• 제목/요약/키워드: helium leak rate

검색결과 11건 처리시간 0.016초

RF-MEMS 소자의 웨이퍼 레벨 밀봉 패키징을 위한 열압축 본딩 (Thermocompression bonding for wafer level hermetic packaging of RF-MEMS devices)

  • 박길수;서상원;최우범;김진상;남산;이종흔;주병권
    • 센서학회지
    • /
    • 제15권1호
    • /
    • pp.58-64
    • /
    • 2006
  • In this study, we describe a low-temperature wafer-level thermocompression bonding using electroplated gold seal line and bonding pads by electroplating method for RF-MEMS devices. Silicon wafers, electroplated with gold (Au), were completely bonded at $320^{\circ}C$ for 30 min at a pressure of 2.5 MPa. The through-hole interconnection between the packaged devices and external terminal did not need metal filling process and was made by gold films deposited on the sidewall of the throughhole. This process was low-cost and short in duration. Helium leak rate, which is measured to evaluate the reliability of bonded wafers, was $2.7{\pm}0.614{\times}10^{-10}Pam^{3}/s$. The insertion loss of the CPW packaged was $-0.069{\sim}-0.085\;dB$. The difference of the insertion loss between the unpackaged and packaged CPW was less than -0.03. These values show very good RF characteristics of the packaging. Therefore, gold thermocompression bonding can be applied to high quality hermetic wafer level packaging of RF-MEMS devices.