Manufacture of Specialty Paper with Hemp Bast Fiber Cultivated in Korea (Part 1) - Characteristics of Hemp-Wood Paper by Soda Pulping - (삼섬유를 이용한 특수기능지 개발 (제 1보) - 소다펄프화 삼 섬유의 수초지 특성 -)

  • Lee, Dah-Hee;Lee, Myoung-Ku
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.45 no.6
    • /
    • pp.30-35
    • /
    • 2013
  • To conserve wood resources for papermaking, chemical compositions of the hemp (Cannabis sativa L.) bast fiber cultivated in Korea such as holocellulose, ${\alpha}$-cellulose, lignin, alcohol-benzene extractives, hot and cold water extractives, and ash contents were investigated to manufacture the specialty packaging paper effectively. Significantly very low klason lignin content of 3.3% was accomplished by removing of the outer shell of bark. Laboratory soda pulping method which is very useful for the nonwood fiber was adapted, and it was found that there was no significant difference in both kappa number and H-factor between 25% and 30% NaOH charge. Hemp pulp cooked with the laboratory digester in 25% NaOH at $170^{\circ}C$ were mixed together with the wood pulp(NBKP:LBKP=1:1) in order to find the optimum mixture ratio which exhibited acceptable paper strength properties such as tensile index, burst index, and tear strength. When 10% of hemp soda pulps was mixed with 90% of wood pulps comprised of SwBKP and HwBKP (1:1), all physical strength increased significantly. The physical strength decreased as the amount of hemp pulp increased because the cell wall of bast fiber is very thick which causes low conformability and low fiber-fiber bonding. These results showed that paper made of hemp-wood pulp can be used for the specialty packaging paper which requires both the characteristic surface properties and the high physical strength of hemp fiber.

Wood Chemical Compositions of Raru Species Originating from Central Tapanuli, North Sumatra, Indonesia: Effect of Differences in Wood Species and Log Positions

  • ISWANTO, Apri Heri;TARIGAN, Fazilla Oktaviani;SUSILOWATI, Arida;DARWIS, Atmawi;FATRIASARI, Widya
    • Journal of the Korean Wood Science and Technology
    • /
    • v.49 no.5
    • /
    • pp.416-429
    • /
    • 2021
  • Raru is a lesser-known plant species originating from North Sumatra, Indonesia. Information on the characteristics is still limited, especially its chemical component. Therefore, this study aims to examine the chemical composition information of Cotylelobium lanceolatum, Cotylelobium melanoxylon, and Vatica pauciflora woods based on their axial log positions (bottom, middle, and top). The wood chemical analysis was performed in terms of the Indonesian National Standard (SNI) method. Furthermore, the analysis measured holocellulose, 𝛼-cellulose, hemicellulose, lignin content, alcohol benzene extractive content, the extractive substance in hot and water, and solubility in NaOH 1%. The results indicated that the species and their log axial positions affected different chemical components, which included 𝛼-cellulose, hemicellulose, and lignin of C. lanceolatum amounting to 41.88%, 19.39%, and 28.68% respectively. Meanwhile, for C. Melanoxylon, they were 42.01%, 21.11%, and 24.76% respectively; and for V. pauciflora wood, they were 42.95%, 23.24%, and 30.11% respectively. The average values of the extractive contents including the solubility in 1: 2 ethanol benzene, NaOH, and hot water for C. lanceolatum, C. melanoxylon, and V. pauciflora wood were (10.58%, 27.62%, 8.13%), (14.54%, 28.22%, 7.82%), and (10.95%, 28.60%, 7.57%) respectively. The wood species had a significant effect on chemical components including lignin, cellulose and hemicellulose, and extractive solubility in cold water. Furthermore, the axial log position had a significant effect on all the parameters of the chemical composition of the wood being tested.

Improvement of Dimensional Stability of Tropical Light-Wood Ceiba pentandra (L) by Combined Alkali Treatment and Densification

  • Deded Sarip NAWAWI;Andita MARIA;Rizal Danang FIRDAUS;Istie Sekartining RAHAYU;Adesna FATRAWANA;Fadlan PRAMATANA;Pamona Silvia SINAGA;Widya FATRIASARI
    • Journal of the Korean Wood Science and Technology
    • /
    • v.51 no.2
    • /
    • pp.133-144
    • /
    • 2023
  • Densification is an effective method for improving the physical and mechanical properties of low-density wood. However, the set-recovery of dimensions was found to be the problem of densified wood due to low fixation during the densification process. Alkali pretreatment before densification is thought to be a modification process to improve the dimensional stability of densified wood. In this research, the wood samples used were boiled in a 1.25 N sodium hydroxide (NaOH) solution at different times, followed by densification for 5 h at 100℃. The alkali pretreatment for 1, 3, and 5 h of boiling increased the dimensional stability of densified woods and anti-swelling efficiency values were 8.52%, 63.24%, and 48.94%, respectively. The boiling of wood in NaOH solution decreased the holocellulose content, as well as lignin to a lesser degree, and a lower crystallinity index was observed. The lower hydroxyl groups and a higher proportion of lignin in treated samples seem to have contributed to the high dimensional stability detected.

Supercritical Water Hydrolysis of Waste Logs after Oak Mushroom Production (초임계수를 이용한 표고버섯 골목의 가수분해)

  • Koo, Bon-Wook;Lee, Jae-Won;Choi, Joon-Weon;Choi, Don-Ha;Choi, In-Gyu
    • Journal of the Korean Wood Science and Technology
    • /
    • v.34 no.6
    • /
    • pp.81-95
    • /
    • 2006
  • In order to investigate the possibility of waste logs after oak mushroom production as a source of an alternative energy and to obtain the fundamental data of supercritical water hydrolysis that has been paid attention as a new saccharification method of lignocellulosics, supercritical water hydrolysis of normal log woods (Quercus acutissima Carruth) and waste logs was carried out. With the increase of reaction time and temperature, the color of the degradation products has been dark and the degradation rate and the crystalline index increased. However the increase of reaction pressure affected the color of the degradation products and the degradation rate at only low reaction temperature. In the early stage of the reaction, the degradation of hemicellulose was progressed, while in the late stage, the cellulose was degraded. The increase of reaction time and reaction temperature (less than $415^{\circ}C$) improved the sugar yield, while at high temperature(more than $415^{\circ}C$), the sugar yield was decreased. Based on the result of the sugar yield, the optimal hydrolysis condition of Q. acutissima Carruth by supercritical water was determined to be $415^{\circ}C$, 60 seconds and 230 pressure bar with the sugar yield of 2.68% (w/w). At the optimal condition, the supercritical water hydrolysis of waste logs after the mushroom production was carried out and the sugar yield was increased to 358% (w/w). The major degradation products of waste logs by supercritical water hydrolysis were 1,1'-oxybis-benzene and 1,2-benzendicarboxylic acid by the GC-MS analysis. At the reaction condition with low degradation rate, the fatty acids such as pentadecanoic acid, 14-methyl-heptadecanoic acid were identified. With the increase of the reaction temperature and time, the amounts of phenol and benzene were increased, but the reaction pressure did not affect the kinds of degradation products. Holocellulose content was 60.6~79.2% in the water insoluble residue and the monosaccharide yield of the water insoluble residue was 49.2~675% by the acid hydrolysis. The monosaccharide yield of water-soluble portion was increased largely by the second hydrolysis using dilute acid.

Characterization of Chemical Composition in Poplar wood (Populus deltoides) by Suppression of CCoAOMT Gene Expression (CCoAOMT 유전자 발현 억제에 의한 현사시나무의 화학조성 변화)

  • Eom, In-Yong;Kim, Kwang-Ho;Lee, Soo-Min;Yi, Yong-Sub;Choi, Joon-Weon
    • Journal of the Korean Wood Science and Technology
    • /
    • v.38 no.3
    • /
    • pp.213-222
    • /
    • 2010
  • In this study, chemical compositions - holocellulose, lignin and monomeric sugars - were characterized with two poplar wood cell walls, one of which was grown at normal condition (CPW) and the other was genetically modified by antisence suppression of CCoAOMT gene expression (ACPW). Milled wood lignins were isolated from CPW and ACPW and subjected to methoxyl group, DFRC, Py-GC/MS, GPC, $^{13}C$-NMR analysis, respectively. There were few differences in holocellulose contents in both cell walls, which were determined to 81.6% in CPW and to 82.3% in ACPW. However, lignin contents in ACPW was clearly decreased by the suppression of CCoAOMT gene expression. In CPW 21.7% of lignin contents was determined, while lignin contents in ACPW was lowered to 18.3%. The relative poor solubility of ACPW in alkali solution could be attributed to the reduction of lignin content. The glucose contents of CPW and ACPW were measured to 511.0 mg/g and 584.8 mg/g and xylose contents 217.8 mg/g and 187.5 mg/g, respectively, indicating that suppression of CCoAOMT gene expression could be also influenced to the formation of monomeric sugar compositions. In depth investigation for milled wood lignin (MWL) isolated from both samples revealed that the methoxyl contents at ACPW was decreased by 7% in comparison to that of CPW, which were indirectly evidenced by $^{13}C$-NMR spectra and Py-GC/MS. According to the data from Py-GC/MS S/G ratios of lignin in CPW and ACPW were determined to 0.59 and 0.44, respectively. As conclusive remark, the biosynthesis of syringyl unit could be further influenced by antisense suppression of CCoAOMT during phenylpropanoid pathway in the plant cell wall rather than that of guaiacyl unit.

Studies on the Hydrolysis of Holocellulose with Trichoderma viride Cellulase - (II) Effects of the Reaction Conditions - (Cellulase에 의(依)한 목재당화(木材糖化)에 관(關)한 연구(硏究) - (II) 반응조건(反應條件)의 효과(効果) -)

  • Min, Du Sik
    • Journal of Korean Society of Forest Science
    • /
    • v.39 no.1
    • /
    • pp.57-63
    • /
    • 1978
  • Enzymatic hydrolysis of the substrate from Alnus hirsuta (Spach) Rupr (8-14years) was investigated using cellulase preparations of Trichoderma viride Pers. ex. Fr. SANK 16374 and conduced on the optimum reaction conditions of the cellulase on saccharification. The crude cellulase was produced by the submerged culture process and produced in the culture fluid was salted out quantitatively by the use of ammonium sulfate. The method of delignification from wood(Saw dust) was treated by the peracetic acid (PA) method. Reducing sugar was determined by the dinitrosalicylic acid (DNS) method. The results were summerized as follows; 1. The optimum pH of cellulase was 5.0 and the range of stability with respect to pH was generally from 4.0 to 6.0 2. The optimum temperature of cellulase was generally $40^{\circ}C$, but reducing sugar formation did not show significent differences at 5% levels in the reaction temperature from $40^{\circ}C$ to $50^{\circ}C$. 3. The redusing sugar were increased with increase of cellulase concentration. 4. The reducing sugar were decreased with increase of substrate concentration. 5. Fructose was a very good inhibitor of the enzyme from Trichoderma viride, but glucose inhibition was generally weak.

  • PDF

Popping Pretreatment for Enzymatic Hydrolysis of Waste Wood (팝핑 전처리를 이용한 폐목재의 효소당화)

  • Kim, Hyun-Joo;Cho, Eun-Jin;Lee, Kwang-Ho;Kim, Su-Bae;Bae, Hyeun-Jong
    • Journal of the Korean Wood Science and Technology
    • /
    • v.39 no.1
    • /
    • pp.95-103
    • /
    • 2011
  • We have investigated pretreatment of waste wood using milling refinery combined with poping method, which can save energy for pretreatment and enzyme loading for enzymatic hydrolysis. The chemical analysis of holocellulose of non and popping treated waste wood showed 65.9% and 58.8%, and the lignin, organic extracts and ash were increased by 3%, 4% and 0.7% after pretreatment, respectively. The reducing sugar yields of pretreated waste wood were increased four times more than non-pretreated one and the synergistic effect of cellulase and xylanase were evaluated compare with individual enzyme treatment. Especially, enzyme cocktail (cellulase 50 U and xylanase 50 U) treatment was very efficient in 1% substrate (50 mg). Also, glucose and xylose conversion rate of pretreated waste wood by GC analysis were 45.9% and 38.7%, respectively.

Cultivation of Several Mushrooms Using Chestnut Peels as an Agricultural By-product (농산 부산물인 밤껍질을 이용한 버섯균의 배양)

  • Lee, Sang-Sun;Lee, Jeong-Woo;Hong, Seong-Woon;Cho, Nam-Seok
    • Journal of the Korean Wood Science and Technology
    • /
    • v.27 no.2
    • /
    • pp.78-86
    • /
    • 1999
  • The two parts of chestnut peels, outer and inner layers, were collected and investigated for cultivation of various mushrooms, i.e., Pleurotus ostreatus, Lentinus edodes, Hericium ramosum and the others. The inner layer of chestnut peels was contaminated with the mycelia of the blue fungi when collected, consisted of 17~20 % holocellulose, being a good material for growths of the above fungi. The outer layer was considered to be poor materials for fungal growth, because of lower amounts of minerals. Both mushrooms of Pleurotus ostreatus and Hericium ramosum grow well, and were produced fruiting bodies on the solid media containing only inner layers of chestnut peels. The Imhyup No.6 and Imhyup No.7 varieties of Lentinus edodes grow well, but produced few fruiting bodies in the solid media containing only inner layers of chestnut peels. The growth patterns of P. ostreatus and L. edodes were evaluated by production of $CO_2$. and considered to be different according to fungi. The inner layers of chestnut peels as agricultural by-products were considered to be a good material for mushroom cultivation, and outer layers could be used as being added with the other additives. The chestnut peels, being the environmental pollutants in rural areas, was considered to be a good substrate for mushroom cultivation.

  • PDF

Chemical Properties and Fiber Dimension of Eucalyptus pellita from The 2nd Generation of Progeny Tests in Pelaihari, South Borneo, Indonesia

  • Lukmandaru, Ganis;Zumaini, Umi Farah;Soeprijadi, Djoko;Nugroho, Widyanto Dwi;Susanto, Mudji
    • Journal of the Korean Wood Science and Technology
    • /
    • v.44 no.4
    • /
    • pp.571-588
    • /
    • 2016
  • Eucalyptus pellita F. Muell is one of pulp woods that is being developed through breeding plantation programs in Indonesia. The research aimed at exploring the chemical and morphological characteristics of fiber, and to determine the rank of plus trees from 4 provenances based on the suitability for pulps. The materials included the plus trees of E. pellita (9 years) from the 2nd generation of progeny tests in Pelaihari, South Borneo. Wood properties under investigation included the chemical properties and morphological fiber characteristics (fiber dimensions and its derived properties). In the present study, data were analyzed using descriptive statistic, Analytic Hierarchy Process (AHP) and Pearson's correlation. Results showed that the chemical properties of E. pellita, i.e. the contents of ethanol-toluene extractives, hot water soluble extractives, holocellulose, alphacelullose, and lignin were $3.08{\pm}1.00%$, $1.41{\pm}0.38%$, $75.26{\pm}2.58%$, $49.02{\pm}2.88%$, and $29.49{\pm}1.86%$, respectively. The average values of wood fiber morphology were $1.02{\pm}0.08$ mm (fiber length), $13.25{\pm}1.64{\mu}m$ (fiber diameter), of $6.94{\pm}1.70{\mu}m$ (lumen diameter), $3.15{\pm}0.52{\mu}m$ (fiber wall thickness), $0.97{\pm}0.30$ (Runkel ratio), $0.57{\pm}0.10$ (Luce's shape factor), $78.21{\pm}10.34$ (slenderness ratio) and $130.91{\pm}33.77{\times}10^3{\mu}m^3$ (solids factor). The AHP scoring rank indicated that the best individuals were 28.4.3.28 (Kiriwo Utara), 12.1.5.28 (North Kiriwo), 19.11.5.45 (Serisa Village), 3.8.4.9 (South Kiriwo), and 6.6.3.15 (South Kiriwo). Pearson correlation analysis showed significant correlations between the levels of fiber length with alpha-cellulose content (r = 0.39) as well as the fiber length with ethanol-toluene extractive contents (r = -0.41).

Anatomical, Morphological, and Chemical Characteristics of Paper-mulberry Wood and Bast Fiber for Raw Material of Korean Paper(Hanji) (한지 원재료인 닥나무와 인피섬유의 해부학적·화학적 특성 연구)

  • Go, In Hee;Jeong, Seon Hwa
    • Journal of Conservation Science
    • /
    • v.34 no.6
    • /
    • pp.517-524
    • /
    • 2018
  • This study using a method different from those employed previously, the anatomical characteristics of paper-mulberry wood were confirmed by observing three different sections. In addition, the factors affecting the pulp and papermaking processes were analyzed in terms of morphological properties such as the fiber length and width, lumen width, and chemical composition of the paper-mulberry bast fiber. The anatomical characteristics of the paper-mulberry wood were a ring porous or semi-ring porous structure with the vessels showing solitary pore and radial array. The medullary ray of the tangential section showed 1-3 rows and common helical thickening. Consequently, the paper-mulberry wood has the same anatomical characteristics throughout. The morphological characteristics of the paper-mulberry bast fiber are a fiber length of 6.58 to 9.01 mm, fiber width of 15.85 to $27.80{\mu}m$, lumen width of 4.50 to $12.54{\mu}m$. The D sample of Gangwon was the most suitable for the pulp and papermaking processes, in terms of its derived morphological ratios. Comparing the chemical compositions, the C sample of Gyeongsang had a high holocellulose content (90%). Thus, the findings herein will aid in determining the quality of Korean paper post production.