This study was carried out to measure formaldehyde emission with the passing of two years from plywood, sliver-board and strand-board bonded with urea resins which were made of 6 f/U molar ratios. The urea resins were manufactured by six kinds of formaldehyde/urea molar ratio of 1.0, 1.2, 1.4, 1.6, 1.8 and 2.0. 1. The plywood with molar ratio of 1.0 satisfied the KS F3101 $F_2$ directly after manufacture. The plywood with molar ratio of 1.2 satisfied m 3 days. The plywood with molar ratio of 1.4 satisfied the $F_3$ in 3 days and the $F_2$ in 600 days. And the plywood with molar ratio of 1.8 and 2.0 satisfied the $F_3$ in 365 days, but didn't satisfy the $F_2$ in 730 days. 2. Sliver-board with molar ratio of 1.0 and 1.2 satisfied the KS F3104 $E_2$ right after manufacture. Sliver-board with molar ratio of 1.4 and 1.6 satisfied in 150 and 360 days, respectively. Sliver-board with molar ratio of 1.8 and 2.0 satisfied in 730 days. 3. Strand-board with molar ratio of 1.0 and 1.2 satisfied the KS F3104$ E_2$ directly after manufacture. Strand-board with molar ratio of 1.4 and 1.6 satisfied in 150 days. But Strand-board with molar ratio of 1.8 and 2.0 didn't satisfied in 730 days.
In this paper, the influence of initial formaldehyde/urea (F/U) molar ratios on the performance of low molar ratio (1.0) urea-formaldehyde (UF) resin adhesives has been investigated. Two initial F/U molar ratios, i.e., the first and second initial molar ratios were used for the alkaline addition reaction. Three levels of the first initial F/U molar ratios (2.0, 3.0, and 4.0) and two levels of the second initial molar ratios (2.0 and 1.7) were employed to prepare a total of six UF resins with an identical final molar ratio (1.0). The basis properties, functional groups, molecular weight, crystallinity, and thermal curing properties of the UF resins were characterized in detail. Higher levels (3.0 and 4.0) of the first initial F/U molar ratio provided the UF resins with better properties (non-volatile solids content, viscosity, gelation time, pH, and specific gravity) than those of the resins prepared with the conventional level F/U molar ratio of 2.0. Statistical analysis suggested that combining the first and second initial molar ratio of 4.0 with 1.7 would result in UF resins with greater adhesion strength and lower formaldehyde emission than those of the resins prepared with other molar ratios. The results showed that higher levels of the first initial molar ratio resulted in a more branched structure, as indicated by GPC, FTIR, DSC, XRD, and greater adhesion strength than those of the other UF resins with an identical final molar ratio of 1.0.
Acid deposition in forest adjacent to the industrial complexes causes soil acidification resulting in the leaching of cations, decreases of buffering capacity and increases of toxic metal concentrations such as Al, Fe, Mn and Cu in soil solution. Changes of nutrient availability equilibria by acid deposition have been known to retard the growth of pine trees. Objective of this research was to assess the critical ratios of Ca/Al and Mg/Al limiting the growth of Pinus thunbergii in the hydroponic culture. The Ca concentration and Ca/Al ratio in stalks of pine tree were increased as increasing Ca/Al molar ratio in the nutrient solution, but were not changed when the Ca/Al molar ratio was adjusted to greater than 1. Growth of Pinus thunbergii was inhibited at the Ca/Al molar ratio lower than l due to the Ca deficiency. The molar ratios of Ca/Al in the needles of Pinus thunbergii showed the similar tendency with the stalks. This indicated that Ca/Al molar ratio of 1 in the growth media was the critical level limiting the growth of Pinus thunbergii. Concentration of Mg and Mg/Al molar ratios in the stalks of pine tree were increased as increasing Mg/Al molar ratio in nutrient solution. Molar ratios of Mg/Al in the needles were increased as increasing Mg/Al ratios in nutrient solution up to 0.83, which was the critical level limiting the growth of Pinus thunbergii.
This study was to measure formaldehyde emission and bonding strength of plywoods manufactured with urea-melamine formaldehyde adhesives, which were made from three different mixing ratios of urea and melamine, and with four different formaldehyde/urea-melamine molar ratios of 1.0,1.1,1.2 and 1.4. The results were as follows 1. Amount of formaldehyde emission was the lowest at the first method of molar ratio(F/(M+U)) 1.0. Amounts of formaldehyde emission of experimental manufactured adhesives were lower than that of commercial adhesive. 2. Bonding strength of dry specimen was the highest at the first method of molar ratio(F/(M+U)) 1.4. Dry bonding strength of molar ratio(F/(M+U)) 1.4 was similar to commercial adhesive. 3. Bonding strength of wet specimen was the highest at the second method of molar ratio(F/(M+U)) 1.4. Bonding strength of wet specimen used by the third method of molar ratio(F/(M+U)) 1.4 was almost equal to commercial adhesive.
This study reports the performance of urea-formaldehyde (UF) resins prepared at two different low formaldehyde/urea (F/U) mole ratios with different numbers of urea addition during synthesis. The second or third urea was added during the synthesis of UF resins to obtain two different low molar ratios of 0.7 and 1.0, respectively. The molecular weights, cure kinetics, and adhesion performance of these resins were characterized by the gel permeation chromatography, differential scanning calorimetry, and tensile shear strength of plywood, respectively. When the number of urea additions and F/U molar ratio increased, the gelation time decreased, whereas the viscosity and molecular weight increased. Further, the UF resins prepared with the second urea and 1.0 molar ratio resulted in greater activation energy than those with third urea and 0.7 molar ratio. Tensile shear strength and formaldehyde emission (FE) of the plywood that bonded with these resins increased when the number of urea additions and molar ratio increased. These results suggest that the UF resins prepared with 0.7 molar ratio and third urea addition provide lower adhesion performance and FE than those resins with 1.0 mole ratio and the second urea addition.
Proceedings of the Korean Society of Soil and Groundwater Environment Conference
/
2002.09a
/
pp.306-309
/
2002
Micellar-enhanced ultrafiltration was investigated to remediate groundwater contaminated with chromate using a cationic surfactant, cetylpyridinium chloride (CPC). Removal of chromate was expressed as a function of molar ratio of CPC to chromate. With 10 molar ratio of CPC, removal efficiency of chromate was reached to over 99%. The rejection of CPC was 90% at 1 molar ratio, gradually increased as the molar ratio increased.
The effect of ferrous/ferric molar ratio on the formation of nano-sized magnetite particles was investigated by a co-precipitation method. Ferrous sulfate and ferric sulfate were used as iron sources and sodium hydroxide was used as a precipitant. In this experiment, the variables were the ferrous/ferric molar ratio (1.0, 1.25, 2.5 and 5.0) and the equivalent ratio (0.10, 0.25, 0.50, 0.75, 1.0, 2.0 and 3.0), while the reaction temperature ($25^{\circ}C$) and reaction time (30 min.) were fixed. Argon gas was flowed during the reactions to prevent the $Fe^{2+}$ from oxidizing in the air. Single-phase magnetite was synthesized when the equivalent ratio was above 2.0 with the ferrous/ferric molar ratios. However, goethite and magnetite were synthesized when the equivalent ratio was 1.0. The crystallinity of magnetite increased as the equivalent ratio increased up to 3.0. The crystallite size (5.6 to 11.6 nm), median particle size (15.4 to 19.5 nm), and saturation magnetization (43 to 71 $emu.g^{-1}$) changed depending on the ferrous/ferric molar ratio. The highest saturation magnetization (71 $emu.g^{-1}$) was obtained when the equivalent ratio was 3.0 and the ferrous/ferric molar ratio was 2.5.
Journal of the Korean Applied Science and Technology
/
v.24
no.3
/
pp.246-252
/
2007
$BaTiO_3$ powders were prepared by sol-gel method from different concentration of KOH aqueous solution and Ba/Ti molar ratio. Particle shape, size and crystal structure of prepared $BaTiO_3$ powders were analyzed by SEM, XRD, and FT-IR. As the result of KOH concentration changing, spherical particles were obtained by condition more than 3 M and particle size decreased as concentration increasing. Different appearance showed between dried and sintered powders against changing of Ba/Ti molar ratio. In case of dried powders, the crystallinity decreased as molar ratio increasing. On the other hand, increased as molar ratio increasing in case of sintered powders.
Five low molar ratio urea-formaldehyde (LUF) resins were synthesized in this study. The effects of molar ratio, free formaldehyde content, and catalysts on the curing characteristics of LUF resins were studied by measuring its free formaldehyde content, pH value change after catalysts added, curing rate, and pot life, observing its cured appearance, and analyzing its thermal behavior. The results indicate that: 1) The LUF resin with lower molar ratio than 1.0 can still cure; 2) Free formaldehyde content is not the main factor in affecting curing rate of LUF resin; 3) Compared with ammonium chloride as a traditional catalyst, persulfate salts markedly accelerate the curing rate of LUF resin, and result in the different appearance; 4) the addition of sodium chloride to catalysts can accelerate the curing rate of LUF resin, but the effect is moderate.
Journal of the Korean Association of Oral and Maxillofacial Surgeons
/
v.41
no.1
/
pp.3-10
/
2015
Objectives: We retrospectively evaluated the impact of mandibular third molars on the occurrence of angle and condyle fractures. Materials and Methods: This was a retrospective investigation using patient records and radiographs. The sample set consisted of 440 patients with mandibular fractures. Eruption space, depth and angulation of the third molar were measured. Results: Of the 144 angle fracture patients, 130 patients had third molars and 14 patients did not. The ratio of angle fractures when a third molar was present (1.26 : 1) was greater than when no third molar was present (0.19 : 1; odds ratio, 6.58; P<0.001). Of the 141 condyle fractures patients, the third molar was present in 84 patients and absent in 57 patients. The ratio of condyle fractures when a third molar was present (0.56 : 1) was lower than when no third molar was present (1.90 : 1; odds ratio, 0.30; P<0.001). Conclusion: The increased ratio of angle fractures with third molars and the ratio of condyle fractures without a third molar were statistically significant. The occurrence of angle and condyle fractures was more affected by the continuity of the cortical bone at the angle than by the depth of a third molar. These results demonstrate that a third molar can be a determining factor in angle and condyle fractures.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.