섬유복합모르터의 뿜칠마감에 의한 고강도콘크리트 기둥부재의 폭렬방지 (Spatting Resistance of High Strength RC Column Covering Spray-on Materials of Fiber Composite Spray Mortar(FCSM))

  • 송용원;한동엽;이건철;고경택;김진수;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2006년도 춘계학술논문 발표대회 제6권1호
    • /
    • pp.5-8
    • /
    • 2006
  • High strength concrete has been increasingly used in high rue building and it is very obvious re consider fire resistance performance of that. Unlike the normal strength concrete, high strength concrete in sudden elevating temperature at fire is susceptible to spalling with severe explosion and surface split, due to high density of concrete. In order to endure the spalling, inner space temperature of concrete should be control less than certain point. Therefore this study investigated the influence of covering materials on high strength concrete finishing spray-on materials of fiber composite spray mortar(FCSM). Both polypropylene(PP) and polyvinyl alcohol(PVA) fiber were used in this test. Test showed that concrete, covering 18mm mortar containing PVA fiber and confining metal lath 2.3mm thickness, decreased 50% of main bar ambient temperature. compared with control concrete. In addition, concrete covering 18mm mortar without fiber caused falling of covering materials and then it was exposed in elevating temperature. As a result, spatting of the concrete occurred same as control concrete. However, concrete covering spray-on mortar containing PVA or PP fiber resisted spatting occurrence.

  • PDF

시멘트계 바탕 바름재용 현무암 석분슬러지 모르타르의 경화 특성 (Hardened properties of the cement based Basalt powder sludge mortar for surface preparation)

  • 장명훈;최희복
    • 한국건축시공학회지
    • /
    • 제15권5호
    • /
    • pp.451-456
    • /
    • 2015
  • 본 연구는 시멘트계 바탕 바름재에 사용되는 바닷모래를 대체하기 위한 재료로서 현무암 가공과정에서 발생되는 현무암 석분슬러지를 재활용하기 위해 현무암 석분슬러지를 사용한 경화모르타르의 특성(연도변화, 응결경화, 흡수계수, 건조수축, 그리고 부착강도 실험)을 평가하였다. 현무암 석분슬러지를 사용한 경화모르타르는 콘크리트 바탕 바름재에 사용되는 기존의 보통모르타르의 특성과 유사하거나 좀 더 향상된 성능을 보였다. 그러나, 현무암 석분슬러지를 사용한 경화모르타르는 보통 모르타르보다 재령 8~9일 이후 건조수축이 증가되었고 부착강도는 감소되었다. 그러나 현무암 석분슬러지를 사용한 경우, KS F 4716 '시멘트계 바탕 바름재'에서 요구하는 최소 품질 규준은 만족하였다.

제지애쉬를 혼입한 모르터의 특성에 관한 실험적 연구 (An Experimental Study on the Properties of Mortar Mixing Paper Ash)

  • 이시우
    • 한국건축시공학회지
    • /
    • 제2권3호
    • /
    • pp.115-121
    • /
    • 2002
  • The purpose of this study is investigating characteristics of paper-ash mortar according to partial replacement of fine aggregate by Paper-ash. For this purpose, selected test variables were mixing ratio with two levels of mortar(1:2, 1:3), and 3 types of paper-ash(A, B, C), and paper-ash content with four levels(5%,, 10%, 15%, 20%). As a result of this study, in all mixes with partial replacement of fine aggregate by Paper-ash generally Produced Paper-ash mortar with decreased compressive strength at ail age as compared to ordinary mixes. The mixing rate 1:2 was the higher increasing rate of strength than the mixing rate 1:3. The flow value and unit weight of paper-ash mortar were decreased with increasing of the paper-ash content. And the thermal conductivity of the thermal conductivity of the paper-ash mortar was lower than normal mixing without paper-ash.

비보강 조적조의 재료특성 평가에 관한 실험연구 (Experimental Study on the Material Properties of Unreinforced Masonry)

  • 박진호
    • 한국지진공학회:학술대회논문집
    • /
    • 한국지진공학회 2000년도 춘계 학술발표회 논문집 Proceedings of EESK Conference-Spring
    • /
    • pp.178-185
    • /
    • 2000
  • A set of tests were accomplished in order to get better insight of the basic material properties of masonry made of normal concrete brick and different type of mortar compositions. Three different types of test were performed. Masonry unit and prism were tested by compressive strength test, Masonry wallets were tested by compressive strength test. Masonry wallets were tested in diagonally under tension. A significant influence of different mortar compositions on compression strength of masonry prism was observed, The tests have shown that for diagonal compression three different mode of failure were possible : tension crack along the loaded diagonal sliding along a mortar joint and combined sliding and diagonal crack according to the adhesive strength of a mortar.

  • PDF

Rubber Mortar의 강도성상에 관한 실험적 연구 (An Experimental Study on the Strength Development of Rubber Mortar)

  • 손종규;김재욱;임유묵;정환욱;문장수;정상진
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1996년도 봄 학술발표회 논문집
    • /
    • pp.30-35
    • /
    • 1996
  • Accumulations of worn-out automobile tires creat fire and health hazards. As a possible solution to the problem of scrap-tire disposal, an experimental study was conducted to examine the potential of using tire chips as aggregate in rubber mortar. This paper examines strength and toughness properties of rubber mortar in which different amounts of rubber-tire particles of several sizes were used as aggregate. The rubber mortar mixtures exhibited lower compressive, bending, tensile than did normal mortar. However, these mixtures did not demonstrate brittle failure, but rather a ductile, plastic failure, and had the ability to absorb a large amount of plastic energy under compressive loads.

  • PDF

현무암석분 슬러지를 재활용한 드라이몰탈의 기초적 성능평가 (Basic Performance Evaluation of Dry Mortar Recycled Basalt Powder Sludge)

  • 고동우;최희복
    • 한국건축시공학회지
    • /
    • 제13권2호
    • /
    • pp.131-138
    • /
    • 2013
  • 본 연구는 최근 제주도 지역에서 현무암 가공과정에서 발생되는 폐기물인 석분슬러지를 재활용하기 위한 방안으로써 일반 시멘트몰탈에 사용되는 잔골재 대신에 현무암 석분슬러지의적용가능성에 대해 실험하였다. 드라이 몰탈의 재료로서의 기초적인 성능을 평가하기 위해 압축강도와 휨강도를 평가하고, SEM을 통해 미세구조를 관찰하였다. 현무암 슬러지 대체율 21%까지는 압축 및 휨강도는 증가하였으며, 보통 드라이몰탈보다 약 40% 강도 증진 효과가 있다. 현무암 슬러지의 대체율 약 20%이상에서는 상대적으로 수화생성물이 적게 생성되었다. 본 연구를 통해 현무암 슬러지 폐기물의 활용성을 확인할 수 있었으며, 콘크리트 2차 제품의 성형에도 가능할 것으로 판단된다.

폐 소나무 수피로부터 콘크리트 혼화제의 제조(II) - 소나무 수피 ASAQ증해 폐액의 표준형 및 촉진형 콘크리트 혼화제로의 전환 - (Preparation of Concrete Admixtures from Pine Bark Wasts(II) -Conversion of Spent Liquor Obtained from Alkaline Sulfite- Anthraquinone(ASAQ) Cooking of Pine Bark Waste to Normal and Accelerating Concrete Admixtures-)

  • 박성천;문성필;문소현;소양섭
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1998년도 봄 학술발표회논문집(II)
    • /
    • pp.747-750
    • /
    • 1998
  • The application of spent liquor(BSL) obtained from alkaline sulfite-anthraquinone cooking of pine bark to cement mortar significantly improved the water-reducing ability and decreased the rate of cement hardening. However, the compressive and flexural strength of BSL addition to cement mortar were lower than that of PLAIN. The application of 0.2% antifoamer to BSL slightly decreased water-reducing ability, but remarkably improved the compressive and flexural strength of cement mortar. On the other hand, BSL decreased the rate of hardening of cement, which exhibited the protperties of the lignosulfonated based retarding water-reducing type. but the setting time of cement could be controlled by addition of Na2CO3 could be used to convert BSL to normal or accelerating concrete admixtures.

  • PDF

Determination of mortar strength using stone dust as a partially replaced material for cement and sand

  • Muhit, Imrose B.;Raihan, Muhammad T.;Nuruzzaman, Md.
    • Advances in concrete construction
    • /
    • 제2권4호
    • /
    • pp.249-259
    • /
    • 2014
  • Mortar is a masonry product which is matrix of concrete. It consists of binder and fine aggregate and moreover, it is an essential associate in any reinforced structural construction. The strength of mortar is a special concern to the engineer because mortar is responsible to give protection in the outer part of the structure as well as at a brick joint in masonry wall system. The purpose of this research is to investigate the compressive strength and tensile strength of mortar, which are important mechanical properties, by replacing the cement and sand by stone dust. Moreover, to minimize the increasing demand of cement and sand, checking of appropriateness of stone dust as a construction material is necessary to ensure both solid waste minimization and recovery by exchanging stone dust with cement and sand. Stone dust passing by No. 200 sieve, is used as cement replacing material and retained by No. 100 sieve is used for sand replacement. Sand was replaced by stone dust of 15%, 20%, 25%, 30%, 35%, 40%, 45% and 50% by weight of sand while cement was replaced by stone dust of 3%, 5%, and 7% by weight of cement. Test result indicates that, compressive strength of specimen mix with 35% of sand replacing stone dust and 3% of cement replacing stone dust increases 21.33% and 22.76% respectively than the normal mortar specimen at 7 and 28 days while for tensile it increases up to 13.47%. At the end, optimum dose was selected and crack analysis as well as discussion also included.

High temperature resistance of self-compacting lightweight mortar incorporating expanded perlite and pumice

  • Karatas, Mehmet;Balun, Bilal;Benli, Ahmet
    • Computers and Concrete
    • /
    • 제19권2호
    • /
    • pp.121-126
    • /
    • 2017
  • This paper presents the effect of aggregate type on high temperature resistance of self-compacting mortars (SCM) produced with normal and lightweight aggregates like expanded perlite and pumice. Silica fume (SF) and fly ash (FA) were used as mineral additives. Totally 13 different mixtures were designed according to the aggregate rates. Mini slump flow, mini V-funnel and viscometer tests were carried out on the fresh mortar. On the other hand, bulk density, porosity, water absorption and high temperature tests were made on the hardened SCM. After being heated to temperatures of 300, 600 and $900^{\circ}C$, respectively, the tensile strength in bending and compressive strength of mortars determined. As a result of the experiments, the increase in the use of lightweight aggregate increased total water absorption and porosity of mortars. It is observed that, the increment in the usage of lightweight aggregate decreased tensile strength in bending and compressive strengths of mortar specimens exposed to high temperatures but the usage of up to 10% expanded perlite in mortar increased the compressive strength of specimens exposed to $300^{\circ}C$.

폴리프로필렌 및 비닐론 섬유를 혼입한 고강도콘크리트의 내화특성 (Fire Resistance of High Strength Concrete with Polypropylene and Vinylon Fiber)

  • 남지현;오상균;김정길
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2005년도 춘계 학술기술논문발표대회 논문집
    • /
    • pp.165-169
    • /
    • 2005
  • The fire damage of building wouid effect on the safety of structure. When the reinforced concrete structure is heated by high temperature due to the fire, the structural resisting-force will be decreased. In a way, it is a requirement to use high strength concrete for high rise building. Particularly, fire resistance properties of high-strength concrete is more important than normal strength concretes. The fire outbreak of a high strength concrete by sudden temperature rise is a main problem, and causes crack by thermal stress, loading to the deterioration of the durability. In this study, normal and high strength mortar were exposed to a high temperature environment. And than fundamental data for the character change of concrete heated highly were presented by measuring compressive strength of concrete with polypropylene and vinylon fiber, before and after heating. As the results, it is proven that high strength mortar with polypropylene and vinylon fiber for prevents deterioration of durability by fiber.

  • PDF