Fresh and hardened properties of rubberized concrete using fine rubber and silpozz

  • Padhi, S.;Panda, K.C.
    • Advances in concrete construction
    • /
    • v.4 no.1
    • /
    • pp.49-69
    • /
    • 2016
  • This work investigates the mechanical properties of conventional concrete (CC) and self compacting concrete (SCC) using fine rubber and silpozz were accompanied by a comparative study between conventional rubberized concrete (CRC) and self compacting rubberized concrete (SCRC). Fine rubber (FR) from scrap tires has replaced the fine aggregate (FA) and Silpozz has been used as a replacement of cement at the proportions of 5, 10 and 15%. Silpozz as a partial replacement of cement in addition of superplasticiser (SP) increases the strength of concrete. Fresh concrete properties such as slump test, compaction factor test for CRC, whereas for SCRC slump flow, $T_{500}$, V-funnel, L-box, U-box, J-ring tests were conducted along with the hardened properties tests like compressive, split tensile and flexural strength test at 7, 28 and 90 days of curing. The durability and microstructural behavior for both CRC and SCRC were investigated. FR used in the present study is 4.75 mm passing with fineness modulus 4.74.M30 grade concrete is used with a mix proportion of 1:1.44:2.91 and w/c ratio as 0.43. The results indicate that as FR quantity increases, workability of both CRC and SCRC decreases. The results also show that the replacement of natural fine aggregate (NFA) with FR particles decreases the compressive strength with the increase of flexural strength observed upto 5% replacement of FR. Also replacement of cement with silpozz resulted enhancement of strength in SCRC.

Buildability for Concrete 3D Printing According to Printing Time Gap (콘크리트 3D프린팅의 적층시간 간격에 따른 적층 성능)

  • Lee, Yoon Jung;Song, Jin-Soo;Choi, Seung-Ho;Kim, Kang Su
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.23 no.4
    • /
    • pp.131-136
    • /
    • 2019
  • Buildability of fresh concrete, a key element of Concrete 3D printing, is the ability to build filaments at a desirable height without excessive deformation or collapse. Buildability is closely related to yield stress, and the higher the yield stress, the better. Also, the shear stress of fresh concrete increases as it hardens over the time after extruded, and consequently the buildability increases. Therefore, in concrete 3D printing, proper time gaps between printed layers (Printing Time Gap, PTG) are required to ensure the buildability of fresh concrete. As the PTG increases, the buildability increases; however, an excessive PTG reduces the bond performance between the printed layers, and the extrudability can be lowered as the printing time increases. In this research, therefore, 3D printing experiments were conducted with the variable of PTG to examine the buildability of 100 MPa-high strength concrete. In addition, a pseudo-layer loading method was applied to simulate the buildability test for 3D concrete printing and its applicability was examined.

Properties of Cold Weather Concrete Using Anti-freeze Agent Based Formate-acetate (포름산-아세트산염계 방동제를 사용한 콘크리트의 특성)

  • Jo, Hyun-Tae;Kim, Ho-Soo;Chun, Jun-Young;Ryu, Deuk-Hyun
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2008.11a
    • /
    • pp.617-620
    • /
    • 2008
  • When fresh concrete is exposed to the cold weather, the concrete may happen frost damage because of freezing at early ages and the strength development may be go down. Therefore, this paper is intend to investigate the properties and availabilities of cold weather concrete using anti-freeze based formate-acetate for ensure of excellent concrete quality on cold temperature. According to test result for concrete in anti-freeze agent, strength properties in sub-zero temperature increases in comparison with concrete of non anti-freeze agent without decline of strength until later age. When anti-freezing agent is added by 3.0% to binder, it gives good effects on the performance of the fresh and harden concrete.

  • PDF

Utilization of Waste Glass Micro-particles in Producing Self-Consolidating Concrete Mixtures

  • Sharifi, Yasser;Afshoon, Iman;Firoozjaei, Zeinab;Momeni, Amin
    • International Journal of Concrete Structures and Materials
    • /
    • v.10 no.3
    • /
    • pp.337-353
    • /
    • 2016
  • The successful completion of the present research would be achieved using ground waste glass (GWG) microparticles in self-consolidating concrete (SCC). Here, the influences of GWG microparticles as cementing material on mechanical and durability response properties of SCC are investigated. The aim of this study is to investigate the hardened mechanical properties, percentage of water absorption, free drying shrinkage, unit weight and Alkali Silica Reaction (ASR) of binary blended concrete with partial replacement of cement by 5, 10, 15, 20, 25 and 30 wt% of GWG microparticles. Besides, slump flow, V-funnel, L-box, J-ring, GTM screen stability, visual stability index (VSI), setting time and air content tests were also performed as workability of fresh concrete indicators. The results show that the workability of fresh concrete was increased by increasing the content of GWG microparticles. The results showed that using GWG microparticles up to maximum replacement of 15 % produces concrete with improved hardened strengths. From the results, when the amount of GWG increased there was a gradual decrease in ASR expansion. Results showed that it is possible to successfully produce SCC with GWG as cementing material in terms of workability, durability and hardened properties.

Properties of High-Performance Concrete Containing High - Reactivity Metakaolin (고반응성 메타카올린을 사용한 고성능 콘크리트의 특성)

  • 원종필;권연성;이존자
    • Journal of the Korea Concrete Institute
    • /
    • v.14 no.3
    • /
    • pp.349-356
    • /
    • 2002
  • This research deals with the properties of fresh and hardened high-performance concrete(HPC) incorporating high-reactivity metakaolin(HRM). The properties of fresh and hardened state concrete were investigated included air content, slump flow, setting time, heat of hydration, compressive strength, resistance to chloride-ion penetration, abrasion and repeated freezing and thawing. The properties of the HRM concrete were also compared with those of the portland cement concrete and silica fume(SF) concrete. The laboratory test results indicate that HRM material can be used as a supplementary cementitious material to produce high-performance concrete.

Effect of crushed waste glass as partial replacement of natural fine aggregate on performance of high strength cement concrete

  • Ajmal, Paktiawal;Mehtab, Alam
    • Advances in materials Research
    • /
    • v.11 no.4
    • /
    • pp.251-277
    • /
    • 2022
  • Disposal of industrial waste in cities where municipal authorities permitting higher floor area ratio coupled with increasing living standards, a lot of demolition waste is being generated. Its disposal is a challenge particularly in megacities where no landfills are available. The ever-increasing cost of building construction materials also necessitates consuming demolition wastes in a useful manner to save fresh natural raw materials. In the present work, the crushed waste glass is used in high-strength concrete as a partial replacement of fine aggregate. The control concrete of grade M60 was proportioned following BIS 10262-2009. The crushed waste glass has been used as a partial replacement with varying percentages of 10, 20, 30, and 40% by weight of fine aggregate. Experimental tests were carried on the fresh and hardened state of the concrete. The effect of crushed waste glass on the workability of the concrete has been investigated. Non-destructive tests, acid attack tests, compressive strength, split tensile strength, and X-ray diffraction analysis was carried out for the control concrete and concrete containing crushed waste glass after 7, 28, and 270 days of normal curing. The results show that for the same w/c ratio, the workability of concrete increases with increasing replaced crushed waste glass content. However, the decrease in compressive strength of the concrete after 28 days of normal curing and further after 28 days of acid attacks, up to 30% replacement level of fine aggregate by the crushed waste glass is insignificant.

An Experimental Study on the Structure Application of High Streength Ready Mixed Concrete - part 2 : Properties of Hardened State and Quality Control - (고강도 레미콘의 구조체 적용에 관한 실험적 연구 - 제2보 : 경화상태 특성 및 품질관리 -)

  • 김기철;이진규;윤기철;연흥흠;최강순;한천구
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1995.04a
    • /
    • pp.18-21
    • /
    • 1995
  • Continued from study on fresh concrete properties of the part 1, this study is designed for analyzing to the increasing trend of the compressive strength according to the curing method, standard deviation, strength properties of pumping before and after, and a length change to the drying shrinkage. And for quality control, this study is designed for analyzing the early estimation of compressive strength by hydrometer method in diluted concrete solution at the fresh state, and non-destructive testing by the Schumidt hammer at the hardened state.

  • PDF

An Effect on the Properties of Antiwashout Underwater Concrete by mixing time and mixing quantity (배합시간과 배합량이 수중불분리성 콘크리트의 특성에 미치는 영향)

  • 박세인;김동명;김종수;김명식
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2000.10a
    • /
    • pp.345-350
    • /
    • 2000
  • The objective of this study makes investigation into the effect on the properties of underwater antiwashout concrete. which is followed by mixing time and mixing quantity. There is an tendency that (the compressive strength of underwater antiwashout concrete made and cured in fresh water or sea water) is increase when dry mixing time, mixing quantity, total mixing time is increase as unit weight grows. The difference of compressive strength (in case of no dry mixing time and 60 second) is averagely 46.8kgf/㎠ in the fresh water and 35.6kgf/㎠ in sea water. it's considered that dry mixing is dispersed by underwater antiwashout admixture.

  • PDF

Properties of Strength Development on Cement Mortar Using Agent for Enduring Cold Climate (내한성 혼화제를 이용한 시멘트 모르타르의 강도증진 특성)

  • 홍상희;김현우;심보길;한민철;한천구
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2000.10a
    • /
    • pp.571-574
    • /
    • 2000
  • When fresh concrete is exposed to low temperature, the concrete may suffer from the frost damage at early ages and the strength development may be delayed. To solve such problems of cold weather concreting admixtures called agent for enduring cold climate are developed to prevent the fresh concrete from being frozen at early ages. In this study, the experiments are carried out on several kinds of agent for enduring cold climate to present their performance. According to experimental results, most kinds of agent for enduring cold climate show the strength development in the range $-5^{\circ}C$ of curing temperature, it tends to be delayed at long term maturity without agents for enduring cold climate. while it gains high strength maturity when agents for enduring cold climate is applied.

  • PDF

Study on Strength Development of Concrete for Top-Down Method (역타공법에 적용을 위한 콘크리트 강도성상 연구)

  • 정근호;이종균;김영회;이영도;정상진
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1998.10c
    • /
    • pp.48-53
    • /
    • 1998
  • The purpose of this study to fine the mixture of concrete for Top-Down method. As a result, In fresh concrete, slump value and slump-flow value were increased as fly ash concrete(10% ratio). When plasticizer was added 1.5% by weigh of binder in concrete, no fly ash concrete and fly ash concrete(10% ratio) all occurred segregation. And, no fly ash concrete and fly concrete(10% ratio) all showed compressive strength development close plain concrete as increasing plasticizer quantity. Especially, in case of 1.5% plasticizer of binder showed high compressive strength development.

  • PDF