• Title/Summary/Keyword: mechanical hardness

Search Result 2,939, Processing Time 0.024 seconds

Effect of Thermomechanical Treatment on the Mechanical Properties of 316L Stainless Steel (316L 스테인리스강의 기계적 성질에 미치는 가공 열처리의 영향)

  • Kang, Chang-Yong;Kwoon, Min-Gi
    • Journal of Power System Engineering
    • /
    • v.18 no.3
    • /
    • pp.100-105
    • /
    • 2014
  • This study is to investigate the effect of thermo mechanical treatment on the mechanical properties of 316L stainless steel. ${\alpha}^{\prime}$ and ${\varepsilon}$-martensite was formed by deformation. With increasing number of thermo mechanical treatment, volume fraction of martensite was increased rapidly, and then unchanged. With increasing number of thermo mechanical treatment, hardness and strength was increased rapidly, and then unchanged while elongation was decreased rapidly, and then unchanged. With increasing volume fraction of martensite formed by thermo mechanical treatment, hardness and strength was increased rapidly, elongation was decreased rapidly. Thus, hardness, strength and elongation of thermo mechanical treated 316L stainless steel was strongly affected by martensite formed by thermo mechanical treatment. Good combination of strength and elongation was obtained from thermomechanical treatment.

A Numerical Simulation for the Spring Hardness of a Free Piston Linear Engine (프리피스톤 리니어엔진의 스프링경도에 따른 수치해석연구)

  • Hung, Nguyenba;Oh, Yong-Il;Park, Kyu-El;Lim, Ock-Taeck
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.23 no.4
    • /
    • pp.404-411
    • /
    • 2012
  • This research numerically analyses the effects of the damping device on the operation characteristics of a free piston linear engine. In this paper, the free piston linear engine uses spring as a damping device. The investigated parameter is spring hardness which is varied at 0.5, 1, 2.9, and 14.7 N/mm. The effects of spring hardness on the dynamic characteristic, thermodynamic characteristic and electric power of the engine are investigated. Beside, the equivalent ratio is also changed to provide more information for this study. The simulation results show that, by increasing spring hardness from 0.5 to 14.7 N/mm, all of parameters related to dynamic characteristic such as piston velocity, acceleration, displacement, and frequency increase accordingly. Beside, the peak pressure in the cylinder and electric power are also increased when increasing spring hardness. The tendency is also observed at varied equivalent ratios.

Evaluation of polymethyl methacrylate resin mechanical properties with incorporated halloysite nanotubes

  • Abdallah, Reham M.
    • The Journal of Advanced Prosthodontics
    • /
    • v.8 no.3
    • /
    • pp.167-171
    • /
    • 2016
  • PURPOSE. This study inspects the effect of incorporating halloysite nanotubes (HNTs) into polymethyl methacrylate (PMMA) resin on its flexural strength, hardness, and Young's modulus. MATERIALS AND METHODS. Four groups of acrylic resin powder were prepared. One group without HNTs was used as a control group and the other three groups contained 0.3, 0.6 and 0.9 wt% HNTs. For each one, flexural strength, Young's modulus and hardness values were measured. One-way ANOVA and Tukey's test were used for comparison (P<.05). RESULTS. At lower concentration (0.3 wt%) of HNT, there was a significant increase of hardness values but no significant increase in both flexural strength and Young's modulus values of PMMA resin. In contrast, at higher concentration (0.6 and 0.9 wt%), there was a significant decrease in hardness values but no significant decrease in flexural strength and Young's modulus values compared to those of the control group. CONCLUSION. Addition of lower concentration of halloysite nanotubes to denture base materials could improve some of their mechanical properties. Improving the mechanical properties of acrylic resin base material could increase the patient satisfaction.

Effects of Two-Step Aging Treatment on the Mechanical Properties of 6061 Al Alloy (A 6061 합금의 기계적 특성에 미치는 2단시효의 영향)

  • Lee, Bo-Bae;Im, Hang-Joon;Jeong, Geol-Chae.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.32 no.2
    • /
    • pp.57-60
    • /
    • 2019
  • The impact of two-step treatment on the mechanical properties of the 6061 Al alloy was investigated by testing the hardness and electrical conductance values. After two-step aging treatment, the hardness and electrical conductivity of the alloy was increased, and if the first aging treatment temperature was lower than the secondary aging treatment temperature, both the hardness and the electrical conductivity were not increased. The higher the temperature of the first aging treatment, the higher the hardness. The temperature of the first aging treatment is $175^{\circ}C$, $150^{\circ}C$, $120^{\circ}C$, and the second is $175^{\circ}C$ and $120^{\circ}C$.

The Characteristics of the Chungja Celadon the Amount of BaTio3 (BaTio3 조성비 변화에 따른 청자소지물질의 특성)

  • Yun, Mi-Young;Kim, Yeon-Jung;Ja, Lim-Hun
    • Journal of the Korean institute of surface engineering
    • /
    • v.45 no.1
    • /
    • pp.31-36
    • /
    • 2012
  • In order to improve the mechanical roperties of the Gangjin celadon $BaTiO_3$ was added into the raw materials of celadon matrix. Through SEM and XRD analysis the structural changes were observed and the hardness values were measured. We could confirm that the mechanical strength considerably increased in the $BaTiO_3$ added celadon through the measurement of hardness values. The increase of mechanical strength values in the celadon may result from the compositional change in the microstructure such as grain boundary area through EDAX analysis. We might suggest a fundamental idea to improve the mechanical intensity of the celadon.

Statistical Properties of Vickers Hardness of Post Weld Heat Treated Friction Welded Parts in Alloy718 (Alloy718 마찰용접 후열처리재의 비커스 경도의 통계적 성질)

  • Kong, Yu-Sik;Kwon, Hyeok-Yong;Kim, Seon-Jin
    • Journal of Ocean Engineering and Technology
    • /
    • v.23 no.6
    • /
    • pp.105-110
    • /
    • 2009
  • The objective of this paper is to investigate the statistical properties of Vickers hardness (HV) for friction welded parts in a Ni-based super alloy (Alloy718). In the case of post weld heat treatment (PWHT) parts, hardness tests were repeated for three different applied loads, 100, 200, and 300 g, with a duration time of 10 seconds. The arithmetic means of the Vickers hardness in heat affected zone (HAZ) materials were smaller than those of the base metal (BM) in all of the applied loads. The coefficient of variation (COV) for the BM and HAZ decreased by increasing the applied load. The probability distribution of the Vickers hardness followed the Weibull distribution well. The distribution of the Vickers hardness was not found to be symmetric. The shape parameter and scale parameter increased by increasing the applied load at both the BM and HAZ.

Degradation Behavior and Micro-Hardness Analysis of a Coolant Rubber Hose for Automotive Radiator (자동차용 냉각기 고무호스의 노화거동과 미소경도분석)

  • Kwak, Seung-Bum;Shin, Sei-Moon;Shin, Wae-Gi;Choi, Nak-Sam
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.31 no.9
    • /
    • pp.915-923
    • /
    • 2007
  • Rubber hoses for automobile radiators are apt to be degraded and thus failed due to the influence of contacting stresses of air and coolant liquid under thermal and mechanical loadings. The aging behaviors of the skin part of the hoses due to thermo-oxidative and electro-chemical stresses were experimentally analyzed. Through the thermo-oxidative aging test, it was shown that the surface hardness IRHD(International Rubber Hardness Degrees) of the rubber increased with a considerable reduction of failure strain as the aging time and temperature increased. On account of the penetration of coolant liquid into the skin part influenced by the electro-chemical degradation(ECD) test the weight of the rubber hose increased, whereas their failure strain and IRHD hardness decreased. The hardness of the hose in the side of the negative pole was the most deteriorated at the test site of the hose skin just below the coolant surface.

The Effect of Heat Treatment Hold Time for Mechanical Properties of Zinc-Magnesium Alloy (아연-마그네슘 합금의 열처리에 따른 기계적 특성 연구)

  • Hwang, Injoo
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.33 no.3
    • /
    • pp.117-123
    • /
    • 2020
  • Due to high corrosion resistance, Zinc has been widely used in the automobile, shipping or construction industries as a galvanizing material. Zinc is popular as a coating element, but its low mechanical strength impede the expansion of applications as a load-bearing structure. The mechanical strength of Zinc can be increased through zinc based alloy process, but the ductility is significantly reduced. In this study, the mechanical strength and ductility of Zinc-Magnesium alloys with respect to heat treatment hold time was investigated. In order to enhance the mechanical strength of Zinc, a Zinc-Magnesium alloy was fabricated by a melting process. The heat treatment process was performed to improve the ductility of Zinc-Magnesium alloy. The microstructure of the heat-treated alloy specimen was analyzed using SEM. The hardness and compressive strength of the specimen were measured by a micro-hardness tester and a nano-indenter, respectively.

Mechanical properties of top neck mollusks shell nano composite in different environmental conditions

  • Masir, Amin Nouroozi;Darvizeh, Abolfazl;Zajkani, Asghar
    • Advances in materials Research
    • /
    • v.7 no.3
    • /
    • pp.185-194
    • /
    • 2018
  • The mechanism of biological materials structure is very complex and has optimal properties compared to engineering materials. Top Neck mollusks shells, as an example of biological materials, have hierarchical structure, which 95 percent of its structure is Aragonite and 5 percent organic materials. This article detected mechanical properties of the Top Neck mollusks shell as a Nano composite using Nano-indentation method in different situations. Research findings indicate that mechanical properties of the Top Neck mollusks shell including elastic modulus and hardness are higher than a fresh one preserved in -50 centigrade and also a Top Neck mollusks shell preserved in environmental conditions. Nano-indentation test results are so close in range, overall, that hardness degree is 3900 to 5200 MPa and elastic modulus is 70 to 85 GPa.

A Study on the Effect of Process Parameters to Mechanical Property in Forward Extrusion of Milli-size Cylindrical Pin (밀리 단위의 원형핀 전방압출에 있어서 공정인자가 기계적 성질에 미치는 영향 연구)

  • 심경섭;김용일;이용신;김종호
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2003.06a
    • /
    • pp.797-801
    • /
    • 2003
  • The mechanical properties such as shear strength and the hardness of milli-size products that manufactured for various process parameters by forward extrusion using square dies are investigated. Shear strength test is implemented for the observation of relation between vickers hardness and shear strength in the interface of head and shaft part of a stepped pin. When the extrusion ratios of pure aluminum and pure copper billets increase, the hardness on both the surface and the center line of a pin also increase, especially the hardness on the surface is shown to be a little higher than on the center. The existence of knock-out pad in extrusion die caused hardness increase in the interface of a extruded pin. As compared shear strength with hardness of a pin, the approximated linear relations are suggested in this study.

  • PDF