수도권 부순모래의 품질특성 및 부순모래 대체율에 따른 콘크리트의 특성에 관한 실험적 연구 (An Experimental Study on the Properties of Crushed Sand in Capital Region and Concrete according to the Replacement Ratio of Crushed Sand)

  • 최세진;정용;박창수;오복진;여병철;김무한
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2004년도 학술.기술논문발표회
    • /
    • pp.51-55
    • /
    • 2004
  • Generally, aggregate may limit the strength of concrete, and aggregate with undesirable properties including strength, shape and grading etc. cannot produce good concrete. Also, the properties of aggregate greatly affect the durability and structural performance of concrete. Recently, it has increased the using of crushed aggregate for concrete due to the exhaustion of good natural aggregate. In case of Korea, the using ratio of crushed stone occupies about 97% of whole coarse aggregate, and ratio of crushed sand occupies about 18.3% of whole fine aggregate. This is an experimental study to compare and analyze the properties of crushed sand for concrete in capital region and concrete according to the replacement ratio of crushed sand to do suitable mix design and improve the concrete quality. According to results, it was found that nearly all the properties of crushed sand satisfied with the value recommended by KS.

  • PDF

LNG저장시설 적용을 위한 매스콘크리트 최적 결합재 혼입율 검토 (Optimum Binder Ratio of Mass Concrete for LNG Tank)

  • 김영진;박상준;김경민;이의배
    • 한국건설순환자원학회논문집
    • /
    • 제1권3호
    • /
    • pp.240-245
    • /
    • 2013
  • 본 연구에서는 LNG저장시설용 수화열 저감형 콘크리트 적용을 위하여 최적의 결합재를 개발하고자 하였다. 결합재는 1종포틀랜드시멘트, 고로슬래그미분말, 플라이애시를 혼합 사용하였다. 또한 여기에 미립자시멘트 및 자극제를 첨가하여 조강성능 향상 및 석회석 고미분말을 사용하여 경제성을 향상시켰다. 검토결과, 압축강도 및 간이 수화열 실험 결과를 종합해 볼 때, Bottom Center의 경우 혼입비율 II(30:30:40), Roof의 경우 혼입비율 III(40:30:30)이 최적 혼입비율인 것으로 평가되었다.

농업용 콘크리트 구조물을 위한 라텍스 개질 보수용 모르타르의 적정 배합비 도출 (Optimum Mix Proportion of Latex Modified Repair Mortar for Agricultural Concrete Structures)

  • 원종필;이재영;박찬기;박성기
    • 한국농공학회논문집
    • /
    • 제49권2호
    • /
    • pp.37-46
    • /
    • 2007
  • The service life of agricultural concrete structures is designed in about 30 to 100 years, but actual service lift is estimated in an average 18 years. Therefore, as the service life of the agricultural concrete structures increases, necessity of repair by aging from various environment condition exposure increases. This study was to determinate the optimum mix proportion of latex modified repair mortar and to improve the durability performance of agricultural concrete structures. The physical and mechanical tests of latex modified repair mortar were performed. Tests of flow, compressive strength, flexural strength and bond strength tests were conducted. Test results show that the optimum nex proportion of latex modified repair mortar, when used in 5% latex volume fraction (weight of cement), 1.5% antifoaming agent (weight of latex), 0.2% PVA fiber volume fraction, 1:2 (binder-sand ratio), 10% silica fume replacement ratio (weight of cement), could result in best performance for the repair of agricultural concrete structures.

매크로 섬유의 저혼입에 따른 콘크리트 포장의 역학적 특성 (Mechanical Properties of Concrete Pavement by Low Fraction of Macro Fiber)

  • 최성용;박영환;정우태;박종섭
    • 한국도로학회논문집
    • /
    • 제14권6호
    • /
    • pp.1-11
    • /
    • 2012
  • PURPOSES : The purpose of the study was to examine dynamic features of concrete after mixing a little macro fiber with small aspect ratio and long length utilized for bridge, tunnel and shotcrete for tensile performance and crack control in domestic/overseas countries with cement concrete pavement mix. METHODS : Coarse aggregates with small aspect ratio and macro fibers with maximum length of approximately 32 mm are introduced in small quantities in the mix proportions of concrete pavement so as to prevent loss of the workability. Then, this study intends to evaluate the applicability of macro fibers in the mix proportions of concrete pavement by examining the basic construction performance, as well as the change of toughness, the equivalent bending strength and the flexural toughness index caused by compression, bending, tension and the flexural stress-displacement curve. RESULTS : As the results, in each kind of macro fiber, polyvinyl alcohol fiber and steel fiber displayed a good performance. CONCLUSIONS : In 0.2 and 0.3% of fiber contents, it is appeared that polyvinyl alcohol fiber has a large effect on improvement of tensile performance and steel fiber on improvement of deforming performance of bending stress.

Effects of Cement Alkalinity on the Time-to-Corrosion of Reinforcing Steel in Concrete under Chloride Exposure

  • Nam, Jingak;Hartt, William H.;Kim, Kijoon
    • Corrosion Science and Technology
    • /
    • 제3권6호
    • /
    • pp.245-250
    • /
    • 2004
  • A series of classical G109 type concrete specimens was exposed to cyclic wet and dry ponding with 15 w/o NaCl solution for approximately five years. Mix design variables included 1) three cement alkalinities (EqA of 0.97, 0.52, and 0.36) and 2) three water-cement ratios (0.50, 0.41, and 0.37). To determine the corrosion initiation time, corrosion potential and macro-cell current between top and bottom bars were monitored. Subsequent to corrosion initiation, specimens were autopsied and visually inspected. Concrete powder samples were collected from top rebar trace and chloride concentration was measured. Also, time-to-corrosion, $T_i$, for specimens of the individual mix designs was represented using Weibull analysis. Time-to-corrosion was a distributed parameter; and because of this, corrosion initiation of four identical specimens for each mix varied, often over a relatively wide range. Specimens fabricated using the lowest water cement ratio and the highest alkalinity cement exhibited the longest time-to-corrosion initiation and the highest chloride threshold levels. Time-to-corrosion did not increase monotonically with cement alkalinity, however, presumably as a consequence of relatively high $Cl^-$ binding in the lower pore water pH range. The chloride threshold level, $Cl_{th}$, increased with increasing $T_i$ and, consequently, was greatest for the highest cement alkalinity specimens.

고강도 콘크리트의 탄성계수에 미치는 배합재료의 영향 평가 (Effect of Mix Ingredients on Modulus of Elasticity of High-Strength Concrete)

  • 손유신;이승훈;김규동;장일영;박훈규
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2001년도 봄 학술발표회 논문집
    • /
    • pp.31-36
    • /
    • 2001
  • This paper report the effects of mix ingredients on the modulus of elasticity of high-strength concrete. The test of 284 cylinder specimens are conducted for type I with 10% replacement of fly-ash cement concretes. Different water-binder ratio, amounts of water and coarse aggregate as variables were investigated. And also analyzed it statistically by using SAS.

  • PDF

고강도 콘크리트의 실용화를 위한 연구 (A Study for the Application of High-Strength Concrete)

  • 이장화;유영찬;민병렬;김긍환
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1991년도 가을 학술발표회 논문집
    • /
    • pp.140-145
    • /
    • 1991
  • Tests were conducted to get a mix proportioning of high strength concrete between σ28 and (C/W) using low quality materials easily purchased in situ. Superplasticizer was used as a chemical admixture to compensate low slump of base concrete keeping it up about 15±2㎝. General material properties such as modulus of elasticity, poisson's ratio, unit weight and stress-strain characteristic of high strength concrete were obtained. Test results show that mix proportioning of high strength concrete proposed in this paper have reasonable validity and these can be used as a design criteria in high strength concrete construction.

  • PDF

바닥용 모르타르의 균열방지를 위한 실험적 연구 (An Experimental Study for Crack Prevention of Floor Mortar)

  • 정재동;최응규;김진근;이칠성;이상순
    • 콘크리트학회지
    • /
    • 제8권3호
    • /
    • pp.167-175
    • /
    • 1996
  • 최근 건설 현장에서 소성수축과 건조수축으로 인한 바닥용 모르타르의 균열은 매우 심가하다. 이러한 바닥용 모르타르의 균열을 방지하기 위하여 필요한 작업성을 유지하면서 단위수량을 최소화하는 최적배합의 선정과 팽창제를 사용하여 수축을 보상하는 방법에 대하여 연구하였다. 현장조사에 의하면 현장에서 사용중인 바닥용 모르타르의 물 시멘트는 약 64%인 것으로 나타났다.그리고 바닥용 모르타르의 물 시멘트를 줄이더라도 조립율이 큰 잔골재를 사용하고 고성능감수제를 적정량만큼 첨가하면 필요한 작업성을 유지할 수 있는 것으로 나타났다. 또한 이 연구에서는 모르타르의 플로우와 물 시멘트비, 잔골재시멘트비, 잔골재의 조립율과의 관계식을 제안하였으며, 제시된 식은 바닥용 모르타르의 배합설계에 유용하게 활용될 것으로 판단된다.

PVA섬유를 혼입한 비소성 황토 콘크리트의 유동특성 및 강도특성에 관한 연구 (A Study on the Fluidity Properties and Strength Properties of Non-sintered Hwangtoh mixed with PVA Fiber)

  • 이상수
    • 한국건축시공학회지
    • /
    • 제10권3호
    • /
    • pp.49-56
    • /
    • 2010
  • 본 연구에서는 PVA섬유를 혼입한 비소성 황토 모르타르 및 콘크리트에 있어, PVA 혼입율 및 비소성 황토의 치환율에 따른 영향을 검토하기 위하여 계획한 실험으로서 물-결합재비는 모르타르와 콘크리트 동일하게 50%, PVA혼입율은 0, 0.3(%)로 하였으며, 비소성 황토 치환율은 모르타르의 경우 0, 25, 50, 75(%), 콘크리트의 경우 0, 15, 30, 50(%)로 각각 4수준에 따른 모르타르 및 콘크리트의 성상을 비교 분석하여 결과를 종합하면 다음과 같다. 비소성 황토의 치환율 30%, PVA섬유 혼입율은 0.3%를 사용할 때 강도 및 유동성, 소성수축에 의한 균열제어 등 양질의 콘크리트를 만들 수 있을 것으로 판단되며, 향후 친환경 콘크리트 시공시에 활용이 가능 할 것으로 사료된다.

감수율에 따른 압축강도와 물-시멘트비 관계에 관한 연구 (A Study on the Relationship between Compressive Strength and Water-Cement Ratio According to Water Reducing Ratio)

  • 김경환;오성록;최욱;최연왕
    • 콘크리트학회논문집
    • /
    • 제26권5호
    • /
    • pp.591-598
    • /
    • 2014
  • 본 연구에서는 감수율에 따른 압축강도와 물-시멘트비의 관계를 평가하였으며, 감수율 3수준(0%, 8% 및 16%) 및 물-시멘트비 3수준(40%, 45% 및 50%)에 따른 콘크리트 배합을 제조하였다. 또한, 신뢰성 확보를 위하여 콘크리트 배합은 3회 반복실험을 실시하였다. 실험결과, 감수율에 따른 압축강도는 약 20% 이상의 강도차이가 발생하였으며, 감수율이 압축강도에 물-시멘트비 이상의 영향을 미치는 것으로 나타났다. 따라서 감수율의 영향을 반영한 새로운 압축강도와 물-시멘트비 관계식을 도출하였으며, 80% 이상의 높은 상관성이 있는 것으로 나타났다.