• 제목/요약/키워드: molten steel

검색결과 240건 처리시간 0.029초

용융아연 도금공정에서의 SNOUT 내부 유동장 해석 ( I ) (Velocity Field Measurement of Flow Inside SNOUT of Zinc Plating Process ( I ))

  • 신대식;최제호;이상준
    • 대한기계학회논문집B
    • /
    • 제23권10호
    • /
    • pp.1265-1273
    • /
    • 1999
  • PIV(Particle Image Velocimetry) velocity field measurements inside the snout of a1/10 scale model of the Zn plating process were carried out at the strip speed $V_s=1.5m/s$. Aluminum powder particles ($1{\mu}m$) and atomized olive oil ($3{\mu}m$) were used as seeding particles to simulate the molten Zinc flow and deoxidization gas flow, respectively. A pulsed Nd:Yag laser and a $2K{\times}2K$ high-resolution CCD camera were synchronized for the PIV velocity field measurement. From flow visualization study, it is found that the liquid flow in the Zn pot is dominantly governed by the uprising flow caused by the rotating sink roll, with its effect on the steel strip inside the snout largely diminished by installing of the snout. The deoxidization gas flow in front of the strip inside the snout can be characterized by a large-scale vortex rotating clockwise direction formed by the moving strip. In the rear side of the strip, a counter-clockwise vortex is formed and some of the flow entrained by the moving strip impinges on the free surface of molten zinc. The liquid flow in front of the strip is governed by the flow entering the snout, caused by the spinning sink roll. Just below the free surface a counter-clockwise vortex is formed near the snout wall. The moving strip affects dominantly the flow behind the strip inside the snout, and large amount of the liquid flow follows the moving strip toward the sink roll. The thickness of the flow following the strip is very thin in the front side due to the uprising flow, however thick boundary layer is formed in the rear side of the strip. Its thickness is increased as moving downstream toward the sink roll. Inside the snout, the deoxidization gas flow above the free surface is much faster than the liquid flow in the zinc pot. Due to the larger influx of the flow following the moving strip in the rear side of the strip, higher percentage of imperfection can be anticipated on the rear surface of the strip.

피스톤 크라운용 단강에 인코넬 718 용접재료로 용접된 용접부의 특성 평가 (Evaluation of Characteristics of Welding Zones Welded with Inconel 718 Filler Metal to Piston Crown Forged Material)

  • 이성열;문경만;정재현;이명훈;백태실
    • 한국해양공학회지
    • /
    • 제30권4호
    • /
    • pp.334-340
    • /
    • 2016
  • The combustion chamber of a diesel engine is often exposed to a more serious wear and corrosion environment than other parts of the engine because its temperature increases as a result of using heavy oil of low quality. Therefore, repair and built-up welding methods must be performed on worn or corroded parts of the piston crown, exhaust valve, etc. from an economical point of view. In this study, Inconel 718 filler metal was used in repair welding on the groove of a forged steel specimen for a piston crown, along with built-up welding on the surface of another forged steel specimen. Then, the corrosion characteristics of the weld metal zone for the repair welding and the deposited metal zone for the built-up welding were investigated using electrochemical methods in a 35% H2SO4 solution. The deposited metal zone indicated better corrosion resistance than the weld metal zone, showing a nobler corrosion potential, higher impedance, and smaller corrosion current density. It is considered that metal elements with good corrosion resistance were generally included in the filler metal, and these elements were also greatly involved in the deposited meta by built-up welding, whereas the weld metal consisted of metal elements mixed with both the filler metal and base metal elements because of the molten pool produced by the repair welding. Finally, it is considered that the hardness of the weld metal was increased by the repair welding, whereas the built-up welding improved the corrosion resistance of the deposited metal.

전기로 폐 MgO-C계 내화재의 제강원료 활용 가능성 연구 (Basic Study on the Recycling of a Waste MgO-C Refractory Material as a Flux for EAF Steelmaking)

  • 왕제필;김행구;고민석;이동헌
    • 자원리싸이클링
    • /
    • 제30권6호
    • /
    • pp.53-60
    • /
    • 2021
  • 현재 EAF 전기로 제강공정에서는 슬래그 중의 MgO 함량을 증가시켜 탈황능과 내화재 수명을 개선시키고자 돌로마이트(백운석) 용제(Flux)를 첨가하고 있으며, 또한 에너지효율을 증가시키기 위해 용강 중에 가탄재를 취입하고 있다. 이러한 견지에서 폐 MgO-C계 내화재를 재활용하는 연구를 진행하였다. 폐 MgO-C계 내화재는 MgO(>70%)과 탄소(>10%)를 대량 함유하고 있기 때문이다. 이런 목적으로 제강 슬래그를 대상으로 해서 폐 MgO-C계 내화재를 첨가하는 효과를 실험하였고 그 결과를 경소 돌로마이트를 첨가한 결과와 비교하여 폐 MgO-C계 내화재 재활용 효과를 평가하였다. 폐 MgO-C계 내화재를 사용해서 얻은 결과가 슬래그 염기도 측면에서 경소 돌로마이트를 사용한 결과와 유사하게 나타남으로써 기존 경소 돌로마이트 대체 가능성을 확인하였다. 특히 폐 MgO-C계 내화재를 사용한 경우에는, 폐 내화재에 다량 함유된 흑연 성분에 의한 슬래그 중의 철산화물과의 환원반응으로 CO가스가 발생하여 생긴 크고 작은 기포들이 관찰되었으며 이로써 슬래그 Foaming 효과를 기대할 수 있는 것으로 확인하였다.

OVERVIEW OF FUSION BLANKET R&D IN THE US OVER THE LAST DECADE

  • ABDOU M. A.;MORLEY N. B.;YING A. Y.;SMOLENTSEV S.;CALDERONI P.
    • Nuclear Engineering and Technology
    • /
    • 제37권5호
    • /
    • pp.401-422
    • /
    • 2005
  • We review here research and development progress achieved in US Plasma Chamber technology roughly over the last decade. In particular, we focus on two major programs carried out in the US: the APEX project (1998-2003) and the US ITER TBM activities (2003-present). The APEX project grew out of the US fusion program emphasis in the late 1990s on more fundamental science and innovation. APEX was commissioned to investigate novel technology concepts for achieving high power density and high temperature reactor coolants. In particular, the idea of liquid walls and the related research is described here, with some detailed examples of liquid metal and molten salt magnetohydrodynamic and free surface effects on flow control and heat transfer. The ongoing US ITER Test Blanket Module (TBM) program is also described, where the current first wall/blanket concepts being considered are the dual coolant lead lithium concept and the solid breeder helium cooled concepts, both using ferritic steel structures. The research described for these concepts includes both thermofluid MHD issues for the liquid metal coolant in the DCLL, and thermomechanical issues for ceramic breeder packed pebble beds in the solid breeder concept. Finally, future directions for ongoing research in these areas are described.

흑연 전극을 이용한 우라늄 전해정련 특성 (Electrorefining Characteristics of Uranium by Using a Graphite Cathode)

  • 강영호;이종현;황성찬;심준보;김응호
    • 방사성폐기물학회지
    • /
    • 제5권1호
    • /
    • pp.1-7
    • /
    • 2007
  • 흑연음극을 이용하여 LiCl-KCl공융염내에서 금속우라늄의 전해정련을 수행하였다. Uraniurn-Graphite Intercalation Compound(U-GIC)의 형성에 의하여 우라늄 전착물의 sell-scraping이 일어나며 전해정련에서 stripping과정을 생략함으로서 전해효율을 높일 수 있다. 우라늄 전착물내의 희토류 원소 오염은 무시할 만 하였으나 약 300ppm정도의 탄소가 오염되어 있는 것으로 관찰되었다. 탄소 오염은 이트륨을 이용한 정제공정 등을 거칠 경우 제거 가능하리라 사료된다. 회수된 우라늄 전착물의 조직 특성을 분석하였으며, 스틸 음극에 의해 회수된 전착물과 비교하였다. 이 결과는 초기 실험결과 이며 보다 심층적 연구를 통하여 사용 후 금속핵연료의 전해정련 개념을 개선시킬 수 있을 것으로 판단된다.

  • PDF

선택적 레이저 용융공정을 이용한 316L 스테인리스강 분말 3차원 조형체의 미세조직 및 경도 연구 (Study on Microstructures and Hardness of STS316L Fabricated by Selective Laser Melting)

  • 신기훈;최준필;김경태;김병기;유지훈
    • 한국분말재료학회지
    • /
    • 제24권3호
    • /
    • pp.210-215
    • /
    • 2017
  • In this study, STS316L powders prepared by gas atomization are used to manufacture bulk structures with dimensions of $10{\times}10{\times}10mm^3$ using selective laser melting (SLM). The microstructures and hardness of the fabricated 316L stainless steel has been investigated with the laser beam overlap varied from 10% to 70%. The microstructures of the fabricated STS316L samples show a decrease in the balling and satellite of powders introducing defect in the bulk samples and the porosity caused by the gap between the molten metal pools disappearing as the overlap ratio increases, whereas a low overlap ratio results in significant balling and a large amount of isolated powders due to the increased gap between the melt pools. Furthermore, the highest value in Vickers hardness is obtained for the sample fabricated by 30% overlapped laser beams. These results show that the overlap ratio of laser beams in the SLM process should be considered as an important process parameter.

적층 가공된 3차원 조형체의 치밀화에 미치는 단일 melt pool 형상의 영향 (The Influence of a Single Melt Pool Morphology on Densification Behavior of Three-Dimensional Structure Fabricated by Additive Manufacturing)

  • 최중호;윤재철;양동열;양상선;유지훈;이창우;김용진
    • 한국분말재료학회지
    • /
    • 제24권3호
    • /
    • pp.187-194
    • /
    • 2017
  • Selective laser melting (SLM) can produce a layer of a metal powder and then fabricate a three-dimensional structure by a layer-by-layer method. Each layer consists of several lines of molten metal. Laser parameters and thermal properties of the materials affect the geometric characteristics of the melt pool such as its height, depth, and width. The geometrical characteristics of the melt pool are determined herein by optical microscopy and three-dimensional bulk structures are fabricated to investigate the relationship between them. Powders of the commercially available Fe-based tool steel AISI H13 and Ni-based superalloy Inconel 738LC are used to investigate the effect of material properties. Only the scan speed is controlled to change the laser parameters. The laser power and hatch space are maintained throughout the study. Laser of a higher energy density is seen to melt a wider and deeper range of powder and substrate; however, it does not correspond with the most highly densified three-dimensional structure. H13 shows the highest density at a laser scan speed of 200 mm/s whereas Inconel 738LC shows the highest density at 600 mm/s.

4휠 시스템을 이용한 슬래그 섬유의 제조 (Fabrication Characteristics of Slag Fiber by 4 Wheel System)

  • 송영환;성환구;박수한;왕효숭;허보영
    • 한국주조공학회지
    • /
    • 제26권5호
    • /
    • pp.222-226
    • /
    • 2006
  • Steel making slag has gained a considerable attraction as one candidate of eco-materials in research fields for recycling resources. Thus, many researches have been performed but were limited to development of substitute for cement being used in the construction field. A little research work also has been done on development of higher value-added materials, including heat resistant and sound absorbing materials. For this reason, the present study were focused on macrostructure characterization of fabricated slag fibers which are applicable to heat resistant materials. The slag fibers were fabricated through a modified melt extraction method. The processing variables employed were the wheel speed and molten slag temperature. The synthesized fibers were characterized by optical microscope and scanning electron microscopy. It was found that the wheel speed of 1400 rpm generated better quality of mineral fibers in terms of the relative amount of shot, diameter and length. This was attributed to the relative extent of contact width between the flowing melt and the rotating wheel. The thickness of the slag fibers also were decreased with increasing the slag melt temperature due mainly to significant decrease in the viscosity of the slag melt. In addition, the lower melt temperature caused an increase in number of shots plus the mineral fibers.

Ca$CN_2$ 첨가에 의한 AM60 마그네슘 합금의 결정립 미세화 및 기계적 성질 (Grain Refinement and Mechanical Properties of AM60 Mg Alloy by $CaCN_2$ Addition)

  • 엄정필;정승규;임수근;신희택;정득수
    • 한국주조공학회지
    • /
    • 제18권4호
    • /
    • pp.383-388
    • /
    • 1998
  • Effects of $CaCN_2$ addition on the grain refinement in the AM60 magnesium ingots were investigated. The effects of the $CaCN_2$ are estimated with different inoculation temperatures, inoculation contents, and holding time to find out the optimum condition. AM60 alloy was melted in the low carbon steel crucible by cylindrical electric furnace under an argon atmosphere. The melting and casting apparatus is specially designed for magnesium alloys. The grain size of AM60 magnesium alloy decreased significantly with an increase in $CaCN_2$ content and, at 0.8 wt% $CaCN_2$ or more, grain size becomes constant at about $85 {\mu}m$. The optimum condition was obtained in the 0.8 wt% $CaCN_2$ for holding molten metal of 30 min. at the temperature of $710^{\circ}C$. The tensile properties of AM60 magnesium alloys were improved due to grain refinement by addition of $CaCN_2$. In the optimum condition, the yield strength, tensile strength and elongation were ${\sigma}_{0.2}=107 MPa$, ${\sigma}_{T.S}=234 MPa$ and e=14.2%. The variation of stress with strain obeyed the relationship of the ${\sigma}=K{\varepsilon}^n$. The strain-hardening exponent, n and strength coefficient, K obtained in the 0.8 wt% $CaCN_2$ added AM 60 magnesium alloy were n=0.21 and K=390 MPa.

  • PDF

FGB SAW 용접부 물성에 미치는 Ni과 Mo의 영향에 관한 연구 (Effect of Ni and Mo on Mechanical Properties of Submerged Arc Welds with Flexible Glasswool Backing)

  • 지춘호;최준태;김대주
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2009년 추계학술발표대회
    • /
    • pp.55-55
    • /
    • 2009
  • FGB(Flexible Glasswool Backing) Submerged Arc Welding has been one of the main welding processes for one side butt welding in shipbuilding industries, which can efficiently improve the welding productivity by the addition of a supplementary filler metal into the molten weld pool. As recent ships have become larger in size, the application of high tensile and higher grade of steels has been continuously increased. Single pass FGB SA welding process accompanies such a high heat input when welding thick plates that the mechanical properties of weld metal can be dramatically degraded. This study has been performed in order to obtain high toughness and tensile properties of high heat input FGB SA welds, and to evaluate the effect of alloy elements on their mechanical properties. To complete welding 25mm-thick EH36 grade steel plate by single pass, 1.2mm diameter and 1.0mm long cut wires has been distributed in the groove before welding, and three different test coupons have been made using C-1.5%Mn, C-1.8%Mn-0.5%Mo, and C-1.4%Mn-1.7%Ni cut wires to investigate the influence of nickel(Ni) and molybdenum(Mo) on the mechanical properties of welds. Test results showed that the addition of Ni and Mo effectively promotes the formation of Acicular Ferrite(AF), while significantly reducing the amount of Grain Boundary Ferrite(GBF) in weld metal microstructures, which resulted in a beneficial effect on low temperature impact toughness and strength.

  • PDF