• Title/Summary/Keyword: insulating breakdown

Search Result 266, Processing Time 0.022 seconds

Tracking Resistance and Aging Characteristics of Epoxy Insulating Materials by the Rotating Wheel Dip Test (Rotating Wheel Dip Test에 의한 에폭시 절연재료의 내트래킹성과 열화 특성)

  • Cho, Han-Goo
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.21 no.6
    • /
    • pp.530-537
    • /
    • 2008
  • This paper describes the results of a study on the tracking performance of outdoor insulating materials based on the rotating wheel dip test(RWDT). And, the influence of surface degradation was evaluated through such as measurement of the flashover voltage after and before tracking test, also aspects of surface degradation using scanning electron microscopy. The time to tracking breakdown of treated filled specimen is longer than untreated filled specimen. And, after the RWDT, the surface of specimen by adding untreated filler appeared heavy erosion. It was found that the addition to surface treated filler, the better tracking resistance. In the RWDT, the breakdown specimen is not affected by the dry flashover voltage, despite the fact that the surface degradation of tracking test has different state on each specimen. This suggests that wet flashover voltage play an important role in evaluating of tracking and erosion on the surface degradation in tracking test. And, the flashover voltage of specimen under wet conditions are greatly affected by the salt concentration and degree of degradation by the RWDT Because of hydrophobicity and degree of degradation by the RWDT, the flashover voltage of treated filled specimen is higher than that of untreated filled specimen. Different types of specimen may have different hydrophobicity and their surface state under contaminated conditions may not be the same.

The Particle-Initiated Breakdown Characteristics on the Spacer Surface for $SF_6$GIS ($SF_6$GIS용 스페이서 표면 파티클에 의한 절연파괴 특성)

  • 김정달;이세훈
    • Journal of the Korean Institute of Illuminating and Electrical Installation Engineers
    • /
    • v.12 no.1
    • /
    • pp.3-11
    • /
    • 1998
  • The influence due to particle contaminated on spacer surface is remarkable in the decreasing of dielectric strength in SF6 GIS. In relation with this problem, We studied, AC flash-over voltage characteristics and breakdown mechanism are investigated under metallic and insulating particle initiated condition in SF6 gas by varying the particle position, particle shape with a plane-plane electrode. The main results are as follows $\circled1$ Influence of the flash-over voltage decrease for particle position is lowest in mid gap and is highest in separated small gap on electrode. $\circled2$ The metallic particle shape which results in the more reduced flash-over voltage, the FOV saturation moved in to the region of low pressure. $\circled3$Insulating particle less than 0.6[mm] are not almost influenced by the flash-over Voltage.oltage.

  • PDF

Efficiency Estimation of Toxicity Free Eire Resistance Cable

  • Yoon, Hun-Ju;Hon, Jin-Woong
    • Transactions on Electrical and Electronic Materials
    • /
    • v.3 no.3
    • /
    • pp.34-38
    • /
    • 2002
  • In this paper, efficiency estimation of toxicity fee fire resistance cable experiments was measured smoke density of toxicity free fire resistance polyolefin insulation material and electric field dependence of tree shape in low density polyethylene (LDPE). One of the most serious causes of failure in high-voltage cables, can be an electrical discharge across an internal gab or void in the insulating material. Treeing due to partial discharge is one of the main causes of breakdown in the insulating materials and reduction of the insulation life. Therefore the necessity for establishing a method to diagnose the aging of insulation materials and to predict the breakdown of insulation and research of the fire resistance character has become important. First, we have studied on electric field dependence of tree shape in LDPE about treeing phenomena occurring on the high electrical field. Second, the measurement method is the attenuation quantity of irradiation by smoke accumulating with in a closed chamber due to non-flaming heat decomposition and flaming combustion. A main cause of fire-growth and generating toxic gas when, it bums, should be dealt with great care in life. safety design. The fire gases were occurred carbon monoxide and decomposition than in polyolefin due to incomplete combustion of PVC, which has high content of carbon in chemical compound.

Analysis of Furanic Compounds Dissolved in Transformer Oil (변압기에 용존된 Furan계 물질 분석)

  • Kim, Jae-Hoon;Lee, Byung-Sung;Lee, Sei-Hyun;Koo, Kyung-Wan;Han, Sang-Ok
    • Proceedings of the KIEE Conference
    • /
    • 2005.07c
    • /
    • pp.1909-1911
    • /
    • 2005
  • The electrical and chemical characteristics in transformer insulations are changed due to thermal stress. In the chemical property, as the Kraft paper ages, the cellulose polymer chains breakdown into shorter lengths with a corresponding decrease in both tensile strength and degree of polymerization(DP). Furthermore, cellulous chains breakdown is accompanied by an increase in the content of various furanic compounds within the dielectric liquid. It is known that furanic components in transformer oil come only from the decomposition of insulating paper rather than from the oil itself. Therefore the analysis of furan products provides a complementary technique to dissolved gas analysis for monitoring transformers when we evaluate the aging of insulating paper by the total concentration of carbon monoxide and carbon dioxide dissolved in oil only. In this paper the accelerated aging process of oil--paper samples have been investigated at a temperature up to $140^{\circ}C$ for 500 hours. The oil-paper insulation samples have been measured at intervals of 100 hours. For analysis we used high performance liquid chromatography(HPLC) in accordance with IEC 61198 method.

  • PDF

Electric Properties of Silicone Rubber on Reinforcing Agent Dependence (보강제 변화에 따른 실리콘 고무의 전기 특성)

  • 이성일
    • Journal of the Korea Safety Management & Science
    • /
    • v.6 no.1
    • /
    • pp.301-309
    • /
    • 2004
  • An inorganic filling agent, ATH (alumina trihydrate) was used to induce inorganic-organic coupling by mixing with stearic acid, acryl silane, vinyl silane as surface treatment agents in order to apply as a high voltage insulating material. Volumetric resistivity was shown to vary with surface treatment agents, and the highest value was obtained in case of the mixture with vinyl silane. The dielectric breakdown intensity was shown to decrease gradually and saturate to a stable value, possibly due to the increase of cross link density in the vinyl radicals introduced to silica surface, resulting in stable dielectric breakdown intensity in the final stages. Tracking and flame retardant properties were also shown to be the best among the samples investigated in this study.

Shape and Dielectric Strength of Thermal Bubbles in Liquid Nitrogen (액체질소 중 열기포 형상 및 절연 특성)

  • Baek, Seung-Myeong;Kim, Hae-Jong
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.28 no.5
    • /
    • pp.326-331
    • /
    • 2015
  • In this paper, we study the insulating properties of the liquid nitrogen(LN2) including the thermal bubbles. The shape of the thermal bubbles in accordance with the current change was observed in the 77 K and 65 K LN2. According to the temperature of liquid nitrogen, bubbles were generated differently. The round shape of the bubble is occurred in 77 K LN2. But the layer shape of bubble is occurred in 65 K LN2. When the bubbles present, the dielectric strength of liquid nitrogen is low. However, the breakdown patterns were different according to the electrode arrangement. AC breakdown voltage(BDV) was lower than the DC BDV due to the influence of bubbles. Therefore, the design of a high-voltage superconducting equipments should consider the bubbles.

Analysis of AC Breakdown Voltage of Composite Insulation for Dry-Air/Epoxy (건조공기/에폭시 복합절연물의 AC 파괴전압 분석)

  • Heo, Jun;Lee, Seung-Su;Lim, Kee-Joe;Jung, Hae-Eun;Kang, Seong-Hwa
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.11a
    • /
    • pp.289-290
    • /
    • 2008
  • The purpose of this paper is to analyze AC Breakdown of solid/air composite insulation depending on the thickness and the pressure of dry air for eco-friendly insulation. SF6 gas has been widely used in electric equipment as gas insulation because of high dielectric strength and arc extinguishing performance. However, because SF6 gas is one of the green house effect gases, alternative insulation such as SF6 mixture, extremely low temperature gas, vacuum, liquid and solid insulating are being investigated.

  • PDF

Characteristics of Dielectric Breakdown in Liquid Nitrogen (액체질소의 절연파괴특성)

  • 추영배;류경우;류강식;김상현
    • The Transactions of the Korean Institute of Electrical Engineers
    • /
    • v.37 no.12
    • /
    • pp.872-878
    • /
    • 1988
  • During the past few years, a great deal of attention has been directed to the application of superconductivity to the electrical systems such as superconducting power transmission lines, superconducting magnet energy storage and so on. Yet in order to develop the practical model of these electrical equiqments utilizing suprconductivety and other phenomena at cryogenic temperautre, it is necessary to know the dielectric behaviour of insulating materials at cryogenic temperature in view of reliability, safety and economy of these machines. Investigation of dielectric properties of cryogenic liquids is very important due to the dual role of those as the dielectric and cooling medium. In this study, we investigated results measured over several kinds of dielectric characteristics of liquid nitrogen taking into consideration for application of high Tc superconductor. Dependence of breakdown voltage of gap width, polarity and pressure is reported in this paper and time delay characteristics of breakdown is also the subject of this discussion.

  • PDF

Breakdown Voltage Characterization of SOI RESURF Diode Using SIPOS (SIPOS를 이용한 SOI RESURF 다이오드의 항복전압 특성)

  • Shin, Dong-Goo;Han, Seung-Youp;Choi, Yearn-Ik;Chung, Sang-Koo
    • Proceedings of the KIEE Conference
    • /
    • 1997.07d
    • /
    • pp.1621-1623
    • /
    • 1997
  • The breakdown voltage of SOI RESURF (REduce SURface Field) diode using a SIPOS (Semi Insulating POlycrystalline Silicon) layer is verified in terms of n-drift layer length and surface oxide thickness by device simulator MEDICI, and compared with conventional SOI RESURF diode. Increasing the n-drift layer length, the breakdown voltage of SOI RESURF diode using the SIPOS layer have increased and saturated at $8{\mu}m$. And it has decreased with increasing the surface oxide thickness.

  • PDF

A Study on the DC Dielectric Breakdown Properties of Epoxy Composites Containing Methacrylate/Polyurethane (Methacrylate/Polyurethane이 함유된 Epoxy 복합재료의 직류 절연 파괴 특성에 관한 연구)

  • Kim, M.H.;Kim, K.H.;Lee, D.J.;Ga, C.H.;Shin, S.K.;Kim, J.H.
    • Proceedings of the KIEE Conference
    • /
    • 1994.07b
    • /
    • pp.1357-1359
    • /
    • 1994
  • In this study, in order to improve the problem that dielectric breakdown strength decrease remarkably at high temperature, simultaneous interpenetrating polymer networks method was Introduced so that epoxy insulating material could have stable temperature characteristics and stable dielectric breakdown characteristics at whole temperature range. So network structure of epoxy/$SiO_2$ composite material was changed by adding MA and MA/PU into epoxy resin. DC voltage is applied into the specimen fabricated by this method, and then the result was compared and investigated.

  • PDF