Proceedings of the Korean Society of Precision Engineering Conference
/
1997.04a
/
pp.567-571
/
1997
Recently, automobile industry has led to increasing use of aluminum alloy for weight reduction. Automobile made of aluminum alloy can be given lighter, stronger and a harder surface by anodizing than one made of steel-alloy. In this paper, we investigate the influence of lap length, adherend thickness and adhesive thickness on adhesive strength of single-lap adhesive joints by conducting tensile-shear tests. Single-lap adhesive joints of aluminum was calculated using joint factor by using adhesive length, adherend thickness of specimen.
Transactions of the Korean Society of Mechanical Engineers
/
v.18
no.1
/
pp.85-92
/
1994
With the wide application of fiber-reinforced composite meterial in aircraft space structures and robot arms, the design and manufacture of composite joints have become a very important research area because they are often the weakest areas in composite structure. In this paper, the torque transmission capacities of the adhesive tubular single lap joint and double lap joint were studied. The stress and torque transmission capacity of the adhesive joints were analyzed by the finite element method and compared to the experimental results. The torque capacity of the double lap joint was increased 2.7 times over that of the single lap joint. Also, the fatigue limit of the double lap joint was increased 16 times over that of the single lap joint.
Journal of the Korea Academia-Industrial cooperation Society
/
v.19
no.5
/
pp.570-576
/
2018
In reinforced concrete structures, the joints of ordinary rebars are usually lap joints, which are bound by binding wires with rebars, and mechanical joints by couplers. In domestic design standards (concrete design code), welded lap joints are restricted for ordinary rebars, but overseas standards allow welded lap joints of ordinary rebars through pre-heating. This study investigated the domestic and international standards/criteria and evaluated the fracture strength by performing the tensile test on the lap welded joint of SD400 grade rebars, which is used the most in the construction sites. The weld length of the specimen for weld lap joints is based on the minimum weld length (8d) given in the KS standard (KS B ISO 17660-1). According to AWS D1.4, the preheating temperature was set to $150^{\circ}C$ for D19 and below, and $260^{\circ}C$ for D22 and above. In the test results, the tensile strength of rebars with welded lap joints exceeded the required strength (125% of the yield strength) according to the concrete design code. To analyze the effect of preheating, the tensile strength of the welded rebars after preheating was not significantly different from that of the welded rebars without preheating. The carbon equivalent content (Ceq) of the rebars used in the test was 0.45% or less. Under AWS D1.4, no preheating is required if the carbon equivalent is less than 0.45%. All specimens with a welded lap length of 8d failed by a bar fracture. The effect of preheating was confirmed to be insignificant due to the low carbon equivalent of the rebar.
In this study, the bonding strengths of adhesively bonded joints are experimentally investigated. A series of lap-shear tests are conducted using single lap type adhesive joints. In order to analyse the joint fabrication factors that affected the bonding strength, the parametric tests are conducted with various thickness of adhesive, surface roughness and fillet of adhesive. In addition, for the comparative study with the welded joint, lap-shear tests using specimens with 2 welded sides and 4 welded sides are also carried out. The quantitative results of the strength analysis are summarized, and some proposals are made on setting up testing standards for adhesively bonded joints.
Transactions of the Korean Society of Mechanical Engineers A
/
v.24
no.8
s.179
/
pp.2022-2031
/
2000
Since the surface roughness of adherends affects much the strength of adhesivelybonded joints, the effect of surface roughness on the fatigue life of adhesively bonded tubular single lap joints was investigated analytically and experimentally by fatigue torsion test. The stiffness of the interfacial layer between adherends and adhesive was modeled as a normal statistical distribution function of surface roughness of adherends. From the investigation, it was found that the optimum surface roughness of adherends for the fatigue strength of tubular single lap joints was dependent on bondthickness and applied load.
Experimental results are presented from tests conducted on reinforced concrete beam-column joints with lap splices under reversed cyclic loading simulating earthquake action. Response curves are compared for twenty-four specimens designed according to Eurocode 2. The main parameters of the investigation are, the geometry of the reinforcing bar extension, the applied axial load (normalized), the available cover over lap splice region extended as length required from Eurocode 2, as well as the shape and the volumetric percentage of the stirrups confining the lap splice zone. The results are evaluated with regards to the load intensity, the energy absorption capacity and the characteristics of the load deflection curve.
Journal of the Korean Society for Nondestructive Testing
/
v.19
no.6
/
pp.439-447
/
1999
One of the problems for practical use of fiber-reinforced plastics is the performance degradation by fatigue damage in the joints. The study is to develop a nondestructive technique for real-time evaluation of adhesively bonded composite-metal joints. From the prior study we confirmed that the bonding strength can be estimated from the correlation between the qualify of bonded parts and AUP's. We obtained a curve showing the correlation between the degree of fatigue damage and AUP's calculated from signals acquired during fatigue loading of single-lap and double-lap joints of CFRP and Al6061. The curve is an analogy to the one showing stiffness reduction ($E/E_o$) of polymer matrix composites by fatigue damage. From those facts, it is plausible to predict the degree of fatigue damage in real-time. Amplitude and AUP2 appeared to be optimal parameters to provide more reliable results for single-lap joints whereas Amplitude and AUP2 did for double-lap joints. It is recommended to select optimal parameters for different geometries in the application for real structures.
Transactions of the Korean Society of Automotive Engineers
/
v.13
no.5
/
pp.42-49
/
2005
In general, multi-lap spot weld joints are frequently present in automobile. Most research, however, has been focused on the single-lap spot weld joints until now. In this paper, tensile-shear strength tests are performed to examine the weldability of 3-lap spot joint welded by using the high strength steel sheet and the zinc coated steel sheet. The indentation depth and nugget diameter are used to propose the optimum welding conditions. The weldability is affected by the welding current and welding time for 3-lap spot joint. Meanwhile the expulsions is round to decrease with the increase of electrode force. The optimum welding conditions are presented for 3-lap spot joints of high strength steel sheet and zinc coated steel sheet.
Transactions of the Korean Society of Automotive Engineers
/
v.11
no.6
/
pp.101-107
/
2003
Since stainless steel sheets have good mechanical properties, weldability, appearance and corrosion resistance, they are commonly used as one of the structural materials of the railroad cars or the commercial vehicles which are manufactured by the spat welding. Among the many kinds of spot welded lap joints, it can be found that multi-lap joints are employed in their body structure. But, fatigue strength of these joints is lower than that of base metal due to high stress concentration at the nugget edge of spot weld and is considerably influenced by welding conditions as well as the mechanical and geometrical factors. Thus, it is necessary to establish a reasonable and systematic design criterion for the long life design of the spot-welded body structures. In this paper, the stress distribution and deformation around the spot-welded multi-lap joints subjected to tensile shear load was numerically analyzed. Also, the $\Delta$P-Nf curve was obtained by fatigue tests. Using these results, $\Delta$P-Nf curves were rearranged in to the ${\Delta}{\sigma}$-Nf relation with the maximum stress at nugget edge of spot weld.
Journal of the Korean Society of Manufacturing Technology Engineers
/
v.7
no.1
/
pp.58-68
/
1998
Advantages of adhesively bonded joints and techniques of weight reduction have led to increasing use of structural adhesives such as LSI(large scale integration) package, automobile, aircraft in the various industries. In spite of such wide applications of adhesively bonded joints, the evaluation method of bonding strength has not been established. Stress singularity occurs at the interface edges of adhesively bonded joints and it is required to analyze it. In this paper, the stress singularity using 2-dimensional elastic boundary element method (BEM) with the changes of the lap length and adhesive for single lap joint was analyzed, and experiments of strength evaluation were carried out. As the results, the evaluating method of bonding strength considering stress singularity at interface edges of adhesively bonded joints and stress intensity factor of interface crack have been proposed in static and fatigue test.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.