• 제목/요약/키워드: hydration property

검색결과 146건 처리시간 0.031초

In vitro에서 키토산 연고의 비타민 $B_{2}$ 방출 특성 (Release Characteristics to Vitamin $B_{2}$ of Chitosan Ointments In vitro)

  • 오세영;황성규;황용현
    • 한국응용과학기술학회지
    • /
    • 제17권1호
    • /
    • pp.43-48
    • /
    • 2000
  • Drug delivery system(DDS) applied to various fields, such as medicine, cosmetics, agriculture and necessities of life. Among these application fields, DDS is often used as the method of drug dosage into the epidermic skin. We investigated characters of transdermal therapeutic system(TTS) and the skin permeability of that with applying DDS. Chitosan was selected as material of TTS. We investigated the permeation of chitosan ointment containing drug in rat skin using horizontal membrane cell model. Permeation properties of materials were investigated for water-soluble drug such as riboflavin in vitro. We used glycerin, PEG 600 and oleic acid as enhancers. Since dermis has more content water(hydration) than the stratum corneum, skin permeation rate at steady state was highly influenced when glycerin was used in water-soluble drug. The permeation rate of content enhancer and drug was found to be faster than that of content water-soluble drug only. These results showed that skin permeation rate of drug across the composite was manly dependent on the property of ointment base and drug. Proper selection of the polymeric materials which resemble and enhance properties of the delivering drug was found to be important in controlling the skin permeation rate.

초고강도 콘크리트의 강도발현에 관한 기초적 연구 (Study of strength Development of Ultra High-Strength Concrete)

  • 민홍준;공민호;임남기;이영도;정상진
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2006년도 추계 학술논문 발표대회 논문집
    • /
    • pp.75-79
    • /
    • 2006
  • Recently, more highly effective construction materials are needed for the reasonable and economical structure system is required as the construction structures become more multi storied, large-sized and diversified. That is to say, the highly qualified concrete is positively promoted as a part of plan to establish the effective space according to the dead load of structures and diminish of segment profile and to build up the economic structures. However, the high strength concrete has the problems such high brittleness and low ductility. Specially, for the high strength concrete, it has different strength from normal concrete as the internal temperature goes up steadily due to high heat of hydration by the quantities of highly level of cement, so the concrete which is mixed with various miscible materials is used. As the development and study for high strength concrete (more than $100N/mm^2$) is under way actively and the strength of high strength concrete increases, the strength different from the existing high strength concrete of ten than $100N/mm^2$, but the study for this is not adequate and indefinite. In addition, the study and report to apply the strength expression and analysis results of internal structure. Therefore, this study is an experiment about using the miscible materials affects what happens to the longitudinal physical property.

  • PDF

투명접합분리 시험체를 활용한 고강도 콘크리트의 강도관리에 관한연구 (Compressive Strength Control of High Strength Concrete Using Transparent Joint Separation Test Body)

  • 기전도;정광식;김학영;김광기;이영도;정상진
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2009년도 춘계 학술논문 발표대회 학계
    • /
    • pp.49-52
    • /
    • 2009
  • This paper aims to evaluate hydration and intensity property of different kind of members and intensity in order to evaluate compressive strength of structural concrete using Joint Separation Test Body(JSTB). In fact it is difficult to test and evaluate already have constructed member. In this case, common method used by construction engineer is that ; Schmidt rebound hammer test, Ultrasonic pulse test, Method of using test specimen previously cast. However, these method to control the structural intensity involve many problem and impossibility to adapt construction. 80, this paper proposes advance an opinion which have proper to examine intensity. has also aims to examine its validity and the plan to make similar environment with structural concrete and joint separation test body in order to verify efficiency assessment and on-site application.

  • PDF

The properties of hydrophobic concrete prepared by biomimetic mineralization method

  • Huang, Chung-Ho;Fang, Hao-Yu;Zhang, Jue-Zhong
    • Computers and Concrete
    • /
    • 제23권5호
    • /
    • pp.351-359
    • /
    • 2019
  • In this study, the calcium hydroxide, an inherent product of cement hydration, was treated using biomimetic carbonation method of incorporating stearic acid to generate the hydrophobic calcium carbonate on concrete surface. Carbonation reaction was carried out at various $CO_2$ pressure and temperatures and utilizing the Scanning Electron Microscope (SEM), chloride-ion penetration test apparatus, and compression test machine to investigate the hydrophobicity, durability, and mechanical properties of the synthesized products. Experimental results indicate that the calcium stearate may change the surface property of concrete from hydrophilicity to hydrophobicity. Increasing reaction temperature can change the particles from irregular shapes to needle-rod structures with increased shear stress and thus favorable to hydrophobicity and microhardness. The contact angle against water for the concrete surface was found to increase with increasing $CO_2$ pressure and temperature, and reached to an optimum value at around $90^{\circ}C$. The maximum static water contact angle of 128.7 degree was obtained at the $CO_2$ pressure of 2 atm and temperature of $90^{\circ}C$. It was also found that biomimetic carbonation increased the permeability, acid resistance and chloride-ion permeability of the concrete material. These unique results demonstrate that the needle-rod structures of $CaCO_3$ synthetized on concrete surface could enhance hydrophobicity, durability, and mechanical properties of concrete.

천연 Brucite의 물성분석 및 이산화황 흡수제로의 응용 (Property Analysis of Natural Brucite and Its Application as Sulfur Dioxide Absorbent)

  • 강성구;김명환;김진배
    • 청정기술
    • /
    • 제15권4호
    • /
    • pp.239-244
    • /
    • 2009
  • 중국 Liaoning에서 산출된 천연 brucite를 원료로 $Mg(OH)_2$ slurry를 제조하고, 그 탈황 성능을 magnesite를 원료로 열분해 및 수화반응으로 제조된, $Mg(OH)_2$ slurry와 비교하였다. Brucite와 magnesite를 원료로 제조된 $Mg(OH)_2$ 분말의 물리/화학적 특성은 유사했지만, brucite를 원료로 제조된 $Mg(OH)_2$ 결정입자의 판상구조가 보다 안정적으로 발달되어 있었다. Brucite와 magnesite를 원료로 제조된 $Mg(OH)_2$ slurry의 탈황효율은 brucite가 조금 높았다. Brucite를 배연탈황용 흡수제로 충분히 적용할 수 있을 것으로 기대된다.

초지연제 혼입률에 따른 저발열 콘크리트의 양생온도별 기초물성평가 (Fundamental Properties of Low-Heat Concrete According to the Mixing Rate of Super Retarding Agent)

  • 박병주;최윤호;현승용;김종;한민철;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2020년도 봄 학술논문 발표대회
    • /
    • pp.90-91
    • /
    • 2020
  • As the construction site has become narrower recently, the importance of mass concrete is naturally being highlighted as skyscrapers become popular. However, it is not possible to install the entire volume per day if the mass concrete is installed due to the Remicon 8⦁5 system and the 52-hour workweek system. When the mass concrete base is divided into several days, cold joints occur because the consolidation of joints is not integrated due to different degree of hardening in the case of the previous layer and the next day. As a result, existing research has shown that if super retarding agent are mixed into Ready Mixed Concrete (hereinafter referred to as Remicon) using sugar as a raw material to delay the curing time of concrete, cold joints are inhibited and cracks are inhibited by reducing the initial hydration heat.

  • PDF

염화마그네슘 첨가율에 따른 산화마그네슘 경화체의 물리 및 역학적 특성 (Physical and Mechanical Properties of Magnesium Oxide Matrix depending on Addition Ratio of Magnesium Chloride)

  • 김헌태;정병열;이상수;송하영
    • 한국건축시공학회지
    • /
    • 제14권4호
    • /
    • pp.308-313
    • /
    • 2014
  • 최근 주거건축물의 장수명화를 위해 건축물을 내부공간구성을 벽식구조에서 라멘구조로 변화하면서 경량복합패널의 사용이 증가하는 추세이다. 따라서 본 연구에서는 염화마그네슘 첨가율에 따른 산화마그네슘 경화체의 공학적 특성을 연구하여 경량복합패널의 표면재로 사용하기 위한 기초적 자료로 사용하고자 한다. 실험결과, 염화마그네슘 첨가량이 증가함에 따라 유동성은 증가되었으며, 공기량은 감소하였고, 초결과 종결은 느려졌다. 휨강도와 압축강도에서는 염화마그네슘 첨가율 40%의 시험체가 가장 높은 강도를 발현하였으며, 흡수율의 경우 염화마그네슘 첨가율 20%의 시험체가 가장 낮은 흡수율을 나타내었다. 길이변화에서는 염화마그네슘 첨가율이 증가함에 따라 팽창양이 증가하는 경향을 나타내었으며, 미시구조를 관찰한 결과 바늘형상의 수화생성물을 볼 수 있었다. 이 수화생성물이 광물성 섬유조직 형태를 가지고 있어 높은 휨강도를 발현한 것으로 판단되며, 또한 팽창의 원인으로 판단된다.

MgO계 세라믹 모르타르를 활용한 콘크리트 보수재료의 기초물성평가 (Fundamental Properties of MgO Base Ceramic Mortar for Concrete Repair Material)

  • 박준우;안기용
    • 콘크리트학회논문집
    • /
    • 제29권4호
    • /
    • pp.407-413
    • /
    • 2017
  • 본 연구는 콘크리트 보수재료로서의 MgO계 세라믹(Magnesia Phosphate Cement: MPC) 모르타르의 기초물성 평가를 위한 것이다. 이를 위해 응결시간, 압축강도, 부착강도를 측정하였으며 수화물의 측정을 위해 X-ray 회절분석을 실시하였다. 시편은 중질 마그네시아(dead burnt magnesia)를 바인더로 사용하였으며 활성제로 칼륨계 인산염을 사용하였고, 응결시간을 지연 시키기 위해 Borax를 지연제로 사용하였다. 또한, 이온침투저항성 평가를 위해 공극구조와 촉진염화물침투시험을 실시하였다. 그 결과 MPC 모르타르의 응결시간은 M/P 비에 따라 16~21분 사이로 빠르게 경화하였으며 지연제인 Borax는 MPC의 응결시간을 68분까지 늦추는 데 도움이 되었다. MPC 모르타르의 압축 강도는 12시간 재령에서 M/P 비에 따라 11.0~30.0 MPa 범위로 발현되었고 특히 M/P 비가 4인 MPC의 압축 강도는 12시간 이내에 30 MPa 정도의 강도를 발현하였다. MPC의 인장 부착강도와 휨 부착강도는 OPC 모르타르에 비해 각각 19 MPa와 17 MPa로 더 높게 측정되었으며 MPC 모르타르의 총 공극량은 OPC 모르타르에 비해 적게 측정되었고 촉진염화물침투시험에서도 MPC 모르타르를 통과한 총 전하가 OPC 모르타르보다 적었으며 이는 공극량과 공극분포로 설명 할 수 있다.

메타카오린의 포조란 효과에 의한 콘크리트 내 알칼리-실리카 반응 억제 효과 (The Inhibition Effect of Alkali-Silica Reaction in Concrete by Pozzolanic Effect of Metakaolin)

  • 이효민;전쌍순;황진연;진치섭;윤지해;옥수석
    • 한국광물학회지
    • /
    • 제17권3호
    • /
    • pp.277-288
    • /
    • 2004
  • 알칼리-실리카반응은 시멘트 내의 알칼리와 화학적으로 불안정한 반응성 골재와의 화학반응으로서, 그 결과 콘크리트의 팽창과 균열을 발생하는 작용이다 본 연구에서는 우수한 포조란반응 특성을 나타내는 새로운 광물혼화재로 부각되고 있는 메타카오린의 알칼리-실리카반응 억제 효과에 대하여 연구하였다. 다양한 치환율로 메타카오린을 혼합한 모르타르 공시체를 제작하여, 알칼리-실리카 반응성 시험(ASTM C 1260), 압축강도 시험 및 유동성 시험을 실시하고, 시멘트 수화물에서의 구성성분 변화에 대한 XRD 정량분석을 실시하였다. 그 결과, 메타카오린의 혼합은 시멘트 페이스트내의 가용 포트랜다이트의 함량을 급속히 감소시키는 빠른 포조란반응 및 수화반응 특성을 나타내어, 알칼리-실리카 반응에 의한 팽창을 억제하고 우수한 압축강도를 발현하는 것으로 나타났다. 시멘트에 메타카오린의 혼합에 의한 알칼리-실리카 반응에 의한 팽창억제는 치환율 15% 이상, 즉 시멘트 페이스 내의 가용 포트랜다이트 함량이 약 10% 이하가 될 경우 효과적이다. 메타카오린의 혼합에 의한 알칼리-실리카 반응에 의한 팽창 억제는 유해성이 높은 알칼리-칼슘-실리카 겔의 형성이 억제된 결과와 포조란 효과에 의한 치밀하고 균질한 시멘트 페이스트 형성으로 인한 알칼리 용액의 침투가 억제된 결과에 의한 것으로 생각된다. 15% 이상의 메타카오린의 혼합은 보통의 모르타르보다 높은 초기강도를 발현하였으며, 후기강도는 전 치환율 범위에서 보통의 모르타르 이상의 아주 우수한 강도를 나타내었다. 강도발현 특징은 메타카오린에 의한 빠른 포조란반응 및 수화특성을 반영하고 있다.

성남 고등동 회곽묘 삼물회의 배합비 분석 (Analysis of the Mix Ratio of Lime Mortar used in Joseon Dynasty Seongnam Godeung-dong Barrier Tombs)

  • 이상옥;배고운;정광용
    • 헤리티지:역사와 과학
    • /
    • 제53권1호
    • /
    • pp.34-51
    • /
    • 2020
  • 성남 고등동 회곽묘는 한 지역에서 다른 시기에 제작된 6기의 회곽묘가 발굴되었으며, 회곽묘 조성에 사용된 삼물회의 다양한 제작 기법이 확인되었다. 삼물회의 제작 기법을 규명하기 위하여 고문헌 기록을 바탕으로 석회 원료와 제작 기법 및 배합 방법을 고찰하였다. 조선시대 고문헌에는 석회의 원료 중 저품위 석회석을 사용한 기록과 배합 재료로 황토와 백토, 기와 가루 등과 같은 석회의 강도를 향상시킬 수 있는 포졸란 물질 사용에 대한 기록이 남아있다. 또한 삼물회의 다양한 배합 방법이 기록되어 있어 이에 대한 재현 실험을 바탕으로 석회 원료, 배합 재료, 배합 비율에 따른 삼물회 제작 기법 분석이 요구되었다. 조선시대 전기에는 석회를 다방면으로 사용하였으나 공급이 적고 기술적인 미숙함으로 지속적인 문제가 발생하였으며, 조선시대 후기에 이르러 대량 생산됨과 함께 석회 제작 기술이 발달하였다. 16세기와 18세기 회곽묘 삼물회의 제작 기법 분석을 바탕으로 고문헌에 기록된 배합비와 배합 방법들이 적용된 것을 알 수 있었으며, 회곽묘 삼물회는 시기에 따라 석회의 품질이 변화하였고 배합 재료 또한 변화됨에 따라 배합 비율이 다르게 나타나는 것으로 판단된다. 회곽묘 삼물회의 배합 비율은 시기에 따라서 변화하였으며, 주례와 가례를 기준으로 정해진 배합 방법으로 제작되었기 때문에 회곽묘 삼물회의 제작 기법에 대한 과학적 분석 자료가 지속적으로 구축된다면 회곽묘 편년 연구에 도움이 될 것으로 기대된다.