• 제목/요약/키워드: iron-copper alloy

검색결과 27건 처리시간 0.024초

Fe-Cu계 소결합금의 이상팽창에 관한 연구 (I) (A Study on Abnormal Expansion of Fe-Cu Sintered Alloy)

  • 송영준;김윤채
    • 한국분말재료학회지
    • /
    • 제11권5호
    • /
    • pp.383-390
    • /
    • 2004
  • In order to investigate behavior of abnormal expansion of the iron-copper compacts, we compared the dilatometric curves of the compacts which mixed the copper powder to the iron powder with those of compacts which mixed the copper powder to the iron-copper alloy powder. The dilatometric curves were obtained below the sintering conditions, which heated up to 115$0^{\circ}C$ by a heating rate of 1$0^{\circ}C$/min, held for 60min at 115$0^{\circ}C$ and cooled down at a rate of 2$0^{\circ}C$/min to room temperature. The dilatometric curves of the compacts showed the different expansion behavior at temperatures above the copper melting point in spite of same chemical composition. All of the compacts of former case showed large expansion, but all of the compacts in latter case showed large contraction. The microstructures of sintered compacts also showed the different progress in alloying of the copper into the iron powder. Namely we could observe the segregation at alloy part of copper into iron powder in case of the sintered compacts, which mixed the copper powder to the iron powder, but could not observe the segregation in compacts which mixed the copper powder to the iron-copper alloy powder. But the penetration of liquid copper into the interstices between solid particles was occurred at both cases. Therefore, the showing of the different dimensional changes in the compacts in spite of same chemical composition is due to more the alloying of copper into iron powder than the penetration of liquid copper into the interstices between solid particles.

Expansion Behavior of Iron-copper Compact Made from (Fe-Cu) Prealloyed Powder

  • Kim, Youn-Che;Suk, Myung-Jin
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.812-813
    • /
    • 2006
  • Dimensional change of compact made from (Fe-Cu) prealloyed powder and copper powder compared to that of compact made from iron-copper elemental powder. The compact made from the prealloyed powder with a copper content of 7.18mass% which is nearly equal to its solution limit and copper powder showed only the large contraction in spite of penetration of liquid copper into grain boundary of the prealloyed powder. But the compact made from iron-copper elemental powder showed the large expansion in spite of same chemical composition with former case.

  • PDF

The Pitting Inhibition of Fe-Cu Alloy in Weakly Alkaline Solution under Wet-Dry Condition

  • Kim, Je-Kyoung;Kang, Tae-Young;Moon, Kyung-Man
    • 전기화학회지
    • /
    • 제10권3호
    • /
    • pp.175-178
    • /
    • 2007
  • Pure iron, Fe-0.4, and 1.2 wt.%Cu alloys were examined by conducting the electrochemical techniques in the weakly alkaline solution, pH9, controlled by $Ca(OH)_2$, solution added with 0.02M NaCl. The $R_P$ measured from ac impedance, selected 10 kHz and 10mHz, in weakly alkaline solutions containing chloride ions indicated that the addition of copper up to 1.2wt.% into the pure iron significantly improved the pitting resistance of iron. In contrast to alloy, the pure iron showed the rapid pitting occurrences in drying period. During the drying period, the corrosion potential of pure iron was shifted to less noble value, pitting initiation.

Characterization of Microstructure and Mechanical Properties of High-Purity Iron Added with Copper

  • Taguchi, O.;Lee, Su Yeon;Uchikoshi, M.;Isshiki, M.;Lee, Chan Gyu;Suzuki, S.;Gornakov, Vladimir S.
    • 열처리공학회지
    • /
    • 제25권1호
    • /
    • pp.22-26
    • /
    • 2012
  • An influence of the addition of copper (0.5, 1.0 and 1.5 mass% Cu) on the microstructure and mechanical properties of high purity iron (99.998 mass%) was characterized. The microstructure and microhardness of high-purity iron based samples, which were rolled at room temperature and subsequently annealed, were investigated in this work. The microstructure of the samples has been observed by electron back scattering diffraction (EBSD) and the mechanical properties have been studied by using micro-Vickers hardness test. The results of microstructural observation showed that deformation band was formed in high purity iron by rolling at room temperature, and it was recovered by annealing up to about 900 K. The microhardness results showed that the softening of high-purity iron occurred by annealing up to about 900 K, while the hardness of iron added with about 0.5-1.5 mass% copper was kept over 100 Hv and at the early time of annealing reached a maximum. The hardness of iron added with a small amount of copper may be attributed to precipitation hardening as well as solution hardening. The orientation of crystal in recrystallized grain was almost same as that of deformed grain.

알루미늄-스테인레스스틸-구리 경사기능재료의 제조 및 특성평가 (Fabrication and Evaluation of the Al-STS-Cu Functionally Graded Materials)

  • 박광재;김다솜;권한상
    • Composites Research
    • /
    • 제36권4호
    • /
    • pp.241-245
    • /
    • 2023
  • 비철계 합금인 알루미늄과 구리 합금은 전기 및 열전도성이 우수하지만 철계 합금대비 상대적으로 기계적 특성은 낮다. 철계 합금인 스테인레스 스틸은 비철계인 알루미늄과 구리 대비 가공성은 나쁘지만 기계적 특성과 내부식성이 우수하여 고강도 공업용 소재로 사용되고 있다. 본 연구에서는 알루미늄과 구리 그리고 스테인레스 스틸을 융복합화 하여 기능 맞춤형 경사기능재료를 분말프로세스를 이용하여 제조하였다. 제조된 경사기능재료는 구리와 철계 합금 대비 경량의 우수한 표면 경도를 나타내었으며 열전도도 역시 단일 알루미늄과 스테인레스 스틸 소재 보다 높은 값을 나타내었다.

국립김해박물관(國立金海博物館) 개관(開館) 전시유물 보존처리 보고(報告) (Report on the Conservation Treatment for the Artifacts Exhibited in the newly-opened Kimhae National Museum)

  • 권혁남;안병찬
    • 박물관보존과학
    • /
    • 제1권
    • /
    • pp.15-26
    • /
    • 1999
  • 국립김해박물관의 개관을 위해 전시유물 200여점을 보존처리 하였다. 처리유물은 대부분 고분출토품이며 재질은 금동, 은, 구리합금제, 철제 등 금속유물이 주종을 이루고 있다. 모두 고대 가야문화를 대표하는 문화재들이다. 유물은 상태에 따라 처리방법을 달리했다. 구리합금제 유물은 부식물의 안정성에 따라 보존과 제거를 결정했다 특히 철제품의 경우 현재 안정한 상태의 유물은 물리적인 방법으로 이물질을 제거해 원형을 찾고 방녹제[상품명:Ballistol]를 이용해 부식을 예방하는데 중점을 두었다. 부식이 진행중인 유물은 원인제거를 위해 2단계 탈염처리를 했다. 제 1단계는 0.3M NaOH 용액함침, 제 2단계는 붕사-증류수 가압탈염법이다. 이밖에 전시를 위한 특수 받침대제작 및 각종 전시보조물인 모형 등에 대한 수정작업도 지원했다.

Microstructural Characterization of Gas Atomized Copper-Iron Alloys with Composition and Powder Size

  • Abbas, Sardar Farhat;Kim, Taek-Soo
    • 한국분말재료학회지
    • /
    • 제25권1호
    • /
    • pp.19-24
    • /
    • 2018
  • Cu-Fe alloys (CFAs) are much anticipated for use in electrical contacts, magnetic recorders, and sensors. The low cost of Fe has inspired the investigation of these alloys as possible replacements for high-cost Cu-Nb and Cu-Ag alloys. Here, alloys of Cu and Fe having compositions of $Cu_{100-x}Fe_x$ (x = 10, 30, and 50 wt.%) are prepared by gas atomization and characterized microstructurally and structurally based on composition and powder size with scanning electron microscopy (SEM) and X-ray diffraction (XRD). Grain sizes and Fe-rich particle sizes are measured and relationships among composition, powder size, and grain size are established. Same-sized powders of different compositions yield different microstructures, as do differently sized powders of equal composition. No atomic-level alloying is observed in the CFAs under the experimental conditions.

Fabrication and Characterization of Immiscible Fe-Cu Alloys using Electrical Explosion of Wire in Liquid

  • Phuc, Chu Dac;Thuyet, Nguyen Minh;Kim, Jin-Chun
    • 한국분말재료학회지
    • /
    • 제27권6호
    • /
    • pp.449-457
    • /
    • 2020
  • Iron and copper are practically immiscible in the equilibrium state, even though their atomic radii are similar. As non-equilibrium solid solutions, the metastable Fe-Cu alloys can be synthesized using special methods, such as rapid quenching, vapor deposition, sputtering, ion-beam mixing, and mechanical alloying. The complexity of these methods (multiple steps, low productivity, high cost, and non-eco-friendliness) is a hinderance for their industrial applications. Electrical explosion of wire (EEW) is a well-known and effective method for the synthesis of metallic and alloy nanoparticles, and fabrication using the EEW is a simple and economic process. Therefore, it can be potentially employed to circumvent this problem. In this work, we propose the synthesis of Fe-Cu nanoparticles using EEW in a suitable solution. The powder shape, size distribution, and alloying state are analyzed and discussed according to the conditions of the EEW.

구상흑연주철의 경화능 (Hardenability of Ductile Cast Iron)

  • 이영호
    • 열처리공학회지
    • /
    • 제1권1호
    • /
    • pp.13-23
    • /
    • 1988
  • The hardenability of alloyed ductile cast irons was studied for 54 different alloy compositions obtained from eight commercial and laboratory foundries. The alloying elements investigated for their effects on hardenability were Si(2.0 to 3.0%), Mn(0.0 to 0.8%), Mo(0.0 to 0.6%), Cu(0.0 to 1.5%), and Ni(0.0 to 1.5%). Two hardenability criteria, a first-pearlite hardenability criterion and a half-hard hardenability criterion, were used to determine hardenability of ductile irons. Prediction models for each hardenability criterion were developed by multiple regression analysis and were well agreed with previous experimental results. Molybdenum was the most potent hardenability promoting element followed by manganese, copper and nickel ; silicon had little effect on hardenability and reduced the hardenability as silicon content increased. When alloying elements were presented in combination, strong synergistic effects on the hardenability were observed especially between molybdenum, copper and nickel. The hardenability of ductile iron was strongly influenced by austenitizing temperature. Increasing austenitizing temperature up to $955^{\circ}C$, hardenability increased gradually but decreasing rate and then decreased as temperature increased above $955^{\circ}C$. Unless reducing segregation by very long-time annealing treatment, the hardenability of ductile iron was not significantly influenced by segregation of alloying elements.

  • PDF

The Effect of Annealing Heat Treatment by Anodic Polarization Impedance Experiments for Cu-10%Ni Alloy

  • Lee, Sung-Yul;Moon, Kyung-Man;Jeong, Jae-Hyun;Lee, Myeong-Hoon;Baek, Tae-Sil
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제39권5호
    • /
    • pp.536-541
    • /
    • 2015
  • Copper has been used extensively as an electric wire or as a base material in various types of machineries owing to its good electrical and thermal conductivity and good fabricating property, as well as its good corrosion resistance compared to iron. Furthermore, the copper-nickel alloy has significant corrosion resistance in severely corrosive environments. Although, cupro-nickel alloy shows better corrosion resistance than the brass and bronze series, this alloy also corroded in severely corrosive environments, including aggressive chloride ions, dissolved oxygen, and condition of fast flowing seawater. In this study, and annealing treatment at various annealing temperatures was carried out on the cupro-nickel (Cu-10%Ni) alloy, and the effects of annealing were investigated using electrochemical methods, such as measuring the polarization and impedance behaviors under flowing seawater conditions. The corrosion resistance increased by annealing compared to non heat treatment in the absence of flowing seawater. In particular, the sample annealed at $200^{\circ}C$ exhibited the best corrosion resistance. The impedance in the presence of flowing seawater showed higher values than in the absence of flowing seawater. Furthermore, the highest impedances was observed in the sample annealed at $800^{\circ}C$, irrespective of the present of flowing seawater. Consequently, the corrosion resistance of cupro-nickel (Cu-10%Ni) alloy in a severely corrosive environment can be improved somewhat by annealing.