GRAVINA, Marco A;QUINTAO, Catia A;KOO, Daniel;ELIAS, Carlos N
The korean journal of orthodontics
/
v.33
no.6
s.101
/
pp.465-474
/
2003
The great variety of commercial brands of orthodontic wires available on the market, stimulated by the so called superior wires (nickel titanium with shape memory effect and superelastic nickel titanium), makes the professional choice for a suitable and less expensive material difficult. The in vitro study of the mechanical properties of the orthodontic wires acts as an auxiliary tool for the professional. In this paper, a comparative study of mechanical properties was made, using stress strain tests for 4 types of orthodontic wires (conventional stainless steel, multistranded steel, superelastic nickel titanium and thermoactivated nickel titanium) separated into 5 groups. A series of 6 tests were tested for each group of wires. Initially, each group was tested 3 times until the wires broke. Furthermore, 3 more tests for each group were performed, stretching the wires under standardized activation loads, for a reliable comparison of their mechanical properties, during loading and unloading. 1 tests were applied to check differences among the groups. In vitro, the results suggest that regarding the mechanical properties supposedly desirable for physiological teeth movement, such as resilience, elasticity modulus, strength liberated during unloading, and the way that strength is liberated, thermoactivated nickel titanium wires, acting under mouth temperature, seems to be a good choice, fellowed by superelastic nickel titanium, multistranded stainless steel, and conventional stainless sleet. Superelasticity was demonstrated for superelastic nickel titanium wires. When at $37^{\circ}C$, thermoactivated nickel titanium wires showed shape memory effect, showing that temperature is important for enhancing the mechanical properties.
Objective: Nickel-titanium alloy wire possesses excellent spring-back properties, shape memory and super-elasticity. In order to adapt this wire to clinical use, it is necessary to bend as well as to control its super-elastic force. The purpose of this study is to evaluate the effects of heat treatment on the load-deflection properties and transitional temperature range (TTR) of nickel-titanium wires. Methods: Nickel-titanium wires of different diameters ($0.016"\;{\times}\;0.022"$, $0.018"\;{\times}\;0.025"$ and $0.0215"\;{\times}\;0.028"$) were used. The samples were divided into 4 groups as follows: group 4, posterior segment of archwire (24 mm) without heat treatment; group 2, posterior segment of archwire (24 mm) with heat treatment only; group 3, anterior segment with bending and heat treatment; group 4, anterior segment with bending and 1 sec over heat treatment. Three point bending test was used to evaluate the change in load-deflection curve and obtained DSC (different scanning calorimetry) to check changes in $A_f$ temperature. Results: In the three point bending test, nickel-titanium wires with heat treatment only had higher load-deflection curve and loading and unloading plateau than nickel-titanium wires without heat treatment. Nickel-titanium wires with heat treatment had lower Af temperature than nickel-titanium wires without heat treatment. Nickel-titanium wires with heat treatment and bending had higher load-deflection curve than nickel- titanium wires with heat treatment and nickel-titanium wires without heat treatment. Nickel-titanium with heat treatment of over 1 sec and bending had the highest load-deflection curve. Nickel-titanium wires with heat treatment and bending had lower Af temperature, Nickel-titanium wires with heat treatment of over Af sec and bending had the lowest Af temperature. Conclusion: From the results of this study, it can be stated that heat treatment for bending of Nickel-titanium wires does not deprive the superelastic property but can cause increased force magnitude due to a higher load-deflection curve.
Objective: To compare the effectiveness of laser-engineered copper-nickel titanium (SmartArch) and superelastic nickel-titanium (SENT) archwires in aligning teeth and inducing root resorption and pain experienced by patients. Methods: Two-arm parallel groups with a 1:1 allocation ratio were used. The participants were patients aged 11.5 years and older with 5-9 mm of mandibular anterior crowding who were indicated for non-extraction treatment. The primary outcome was alignment effectiveness, assessed using Little's irregularity index (LII) over 16 weeks with a single wire (0.016-inch) in the SmartArch group and 2 wires (0.014- and 0.018-inch) in the SENT group (8 weeks each). Secondary outcomes included root resorption evaluated by pre- and post-intervention periapical radiographs and pain levels recorded by the participants during the first week. Results: A total of 40 participants were randomly allocated into 2 groups; 33 completed the study and were analyzed (16 in the SmartArch group and 17 in the SENT group, aged 16.97 ± 4.05 years). The total LII decrease for the SmartArch and SENT groups was 5.63 mm and 5.29 mm, respectively, which was neither statistically nor clinically significant. Root resorption was not significantly different between the groups. The difference in pain levels was not statistically significant for the first 5 days following wire placement; however, there was a significant difference favoring the SENT group in the final 2 days. Conclusions: SmartArch and SENT archwires were similarly effective during the alignment phase of orthodontic treatment. Root resorption should be observed throughout the treatment with either wire. SmartArch wires demonstrated higher pain perception than SENT wires.
The purpose of this study was to investigate the change of mechanical properties, surface topography and frictional force of various nickel titanium wires after recycling. Three types of nickel-titanium wires and one type of stainless steel wire were divided to three groups: as-received condition(T0:control group), treated in artificial saliva for four weeks(T1) and autoclaved after being treated in artificial saliva(T2). Some changes were observed for the selected mechanical properties in tensile test, surface topography by means of SEM and 3D profilogram, and frictional coefficient. The findings suggest that: 1. Nickel-titanium wires demonstrated no statistically significant differences in maximum tensile strength, elongation rate and modulus of elasticity, but stainless steel wire demonstrated statistically significant differences in maximum tensile strength, elongation rate and modulus of elasticity between the groups(p<0.05). 2. NiTi, Optimalloy, Stainless Steel wires demonstrated increased pitting and corrosion in SEM finding. 3. Recycled NiTi, Optimalloy and stainless steel wires demonstrated significantly greater surface roughness(Ra and Rq) through 3D profilogram when compared with the control wires(p<0.05), but Sentalloy didn't demonstrate significant difference. 4. Recycled NiTi, Optimalloy and stainless steel wires demonstrated significantly greater maximum frictional coefficient when compared with the control wires(p<0.05), but Sentalloy didn't demonstrate significant difference The changes of surface roughness and frictional coefficient in NiTi and Optimalloy had no clinical implication. Consequently recycled nickel titanium wires demonstrated no clinical problem in tensile properties, surface topography and frictional coefficient.
Objective: The purpose of this study was to compare changes in frictional resistance between the bracket and wire under dry and wet conditions according to a change in moment. Methods: A stainless steel bracket of $0.022"{\times}0.028"$ slot, and $0.019"{\times}0.025"$ stainless steel, beta-titanium, and nickel-titanium wires were used. A 10 mm length lever was attached to the test (sliding) brackets to generate a moment. The experimental model was designed to allow tipping until contacts were established between the wire and the mesiodistal edges of the bracket slot. The moment was generated by suspending a 100 g or 200 g weight on the end of the lever. The moments applied were $1000g{\cdot}mm\;(100g{\times}10mm)\;and\;2000g{\cdot}mm\;(200g{\times}10mm)$. The test brackets were ligated with elastomeric ligature for a constant ligation force and the fixed brackets were ligated with stainless steel ligature. Brackets were moved along the wire by means of an universal testing machine, and maximum frictional resistances were recorded. Results: Stainless steel wire showed least frictional resistance and there was no significant difference between beta-titanium and nickel-titanium except at $2000g{\cdot}mm$ moment in wet conditions. Frictional resistance of all wires increased as the moment increased from $1000g{\cdot}mm\;to\;2000g{\cdot}mm$. Under wet conditions, the frictional resistance of stainless steel wires increased in both $1000g{\cdot}mm\;and\;2000g{\cdot}mm$ moment conditions, but frictional resistance of nickel-titanium and beta-titanium increased only in $2000g{\cdot}mm$ conditions. Conclusion: These results indicated that various conditions influence on frictional resistance. Therefore, laboratory studies of frictional resistance should simulate clinical situation.
Objective: The aim of this trial was to compare the alignment efficiency and intermaxillary arch dimension changes of nickel-titanium (NiTi) or copper-nickel-titanium (CuNiTi) round archwires with increasing diameters applied sequentially to the mandibular arch. Methods: The initial alignment phase of fixed orthodontic treatment with NiTi or CuNiTi round archwires was studied in a randomly allocated sample of 66 patients. The NiTi group comprised 26 women, 10 men, and the CuNiTi ($27^{\circ}C$) group comprised 20 women, 10 men. The eligibility criteria were as follows: anterior mandibular crowding of minimum 6 mm according to Little's Irregularity Index (LII), treatment requiring no extraction of premolars, 12 to 18 years of age, permanent dentition, skeletal and dental Class I malocclusion. The main outcome measure was the alignment of the mandibular anterior dentition; the secondary outcome measure was the change in mandibular dental arch dimensions during 12 weeks. Simple randomization (allocation ratio 1:1) was used in this single-blind study. LII and mandibular arch dimensions were measured on three-dimensional digital dental models at 2-week intervals. Results: No statistically significant difference was observed between NiTi and CuNiTi according to LII (p > 0.05). Intercanine and intermolar arch perimeters increased in the CuNiTi group (p < 0.001). Inter-first premolar width showed a statistically significant interaction in week ${\times}$ diameter ${\times}$ application (p < 0.05). Conclusions: The effects of NiTi and CuNiTi round archwires were similar in terms of their alignment efficiency. However, the intercanine and intermolar arch perimeters, and the inter-first premolar width changes differed between groups.
Jung, Jong Moon;Wi, Young Joo;Koo, Hyun Mo;Kim, Min Ji;Chun, Youn Sic
The korean journal of orthodontics
/
v.47
no.4
/
pp.268-274
/
2017
The purpose of this article is to introduce a simple appliance that uses a setup model and a nickel-titanium (Ni-Ti) wire for correcting the mesial rotation and drift of the permanent maxillary first molar. The technique involves bonding a Ni-Ti wire to the proper position of the target tooth on a setup model, followed by the fabrication of the transfer cap for indirect bonding and its transfer to the patient's teeth. This appliance causes less discomfort and provides better oral hygiene for the patients than do conventional appliances such as the bracket, pendulum, and distal jet. The treatment time is also shorter with the new appliance than with full-fixed appliances. Moreover, the applicability of the new appliance can be expanded to many cases by using screws or splinting with adjacent teeth to improve anchorage.
Objective: To evaluate the therapeutic effects of a preformed assembly of nickel-titanium (NiTi) and stainless steel (SS) archwires (preformed C-wire) combined with temporary skeletal anchorage devices (TSADs) as the sole source of anchorage and to compare these effects with those of a SS version of C-wire (conventional C-wire) for en-masse retraction. Methods: Thirty-one adult female patients with skeletal Class I or II dentoalveolar protrusion, mild-to-moderate anterior crowding (3.0-6.0 mm), and stable Class I posterior occlusion were divided into conventional (n = 15) and preformed (n = 16) C-wire groups. All subjects underwent first premolar extractions and en-masse retraction with preadjusted edgewise anterior brackets, the assigned C-wire, and maxillary C-tubes or C-implants; bonded mesh-tube appliances were used in the mandibular dentition. Differences in pretreatment and post-retraction measurements of skeletal, dental, and soft-tissue cephalometric variables were statistically analyzed. Results: Both groups showed full retraction of the maxillary anterior teeth by controlled tipping and space closure without altered posterior occlusion. However, the preformed C-wire group had a shorter retraction period (by 3.2 months). Furthermore, the maxillary molars in this group showed no significant mesialization, mesial tipping, or extrusion; some mesialization and mesial tipping occurred in the conventional C-wire group. Conclusions: Preformed C-wires combined with maxillary TSADs enable simultaneous leveling and space closure from the beginning of the treatment without maxillary posterior bonding. This allows for faster treatment of dentoalveolar protrusion without unwanted side effects, when compared with conventional C-wire, evidencing its clinical expediency.
The purpose of this study is to investigate the changes of mechanical properties and surface topography of various nickel titanium wires after heat sterilization for recycling with quantitative method. The materials used were four kinds of nickel titanium orthodontic wires including a Korean product. Experimental specimens were treated with two kinds of heat sterilization methods ; dry heat ($180^{\circ}C$, 60min) and autoclave ($121^{\circ}C$, 15-20psi, 30min). Mechanical properties were evaluated by tensile test with Instron 4466 (load cell capacity:.1000 kg, cross head speed:5mm/min, grip distince:40mm in room temperature). Surface topography of various wires was compared with each other qualitatively by using scanning electron microscopy and quantitatively by using profilometer. The findings were analyzed statistically with student t-tests. The results were as follows; 1. Neither method of heat sterilization had any effects on tensile properties of the nickel-titanium wires used in this experiment. 2. Before heat sterilization, the surface smoothness was highest in Optimalloy, followed by Align and Sentalloy, with NiTi showing the lowest smoothness value. 3. In surface topography, Align and Optimalloy were not influenced by heat sterilization. NiTi, on the other hand, had increased roughness after dry heat sterilization and Sentalloy showed the same tendency after each of the two heat sterilization procedures.
Objectives: It was aimed to compare the cyclic fatigue resistances of ProTaper Universal (PTU), ProTaper Next (PTN), and ProTaper Gold (PTG) and the effects of sterilization by autoclave on the cyclic fatigue life of nickel-titanium (NiTi) instruments. Materials and Methods: Eighty PTU, 80 PTN, and 80 PTG were included to the present study. Files were tested in a simulated canal. Each brand of the NiTi files were divided into 4 subgroups: group 1, as received condition; group 2, pre-sterilized instruments exposed to 10 times sterilization by autoclave; group 3, instruments tested were sterilized after being exposed to 25%, 50%, and 75% of the mean cycles to failure, then cycled fatigue test was performed; group 4, instruments exposed to the same experiment with group 3 without sterilization. The number of cycles to failure (NCF) was calculated. The data was statistically analyzed by using one-way analysis of variance and post hoc Tukey tests. Results: PTG showed significantly higher NCF than PTU and PTN in group 1 (p < 0.05). Sterilization significantly increased the NCF of PTN and PTG (p < 0.05) in group 2. PTN in group 3 had significantly higher cyclic fatigue resistance than PTN group 4 (p < 0.05). Also, significantly higher NCF was observed for PTG in group 2 than in groups 3 and 4 (p < 0.05). Conclusions: PTG instrument made of new gold alloy was more resistant to fatigue failure than PTN and PTU. Autoclaving increased the cyclic fatigue resistances of PTN and PTG.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.