior studies have been limited to only measuring skin-subcutaneous fat thickness (S-ScFT) at one site at specific pregnancy points. This study aimed to measure S-ScFT across several abdominal sites and over the gestational period in Korean pregnant women. This can identify which site would be relatively safe for subcutaneous injection during pregnancy. Methods: Healthy women over 24 weeks of pregnancy in Korea were invited to voluntarily participate in this descriptive study. For the 142 women, S-ScFT of 12 sites in the abdomen were measured by ultrasound, several times over the pregnancy. Each incidence was treated as a case and a total of 262 cases were analyzed. Results: The mean S-ScFT during pregnancy was 1.14±0.47 cm (1.25±0.54 cm at 24+0-27+6 weeks; 1.17±0.48 cm at 28+0-31+6 weeks; 1.09+0.40 cm at 32+0-35+6 weeks; and 1.06±0.47 cm at 36+0-40 weeks of pregnancy). Most S-ScFT were thicker than 10 mm. But S-ScFTs in the lateral abdomen and some sites were suboptimal (<6 mm), especially in the pre-pregnancy underweight body mass index group, who had a high rate of suboptimal thickness (27.1% overall and 33.9% in the lateral side). Conclusion: The whole abdomen seems to be appropriate for subcutaneous injection in most Korean women during pregnancy, with a 4 to 5-mm short needle. However, for the lateral abdomen, making the skin fold might be needed for fetal safety.

평면 초음파를 이용한 미소 간극 측정 (Thickness Measurement of A Thin Layer Using Plane Ultrasonic waves)

  • 김노유
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1995년도 추계학술대회 논문집
    • /
    • pp.415-418
    • /
    • 1995
  • This paper describes a new technique for thickness measurement of a very thin layer less than one-quarter of the wavelength of ultrasonic wave using ultrasonic pulse-echo method. The technique determines the thickness of a thin layer in a layered medium form the amplitudes of the total reflected waves from the back side layer of interst. Thickness of a very thin layer few inch deep inside the media can be measured without using a very high frequency ultrasonic transducer over 100MHz which must be used in the conventional techniques for the precision measurement of a thin layer. The method also requires no inversion process to extract the thickness from the waveform of the reflected waves, so that it makes possible on-line measurement of the thickness of the layer.

  • PDF

RF 마그네트론 스퍼터링으로 증착한 두께에 따른 PZT 박막의 강유전 특성에 관한 연구 (Thickness dependence of the piezoelectric characteristic for PZT films using by rf magnetron sputtering)

  • 이태용;박영;송준태
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 추계학술대회 논문집 Vol.16
    • /
    • pp.313-316
    • /
    • 2003
  • The lead zirconate titanate, $Pb(Zr_{0:52}Ti_{0:48})O_3$, films of $0.5\;{\mu}m,\;1\;{\mu}m$ and $2\;{\mu}m$ thickness were fabricated on $Pt/Ti/SiO_2/Si$ substrate by the rf magnetron sputtering method. The PZT films were annealed using by a rapid thermal annealing (RTA) method. The thickness dependence of the film structure, dielectric properties, Polarization-electric field hysteresis loops and capacitance-voltage characteristics were investigated over the thickness range of $0.5\;{\mu}m,\;1\;{\mu}m$ and $2\;{\mu}m$. According to the XRD patterns of the films, (110) peak intensity increases with film thickness increased. The increase of PZT films thickness leads to the decrease of the remanent polarization and the dielectric constant.

  • PDF

알루미늄 튜브(A3003, A6061)의 축관률에 따른 두께 변화에 관한 연구 (A study on the thickness change according to the necking ratio of aluminum tube(A3003, A6061))

  • 오종성;민경호;이춘규
    • Design & Manufacturing
    • /
    • 제15권4호
    • /
    • pp.37-42
    • /
    • 2021
  • The tube necking process increases the thickness of the material, and some of the tube necking products require cutting on the inside of the formed product as a post-process. In order to prevent over-cutting or un-cutting due to increased thickness during cutting, it is necessary to know in advance the increase in thickness after forming. Therefore, in this study, the thickness change according to the tube necking was observed. Aluminum 3003-F and 6061-O were used for the materials used in the experiment, and necking was carried out up to 50% of the outer diameter of the tube through five processes. The two materials were formed under the same conditions, and the thickness of three points was observed in each process. In addition, the thickness increase of the two materials was compared, and the trend of thickness increase according to the cumulative necking ratio was observed. As a result of the experiment, both materials had the smallest thickness at the end of the formed product. In addition, as a result of comparing the thickness measurement values of the two materials, the maximum difference was 0.1mm, indicating that there was no difference in thickness between the two materials.

Use of a Barbed Suture Tie-Over Technique for Skin Graft Dressings: A Case Series

  • Joyce, Kenneth M.;Joyce, Cormac W.;Mahon, Nicola;Kelly, Jack L.
    • Archives of Plastic Surgery
    • /
    • 제42권3호
    • /
    • pp.341-345
    • /
    • 2015
  • Background A tie-over dressing is the accepted method to secure skin grafts in order to prevent haematoma or seroma formation. We describe the novel application of a barbed suture tie-over for skin graft dressing. The barbs act as anchors in the skin so constant tensioning of the suture is not required. Methods From January 2014 to August 2014 we used the technique in 30 patients with skin defects requiring split-thickness or full-thickness grafts. Patient demographics, clinicopathological details and graft outcome were collected prospectively. Results The majority of cases were carried out for split-thickness skin grafts (n=19) used on the lower limb (n=20). The results of this novel technique were excellent with complete (100%) graft take in all patients. Conclusions Our results demonstrate the clinical application of a barbed device for securing skin grafts with excellent results. We find the technique quick to perform and the barbed device easy to handle, which can be applied without the need for an assistant.

Investigation on stability characteristics of 2G HTS coated conductor tapes with various stabilizer thickness

  • Quach, Huu Luong;Kim, Ji Hyung;Hyeon, Chang Ju;Chae, Yoon Seok;Moon, Jae Hyung;Kim, Ho Min
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제20권1호
    • /
    • pp.19-22
    • /
    • 2018
  • The thermal and electrical properties of the conductor are critical parametersfor the design and optimization of the superconducting magnet. This paper presents simulation code to analyze electrical and thermal stability characteristics of the second generation (2G) high-temperature superconductor (HTS) by varying copper stabilizer thickness. Two types of commercial 2G HTS coated conductor tapes, YBCO and GdBCO were used in this study. These samples were cooled by Liquid Nitrogen ($LN_2$) having boiling at 77.3 K and an equivalent electrical circuit model for them is choosen and analysed in details. Also, an over-current pulse test in which a current exceeding a critical current was performed. From the simulation results, the influences of the copper stabilizer thickness on the stability characteristics of these samples are presented.

Experimental study on the shear thinning effects of viscosity index improver added lubricant by in-situ optical viscometer

  • Jang, Siyonl
    • Korea-Australia Rheology Journal
    • /
    • 제15권3호
    • /
    • pp.117-124
    • /
    • 2003
  • Elastohydrodynamic lubrication (EHL) film is measured under the condition of viscosity index improver added to base oil. In-situ optical contact method using the interference principle make the measuring resolution of ~5 nm possible and enables the measuring range all over the contact area of up to ~300 $\mu\textrm{m}$ diameter. What is more important to the developed method by the author is that the measurement of EHL film thickness is possible in the range from 100 nm to 2 $\mu\textrm{m}$, which is the regime of worst contact failures in precision machinery. Viscosity index improver (VII) is one of the major additives to the modem multigrade lubricants for the viscosity stability against temperature rise. However, it causes shear thinning effects which make the film thickness lessened very delicately at high shear rate (over $10^5 s^{-1}$) of general EHL contact regime. In order to exactly verify the VIIs performance of viscosity stability at such high shear rate, it is necessary to make the measurement of EHL film thickness down to ~100 nm with fine resolution for the preliminary study of viscosity control. In this work, EHL film thickness of VII added lubricant is measured with the resolution of ~5 nm, which will give very informative design tool for the synthesis of lubricants regarding the matter of load carrying capacity at high shear rate condition.