THE THREE DIMENSIONAL FINITE ELEMENT ANALYSIS OF STRESS DISTRIBUTION AND DISPLACEMENT IN MANDIBLE ACCORDING TO TREATMENT MODALITIES OF MANDIBULAR ANGLE FRACTURES (하악각 골절의 치료 방법에 따른 하악골의 응력 분포 및 변위에 관한 삼차원 유한요소법적 연구)

  • Ku, Je-Hoon;Kim, Il-Kyu;Chang, Jae-Won;Yang, Jung-Eun;Sasikala, Balaraman;Wang, Boon
    • Maxillofacial Plastic and Reconstructive Surgery
    • /
    • v.32 no.3
    • /
    • pp.207-217
    • /
    • 2010
  • The purpose of this study was to evaluate the effects of the stress distribution and displacement in mandible according to treatment modalities of mandibular angle fractures, using a three dimensional finite element analysis. A mechanical model of an edentulous mandible was generated from 3D scan. A 100-N axial load and four masticatory muscular supporting system were applied to this model. According to the number, location and materials of titanium and biodegradable polymer plates, the experimental groups were divided into five types. Type I had a single titanium plate in the superior border of mandibular angle, type II had two titanium plates in the superior tension border and in the inferior compression border of mandibular angle, type III had a single titanium plate in the ventral area of mandibular angle, type IV had a single biodegradable polymer plate in the superior border of mandibular angle, type V had a single biodegradable polymer plate in the ventral area of mandibular angle. The results obtained from this study were follows: 1. Stress was concentrated on the condylar neck of the fractured side except Type III. 2. The values of von-Mises stress of the screws were the highest in the just-posterior screw of the fracture line, and in the just-anterior screw of Type III. 3. The displacement of mandible in Type III was 0.04 mm, and in Type I, II, IV, and V were 0.10 mm. 4. The plates were the most stable in the ventral area of mandibular angle (Type III, V). In conclusion, the ventral area of mandibular angle is the most stable location in the fixation of mandibular angle fractures, and the just- posterior and/or the just-anterior screws of the fracture line must be longer than the other, and surgeons have to fix accurately these screws, and the biodegradable polymer plate also was suitable for the treatment of mandible angle fracture.

An Analysis of Stress Transfer Behaviors within the Necrotic Cancellous Bone following Surgical Procedures or the Management of the Osteonecrosis of the Femoral Head (대퇴골두 무혈성 괴사증의 수술적 기법 적용 후 괴사 망상골 내에서의 응력 변화 해석)

  • Kim, J.S.;Lee, S.J.
    • Proceedings of the KOSOMBE Conference
    • /
    • v.1997 no.11
    • /
    • pp.245-248
    • /
    • 1997
  • Operative interventions for the management of osteonecrosis of the femoral head (ONFH) include core drilling, with or without vascularized fibular bone grafting. Nevertheless, their clinical results have not been consistently satisfactory. Recently, a new surgical procedure that incorporates cementation with polymethylmethacrylate (PMMA) after core drilling has been tried clinically. In this study, a biomechanical analysis using a finite element method(FEM) was undertaken to evaluate surgical methods and their underlying surgical parameter. Our finite element models included five types. They were (1) normal model (Type I), (2) necrotic model (Type II), (3) core decompressed model (Type III). (4) fibular bone grafted model (Type IV), and (5) cemented with PMMA model (Type V). The geometric dimensions of the femur were based on digitized CT-scan data of a normal person. Various physiological loading conditions and surgical penetration depths by the core were used as mechanical variables to study their biomechanical contributions in stress transfer within the femoral head region. In addition. the peak von Mises stress(PVMS) within the necrotic cancellous bone of the femoral head was obtained. The fibular bone grafted method and cementation method provided optimal stress transfer behaviors. Here. substantial increase in the low stress level was observed when the penetration depth was extended to 0mm and 5mm from the subchondral region. Moreover, significant decrease in PVMS due to surgery was observed in the fibular bone grafted method and the cementation method when the penetration depths were extended up to 0 and 5mm from the subchondral region. The drop in PVMS was greater during toe-off than during heel-strike (57% vs. 28% in Type IV and 49% vs. 22% in Type V). Both the vascularized fibular bone grafting method (Type IV) and the new PMMA technique (Type V) appear to be very effective in providing good stress transfer and reducing the peak Von-Mises stress within the necrotic region. Overall results show that fibular bone grafting and cementation methods are quite similar. In light of above results, the new cementation method appears to be a promising surgical alternative or the treatment of ONFH. The use of PMMA for the core can be less prone to surgical complication as opposed to preparation of fibular bone graft and can achieve more immediate fixation between the core and the surrounding region.

  • PDF

Elbow Arthrodesis with bone Autograft for the Management of Gunshot Fracture in a Dog (총상 골절 개에서 자가골 이식과 주관절 고정술)

  • Lee Jong Il;Alam Md. Rafiqul;Kim Nam soo
    • Journal of Veterinary Clinics
    • /
    • v.22 no.1
    • /
    • pp.60-64
    • /
    • 2005
  • A 6year-old intact male hound cross dog, weighing 23 kg, was presented to the Teaching Animal Hospital, Chonbuk National University with the history of gunshot wound at the left elbow joint. Survey radiographs of the affected elbow revealed the presence of a metallic bullet caudal to the olecranon processes and comminuted fracture of the proximal radius and ulna. The first treatment strategy included removal of the bullet and fixation of the radius and ulna using separate bone plates, bone screw, K-wire and surgical wire, was failed. The second treatment strategy included olecranon osteotomy and rigid immobilization of the elbow joint with a bone plate applied to the caudal aspect of the humerus and ulna along with autogenous bone grafts collected from the 13th rib. The optimal angle of the joint following arthrodesis of this case appeared to be 130°. This resulted in improving the case but after 60 weeks the plate was bent and there was exudation from the wound. The third treatment strategy was the same with the second except for that the bone autografts were collected from the proximal metaphyses of the ipsilateral humerus. This resulted in a successful arthrodesis 6 weeks after the surgery. Elbow arthrodesis with bone autograft resulted in acceptable function, but abnormal gait remained in the dog due to mechanical interference with the movement of the joint.

Treatment of Phalangeal Bone Defect Using Autologous Stromal Vascular Fraction from Lipoaspirated Tissue (자가기질혈관분획을 이용한 수지골 결손 환자의 치료)

  • Jeong, Tae-Won;Ji, Yi-Hwa;Kim, Deok-Woo;Dhong, Eun-Sang;Yoon, Eul-Sik
    • Archives of Plastic Surgery
    • /
    • v.38 no.4
    • /
    • pp.438-444
    • /
    • 2011
  • Purpose: Adipose-derived stromal cells (ASCs) are readily harvested from lipoaspirated tissue or subcutaneous adipose tissue fragments. The stromal vascular fraction (SVF) is a heterogeneous set of cell populations that surround and support adipose tissue, which includes the stromal cells, ASCs, that have the ability to differentiate into cells of several lineages and contains cells from the microvasculature. The mechanisms that drive the ASCs into the osteoblast lineage are still not clear, but the process has been more extensively studied in bone marrow stromal cells. The purpose of this study was to investigate the osteogenic capacity of adipose derived SVF cells and evaluate bone formation following implantation of SVF cells into the bone defect of human phalanx. Methods: Case 1 a 43-year-old male was wounded while using a press machine. After first operation, segmental bone defects of the left 3rd and 4th middle phalanx occurred. At first we injected the SVF cells combined with demineralized bone matrix (DBM) to defected 4th middle phalangeal bone lesion. We used P (L/DL)LA [Poly (70L-lactide-co-30DL-lactide) Co Polymer P (L/DL)LA] as a scaffold. Next, we implanted the SVF cells combined with DBM to repair left 3rd middle phalangeal bone defect in sequence. Case 2 was a 25-year-old man with crushing hand injury. Three months after the previous surgery, we implanted the SVF cells combined with DBM to restore right 3rd middle phalangeal bone defect by syringe injection. Radiographic images were taken at follow-up hospital visits and evaluated radiographically by means of computerized analysis of digital images. Results: The phalangeal bone defect was treated with autologous SVF cells isolated and applied in a single operative procedure in combination with DBM. The SVF cells were supported in place with mechanical fixation with a resorbable macroporous sheets acting as a soft tissue barrier. The radiographic appearance of the defect revealed a restoration to average bone density and stable position of pharyngeal bone. Densitometric evaluations for digital X-ray revealed improved bone densities in two cases with pharyngeal bone defects, that is, 65.2% for 4th finger of the case 1, 60.5% for 3rd finger of the case 1 and 60.1% for the case 2. Conclusion: This study demonstrated that adipose derived stromal vascular fraction cells have osteogenic potential in two clinical case studies. Thus, these reports show that cells from the SVF cells have potential in many areas of clinical cell therapy and regenerative medicine, albeit a lot of work is yet to be done.

Mechanical behaviour of waterway culvert structure assembled by precast segments (프리캐스트 세그먼트를 이용한 조립식 수로암거구조물의 역학적 거동 특성)

  • Lee, Gyu-Phil;Hwang, Jae-Hong;Shin, Hyu-Sung;Hong, Se-Kyun
    • Journal of Korean Tunnelling and Underground Space Association
    • /
    • v.12 no.2
    • /
    • pp.193-200
    • /
    • 2010
  • Due to the characteristic of culvert structure, the standard section of the culvert has been established and applied in field. However, this becomes a limitation in selecting a section design corresponding to various field conditions although it can improve the design and applicability of culvert structure. In order to overcome this limitation, we have developed the design and application technology of culvert structure corresponding to the field conditions that various shapes of culvert structure can be covered by assembly of precast segments. Because the structural characteristics of assembling-type waterway culvert structure, the thickness of structure and amount of reinforcing rods can vary according to the fixation or internal hinge status in the connection part of precast segments. This has a strong influence on the applicability and economic efficiency of culvert structure. Accordingly, in order to suggest a reasonable modeling technique of segment connection parts, this study has conducted the field experiment and numerical analysis. According to the results of field experiment and numerical analysis, the slab, wall and base slab with mortar splice sleeves have shown that the assembling-type of waterway culvert structure behaves like an integrated structure.

A study of the cause of metal failure in treatment of femur shaft fracture - Fractographical and clinical analysis of metal failure- (대퇴골 간부 골절시 사용한 금속물의 금속부전(Metal failure)의 기전에 대한 연구)

  • Jeon, Chun-Bae;Seo, Jae-Sung;Ahn, Jong-Chul;Ahn, Myun-Whan;Ihn, Joo-Chyl
    • Journal of Yeungnam Medical Science
    • /
    • v.7 no.1
    • /
    • pp.81-93
    • /
    • 1990
  • The author fractographically analyized the cause of metal failure(the first time this procedure has been used for this metal failure)and also analyized it clinically. In this study, I selected eight cases which have been analyized fractographically. In all these cases, the analysis was done after treatment of metal failure of implants internally fixed to femur shaft fractures at the Department of Orthopedic Surgery, Yeung-Nam University Hospital during the six year period from May 1983 to September 1989. 1. Metal failure occured in five dynamic-compression plates, one Jewett nail, one screw in Rowe plate, and one interlocking nail. 2. The clinical cause of metal failure was deficiency of medial butress in five cases, incorrect position of implant in one case, and incorrect selection of implant in two cases. 3. The time interval between internal fixation and metal failure was four months in one case, between five months to twelve months in six cases, three years in one case. 4. The fractographically analytical cause of metal failure was ; first, impact failure, one case, second, fatigue failure, six cases, machining mark(stress liser), four cases type : low consistent cyclic fatigue failure irregular cyclic fatigue failure third, stress corrosion crack, one case. 5. 316L Stainless Steel has good resistance to corrosion. However, when its peculiar surface film is destroyed by fretting, it shows pitting corrosion. This is, perhaps, the main cause of metal failure. 6. It is possible that mechanical injury occured in implants during the manufacturing of implants or that making a screw hole is the main cause of metal failure.