• 제목/요약/키워드: nanoindentation

검색결과 216건 처리시간 0.024초

응력완화 경로분석과 압입자/시편간 접촉형상 모델링에 바탕한 박막재료의 국소 잔류응력 평가 (Evaluation of Thin Film Residual Stress through the Analysis of Stress Relaxation Path and the Modeling of Contact Morphology)

  • 이윤희;김성훈;장재일;권동일
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2001년도 춘계학술대회논문집A
    • /
    • pp.237-242
    • /
    • 2001
  • Residual stress is a dominant obstacle to efficient production and safe usage of products by reducing the mechanical strength and failure properties. Especially, it causes interfacial failure and substrate deflection in the case of thin film. So, the exact evaluation and optimum control of thin film residual stress is indispensable. However, hole drilling or X-ray diffraction techniques have some limits in application to thin film. And, curvature technique for thin film materials cannot give the information about local stress variation. Therefore, we applied the nanoindentation technique in evaluating the thin film residual stress. In this study, we modeled the change of indentation loading curve for residually stressed and stress-free thin films during stress relaxation. The value of residual stress was directly related to the indentation depth change by relaxation. The residual stress from nanoindentation analysis was consistent with the result from curvature technique.

  • PDF

수소주입시킨 680MPa DP강의 나노인덴터 시험 (Nanoindenter Test of 680MPa Dual Phase Steel Charged with Hydrogen)

  • 최종운;박재우;강계명
    • 한국표면공학회지
    • /
    • 제47권1호
    • /
    • pp.33-38
    • /
    • 2014
  • Nanoindentater tests were conducted to conducted nanoindentation microhardness of the individual phase of ferrite and martensite of 680MPa dual-phase (DP) steel charged with hydrogen. Hydrogen was charged by electrochemical method with current densities of 150, $200mA/cm^2$ for charging times of 5, 10, 25, 50 hours, respectively. Nanoindenter test results showed that the nanoindentation microhardnesses of ferrite phase of DP steel were varied from min. 1.58 GPa to max. 2.82 GPa, and the nanoindentation microhardnesses of martensite phase varied from min. 3.19 GPa to max. 5.16 GPa with the variation of hydrogen charging conditions. It was observed that the variations of the nanoindention microhardnesses of martenstie phase were higher than those of ferrite phases. It was thought that martensite phase in the 680MPa DP steel was more sensitive than ferrite phase to hydrogen embrittlement.

나노인덴테이션 해석을 통한 Ag/Cu층에서 발생하는 Misfit 전위의 slip 특성에 대한 연구 (Nanoindentation on the Layered Ag/Cu for Investigating Slip of Misfit Dislocation)

  • 트란딘 롱;유용문;전성식
    • Composites Research
    • /
    • 제24권3호
    • /
    • pp.17-24
    • /
    • 2011
  • Ag/Cu층에서 발생하는 misfit 전위를 분석하기 위하여, EAM기법을 활용한 나노인덴테이션 해석을 수행하였다. N$\'{o}$se-Hoover 서모스텟 조건에 의거하여, 2-5nm 정도의 두께를 갖는 필름층에 구형 인덴터로 압입하였다. 해석결과는 misfit 전위에 대한 상대적인 압입위치가, 4nm이하의 필름에 대하여 영향을 미치는 것으로 나타났다. 전위에 의한 슬립 발생할 때 탄성에너지 변화는 Ag/Cu의 연화의 중요한 변수로 작용하며, 각각의 경우에 대하여 임계필름두께에 대해서도 고찰하였다.

나노인덴테이션과 주사탐침현미경을 이용한 박막 재료의 특성평가 (Characterization of Thin Film Materials by Nanoindentation and Scanning Probe Microscopy)

  • 김봉섭;윤존도;김종국
    • 한국재료학회지
    • /
    • 제13권9호
    • /
    • pp.606-612
    • /
    • 2003
  • Surface and mechanical properties of thin films with submicron thickness was characterized by nanoindentation with Berkovich and Vickers tips, and scanning probe microscopy. Nanoindention was made in a depth range of 15 to 200 nm from the surface by applying tiny force in a range from 150 to $9,000 \mu$N. Stiffness, contact area, hardness, and elastic modulus were determined from the force-displacement curve obtained. Reliability was first tested by using fused quartz, a standard sample. Elastic modulus and hardness values of fused quartz measured were the same as those reported in the literature within two percent of error. Mechanical properties of ITO thin film were characterized in a depth range of 15∼200nm. As indentation depth increased, elastic modulus and hardness decreased by substrate effect. Ion beam deposited DLC thin films were indented in a depth range of 40∼50 nm. The results showed that the DLC thin film using benzene and bias voltage 0∼-50 V has elastic modulus and hardness value of 132 and 18 GPa respectively. Pure DLC thin films showed roughnesses lower than 0.25 nm, but silicon-added DLC thin films showed much higher roughness values, and the wavy surface morphology.

나노인덴테이션에 의한 Al-Si-Cu-Mg 합금 폼 셀 벽의 기계적 물성 연구 (A Nanoindentation Based Study of Mechanical Properties of Al-Si-Cu-Mg Alloy Foam Cell Wall)

  • 하산;김엄기;이창훈;이학주;고순규;조성석
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2004년도 춘계학술대회
    • /
    • pp.382-387
    • /
    • 2004
  • Nanoindentation technique has been used to measure the mechanical properties of aluminium alloy foam cell walls. Al-Si-Cu-Mg alloy foams of different compositions and different cell morphologies were produced using powder metallurgical method. Cell morphology of the foam was controlled during production by varying foaming time and temperature. Mechanical properties such as hardness and Young's modulus were calculated using two different methods: a continuous stiffness measurement (CSM) and an unloading stiffness measurement (USM) method. Experimental results showed that hardness and Young's modulus of Al-5%(wt.)Si-4%Cu-4%Mg (544 alloy) precursor and foam walls are higher than those of Al-3%Si-2%Cu-2%Mg (322 alloy) precursor and foam walls. It was noticed that mechanical properties of cell wall are different from those of precursor materials.

  • PDF

Application of a Dynamic-Nanoindentation Method to Analyze the Local Structure of an Fe-18 at.% Gd Cast Alloy

  • Choi, Yong;Baik, Youl;Moon, Byung M.;Sohn, Dong-Seong
    • Nuclear Engineering and Technology
    • /
    • 제49권3호
    • /
    • pp.576-580
    • /
    • 2017
  • A dynamic nanoindentation method was applied to study an Fe-18 at.% Gd alloy as a neutron-absorbing material prepared by vacuum arc-melting and cast in a mold. The Fe-18 at.% Gd cast alloy had a microstructure with matrix phases and an Fe-rich primary dendrite of $Fe_9Gd$. Rietveld refinement of the X-ray spectra showed that the Fe-18 at.% Gd cast alloy consisted of 35.84 at.% $Fe_3Gd$, 6.58 at.% $Fe_5Gd$, 16.22 at.% $Fe_9Gd$, 1.87 at.% $Fe_2Gd$, and 39.49 at.% ${\beta}-Fe_{17}Gd_2$. The average nanohardness of the primary dendrite phase and the matrix phases were 8.7 GPa and 9.3 GPa, respectively. The fatigue limit of the matrix phase was approximately 37% higher than that of the primary dendrite phase. The dynamic nanoindentation method is useful for identifying local phases and for analyzing local mechanical properties.

Ag 필름/ Cu기판의 나노인덴테이션 거동 해석 (Nanoindentation behaviours of silver film/copper substrate)

  • 트란딘롱;김엄기;전성식
    • Composites Research
    • /
    • 제22권3호
    • /
    • pp.9-17
    • /
    • 2009
  • 본 논문에서는 분자동력학 방법을 이용하여 Ag 필름/Cu기판에 대한 나노인덴테이션 특성을 파악하였다. 필름의 강성과 경도는 필름의 두께에 관계되어있으며, 임계범위 내에서, 그래인 크기가 증기하면 강성과 경도도 증가하는 것을 확인하였다. 5nm 두께 이하의 Ag필름/Cu기판의 강성과 경도는 벌크 Ag의 경우에 비해 낮은 값을 나타내었다. 특히 4nm 두께 이하의 Ag필름/Cu기판의 인덴테이션에 있어서, 전위 집적과 불일치 전위사이의 상호작용에 의해 계면상에서 꽃모양의 전위 루프가 발생 하였다. 이는 인덴테이션 하중과 변위 커브에서 하중이 저하되는 것과 관계있는 것으로 사료되고 있다.

듀티 싸이클 및 펄스 주파수가 TiAlN 코팅막의 미세구조와 기계적 특성에 미치는 영향에 관한 연구 (Effects of Duty Cycle and Pulse Frequency on the Microstructure and Mechanical Properties of TiAlN Coatings)

  • 전성용;황주연
    • 한국세라믹학회지
    • /
    • 제51권5호
    • /
    • pp.447-452
    • /
    • 2014
  • This paper presents the effects of pulse plasma parameters such as duty cycle and pulse frequency on the properties of TiAlN coatings deposited by asymmetric bipolar pulsed DC magnetron sputtering systems. The results show that, with decreasing duty cycle and increasing pulse frequency, the coating morphology changes from a columnar structure to a dense structure with finer grains. Pulsed sputtered TiAlN coatings showed higher hardness, higher residual stress, and smaller grain sizes than did DC prepared TiAlN coatings. Moreover, residual stress and nanoindentation hardness of pulsed sputtered TiAlN coatings increased with increasing pulse frequency. Meanwhile, the surface roughness decreased continuously with increasing pulsed DC frequency up to 50 kHz.

Understanding the role of hydrogen on creep behaviour of Zircaloy-4 cladding tubes using nanoindentation

  • Suman, Siddharth
    • Nuclear Engineering and Technology
    • /
    • 제52권9호
    • /
    • pp.2041-2046
    • /
    • 2020
  • The present article investigates the influence of hydrogen concentration on the creep performance of cold-worked stress-relieved unirradiated Zircaloy-4 cladding tube using nanoindentation technique. The as-received Zircaloy-4 tube is hydrided to the concentrations of 600 ppm and 900 ppm using gaseous hydrogen charging method. Constant load indentation creep tests are performed for a dwell period of 600 s in the temperature range of 300℃-500 ℃ at 1000 μN, 2000 μN, and 3000 μN. The impact of hydrogen is evaluated in terms of steady state power law creep exponent and activation energy. The power law creep exponent decreases with increase in hydrogen concentration, however, it remains fairly constant with increase in temperature up to 500 ℃. Moreover, activation energy too decreases significantly with increase in hydrogen concentration. The mean stress exponent and activation energy are found to be 3.58 and 28.67 kJ/mol, respectively, for as-received sample.