• Title/Summary/Keyword: freeze-thaw durability

Search Result 156, Processing Time 0.02 seconds

Strength and Durability Properties of Concretes Using Ground Granulated Blast-Furnace Slag According to Steam Curing Types (고로(高爐)슬래그 미분말(微分末)을 사용한 콘크리트의 증기양생(蒸氣養生)에 따른 강도(强度) 및 내구특성(耐久特性))

  • Hong, Chang-Woo;Jang, Ho-Sung;Jeong, Won-Kyong
    • Resources Recycling
    • /
    • v.15 no.4 s.72
    • /
    • pp.52-59
    • /
    • 2006
  • The purpose of this study was to evaluate the effects of ground granulated blast-furnace slag on strength development and durability of ordinary portland cement concrete (OPC) with steam curing types. Main experimental variables were slag contents(0%, 10%, 30%, 50%, 70%) and curing types (standard, accelerated curing). It were performed to check the basic properties of concretes that compressive strength, rapid chloride ion permeability and chemical resistance. From the result, we have found that increasing the amount of blast-furnace slag produced concrete with increased compressive strength and permeability resistance. Rapid freezing-thawing test showed that they were good enough to protect the concrete structures and to carry out cyclic freezing and thawing. The freeze-thaw resistance of blast-furnace slag produced concretes maintained above 90% of relative dynamic modulus after 300 freezing-thawing cycles. Increasing the amount of blast-furnace slag produced concretes with increased chemical resistance.

Studies on the Durable Characteristics of Self-Healing Concrete with High Water-Tightness for Artificial Ground (인공지반용 고수밀 기반 자기치유성 콘크리트의 내구특성에 관한 연구)

  • Song, Tae-Hyeob;Park, Ji-Sun;Kim, Byung-Yun
    • Journal of the Architectural Institute of Korea Structure & Construction
    • /
    • v.35 no.9
    • /
    • pp.199-206
    • /
    • 2019
  • Experimental study on the durability characteristics to examine the feasibility of concrete with high water-tightness and self-healing performance to minimize maintenance of concrete for artificial ground is as follows. 1) When blending agent, swelling agents, and curing accelerator were added on the ternary system cement with blast-furnace slag fine particles and fly ash to give a self-healing property, higher blending strengths by 82% at design standard strength of 24MPa and by 74% at design strength of 30MPa, respectively could be obtained. 2) The permeability test for the specimens having high water-tightness and no shrinkage showed that the permeability was reduced at maximum of 98%. However, the permeability was decreased as the design strength was increased, showing the reduction rate of 87% at the design strength of 50MPa. 3) The depth of carbonation of blast-furnace slag and fly ash was increased in all the specimens compared with those of OPC only. However, as the material age was increased, carbonation penetration depth was decreased compared with the reference blend. 4) Compared with the reference blending using only OPC, the freeze-thaw resistance was higher in the case of blending with 40% of blast-furnace slag and 10% of fly ash at the design standard strength of 50MPa. In addition, the freeze-thaw resistance in general was superior in the design standard strength of 50MPa with the lower water-binder ratio (W/B) as compared with the design standard strength of 24MPa and 30MPa with the high water-binder ratios.

Material Properties of 3D Printed Mortars Produced with Synthetic Fibers and Biopolymers (합성섬유 및 바이오 폴리머를 혼입한 3D 프린팅 모르타르의 재료특성)

  • Hyo-Jung Kim;Byung-Jae Lee;Yun-Yong Kim
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.27 no.4
    • /
    • pp.78-85
    • /
    • 2023
  • In this study, synthetic fibers were applied to reduce shrinkage cracks that may occur in mortar produced by 3D printer. We used a biopolymer in powder form made from cactus stem (CS) as an admixture. The material properties of 3D printed mortar were experimentally evaluated. Replacing methylcellulose(MC) with 10% CS increases compressive strength by 9.84-23.92% regardless of the casting method. In addition, regardless of the casting method, shrinkage change, freeze-thaw resistance, and crack resistance are more effective than Plain. Incorporation of CS increases the polysaccharide macromolecular structure and improves durability. Mortars reinforced with synthetic fibers do not affect compressive strength and freeze-thaw. It is also effective for shrink deformation and crack resistance. Incorporating CS and fibers from 3D-printed mortar was found to be effective for durability and crack resistance.

Durability studies on concrete with partial replacement of cement and fine aggregates by fly ash and tailing material

  • Sunil, B.M.;Manjunatha, L.S.;Yaragalb, Subhash C.
    • Advances in concrete construction
    • /
    • v.5 no.6
    • /
    • pp.671-683
    • /
    • 2017
  • Commonly used concrete in general, consists of cement, fine aggregate, coarse aggregate and water. Natural river sand is the most commonly used material as fine aggregate in concrete. One of the important requirements of concrete is that it should be durable under certain conditions of exposure. The durability of concrete is defined as its ability to resist weathering action, chemical attack or any other process of deterioration. Durable concrete will retain its original form, quality and serviceability when exposed to its environment. Deterioration can occur in various forms such as alkali aggregate expansion, freeze-thaw expansion, salt scaling by de-icing salts, shrinkage, attack on the reinforcement due to carbonation, sulphate attack on exposure to ground water, sea water attack and corrosion caused by salts. Addition of admixtures may control these effects. In this paper, an attempt has been made to replace part of fine aggregate by tailing material and part of cement by fly ash to improve the durability of concrete. The various durability tests performed were chemical attack tests such as sulphate attack, chloride attack and acid attack test and water absorption test. The concrete blend with 35% Tailing Material (TM) in place of river sand and 20% Fly Ash (FA) in place of OPC, has exhibited higher durability characteristics.

A Study on Durability of Concrete According to Mix Condition by Marine Environment Exposure Experiment (해양환경폭로실험을 통한 배합조건별 콘크리트의 내구성에 관한 연구)

  • Jo, Young-Jin;Choi, Byung-Wook;Choi, Jae-Seok;Jung, Yong-Wook
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.14 no.9
    • /
    • pp.4542-4551
    • /
    • 2013
  • Recently, much attention has focused on the study of eco-friendly concrete using recycled by-products for protecting marine ecosystem and durability of concrete exposed to marine condition. This study evaluated the durabilities of 4 different type of concrete mixtures(Control, Marine, Porous, New slag) with the seawater resistance by marine environment exposure experiment and freeze-thaw resistance, resistance to chloride ion penetration considering severe deterioration environment. In this study, we conducted seawater resistance using compressive strength according to the age(7/28/56 days) of specimen and curing conditions(standard(fresh water), tidal, immersion, artificial seawater). The results show that compressive strength of concrete exposed to marine environment exposure condition was lower than those of the standard curing condition. Also, compressive strength of New slag using eco-friendly materials for protecting marine ecosystem was lower than those of other concretes, there is need to improve the performance of New slag. The results for freeze-thaw resistance showed that all mixtures have excellent, but the Porous and New slag were lower than others. Also, the more improved resistance to chloride ion penetration than those of the Marine was measured in the New slag regardless of curing condition.

Experimental Study to Evaluate the Durability of 100 MPa Class Ultra-high Strength Centrifugal Molding Concrete (100MPa급 초고강도 원심성형 콘크리트의 내구성 평가를 위한 실험연구)

  • Jeong-Hoi Kim;Sung-Jin Kim;Doo-Sung Lee
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.28 no.1
    • /
    • pp.12-23
    • /
    • 2024
  • In this study, a structural concrete square beam was developed using the centrifugal molding technique. In order to secure the bending stiffness of the cross section, the hollow rate of the cross section was set to 10% or less. Instead of using the current poor mixture of concrete and a concrete mixing ratio with a high slump (150-200) and a design strength of 100 MPa or more was developed and applied. In order to investigate the durability of centrifugally formed PSC square beams to be used as the superstructure of the avalanch tunnel or ramen bridge, the durability performance of ultra-high-strength centrifugally formed concrete with a compressive strength of 100 MPa was evaluated in terms of deterioration and chemical resistance properties.Concrete durability tests, including chloride penetration resistance, accelerated carbonation, sulfate erosion resistance, freeze-thaw resistance, and scaling resistance, were performed on centrifugally formed square beam test specimens produced in 2022 and 2023. Considering the information verified in this study, the durability of centrifugally molded concrete, which has increased watertightness in the later manufacturing stage, was found to be superior to that of general concrete.

A Study on the Durability of PCM Mixed Concrete for the Reduction of Cold and Hot Damage (혹한·혹서 피해 저감용 PCM 혼입콘크리트의 내구성에 관한 연구)

  • Hoyeol Kim;Il Young Jang
    • Journal of the Society of Disaster Information
    • /
    • v.20 no.2
    • /
    • pp.390-397
    • /
    • 2024
  • Purpose: In this study, PCM was used to give thermal performance to concrete and analyze its effect on durability to prevent disasters that may occur in concrete when exposed to hot and cold environments. Method: After preparing concrete specimens containing 10, 30, and 50% of the two types of PCMs compared to the cement volume, the pore volume, freeze melting resistance, and scaling resistance were evaluated. Result: Regardless of the type, when PCM powder was mixed with concrete, the amount of pores decreased, and when 10% and 30% were mixed, the freeze-melting resistance was also improved. It was also confirmed that the higher the mixing amount, the better the scaling resistance. Conclusion: When mixing powdered PCM into concrete, it is believed that durability can be improved to a certain level by the filling effect, and additional various studies should be supported for actual field application.

Accelerated Test Program for Durability Characteristics of GFRP Rebars (내구특성 파악을 위한 GFRP 보강근의 촉진실험 연구)

  • Kim, Hyeong-Yeol;You, Young-Jun;Park, Young-Hwan
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.10 no.1
    • /
    • pp.157-164
    • /
    • 2006
  • This paper presents the durability characteristics of commercially available CFRP rebars under various environmental conditions. Two types of GFRP rebars were tested by using an accelerated aging method. A total of 264 rebar specimens were conditioned up to 132 days in the moisture, chloride. alkaline, and freeze-thaw environmental conditions. The durability characteristics of conditioned rebars were obtained by comparing the tensile strength, horizontal shear strength, and elastic modulus between the unconditioned and conditioned GFRP rebars. The test results indicated that the mechanical properties of GFRP were significantly reduced after conditioning. Long-term degradation of GFRP rebars was also estimated using the results of a short-term durability test.

Mechanical and Durability Characteristics of Latex-Modified Concrete Using Ultra Rapid Hardening Cement (초속경 시멘트를 이용한 라텍스 개질 콘크리트의 역학성능과 내구성능)

  • Park, Sang-Hyun;Jung, Si-young;Kim, Hyun-yu;Choi, Kyoung-Kyu
    • Journal of the Architectural Institute of Korea Structure & Construction
    • /
    • v.35 no.5
    • /
    • pp.153-160
    • /
    • 2019
  • The purpose of this study was to investigate the mechanical and durability characteristics of latex-modified concrete using ultra rapid hardening cement : four types of mechanical tests including compressive strength, modulus of elasticity, flexural strength and bond strength were performed; and seven types of durability tests including resistance of concrete to chloride ion penetration, freeze-thaw resistance, scaling resistance, coefficient of thermal expansion, cracking tendency, abrasion resistance and drying shrinkage were performed. Required material performance of each test was determined in accordance with the Korea specification for repair of concrete and pavement repairing materials. The test results satisfied the required material performances, and presented a good mechanical and durability characteristics. In particularly, the materials showed early development of compressive strength, flexural strength and bond strength at 3 and 4 hours after curing. SEM photos were also taken to investigate the micro structures of the materials after chloride ion penetration test.

An experimental study on the durability of steel fiber reinforced concrete containing waste glass (폐유리를 활용한 강섬유보강 콘크리트의 내구성에 관한 실험적 연구)

  • 정명일;조광연;이봉춘;김경훈;박승범
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2002.10a
    • /
    • pp.841-846
    • /
    • 2002
  • As growing of industrialization and increasing of population. the quantities of waste are rapidly growing in the earth. It cause some problems such as the waste of natural resources and environmental pollution. In this context, recycling waste glass as a material of concrete has a great advantage environmentally and economically. On that score, other contries have start recycling waste glass widely and accoumulatig the technology of manufacturing equipment and construction. However, few studies have been done in this country. Therefore, this study was conducted freeze-thaw resistance test and neutralization reaction test to analyze the durability properties of steel fiber reinforced concrete containing waste glass as fine aggregate and containing industrial by-products(Fly ash).

  • PDF