하이브리드 코팅에 의한 고경도 소재용 Ti-Al-Si-N코팅 엔드밀의 절삭성능평가 (Cutting Performance of Ti-Al-Si-N Coated Endmill for High-Hardened materials by Hybrid Coating System)

  • 김경중;강명창;이득우;김정석;김광호
    • 한국공작기계학회:학술대회논문집
    • /
    • 한국공작기계학회 2003년도 추계학술대회
    • /
    • pp.89-94
    • /
    • 2003
  • Hard coatings are known to improve the performance of cutting tools in aggressive machining applications, such as high speed machining. New superhard Ti-Al-Si-W films, characterized by a nanocomposite nano-sized (Ti,Al,Si)N crystallites embedded in amorphous $Si_3 N_4$ matrix, could be successfully synthesized on WC-Co substrates by a hybrid coating system of arc ion plating(AIP) and sputtering method. The hardness of Ti-Al-Si-N film increased with incorporation of Si, and had the maximum value ~50 GPa at the Si content of 9 at.%, respectively. And the X-ray diffraction patterns of Ti-Al-Si-N films with various Si content is investigated. In this study, Ti-Al-Si-N coatings were applied to end-mill tools made of WC-Co material by a hybrid coating system. Cutting tests fir the high-hardened material (STD11,$H_R$)C62 and their performances in high speed cutting conditions were studied. Also, the tool wear and tool lift of Ti-Al-Si-N with various si(6, 9, 19) contents were measured.

  • PDF

물리적 증착 방법에 의한 TiC, TiN코팅에 따른 자동차 구조용 재료의 트라이볼로지 특성 (Tribological Characteristics of TiC, TiN Coating for PVD Method with Automotive structural Materials)

  • 오성모
    • 한국산학기술학회논문지
    • /
    • 제8권3호
    • /
    • pp.432-436
    • /
    • 2007
  • 자동차 구조용 재료에 대하여 물리적 증착 코팅방법에 의한 트라이볼로지 특성을 연구 하였다. 코팅 재료는 탄화티탄(TiC)과 질화티탄(TiN)이다. 실험은 펠렉스 마찰 마모시험기를 이용하여 하중과 온도에 다양한 조건을 적용하여 마찰과 마모 거동에 대하여 트라이볼로지 특성을 결정하고 평가하였다. 연구결과 코팅하지 않았을 때보다 코팅하였을 때가 윤활 특성이 향상 되었고, 특히 내마모성 및 극압성 그리고 열 안정성이 훌륭하였다.

  • PDF

비구면 유리렌즈 성형용 SiC 코어의 DLC 코팅에 관한 연구 (A Research on DLC Thin Film Coating of a SiC Core for Aspheric Glass Lens Molding)

  • 박순섭;원종호
    • 한국정밀공학회지
    • /
    • 제27권12호
    • /
    • pp.28-32
    • /
    • 2010
  • Technical demands for aspheric glass lens formed in market increases its application from simple camera lens module to fiber optics connection module in optical engineering. WC is often used as a metal core of the aspheric glass lens, but the long life time is issued because it fabricated in high temperature and high pressure environment. High hard thin film coating of lens core increases the core life time critically. Diamond Like Carbon(DLC) thin film coating shows very high hardness and low surface roughness, i.e. low friction between a glass lens and a metal core, and thus draw interests from an optical manufacturing industry. In addition, DLC thin film coating can removed by etching process and deposit the film again, which makes the core renewable. In this study, DLC films were deposited on the SiC ceramic core. The process variable in FVA(Filtered Vacuum Arc) method was the substrate bias-voltage. Deposited thin film was evaluated by raman spectroscopy, AFM and nano indenter and measured its crystal structure, surface roughness, and hardness. After applying optimum thin film condition, the life time and crystal structure transition of DLC thin film was monitored.

자외선 경화코팅 필름-기질 계면에서의 주름현상에 대한 연구 (Experimental Studies of Wrinkle Formation in the UV Cured Coating Around Film-Substrate Insterface)

  • 홍진후;이행우
    • 대한화학회지
    • /
    • 제38권7호
    • /
    • pp.480-484
    • /
    • 1994
  • 자외선 경화코팅 필름-기질 계면에서의 견딤성에 대하여 조사하였다. 특히, UV 경화 우레탄 아크릴레이트계 배합물에서 모노머 및 올리고머의 코팅필름 주름현상에 미치는 영향은 조사하였다. 실험결과, 주름현상은 DMTA이 손실모듈러스 피크가 넓고 shouldr가 있을수록 덜 나타났다. 특히, 변성된 방향족 우레탄 아크릴레이트를 지방족계에 첨가하므로서 hard하면서도 flexible한 코팅필름을 얻을 수 있음을 알 수 있었다. 따라서 주름현상 방지효과는 높은 손실모듈러스값 때문인 것으로 나타났다. SEM 및 instron 실험결과도 위의 결론을 입증하고 있음을 알 수 있었다.

  • PDF

콜로이달 실리카와 실란으로부터 합성된 나노하이브리드 코팅 박막의 특성 (Properties of Nano-Hybrid Coating Films Synthesized from Colloidal Silica-Silane)

  • 나문경;안명상;강동필
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 하계학술대회 논문집 Vol.7
    • /
    • pp.232-233
    • /
    • 2006
  • In recent years the interest in organic/inorganic hybrid materials has increased at a fast rate. Nano organic-inorganic hybrid composites have shown advantages for preparing hard coating layers. Especially, nano hybrid composite has low environmental pollution. It has high transparency, hardness, toughness, thermal dissociation temperature, hydrophobicity by using nano sized inorganic material. There are many ways in which these materials may be synthesized, a typical one being the use of silica and silanes using the sol-gel process. The structure of sol-gel silica evolves as a result of these successive hydrolysis and condensation reactions and the subsequent drying and curing. The sol-gel reactions are catalyzed by acids and produce silica sol solutions. The silica sol grows until they reach a size where a gel transition occurs and a solid-like gel is formed. Colloidal silica(CS)/silane sol solutions were synthesized in variation with parameters such as different acidity and reaction time. In order to understand their physical and chemical properties, sol-gel coating films were fabricated on glass. From all sol-gel solutions, seasoning effect of sol-gel coating layer on glass was observed.

  • PDF

CrN과 TiN 코팅을 적용한 증기 발생기 세관의 프레팅 마모에 대한 연구 (A Study on Fretting Wear of CrN and TiN coated Tubes in a Nuclear Steam Generator)

  • 이영제;박정민;정성훈;김진선;박세민
    • Tribology and Lubricants
    • /
    • 제24권5호
    • /
    • pp.250-254
    • /
    • 2008
  • The steam generator of nuclear power plant is composed with the bundles of long tubes. It is exposed fluid flow and weak in the vibration. The tubes are supported by anti-vibration bars. Due to vibration the wear damage is called as the fretting wear. It should be minimized for the safety of the plants. The hard coatings are very effective to reduce the amount of wear. The coatings of TiN and CrN are introduced in this study to protect the fretting surfaces. The tube-on-flat type tester was used for fretting wear tests. The results show that the wear amounts of the coated tubes were decreased depending on coating thickness. CrN was very effective to reduce the wear. In case of TiN the wear amounts were dependent on the coating thickness. Thick coating of TiN was very effective for wear resistance.

실리카-PMMA 나노 하이브리드 코팅액 제조 및 특성에 관한 연구 (Studies on the Synthesis and Characteristic of Silica-PMMA Nano Hybrid Material)

  • 손대희;김대성;이성호;김송혁;이근대;박성수
    • 공업화학
    • /
    • 제23권1호
    • /
    • pp.53-58
    • /
    • 2012
  • 투명한 플라스틱 필름의 표면경도를 향상시키기 위하여 유-무기 하이브리드 코팅 용액을 졸-겔 공정을 이용하여 합성하였다. 무기성분으로 콜로이드 실리카와 유기성분으로 PMMA, 유-무기 성분 간의 결합력을 향상시켜 하이브리드 코팅 층의 특성을 더욱 향상시키기 위하여 실란커플링제로서 vinyl trimethoxy silane (VTMS)과 [3-(metha cryloyloxy)] propyl trimethoxy silane (MAPTMS)를 이용하였고, 알콕시 실란의 종류, 콜로이드 실리카/PMMA의 함량비 등의 반응조건에 따라 콜로이드 실리카/PMMA 졸을 합성하였다. 이러한 졸을 PET 필름에 바코팅시키고, 열경화 시켜 하드코팅막을 제조하여 물리적 화학적 특성을 조사하였다. PMMA에 비해서 하이브리드 형태에서 코팅 막의 연필경도와 기재와의 부착력이 우수하였다.

The properties and wear behavior of HVOF spray coating layer of Co-alloy powder

  • Cho, Tong-Yul;Yoon, Jae-Hong;Kim, Kil-Su;Youn, Suk-Jo;Back, Nam-Ki;Chun, Hui-Gon
    • 한국결정성장학회지
    • /
    • 제16권6호
    • /
    • pp.273-277
    • /
    • 2006
  • High velocity of oxy-fuel (HVOF) thermal spray coating is progressively replacing the other classical hard coatings such as chrome plating and ceramic coating by the classical methods, since the very toxic $Cr^{6+}$ ion is well known as carcinogen causing lung cancer, and the ceramic coatings are brittle. Co-alloy T800 powder is coated on the Inconel 718 substrates by the HVOF coating procesess developed by this laboratory. For the study of the possibility of replacing of chrome plating, the wear properties of HVOF Co-alloy T800 coatings are investigated using the reciprocating sliding tester with a counter sliding SUS 304 ball both at room and at an elevated temperature of $1000^{\circ}F\;(538^{\circ}C)$. The possibility as durability improvement coating is studied for the application to the high speed spindles vulnerable to frictional heat and wear. Wear mechanisms at the reciprocating sliding wear test are studied far the application to the systems similar to the sliding test such as high speed spindles. Wear debris and frictional coefficients of T800 coatings both at room and at an elevated temperature of $538^{\circ}C$ are drastically reduced compared to those of non-coated surface of Inconel 718 substrates. Wear traces and friction coefficients of both coated and non-coated surfaces are drastically reduced at a high temperature of $538^{\circ}C$ compared with those at room temperature. These show that the coating is highly recommendable far the durability Improvement coating on the surfaces vulnerable to frictional heat and wear.

유한요소해석에 의한 코팅면의 브리넬 경도 평가: 제2보 - 모재와 코팅두께의 영향 (Evaluation of Brinell Hardness of Coated Surface by Finite Element Analysis: Part 2 - Influence of Substrate and Coating Thickness)

  • 박태조;강정국
    • Tribology and Lubricants
    • /
    • 제37권4호
    • /
    • pp.144-150
    • /
    • 2021
  • The most cost-effective method of reducing abrasive wear in mechanical parts is increasing their hardness with thin hard coatings. In practice, the composite hardness of the coated substrate is more important than that of the substrate or coating. After full unloading of the load applied to an indenter, its indentation hardness evaluated based on the dent created on the test piece was almost dependent on plastic deformation of the substrate. Following the first part of this study, which proposes a new Brinell hardness test method for a coated surface, the remainder of the study is focused on practical application of the method. Indentation analyses of a rigid sphere and elastic-perfect plastic materials were performed using finite element analysis software. The maximum principal stress and plastic strain distributions as well as the dent shapes according to the substrate yield stress and coating thickness were compared. The substrate yield stress had a significant effect on the dent size, which in turn determines the Brinell hardness. In particular, plastic deformation of the substrate produced dents regardless of the state of the coating layer. The hardness increase by coating behaved differently depending on the substrate yield stress, coating thickness, and indentation load. These results are expected to be useful when evaluating the composite hardness values of various coated friction surfaces.

졸-겔 법에 의한 콜로이드 실리카와 유기 실란을 이용한 하드코팅 용액의 제조 및 특성 (Synthesis and Characteristics of Hard Coating Solution Using Colloidal Silica and Organic Silane through Sol-Gel Process)

  • 손대희;이윤이;김성진;홍성수;이근대;박성수
    • 공업화학
    • /
    • 제22권6호
    • /
    • pp.691-696
    • /
    • 2011
  • 졸-겔 공정을 활용하여 유무기 하이브리드 형태의 투명 필름용 하드코팅층에 사용되는 코팅졸을 제작하였다. 콜로이드 실리카와 알콕시 실란{vinyltrimethoxy silane : (VTMS)와 [3-(methacryloyloxy)] propyltrimethoxysilane : (MAPTMS)}을 이용하였고 다양한 조건에 따라 실험을 실시하였다. 이 졸은 PMMA와 교반하여 PET필름에 코팅막을 형성하였다. 코팅막에 대한 특성은 여러 가지 측정에 의해 확인하였다. 코팅막은 PMMA 단독에 비해서 유기실란 양이 첨부된 형태에서 코팅막의 연필경도와 기재와의 부착력이 우수하였고 실험된 조건에서 시란의 양이 증가할수록 연필경도가 증가하는 경향이 나타났다.