• 제목/요약/키워드: mill scale

검색결과 87건 처리시간 0.026초

밀 스케일을 활용한 Sr-페라이트 소결자석의 연구 (Study on the Sr-ferrite sintered magnets using mill scale)

  • 조태식
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 하계학술대회 논문집
    • /
    • pp.82-85
    • /
    • 2002
  • High-quality Sr-ferrite sintered magnets have been studied by using mill scale added SrCO$_3$ and oxidents before oxidation process. The pre-added SrCO$_3$ powders were improved the degree of oxidation and crush of mill scale and the magnetic properties of Sr-ferrite sintered magnets. The small added NaNO$_3$ oxidant was also highly improved the degree of oxidation and crush of mill scale and the magnetic properties of Sr-ferrite sintered magnets; 3805 G of remanent flux density, 3240 Oe of intrinsic coercivity, and 3.45 MGOe of maximum energy product.

  • PDF

인제거용 흡착제로서 밀스케일로부터 선별된 마그네타이트 적용 연구 (A study on the application of mill scale-derived magnetite particles for adsorptive removal of phosphate from wastewater)

  • 김윤중;엘라;최영균
    • 상하수도학회지
    • /
    • 제31권4호
    • /
    • pp.281-287
    • /
    • 2017
  • Mill scale, an iron waste, was used to separate magnetite particles for the adsorption of phosphate from aqueous solution. Mill scale has a layered structure composed of wustite (FeO), magnetite ($Fe_3O_4$), and hematite ($Fe_2O_3$). Because magnetite shows the highest magnetic property among these iron oxides, it can be easily separated from the crushed mill scale particles. Several techniques were employed to characterize the separated particles. Mill scale-derived magnetite particles exhibited a strong uptake affinity to phosphate in a wide pH range of 3-7, with the maximum adsorptive removal of 100%, at the dosage of 1 g/L, pH 3-5. Langmuir isotherm model well described the equilibrium data, exhibiting maximum adsorption capacities for phosphate up to 4.95 and 8.79 mg/g at 298 and 308 K, respectively. From continuous operation of the packed-bed column reactor operated with different EBCT (empty bed contact time) and adsorbent particle size, the breakthrough of phosphate started after 8-22 days of operation. After regeneration of the column reactor with 0.1N NaOH solution, 95-98% of adsorbed phosphate could be detached from the column reactor.

Mill Scale을 이용한 M형 Ferrite의 합성 (Preparation of M Type Hexa-Ferrite Using the Mill Scale)

  • 오영우
    • 한국자기학회지
    • /
    • 제6권4호
    • /
    • pp.204-210
    • /
    • 1996
  • 제철소의 부산물인 mill scale과 $Fe_{2}O_{3}$, 그리고 이들의 혼합물을 사용하여 M형 ferrite를 제조하였다. $Fe_{2}O_{3}$$BaCO_{3}$의 몰비를 5.2~6.0으로 변화시킨 혼합물의 하소 및 소결은 각각 $1150^{\circ}C,\;1250^{\circ}C$에서 2시간 행하였으며, 하소시에 mill scale 중의 불순물 성분인 $SiO_{2},\;Al_{2}O_{3},\;MgO,\;CaO\;및\;Na_{2}O$를 적당량 첨가한 시편으로 자기적 특성과 형상을 조사하였다. $Na_{2}O$를 첨가한 시편은 미반응의 $Fe_{2}O_{3}$와 중간 화합물인 $BaFe_{2}O_{4}$의 영향으로 자기적 특성이 감소하였으나, $BaO.5.6Fe_{2}O_{3}$ 조성에 $SiO_{2}$$Al_{2}O_{3}$의 첨가는 특성의 증진을 보였으며, 특히 $Al_{2}O_{3}$$M_{s}$ 값은 감소시켰으나 $_{B}H_{c}$ 값을 증가시켰다. BM($BaCo_{3}$와 mill scale의 혼합물)과 BFM($BaCO_{3},\;Fe_{2}O_{3}$, mill scale의 혼합물) 소결 시편의 ${(BH)}_{max}$는 각각 0.86, 1.04 MGOe였으며, $440^{\circ}C$ 부근에서 자기 특성의 변화를 보였다.

  • PDF

인 흡착을 위한 Mill Scale 전처리 및 Magnetite 제조 연구 (A Study on the Mill Scale Pretreatment and Magnetite Production for Phosphate Adsorption)

  • 천현철;최영균
    • 대한환경공학회지
    • /
    • 제37권4호
    • /
    • pp.246-252
    • /
    • 2015
  • 철강공장의 열연공정에서 발생하는 폐부산물인 mill scale을 원료로 하여 인흡착에 효율적인 무기흡착제인 magnetite를 생산하고자 하였다. Mill scale의 주요 구성성분은 wustite (FeO), magnetite (FeO), hematite (FeO)였으며, 산처리를 수행할 경우 대부분의 wustite가 magnetite와 hematite로 전환되었다. Mill scale의 산처리는 HCl과 $H_2O_2$를 이용하여, 염기처리는 NaOH 이용하여, 산-염기 복합처리는 $H_2SO_4$와 NaOH를 이용하여 수행하였다. Oil 제거 및 DI water로 rinsing만 한 경우, 인 흡착용량은 0.28 mgP/g으로 나타난 반면, 염기처리를 한 경우 0.68, 산처리를 한 경우 1.19 mgP/g으로 인 흡착용량이 증가하였다. 산-염기 복합처리 과정을 통해 단일상의 magnetite 입자를 얻을 수 있었으며, 이 입자의 인 흡착용량은 3.11 mgP/g 이상인 것으로 파악되었다. 산화철의 인 흡착에 대한 동력학적 특성 분석결과 Freundlich와 Langmuir 두 등온 흡착모델 모두 magnetite의 인 흡착 거동을 잘 모사하였다. Freundlich 모델의 흡착능(K)과 흡착강도(1/n)를 조사한 결과, 온도가 증가할수록 강한 흡착능을 보이는 것으로 나타났다. Langmuir 모델 적용결과 최대 흡착용량은 $20^{\circ}C$에서 5.1 mgP/g인 것으로 파악되었다.

전기로 분진과 압연 Scale의 환원 및 탄화거동 (Behavior of Reduction and Carburization of EAF Dust and Mill Scale)

  • 황호순;정우창;정원섭;정원배
    • 자원리싸이클링
    • /
    • 제12권5호
    • /
    • pp.50-56
    • /
    • 2003
  • 전기로에서 발생하는 분진과 압연스케일의 재활용을 위하여 전기로의 철원과 열원을 동시에 사용할 수 있는 탄화철 제조가 필요하다. 이를 위한 기초 자료를 확보하기 위하여 전기로 분진과 압연스케일의 환원거동과 탄화 거동을 조사하였다. $650^{\circ}C$ 이하의 온도에서 일산화탄소 100%로 탄화를 시키면 유리탄소는 생성되지 않으면서 세멘타이트보다 탄소함량이 더 높은 탄화철(약 9wt% C)을 생성할 수 있었다. 전기로 분진의 환원에 필요한 탄재의 양은 이론 탄재양의 약 1.2배, 그리고 환원온도는 $900^{\circ}C$가 가장 적당하였다. 압연 스케일의 환원온도는 $1000^{\circ}C$가 가장 적당하였다. 전기로 분진 및 압연 스케일의 탄화속도는 압연 스케일의 경우가 모두 빠르게 나타났다. 그리고 슈퍼탄화철의 성분은 대부분 $Fe_2$C이었다.

소형 Ball Mill에 의한 고령토의 분쇄 일지수 측정방법의 검토 (Investigation of a Method Measuring Bond에s Work Index of Korean Kaolin by Laboratory Ball Mill)

  • 심철호;강용식;서태수
    • 한국세라믹학회지
    • /
    • 제24권1호
    • /
    • pp.47-55
    • /
    • 1987
  • The purpose of this work is to establish the basic calibration data for the efficiency of grinding by investigating the Bond's Work Index employing Korean Kaolin as a reference mateial with the laboratory-scale ball mill. A small ordinary ball mill has a dimension of 133 inside diameter and 144mm long. The analysis of the experimental results in this work sets up a equivalent calibration method with the laboratory-scale ball mill to those with special mill. The theoretical expression, derived from the rate equation proposed by Miwa, is obtained to anticipitate the stable revolution number for the next grinding cycle. The proposed equation is more systematic and acurate than lshihara's empirical equation is more systematic and acurate than lshihara's empirical equation for the measurement of gindability of a ball mill.

  • PDF

다구찌 방법을 이용한 밀스케일 재활용에 대한 공정변수의 최적화 (Optimization of Process Parameters for Mill Scale Recycling Using Taguchi Method)

  • 백석흠;주원식;김창기;정유엽;신상운;홍순혁
    • 한국정밀공학회지
    • /
    • 제25권2호
    • /
    • pp.88-95
    • /
    • 2008
  • With society focusing more and more on environmental issues, the recycling of materials of all types has become an important concern. In this paper, optimization method is developed for reducing cost and improving quality in mill scale recycling. An experimental investigation into the process parameter effects is presented to determine the optimum configuration of parameters for performance, quality and cost. Taguchi's optimization approach was used to obtain the optimal parameters. The significant parameters were identified and their effects on mill scale recycling were studied. As a results, a confirmation experiment with the optimal levels of process parameters was carried out in order to demonstrate the effectiveness of the Taguchi method.

밀 스케일을 사용한 Sr-페라이트의 특성에 미치는 산화제의 영향 (Effects of Oxidant on the Properties of Sr-ferrites Using Mill Scale)

  • 조태식;최승덕
    • 한국전기전자재료학회논문지
    • /
    • 제24권2호
    • /
    • pp.131-135
    • /
    • 2011
  • We have been studied the effects of oxidant on the properties of Sr-ferrite magnets using mill scale for motor. The small-added (0.5 wt%) $NaNO_3$ oxidant improved significantly the degree of oxidation and the grindability of mill scale, and then highly enhanced the magnetic properties of anisotropic Sr-ferrite sintered magnets; such as the remanent flux density from 3.55 to 3.80 kG, the intrinsic coercivity from 2.75 to 3.22 kOe, and the maximum energy product from 2.90 to 3.45 MGOe.

밀스케일과 적점토를 원료로한 축열재에서 원료성분과 소성조선에 따른 특성 변화 (Property Change of Heat-reservoir Refractory Brick With Varying Compositions and Sintering Conditions Utilizing Mill-scale and Red-firing Clay As Raw Materials)

  • 김정석;김홍
    • 자원리싸이클링
    • /
    • 제8권1호
    • /
    • pp.23-28
    • /
    • 1999
  • 적점토와 밀스케일, 물유리를 원료로한 축열용 난방재를 개발하기 위해 제반 기초적 실험을 수행하였다. 원료배합 및 소성 조건에 따른 축열재 시료의 소성특성, 열용량, 항절력, 미세조직 등을 분석하였다. 소성체의 수축은 적점토의 비율이 높을수록 증가하였다. $300^{\circ}C$까지는 건조수축이, $300~700^{\circ}C$ 영역에서는 산화철의 상변화에 의한 완만한 팽창, $1200^{\circ}C$ 이상에서는 급격한 팽창을 나타내었다. 항절력은 밀스케일 : 적점토 비가 1:1에서 3:1로 변함에 따라 5.6MPa에서 2.35MPa로 감소하였다. 열용량은 밀스케일 : 적점토의 비율이 1:1~3:1인 경우, $1.25~1.35J/g^{\circ}C$의 값을 나타내었다. 시험편과 공기와의 접촉을 제한함으로써, 시료 내 밀스케일 성분이 소성과정에서 용융하여 시편 표면으로 용출되는 현상을 억제시킬 수 있었고, 이에 따라 균일한 표면의 시료를 제작할 수 있다. 밀스케일의 첨가는 소성체를 다공질화시켜, 축열재의 축열 후 냉각속도를 낮추는데 기여할 것으로 판단된다.

  • PDF

부식 및 스케일 억제제에 의한 냉각수 수질향상 (Improvement of Cooling Water Quality by Corrosion and Scale Inhibitor)

  • 조관형;우달식;황병기
    • 한국환경과학회지
    • /
    • 제18권2호
    • /
    • pp.187-195
    • /
    • 2009
  • This study was investigated to control the corrosion and scale at the cooling water system in steel works. Laboratory and field tests were performed for the indirect cooling water system of plate mill. Throughout the experiment, various factors such as leakage of pipes, heating rate and capacity, and the reaction between existing and substitute inhibitors were carefully monitored. The results showed that the harmful effect of high temperature could be minimized, and satisfactory corrosion/scale controls were effectively achieved using inhibitor, even at the increased temperature of $80^{\circ}C$. The batch and field tests in the gas scrubbing cooling water system of blast furnace and cooling water system of corex plant indicated that the new inhibitor was more effective for the prevention of corrosion and scale than the existing one.