Effect of Copper Retention on Copper Leaching in Wood Treated with Copper-based Preservatives

  • Ra, Jong-Bum;Kang, Sung-Mo;Kang, Shin-Kwon
    • Journal of the Korean Wood Science and Technology
    • /
    • v.37 no.5
    • /
    • pp.421-425
    • /
    • 2009
  • This research investigates the effect of copper retention on copper leaching in wood treated with copper-based preservatives. Radiata pine (Pinus radiata D. Don) sapwood samples were ground in a Wiley mill equipped with a 20-mesh screen. The ground wood was vacuum-treated with various concentrations of alkaline copper quat (ACQ), bis-(N-cyclohexyl-diazeniumdioxy)-copper (CB-HDO), and copper azole (CUAZ). The treated samples were conditioned at $70^{\circ}C$ and 100% RH for 72 hours. The samples were leached by using the distilled water for four weeks, and the copper contents in each sample were measured by X-ray spectroscopy. As expected, the copper leaching was increased with increasing of copper retention. The copper leaching from the ACQ and CB-HDO treated samples were gradually decreased with increasing copper retention: however, the copper losses from the CUAZ treated samples appeared to be proportionally increased with the increase in copper retention in all retention levels tested. The results indicate that at the conditions of the same copper retention ACQ and CB-HDO treated wood have a better leaching resistance compared to CUAZ treated wood.

The Study of the Changeable Table Design with Units that made of Wasted Wood (소경단목재(小輕短木材) 접목을 활용한 유니트 가변형 테이블디자인 연구개발)

  • Kim, Myeong-Tae;Seo, Seok-Min
    • Journal of the Korea Furniture Society
    • /
    • v.23 no.1
    • /
    • pp.26-37
    • /
    • 2012
  • This is the study about the New Formation Developement, the Changeable Table Design with Units that made of Wasted Wood to use restricted material rationally and to improve the space efficiency in the Table Design. We made some changeable table design with units that made of laminated wood wasted. And we found out the following formative characteristic and physical merits through this study. First, the space efficiency can be improve technically through the unit combination and organic transfomation of the specific form and a new method by laminated wood make the personal originality and the structral stability be built up. Second, there are some merits, moveable convenience and variable layout by the combination or transformation or personal fondness so that economical efficiency and variable of design can be improved. Third, we can remove original faults inside wood like a knot or not-uniform of wood organ when we laminate wood so that we use proper units that have original beauty of wood and can represent mild mood of furniture wholly. Fourth, much more strengthen tensile strength by the reciprocal action among the units that be made of laminated wood reduces wood's metamorphosis like bending or twisting so that the uniformity of wood can be gain and furniture's metamorphosis can be reduced. According to changes of nature environment, the difficulty of supply and demand for wood may be happen. According to changes of life style these days, supply and demand for environment friendly material, processing technique and developement of design to improve the efficiency of using space must be very important factor in morden furniture design. So we propose changeable furniture design by using new environment friendly meterial and processing method from this study.

  • PDF

Radon Exhalation from Five Wood Species

  • Lee, Ju Yong;Choi, Gyu Woong;Kang, Seog Goo
    • Journal of the Korean Wood Science and Technology
    • /
    • v.46 no.6
    • /
    • pp.735-747
    • /
    • 2018
  • Radon radiation exposures in home have been posed as a potential cancer hazard. This research aims to present the basic data of the indoor radon concentration level by examining the radon exhalation rates of wood species. Radon exhalation rates from five commonly used wood species in Korean wood building construction were measured with Continuous Radon Monitor (CRM), Model 1028 (Sun Nuclear Co., USA) using the Closed Chamber Method (CCM). The mass exhalation rate was observed to vary from $0.00089Bq{\cdot}kg^{-1}{\cdot}h^{-1}$ to $0.00181Bq{\cdot}kg^{-1}{\cdot}h^{-1}$, whereas the surface exhalation rate was observed to be $0.00677-0.01517Bq{\cdot}m^{-2}{\cdot}h^{-1}$. The radon exhalation rate of Quercus accutissima Carruth (white oak) which has the highest density showed the highest figure among the five wood species, on the other hand, the rest of four species showed similar results which were similar to the radon exhalation rates of wood in the U.S.A. and Canada. The average of the concentration measured by the CCM represented well up to the second half-life period (7.7 days). Because result of these small quantities seems to indicate that radon exhalation from the tested wood species has almost negligible impact, the main culprit of the high indoor radon concentration is clearly derived from the background of surrounding wood house. Therefore, as a safety precaution, infrastructures made of wood materials should be designed with the consideration of influx of radon and built accordingly. Furthermore, it is highly desirable that wood will be needed to use for furniture and interior finishing material in indoor environment.

Microscopic Observation of Kenaf by Optical and Scanning Electron Micrograph (Kenaf 구성 세포의 현미경적 관찰)

  • Yoon, Seung-Lak
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.41 no.2
    • /
    • pp.47-54
    • /
    • 2009
  • Anatomical characteristics of kenaf were investigated in transverse, radial and tangential direction by optical and scanning electron micrograph. Kenaf was made up of bast fibers, wood fibers, vessels and parenchyma cells. Bast fibers were long slender cells with different types of pits. The shape of wood fibers were in various ways and pointed at the ends. The pits were observed on the surface of bast fibers. Kenafs were diffuse and radial porous. and composed of solitary pores and two or three radial pore multiples. Various types of vessels were observed. The pits showed alternate pitting and larger diameter than other cells. Parenchyma cells were rectangular or square with different shapes of pith parenchyma cells compared to conventional types of parenchyma cells in wood. The number of pith on the surfaces were small.

Manufacture of Rainbow-colored Veneer by Natural Dyeing

  • Suh, Jin Suk;Park, Ryeong Jae;Cho, Yeong Hee;Song, Eon Ja;Kim, Jong In;Park, Sang Bum
    • Journal of the Korea Furniture Society
    • /
    • v.26 no.3
    • /
    • pp.286-290
    • /
    • 2015
  • The wood veneers were clearly rainbow-colored with natural dyes. As shown through Korean-style jacket with stripes of multi-colors beyond traditional obang colors (red, blue, yellow, black and white colors), eco-friendly coloring methods representing Korean colors familiar from old times could be used nobly by coloring natural wood veneer being raw material of wood products. In terms of industrialization, the study to manifest korean color, substituting chemical stains such as dye and pigment, would be necessary. In order to realize this purpose, the study about economical dyeing materials and characteristics, that is, mordant, dyeing and drying techniques showing environment-friendly coloring and high coloration level ought to be followed. In addition to this, investigating discoloration transition by fading test for interior and exterior uses would have to be carried out.

Changes of Distribution Coefficients of Cu, Cr, and As in Different Soil Matrix in a Laboratory Scale

  • Kang, Sung-Mo;Ra, Jong-Bum;Kim, Suk-Kuwon
    • Journal of the Korean Wood Science and Technology
    • /
    • v.37 no.2
    • /
    • pp.137-140
    • /
    • 2009
  • Chromated copper arsenate (CCA), a long history of successful preservative, have raised environmental concerns. Adsorption characteristics of domestic soils for chromium, copper, and arsenic were assessed by measuring distribution coefficient ($K_d$) values of these metal components in a laboratory scale. The results revealed that $K_d$ values were higher in chromium, followed by arsenic and copper in soil matrix. Different soil matrixes resulted in varying mobilities of CCA components. The values of $K_d$ for all three metals increased with organic matter contents. The results suggest that the mobility of metal components may be very limited to the surface area adjacent to CCA-treated wood due to their fairly large distribution coefficient ($K_d$). However, the metal components would be persistent and accumulated in the soil, resulting in high chemical concentration in service area of treated wood.

Peracetic Acid Treatment as an Effective Method to Protect Wood Discoloration by UV Light

  • PARK, Kyoung-Chan;KIM, Byeongho;PARK, Hanna;PARK, Se-Yeong
    • Journal of the Korean Wood Science and Technology
    • /
    • v.50 no.4
    • /
    • pp.283-298
    • /
    • 2022
  • Wood has always been used for various day-to-day applications such as interior or exterior construction materials, and household products. However, it can undergo photodegradation and discoloration by environmental factors including ultraviolet (UV) light, and thus has shortened its service life. Bleaching or delignification of wood surfaces is a suitable solution to stabilize wood against weathering by UV because these techniques can alter or remove the chromophores in lignin, which is a main factor of wood discoloration. To improve the color stability of wood surface according to the lifespan, surface delignification was conducted using peracetic acid (PAA) and hydrogen peroxide (HP) on the woods of Larix kaempferi and Quercus mongolica. After the PAA treatment, L* increased considerably from 60-70 to 90-95. Furthermore, wood surface color did not change significantly after UV exposure. The color differences (𝜟E*) between before and after PPA treatment of wood showed the 4.8-12.2 of L. kaempferi, and 1.7-3.7 of Q. mongolica, respectively. The lignin-related peaks in Fourier transform infrared spectroscopy (FT-IR) spectra disappeared with increased duration of PAA treatment. These results confirmed that the lignin component was partially or completely removed after the PAA treatment; the color differences (𝜟E*) clearly showed that there was a reduction in redness (a*) and yellowness (b*), and an increase in lightness (L*) owing to the removal of lignin. Based on these results, this study demonstrated that the partial removal of lignin from wood surfaces is a fundamental method for resolving photo-degradation.

Understanding the Technical Properties of Delonix regia (HOOK.) RAF. Wood: A Lesser Used Wood Species

  • Funke Grace Adebawo;Olayiwola Olaleye Ajala;Olaoluwa Adeniyi Adegoke;Timileyin Samuel Aderemi
    • Journal of Forest and Environmental Science
    • /
    • v.39 no.1
    • /
    • pp.55-64
    • /
    • 2023
  • Properties of a lesser-used wood species were investigated to determine its potential for structural utilization. Trees of Delonix regia were felled and sampled at the base, middle and top and then sectioned to inner wood, middle wood, and outer wood for variation across the axial and radial directions. Hence, selected physical and mechanical properties as well as natural durability of D. regia along the radial and axial directions were examined. Obtained data were analyzed using analysis of variance (ANOVA) at α0.05. There was no significant difference in the Moisture content (MC) of the wood but specific gravity (SG) decreased from base to top ranging from 0.35-0.44. Water absorption, volumetric swelling, and volumetric shrinkage range from 46.18-51.86%, 2.57-4.02%, and 2.26-3.96% respectively along the axial plane. The weight loss for graveyard exposure and accelerated laboratory decay test ranged from 25.14-48.00% and 32.02-44.45% respectively. Modulus of Rupture and Modulus of Elasticity values range from 29.42-72.68 Nmm2 and 3,834.54-8,830.37 Nmm2 respectively. The SG values has confirmed the species as a medium density wood and values of other properties tested showed that the wood is dimensional stable and moderately resistance to fungi and termite. Hence, it could be used for light construction purposes such as furniture and other interior woodwork.

The Analysis of Mechanism on Color Scheme and Emotional Affectivity Preferences according to Wood Material Finishing in the Cafe Images (카페 이미지에서 목재 마감재에 따른 색채배색과 감성 선호도 분석 메커니즘)

  • Choi, Jin-Kyung;Kim, Ju-Yeon
    • Journal of Korean Living Environment System
    • /
    • v.24 no.5
    • /
    • pp.654-664
    • /
    • 2017
  • The use of environmentally friendly finishing materials allows us to create a space where we can feel nature and to have stability and peace in the city center. In this paper, we examined the sensitivity of people to the three café spaces where wooden finishing materials are used in the space elements that change according to people's demands for environmentally friendly space due to pollution of living environment. First, we examined the wood and finishing materials and emotional vocabulary through literature review and previous research. Second, the values of L *, a *, b* and sR, sG and sB values were extracted by using a line spectrophotometer (Ci6X). Third, we conducted a 7 - point scale questionnaire based on the extracted 13 pairs of emotional vocabulary. Using SPSS 21, frequency analysis by descriptive statistics, crossover analysis by visiting purpose and intention, and emotional lexical factor analysis were performed. Through the study, the following points were found. First, CB (The Coffee Bean), SB (Starbucks) and HS (Hollys Coffee) showed differences in CB (65%), SB (40%) and HS (37%) in the spatial analysis. Second, CB gave color similar to the color of wall and furniture wood, but HS changed the color or brightness of wood finishing color of furniture. HS or SB showed favorable use of wood color scheme. Third, SB (26.3%) and HS (19.7%) were selected by taste. Fourth, there were differences in the items of CB, 'local-exotic' and SB 'dark-bright' in the factor value. The use of wood finishing materials differed in the atmosphere evaluation depending on the spatial factors and the color of the furniture. However, in this study, there are many factors that are insufficient in the accuracy of the ratio of the applied wood finishing material to the space element and the amount of the survey. If we further study the evaluation of emotional image according to the ratio of wood finishing materials, we think that it is necessary to study now that interest in environmentally friendly is increasing.

VOCs Emission Characteristics of Coating Materials for Wood Finishing (목재용 마감도료의 휘발성유기화합물 방출특성)

  • Park, Sang-Bum;Lee, Min;Lee, Sang-Min;Kang, Yeong-Seok
    • Journal of the Korea Furniture Society
    • /
    • v.26 no.1
    • /
    • pp.22-30
    • /
    • 2015
  • In order to prevent decay, distortion, bending, twist on wood products such as wooden furnitures, variety of coating materials were developed and used so far. The coating materials for wood finishing can be synthesized by natural resource or petroleum. However, these coating materials can cause contamination of indoor air quality due to emission of volatile organic compounds (VOCs). In this study, commercialized coating materials for wood finishing such as varnish, coat, and stain were evaluated on emission characteristics of VOCs. Among the varnish, eco-friendly products had about 15~46% lower TVOC emission ($1,042{\mu}g/m^2h{\sim}3,257{\mu}g/m^2h$, respectively, than typical product ($7,100{\mu}g/m^2h$). Natural resource based coating material showed lowest TVOC emission level. However, one of natural resource based waterborne stain showed higher TVOC emission level because waterborne stain already contained higher amount of natural VOC. Oil-based stain might not be suitable for indoor use on interior wall and furniture due to exceed amount of TVOC. Based on results, natural resource based coat or waterborne stain are recommenced to use on wood products.