• Title/Summary/Keyword: metal joints

Search Result 399, Processing Time 0.034 seconds

Analysis and design of metal-plate-connected joints subjected to buckling loads

  • Hussein, R.
    • Structural Engineering and Mechanics
    • /
    • v.9 no.5
    • /
    • pp.417-432
    • /
    • 2000
  • A comprehensive analytic study has been conducted to investigate the instability problems of metal-plate-connected (MPC) joints in light frame trusses. The primary objective in this study is to determine the governing factors that constitute the buckling of the metal connectors and their effects on the structural response of joints. Another objective is to recommend design curves for the daily structural design of these joints. The numeric data presented in this paper has emerged from a broad base that was founded on over 350 advanced computer simulations, and was supported by available experimental results obtained by others. This basic-to-applied research includes practical engineering parameters such as size of gaps, shear lengths, gauge (plate thickness) of connectors, size of un-braced areas, failure modes, and progressive disintegration of joints. Square-end members have been emphasized though the results cover the custom-made fitted joints. The results indicate that chord shears cause and dominate the buckling of MPC joints, and the shear length has a more pronounced effect than the size of gaps. Further, large gauges and small un-braced areas improve the buckling response. Several practical recommendations have been suggested throughout the paper such as keeping the ratio of gap/shear length below 3/4 for improving the buckling strength. The study reveals that multi-area joints should not be simplified as single web-to-chord MPC joints such as keeping the ratio of gap/shear length below 3/4 for improving the buckling strength, even where one web is in tension and the other in compression. Finally, the results obtained from this study favorably agree with experimental data by others, and the classic buckling theories for other structural components.

Characteristics of Liquid Phase Diffusion Bonded Joints Using Newly Developed Ni-3Cr-4Si-3B Insert Metal of Heat Resistant Alloy (신개발 Ni-3Cr-4Si-3B 삽입금속으로 액상확산접합한 내열주강 접합부의 특성)

    • Journal of Welding and Joining
    • /
    • v.18 no.6
    • /
    • pp.62-67
    • /
    • 2000
  • Metallurgical characteristics of bonded region and high temperature mechanical properties of heat resistant alloy, Fe-35Ni-26Cr during liquid phase diffusion bonding were investigated employing AM17 insert metal. The insert metal for bonding, AM17 was newly developed Ni-base metal using interpolation method. Bonding of specimens were carried out at 1,403~1,463K for 600s in vacuum. The microconstituents in the bonded interlayer disappeared in the bonding temperature over 1,423K. The microstructures, alloying elements and hardness distribution in the base metal. The tensile strength and elongation of the joints at elevated temperatures were the same level as one of the base metal in the bonding temperature over 1,423K. The creep rupture strength and rupture lives of joints were almost identical to those of base metal.

  • PDF

Effect of Heating Rates on Microstructures in Brazing Joints of STS304 Compact Heat Exchanger using MBF 20 (MBF 20으로 브레이징한 STS304 콤팩트 열교환기 접합부의 미세조직에 미치는 가열속도의 영향)

  • Kim, Jun-Tae;Heo, Hoe-jun;Kim, Hyeon-Jun;Kang, Chung-Yun
    • Journal of Welding and Joining
    • /
    • v.34 no.2
    • /
    • pp.46-53
    • /
    • 2016
  • Effect of heating rate on microstructure of brazed joints with STS 304 Printed Circuit Heat Exchanger (PCHE),which was manufactured as large-scale($1170(L){\times}520(W)){\times}100(T)$, mm), have been studied to compare bonding phenomenon. The specimens using MBF 20 was bonded at $1080^{\circ}C$ for 1hr with $0.38^{\circ}C/min$ and $20^{\circ}C/min$ heating rate, respectively. In case of a heating rate of $20^{\circ}C/min$, overflow of filler metal was observed at the edge of a brazed joints showing the height of filler metal was decreased from $100{\mu}m$ to $68{\mu}m$. At the center of the joints, CrB and high Ni contents of ${\gamma}$-Ni was existed. For the joints brazed at a heating rate of $0.38^{\circ}C/min$, the height of filler was decreased from $100{\mu}m$ to $86{\mu}m$ showing the overflow of filler was not appeared. At the center of the joints, only ${\gamma}$-Ni was detected gradating the Ni contents from center. This phenomenon was driven from a diffusion amount of Boron in filler metal. With a fast heating rate $20^{\circ}C/min$, diffusion amount of B was so small that liquid state of filler metal and base metal were reacted. But, for a slow heating rate $0.38^{\circ}C/min$, solid state of filler metal due to low diffusion amount of B reacted with base metal as a solid diffusion bonding.

Evaluation of Static Strength Applying to Fracture Mechanics on Ceramic/Metal bonded Joint (세라믹/금속 접합재에 대한 정적강도의 파괴역학적 평가)

  • 김기성
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.5 no.4
    • /
    • pp.53-62
    • /
    • 1996
  • Recently, ceramic / metal bonded joints have led to inccreasing use of structural materials such as automobile, heat engine in various industries. In this paper, a method to analyze an interface crack under both residual stresses and applied loading was proposed. and some results of boundary element method(BEM) analysis Were presented, Fracture thoughness tests of ceramic/metals bonded joints with an interface crack Were carried out, and the stress intensity factors of these joints Ware analyzed by BEM. Also crack propagtion direction was simulated numerically by using BEM. Crack propagation angle was able to easily determine based on the maximum stress concept. The prediction of fracture strength by the fracture thoughness of the ceramics/metals bonded joints was proposed.

  • PDF

Effect of Hot-stamping Heat Treatment on Microstructure and Hardness in TWB Laser Joints of Al-Si-coated Boron Steel and Zn-coated DP Steel (Al-Si 도금된 보론강과 Zn 도금된 DP강의 TWB 레이저 용접부 미세조직과 경도에 미치는 핫 스탬핑 열처리의 영향)

  • Jung, Byung-Hun;Kong, Jong-Pan;Kang, Chung-Yun
    • Korean Journal of Metals and Materials
    • /
    • v.50 no.3
    • /
    • pp.224-232
    • /
    • 2012
  • In this study, the effect of hot-stamping heat treatment on the microstructure and hardness of TWB(Tailor Welded Blank) laser joints in Al-Si-coated boron steel and Zn-coated DP(Dual Phase)590 steel was investigated. In the TWB joints without heat treatment, hardness profiles showed local hardness deviation near the fusion zone. However, there was no hardness deviation in the heat treated specimen and its hardness was higher than that of the one without the heat treatment, due to a fully martensite microstructure. In the TWB joints of both the boron and DP steels, the maximum hardnesses were observed at the HAZ(Heat Affected Zone) near the base metal, and the hardness decreased gradually to the base metal. In the heat treated joints, the hardnesses of the HAZ and the base metal of the boron steel side were similar to the maximum hardness of the weld, while those of the HAZ and the base metal of the DP steel side were higher than the maximum hardness.

Design of Joints Using Metal Seals in Turbopump (금속 실을 이용한 터보펌프 체결부 설계)

  • Yoon, Suk-Hwan;Jeon, Seong Min;Kim, Jinhan
    • Journal of Aerospace System Engineering
    • /
    • v.8 no.1
    • /
    • pp.24-29
    • /
    • 2014
  • Turbopump is typically an assembly of rotors and casings, and there are a number of joints between them. Every joint should be leak-proof, so there is always a seal to accomplish the goal. Among various seals, metal seals are advantageous in that they are robust at high pressure, and at wide range of temperature. On the other hand, they require very high tightening forces, so that flanges, bolts and nuts should be carefully designed to ensure structural integrity and to prevent detrimental yielding of components. In this study, flange joints using conical seals made of stainless steel, solid flat metal seals made of copper and metal C-seals made of Inconel 718 were structurally designed and analyzed, considering both initial tightening and operating conditions.

Short-term cyclic performance of metal-plate-connected wood truss joints

  • Gupta, Rakesh;Miller, Thomas H.;Freilinger, Shawn M. Wicks
    • Structural Engineering and Mechanics
    • /
    • v.17 no.5
    • /
    • pp.627-639
    • /
    • 2004
  • The objective of this research was to evaluate the performance of metal-plate-connected truss joints subjected to cyclic loading conditions that simulated seismic events in the lives of the joints. We also investigated the duration of load factor for these joints. We tested tension splice joints and heel joints from a standard 9.2-m Fink truss constructed from $38-{\times}89-mm$ Douglas-fir lumber: 10 tension splice joints for static condition and for each of 6 cyclic loading conditions (70 joints total) and 10 heel joints for static condition and for each of 3 cyclic loading conditions (40 joints total). We evaluated results by comparing the strengths of the control group (static) with those of the cyclic loading groups. None of the cyclic loading conditions showed any strength degradation; however, there was significant stiffness degradation for both types of joint. The results of this research show that the current duration of load factor of 1.6 for earthquake loading is adequate for these joints.

A Study on The Strength Evaluation of welded Joints for Degraded Material (열화재 용접부의 강도평가에 관한 연구)

  • 정의정;윤한용
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2002.05a
    • /
    • pp.705-710
    • /
    • 2002
  • Welding is used not only during the shipbuilding, but also during the repairing of ships. While repairing of ships, it is inevitable to weld new materials with degraded materials. In this case, it is predicted that the strength of both the sections is not identical each other. In this study, the respective welded joints in terms of mechanical properties such as microstructure, mechanical strength and fatigue crack propagation, with the component obtained from the barge used for a long-term period, were analyzed. It was found that the material degradation had a significant effect on the welded joints. The fatigue crack propagation in welded sections showed a big difference. The rate of fatigue crack growth of degraded material for both heat affected zone and parent metal was faster than that of new material. By contrast, The result within identical materials showed that the heat-affected zone was slower than that of parent metal

  • PDF

A Study on the Strength Evaluation of Welded Joints for Degraded Material (열화재 용접부의 강도평가에 관한 연구)

  • 정의정;윤한용;임명환;김태식
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.19 no.11
    • /
    • pp.75-82
    • /
    • 2002
  • Welding is used not only for the shipbuilding, but also for the repairing of ships. While repairing of ships, it is inevitable to weld new materials with degraded materials. In this case, it is predicted that the strength of both the sections is not identical each other. In this study, the respective welded joints in terms of mechanical properties such as microstructure, mechanical strength and fatigue crack propagation, with the component obtained from the barge used for a long-term period, were analyzed. It was found that the material degradation had a significant effect on the welded joints. The fatigue crack propagation in welded sections showed a big difference. The rate of fatigue crack growth of degraded material for both heat affected zone and parent metal was faster than that of new material. By contrast, the result from identical materials showed that the rate of fatigue crack growth of the heat-affected zone was slower than that of parent metal.

Effect of Bonding Condition on High Temperature Mechanical Properties of TLP Bonded Joints of FE-35Ni-26Cr Alloy (Fe-35Ni-26Cr 주강 액상확산접합부의 고온기계적 특성에 미치는 접합조건의 영향)

  • 김대업
    • Journal of Welding and Joining
    • /
    • v.18 no.4
    • /
    • pp.96-103
    • /
    • 2000
  • This study investigated the effects of bonding temperature and bonding atmosphere on high temperature mechanical properties of transient liquid phase(TLP) bonded joints of heat resistant alloy using MBF-50 insert metal. Specimens were bonded at 1,423~1,468K for 600s. Microconstituents of {TEX}$Cr_{7}(C,B)_{3}${/TEX}were formed in the bonded region when the bonding temperature was low. The amount of microcostituents in the bonded layer decreased with increasing the bonding temperature, and the microconstituents in the bonded layer disappeared at the bonding temperature above 1,468K. The tensile strength of the joints at elevated temperatures increased with the increase the bonding temperature and was the same level as one of the base metal in the bonding temperature over 1,453K. Microstructure and alloying element distributions of the bonded region bonded in Ar and $N_2$atmosphere were similar to those of the bonded in vacuum. The creep rupture strength and rupture lives of joints were almost identical to those of base metal.

  • PDF