• Title/Summary/Keyword: low porosity

Search Result 523, Processing Time 0.034 seconds

A Study to Effect on the Porosity when Model Making for Control of Vibrator (진동기의 단계별 조절이 모형 제작시 기포발생에 미치는 영향에 관한 연구)

  • Lee, Do-Kyeng
    • Journal of Technologic Dentistry
    • /
    • v.13 no.1
    • /
    • pp.15-19
    • /
    • 1991
  • This study was made to effect on the porosity when model making for control of vibrator. Samples of total 600 were made by plaster and stone divided low, medium and high which is 100 each. The following results were obtained to observation porosity of surface by eyes. 1. Second stage was fewer than third stage, first stage was fewer than third stage in porosity number of plaster model. 2. Second stage was fewer than first stage in porosity number of stone model. 3. Stone model was fewer than plaster model in porosity number of third stage.

  • PDF

Effects of Substrate Materials on the Porosity Formation of Spary Cast Deposit (분사주조 성형체의 기공형성에 대한 기판재료의 영향)

  • Kim, Dong-Gyu
    • Journal of Korea Foundry Society
    • /
    • v.13 no.5
    • /
    • pp.476-483
    • /
    • 1993
  • The influence of substrate materials on the degree of basal porosity during spray casting process has been investigated. Different conditions of droplet spreading on the substrate were induced by varying the substrate material. Flat sections of cast iron and aluminum have been spray deposited via spray casting process onto an aluminum substrate, a low carbon steel substrate, and an alumina based refractory substrate. Results for cast iron and aluminum sprayed onto the aluminum substrate showed significant improvements in the surface condition and degree of basal porosity with evidence of substrate deformation that round pits ranging from $5{\mu}m$ to $20{\mu}m$ in diameter are distributed on the surface of aluminum substrate. The lowest level of porosity was developed in alumina based refractory material. Several mechanisms for porosity formation were discussed with droplet impact pressure and droplet spreading. Adopting a spray cutting mechanism for removing the periphery of spray cone, porosity level was remarkably decreased.

  • PDF

Fabrication of Low Density Sintered Stainless Steel Filter

  • Seok, Se-Hoon;Park, Dong-Kyu;Jung, Kwang-Chul
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.611-612
    • /
    • 2006
  • In a manufacturing technique of the sintered filter, pressureless sintering method has good permeability, it is not need the binder and lubricant used on compacting process, so it has little contamination and it is easy to control the pore size and shape but the mechanical strength is low relatively and it is difficult that parts of complicate form are manufactured. In the case of manufacturing the filter by press and sintering method, in order to be satisfactory characteristic of un-pressed filter, in this study sintered metal filter fabricated by using 30-40mesh stainless steel 316L powder and additive agents. Porosity and structure of pores, permeability and mechanical strength of the sintered filter were investigated with the variation sintering conditions. Porosity was nearly constant about $60{\sim}70%$, density, permeability and mechanical strength were changed markedly with quantity of additive materials and sintering conditions.

  • PDF

Effect of Clay-Mineral Composition on Flexural Strength of Clay-based Membranes (점토 광물 조성이 점토기반 분리막의 곡강도에 미치는 영향)

  • Lee, Young-Il;Eom, Jung-Hye;Kim, Young-Wook;Song, In-Hyuck
    • Journal of the Korean Ceramic Society
    • /
    • v.51 no.5
    • /
    • pp.380-385
    • /
    • 2014
  • Clay-based membranes with submicron pore size were successfully prepared by a simple pressing process using low-cost starting materials(e.g., kaolin (K), bentonite (B), talc (T), and sodium borate). The green bodies were sintered at $1000^{\circ}C$ for 2 h in air. The effect of clay-mineral composition on the flexural strength of clay-based membranes was investigated. The porosity of the clay-based membranes could be controlled within the range of 34 - 42% by adjusting the starting composition. The flexural strength of the low-cost membranes depended on both the porosity and the ${\alpha}$-quartz content. In turn, the porosity and ${\alpha}$-quartz content were affected by the (B+T) /(K+B+T) ratio. The plot of strength relative to this ratio, showed a maximum when the ratio was 0.4. The typical flexural strength of these clay-based membranes (with ratio 0.4) was 28 MPa at 34% porosity.

Low Temperature Processing and Properties of Porous Frit-Bonded SiC Ceramics (프릿을 이용한 다공질 SiC 세라믹스의 저온 제조 공정 및 물성)

  • Chae, Su-Ho;Kim, Young-Wook;Song, In-Hyuck;Kim, Hai-Doo;Bae, Ji-Soo;Na, Sang-Moon;Kim, Seung-Il
    • Journal of the Korean Ceramic Society
    • /
    • v.46 no.5
    • /
    • pp.488-492
    • /
    • 2009
  • Porous frit-bonded SiC ceramics were successfully prepared at a temperature as low as $800^{\circ}C$ from SiC, frit, and microbeads (glass or polymer). The effects of SiC starting particle size and microbead addition on microstructure, porosity, and flexural strength were investigated. The addition of hollow glass microbead improved the strength of frit-bonded SiC ceramics without the loss of porosity by acting additional binder phase between SiC grains. The 65 ${\mu}m$-sized SiC resulted in lower porosity and higher strength than 50 ${\mu}m$-sized SiC because of higher packing density. Typical flexural strengths of frit-bonded SiC were 23 MPa at 46% porosity and 19 MPa at 49% porosity.

Analysis of a functionally graded nanocomposite sandwich beam considering porosity distribution on variable elastic foundation using DQM: Buckling and vibration behaviors

  • Nejadi, Mohammad Mehdi;Mohammadimehr, Mehdi
    • Computers and Concrete
    • /
    • v.25 no.3
    • /
    • pp.215-224
    • /
    • 2020
  • In the present study, according to the important of porosity in low specific weight in comparison of high stiffness of carbon nanotubes reinforced composite, buckling and free vibration analysis of sandwich composite beam in two configurations, of laminates using differential quadrature method (DQM) is studied. Also, the effects of porosity coefficient and three types of porosity distribution on critical buckling load and natural frequency are discussed. It is shown the buckling loads and natural frequencies of laminate 1 are significantly larger than the results of laminate 2. When configuration 2 (the core is made of FRC) and laminate 1 ([0/90/0/45/90]s) are used, the first natural frequency rises noticeably. It is also demonstrated that the influence of the core height in the case of lower carbon volume fractions is negligible. Even though, when volume fraction of fiber increases, the critical buckling load enhances smoothly. It should be noticed the amount of decline has inverse relationship with the beam aspect ratio. Investigating three porosity patterns, beam with the distribution of porosity Type 2 has the maximum critical buckling load and first natural frequency. Among three elastic foundations (constant, linear and parabolic), buckling load and natural frequency in linear variation has the least amount. For all kind of elastic foundations, when the porosity coefficient increases, critical buckling load and natural frequency decline significantly.

Synthesis and Densification of $Ti_5Si_3$-base Intermetallic Compounds by Reactive Sintering and Electro-Pressure Sintering (반응소결법 및 통전가압소결법에 의한 $Ti_5Si_3$계 금속간화합물의 합성 및 치밀화)

  • 유호준
    • Journal of Powder Materials
    • /
    • v.4 no.4
    • /
    • pp.283-290
    • /
    • 1997
  • $Ti_5Si_3$ intermetallics containing 0-6 wt% of Cu were made by reactive sintering (RS) under vacuum using elemental powder mixtures (Process 1), electro-pressure sintering (EPS) using RS'ed materials (Process2), and EPS using elemental powder mixtures (Process 3). Relatively low dense titanium silicides were gained by process 1, in which porosity decreased with increasing Cu content. For example, porosity changed from 42 to 19.4% with the increase in Cu content from 0 to 6 wt%, indicating that Cu is a useful sintering aid. The titanium silicides fabricated by Process 2 had a higher density than those by Process 1 at given composition, and porosity decreased with increasing Cu content. For example, porosity decreased from 38 to 6.8% with the change in Cu content from 0 to 6 wt%. A high dense titanium silicides were obtained by Process 3. In this Process, porosity decreased a little by Cu addition, and was almost insensitive to Cu content. Namely, about 9 or 7% of porosity was shown in 0 or 1-6 wt% Cu containing silicides, respectively. The hardeness increased by Cu addition, and was not changed markedly with Cu content for the silicides fabricated by Process 3. This tendency was considered to be resulted from porosity, hardening of grain interior by Cu addition, and softening of grain boundary by Cu-base segregates. All these results suggested that EPS using elemental powder mixtures (Process 3) is an effective processing method to achieve satisfactorily dense titanium silicides.

  • PDF

Assessing the effects of mineral content and porosity on ultrasonic wave velocity

  • Fereidooni, Davood
    • Geomechanics and Engineering
    • /
    • v.14 no.4
    • /
    • pp.399-406
    • /
    • 2018
  • The influences of mineral content and porosity on ultrasonic wave velocity were assessed for ten hornfelsic rocks collected from southern and western parts of the city of Hamedan, western Iran. Selected rock samples were subjected to mineralogical, physical, and index laboratory tests. The tested rocks contain quartz, feldspar, biotite, muscovite, garnet, sillimanite, kyanite, staurolite, graphite and other fine grained cryptocrystalline matrix materials. The values of dry unit weight of the rocks were high, but the values of porosity and water absorption were low. In the rocks, the values of dry unit weight are related to the presence of dense minerals such as garnet so not affected by porosity. The statistical relationships between mineral content, porosity and ultrasonic wave velocity indicated that the porosity is the most important factor influencing ultrasonic wave velocity of the studied rocks. The values of P-wave velocity of the rocks range from moderate to very high. Empirical equations, relevant to different parameters of the rocks, were proposed to determine the rocks' essential characteristics such as primary and secondary wave velocities. Quality indexes (IQ) of the studied samples were determined based on P-wave velocities of them and their composing minerals and the samples were classified as non-fissured to moderately fissured rocks. Also, all tested samples are classified as slightly fissured rocks according to the ratio of S-wave to P-wave velocities.

Surface Image Analysis for Evaluating Porosity and Permeability Coefficient of Permeable Concrete Block (투수 콘크리트 블록 공극률 및 투수계수 평가를 위한 표면 이미지 분석 기법 개발)

  • Jo, Sangbeom;Son, Younghwan;Kim, Donggeun;Jeon, Jihun;Kim, Taejin
    • Journal of The Korean Society of Agricultural Engineers
    • /
    • v.65 no.2
    • /
    • pp.47-57
    • /
    • 2023
  • The increase of impermeable area ratio is causing hydrologic cycle problems in urban areas and groundwater depletion in rural areas, permeable pavements are getting attention to expand permeable areas. The performance of the permeable concrete block pavement, which is part of the permeable pavement, is greatly affected by the porosity. In addition, the permeability coefficient is a major factor when designing permeable concrete block pavement. Existing porosity and permeability test methods have problems such as uneconomical or poor field applicability. The object of this study was to develop a methodology for evaluating porosity and permeability coefficient using a surface image of a permeable concrete block. Specimens are manufactured with various porosity ranges and porosity and permeability tests are performed. After surface image preprocessing, normalization and binarization methods were compared. Through this, the method with the highest correlation with the lab test result was determined. From the results, the PDR (pore determined ratio) was obtained. Simple linear regression analysis is performed with PDR and lab test results. The results showed a high correlation of R2 more than 0.8, and the errors were also low.

Fabrication and Wear Property Evaluation for FeCrSi/AC8A Composite by Low-pressure Infiltration (저압함침법에 의한 FeCrSi/AC8A 복합재료의 제조와 마모특성 평가)

  • Song, Tae-Hoon;Lee, Hyun-Jun;Choi, Yong-Bum;Kim, Sung-Jin;Park, Won-Jo
    • Journal of Ocean Engineering and Technology
    • /
    • v.22 no.5
    • /
    • pp.106-111
    • /
    • 2008
  • In this paper, study about property evaluation for the metal matrix composites fabricated by low pressure infiltration process. Aluminum alloy composite which is reinforced by Metal fiber preform was fabricated by low pressure casting process. Infiltration condition was changed the pressure infiltration time of 1 sec, 2 sec and 5 sec under a constant pressure of 0.4 MPa. The molten alloy completely infiltrated the FeCrSi metal perform regardless of the increase in the pressure acceleration time. The the porosity in the FeCrSi/AC8A composite was investigated. The porosity was reduced as the pressure acceleration time as shorter. The FeCrSi/AC8A composite was investigated the wear test for to know the relationship between Porosity and wear resistance. FeCrSi/AC8A composite at pressure acceleration time of 1sec is shown excellent wear resistance.