A Study on CdS Deposition using Sputtering (Sputtering을 이용한 CdS 증착에 관한 연구)

  • Lee, Dal-Ho;Park, Jung-Cheul
    • The Journal of Korea Institute of Information, Electronics, and Communication Technology
    • /
    • v.13 no.4
    • /
    • pp.293-297
    • /
    • 2020
  • This paper tried to find the best conditions that could be applied to solar cells by deposition of CdS thin film on ITO glass using multiplex displacement sputter system. RF power was changed to 50W, 100W, and 150W and sputtering time was set to 10 minutes. As a result of the measurement of transmittance, the average transmittance in the area of 400 to 800 nm was measured from 60% to 80% and the best characteristic was measured at 150W at 84%. The band gap was also measured at 3.762eV at 50W, 4.037eV at 100W and 4.052eV at 150W. In XRD analysis, even as RF power was increased, it was observed as a structure called Wurtzite (hexagonal) of CdS. And as RF power increased, the particles were large and uniformly deposited, but at 100W the particles were densely composed and dense. And the thickness measurement showed that the RF power increased uniformly.

A Study on the Characteristics of CdS Thin Film by Annealing Time Change (열처리시간 변화에 의한 CdS 박막 특성에 관한연구)

  • Chung, Jae-Pil;Park, Jung-cheul
    • The Journal of Korea Institute of Information, Electronics, and Communication Technology
    • /
    • v.14 no.5
    • /
    • pp.438-443
    • /
    • 2021
  • This paper uses a multiplex deposition sputter system and aims to improve transmittance and reduce production costs by depositing a CdS thin film on an ITO glass substrate. When manufacturing CdS thin films, we wanted to find excellent conditions when manufacturing solar cells by changing heat treatment time. It was observed that thickness and sheet resistance were not significantly different depending on heat treatment time changes. The specific resistance was measured from a minimum of 6.68 to a maximum of 6.98. When the heat treatment time was more than 20 minutes, the transmittance was measured to be more than 75%. When the heat treatment time was 10 minutes, the bandgap was 3.665 eV and more than 20 minutes was 3.713 eV, which was measured as the same result. The XRD analysis showed that the structure of CdS was hexagonal and only CdS thin films were deposited without any other impurities. The result of calculating the FWHM was a maximum of 0.142 when the heat treatment time was 20 minutes, and a minimum of 0.133 when the heat treatment time was 40 minutes, so there was no significant difference in the FWHM when the heat treatment time was changed. The particle size was measured at 11.65 Å when the heat treatment time was 40 minutes, and at 10.93 Å when the heat treatment time was 20 minutes.

The Korea Institute of Information, Electronics, and Communication Technology (RF Power 변화에 의한 CdS 박막 특성에 관한 연구)

  • Lee, Dal-Ho;Park, Jung-Cheul
    • The Journal of Korea Institute of Information, Electronics, and Communication Technology
    • /
    • v.14 no.2
    • /
    • pp.122-127
    • /
    • 2021
  • This paper produces CdS thin film using ITO glass as substrates. The MDS (Multiplex Deposition Sputter System) was used to produce devices by changing RF power and deposition time. The manufactured specimen was analyzed for its optical properties. The purpose of this paper is to find the fabrication conditions that can be applied to the photo-absorbing layer of solar cells. When RF power was 50W and deposition time was 10 minutes, the thickness was measured at 64Å. At 100W, the thickness was measured at 406Å and at 150 W, the thickness was measured at 889Å. Thin films were found to increase in thickness as RF power increased. As a result of the light transmittance measurement, 550-850nm was observed to have a transmittance of approximately 70% or more when the RF power was 50W, 100W, and 150W. Increasing RF power increased thickness and increased particle size, resulting in increased thin film density, resulting in reduced light transmittance. When RF power was 100W and deposition time was 15 minutes, the band gap was calculated at 3.998eV. When deposition time is 20 minutes, it is 3.987eV, 150W is 3.965eV at 15 minutes, and 3.831eV at 20 minutes. It was measured that the band gap decreased as the RF power increased. At XRD analysis, diffraction peaks at 2Θ=26.44 could be observed regardless of changes in RF power and deposition time. The FWHM was shown to decrease with increasing deposition time. And it was measured that the particle size increased as RF power was constant and deposition time was increased.