PURPOSE. This study evaluated marginal fit of glass infiltrated alumina cores fabricated using two techniques and their marginal stability after firing cycles of veneering porcelain. MATERIALS AND METHODS. Fifteen standardized all-ceramic crowns were fabricated on a metal die using each technique: slip cast technique of VITA In-Ceram sprint Alumina (Group A as control) and plastic foil matrix technique of Turkom-Cera fused alumina core system (Group B). Copings were compared between groups and within groups at coping stage and after firing each layer of veneering porcelain. A device was used to standardize seating of copings on the metal die and positioning of the specimens under the microscope after each stage of fabrication. The specimens were not cemented and marginal gap was measured using an image analyzing software (Imagepro Express) on the photographs captured under an optical microscope. Two tailed unpaired 't test' was used to compare marginal gaps in two groups and one way ANOVA was used to analyze marginal distortion within each group at 95% confidence interval. RESULTS. The marginal gap was smaller at the coping stage in group B ($60+30{\mu}M$) than group A ($81+21{\mu}M$) with statistical significance. After firing of veneering porcelain the difference was insignificant. At the final stage, both groups exhibited lower mean marginal gaps than at the initial coping stage with the difference of $11.75{\mu}M$ for group A and $11.94{\mu}M$ for group B, but it was statistically insignificant due to high value of standard deviation. CONCLUSION. Within the limitations of this study, it was concluded that both techniques produced copings with comparable and acceptable marginal fit and marginal stability on firing veneering porcelain.
When the marginal fit of fixed dental prosthesis decreases, biological and technical complications, such as plaque accumulation, periodontal disease, hypersensitivity, components fracture, cement loss, can happen. The complications affect the long-term success and survival of prostheses. This case report describes a clinical procedure to minimize the marginal gap of implant-supported screw-and-cement retained prosthesis by removing prosthesis-abutment complex and burnishing the interface area. The marginal gap was measured before and after the burnishing using a stereomicroscope and compared. This technique improves the marginal fit, thereby contributing the longevity of the prosthesis.
Purpose: The aim of this study was to evaluate the marginal and internal gap of zirconia copings fabricated by CAD/CAM system and to research the effect of cement space on the fit of zirconia prosthesis. Methods: Zirconia copings were designed using 3shape software and then milled from presintered zirconia blocks by Kavo dental milling machine. The cement space was set at $0{\mu}m$ around the margins for all groups, and additional cement space appling 1 mm above the finish lines of tooth. The samples were classified into 4 groups according to the cement space setting(Cs-0, Cs-40, Cs-80, Cs-120). Replica technique used to investigate marginal and internal gap. The silicone film thickness was recorded using a optical microscope with image software analysis system at 75${\times}$magnification. The assessment performed on the six points in bucco-lingual and mesio-distal sections(4 groups, 10 copings per group, 12 measuring points per coping). The data were statistically analyzed with one-way ANOVA followed by pair-wise Tukey's post hoc tests(${\alpha}$<0.05). Results: Better marginal and internal fit values were exhibited by $80{\mu}m$ cement space. The results showed that different cement space values had statistically significant effect on the marginal and internal gap of zirconia copings(p<0.001). The gap of margin and axial wall area was smaller than that the gap of occlusal area in all groups(p<0.001). Conclusion : Effect of different cement spaces on the marginal and internal gap of zirconia copings.
The purpose of this study was to estimate the ability of the marginal fit of Glass ionomer cement. Using the human extracted teeth and 2% acqueous solution of methylene blue, the author investigated the marginal penetration of dye in restorative materials such as Amalgam, Hi-Pol, Glass ionomer cement, Estic microfill and Restodent. The results were as follows. 1. All filling materials showed some degree of marginal penetration. 2. Glass ionomer cement revealed nearly the same microleakage as Estic microfill and Hi-Pol, but showed inferior effect of the marginal seal as compared with Restodent. 3. It is appeared that Amalgam has more effective ability of the marginal fit than the others within a week.
There have been many studies about marginal discrepancy of single restorations made by various systems and materials. But many of statistical inferences are not definite because of sample size, measurement number, measuring instruments. etc. The purpose of this study was to compare the marginal adaptations of the anterior single restorations made by different systems and to consider more desirable statistical methods in analysing the marginal fit. The in vitro marginal discrepancies of three different all-ceramic crown systems (Celay In-Ceram. Conventional In-Ceram. IPS Empress 2 layering technique) and one control group (PFM) were evaluated and compared. The crowns were made from one extracted maxillary central incisor prepared with a 1mm shoulder margin and $6^{\circ}$ taper walls by milling machine. 10 crowns per each system were fabricated. Measurements or a crown were recorded at 50 points that were randomly selected for marginal gap evaluation. Non-parametric statistical analysis was performed for the results. Within the limits of this study, the following conclusions were drawn: 1 Mean gap dimensions and standard deviations at the marginal opening for the maxillary incisor crowns were $98.2{\pm}40.6{\mu}m$ for PFM, $83.5{\pm}18.7{\mu}m$ for Celay In-Ceram, $104.9{\pm}44.1{\mu}m$ for conventional In-Ceram, and $45.5{\pm}11.5{\mu}m$ for IPS Empress 2 layering technique. The IPS Empress 2 system showed the smallest marginal gap (P<0.05). The marginal openings of the other three groups were not significantly different (P<0.05). 2 The marginal discrepancies found in this study were all within clinically acceptable standards ($100\sim150{\mu}m$). 3. When the variable is so controlled that the system may be the only one, mean value is interpreted to be the marginal discrepancy of a restoration which is made by each system and standard deviation is to be technique-sensitivity of each one. 4. From the standard deviations. the copy-milling technique (Celay/In-Ceram) was not considered to be technique-sensitive in comparison with other methods. 5. Parametric analysis is more reliable than non-parametric one in interpretation of the mean and standard deviation. The sample size of each group has to be more than 30 to use parametric statistics. The level of clinically acceptable marginal fit has not been established. Further studies are needed.
The recently introduced castable glass ceramics incorporate properties characteristic of natural teeth and they are regarded as an ideal material to restore lost tooth structure. The purpose of this study was to compare the marginal fit of castable ceramic crown with that of the metal-ceramic crown in the process of heat treatment. Two master dies for castable ceramic crowns and metal-ceramic crowns were fabricated from being cast with the base metal. Each master die was duplicated with addition silicone and hard stone. Ten castable ceramic crowns were made on each hard stone die and their marginal openings were measured three times first, after casting; second, after ceramming; third, after shading. The other ten metal-ceramic crowns were made on each hard stone die and their marginal openings were measured three times : first, after casting; second, after degassing; third, after porcelain veneering. Each crown was seated on its master die with the constant force delivered by loading jig. And then, marginal openings were measured on four locations by optical projector at X50 magnification. The results were as follows: 1. The mean marginal openings of castable ceramic crowns were $31.1{\pm}12.7{\mu}m$ after casting; $44.6{\pm}12.8{\mu}m$ after ceramming; $51.2{\pm}16.8{\mu}m$ after shading. 2. The mean marginal openings of the metal-ceramic crowns were $26.2{\pm}13.8{\mu}m$ after casting; $29.8{\pm}10.3{\mu}m$ after degassing; $38.0{\pm}14.5{\mu}m$ after porcelain veneering. 3. There was significant increase in the marginal opening of castable ceramic crowns after ceramming, while metal-ceramic crowns sho(wed significant increase after porcelain veneering (p<0.05). 4. Marginal fit of metal-ceramic crown was better than that of castable ceramic crown (p<0.01).
PURPOSE. Few studies have investigated the marginal accuracy of 3-unit zirconia fixed partial dentures (FPDs) fabricated by computer-aided design/computer-aided manufacturing (CAD/CAM) system. The purpose of this study was to compare the marginal fit of zirconia FPDs made using two CAD/CAM systems with that of metal-ceramic FPDs. MATERIALS AND METHODS. Artificial resin maxillary central and lateral incisors were prepared for 3-unit FPDs and fixed in yellow stone. This model was duplicated to epoxy resin die. On the resin die, 15 three-unit FPDs were fabricated per group (45 in total): Group A, zirconia 3-unit FPDs made with the Everest system; Group B, zirconia 3-unit FPDs made with the Lava system; and Group C, metal-ceramic 3-unit FPDs. They were cemented to resin dies with resin cement. After removal of pontic, each retainer was separated and observed under a microscope (Presize 440C). Marginal gaps of experimental groups were analyzed using one-way ANOVA and Duncan test. RESULTS. Mean marginal gaps of 3-unit FPDs were $60.46{\mu}m$ for the Everest group, $78.71{\mu}m$ for the Lava group, and $81.32{\mu}m$ for the metal-ceramic group. The Everest group demonstrated significantly smaller marginal gap than the Lava and the metal-ceramic groups (P<.05). The marginal gap did not significantly differ between the Lava and the metal-ceramic groups (P>.05). CONCLUSION. The marginal gaps of anterior 3-unit zirconia FPD differed according to CAD/CAM systems, but still fell within clinically acceptable ranges compared with conventional metal-ceramic restoration.
Background: This study aimed to compare and evaluate the marginal fit of nanocomposite computer-aided design/computer-aided manufacturing (CAD/CAM) inlays. Three types of nanocomposite CAD/CAM blocks (HASEM, VITA Enamic, and Lava Ultimate) were used as materials. Methods: Class II disto-occlusal inlay restorations were prepared on a typodont mandibular right first molar using diamond rotary instruments. The inlays were fabricated using CAD/CAM technology and evaluated using the silicone replica technique to measure marginal gaps at five locations on each inlay. The data were analyzed by two-way analysis of variance and Tukey post hoc tests (α=0.05). Results: There were no significant differences in the marginal gaps based on the type of nanocomposite CAD/CAM inlay used (p=0.209). However, there was a significant difference in the marginal gaps between the measurement regions. The gingival region consistently exhibited a larger marginal gap than the axial and occlusal regions (p<0.001). Conclusion: Within the limitations of this in vitro study, the measurement location significantly influenced the marginal fit of class II disto-occlusal inlay restorations. However, there were no significant differences in the marginal gaps among the different types of CAD/CAM blocks. Furthermore, the overall mean marginal fits of the class II disto-occlusal inlay restorations made with the three types of nanocomposite CAD/CAM blocks were within the clinically acceptable range.
Marginal and internal fit is an important part of the longevity of dental restorations. The purpose of this study was to analysis the marginal and internal fit of zirconia core by dental CAD/CAM system using innovative and non-destructive methods such as optical coherence tomography(OCT) and compare with conventional method such as silicone replica technique(SRT). Ten dental stone models of abutment of maxillary right central incisal were manufactured and scanned. Ten zirconia cores were fabricated with commercial CAD/CAM system. To measure the marginal and internal fit of each sample, five point of fitness were measured using 2 different methods(OCT and SRT). Statistical analysis was performed using independent sample t-test(${\alpha}$=0.05). OCT and SRT groups were not significantly different(P>0.05). By this results, analysis the fitness of dental restorations using OCT were acceptable measuring method.
PURPOSE. The purpose of this study was to evaluate the effect of the span length on the fit of zirconia framework fabricated using CAD/CAM system. MATERIALS AND METHODS. Abutments for single, 4-unit and 6-unit fixed partial prostheses were fabricated. Ten zirconia frameworks were fabricated for each group. The marginal and internal gap were presented by means of replica technique and measured by measuring microscope ($AXIO^{(R)}$, Carl Zeiss, Rochester, NY) and software (I-$solution^{(R)}$, IMT i-solution Inc., Vancouver, BC, Canada). The results were statistically analyzed by multivariate analysis test and Dunnett T3 test for post hoc test (${\alpha}$=.05). RESULTS. There were statistically significant differences at 2, 4, 7, 8 points (mesio-distal section) and b, d, e, f, g (labio-lingual section). In some marginal reference points of 6-unit group (P<.05), the marginal gap were larger than 120 ${\mu}m$. CONCLUSION. Span length of zirconia core may have an influence on marginal and internal fit. Within the limitation of this study, the increase of span length of zirconia framework of 6 or more-unit fixed partial denture may decrease the marginal and internal fit.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.