In order to obtain the maximum flame retardancy with the minimal deterioration of physical properties of PU flame-retardant coatings, chlorine and phosphorous functional groups were introduced into the pre-polymer of modified polyesters. In the first step, the tetramethylene bis(orthophosphate) (TBOP) and neohexanediol dichloroacetate (DCA-adduct) intermediates were synthesized. In the second step, 1,4-butanediol and adipic acid monomers were polymerized with the two kind of intermediates to obtain copolymer. The modified polyesters containing chlorine and phosphorous (ATBA-10C, -20C, and -30C) were synthesized by adjusting the contents of chlorine compound (dichloroacetic acid, 10, 20, 30 wt%) with fixed the content of phosphorous compound (2 wt%). The PU flame-retardant coatings (TTBAH -10C, -20C, and -30C) were prepared using the synthesized ATBAs and HDI-trimer as curing agent at room temperature. The physical properties of PU flame-retardant coatings with chlorine and phosphorous were inferior to those with phosphorous only and the properties were getting worse with increasing chlorine content. Flame retardancy was tested with three methods. With the vertical method, Complete combustion time of ATBAHs were $259^{\sim}347$ seconds, which means that the prepared coatings are good flame-retardant. With the $45^{\circ}$ Meckel burner method, char lengths of the three prepared coatings were less than 2.9 cm, which indicates that the prepared coatings are 1st grade flame retardancy. With the limiting oxygen index (LOI) method, the LOI values of the three prepared coatings were in the range of $30^{\sim}35%$, which proves good flame retardancy of the prepared coatings. From the results of flame retardancy tests of the specimens that contain the same amounts of flame retarding compounds, it was found that the coatings containing both phosphorous and chlorine show higher flame retardancy than the coatings containing phosphorous alone. This indicates that some synergy effect of flame retardancy exists between phosphorous and chlorine.
(2,3-Dibromopropyl) phenyl lauroyl phosphate[DPPL] was synthesized by adding lauric acid to (2,3-dibromopropyl)chloro phenyl phosphate [DPP]. which prepared from phenyl phosphoric acid dichloride with 2,3-dibromo propyl alcohol. Flame retardants of DPPF and DPPLF were prepared respectively. DPPF was a water soluble flame retardant, and DPPLF was o/w type emulsion flame retardant. After flame retardant treating two kinds of flame retardants to the various synthetic fabrics respectively. the flame retardancy and tear strength were measured. As the results of the measurement. DPPF had only name retardancy, but DPPLF had both of flame retardancy and softness.
고분자 물질의 화재 위험성 및 화재시 인명 피해의 감소를 위한 기초자료로 제시하고자 점토질의 첨가에 의한 난연성 평가를 수행하였다. 본 연구에서는 에폭시 수지의 난연성 향상과 연기의 발생량을 감소시키기 위하여 점토질의 montmorillonite(MMT)와 같은 천연 물질을 삽입하여 연소 특성을 살펴보았다. 이 연구를 위하여 한계산소지수(limiting oxygen index, LOI), 탄화층 생성량(char yield), 연기 밀도(smoke density) 측정 둥의 난연성 실험을 실시하였다. Epoxy/MMT의 복합재료는 MMT의 농도가 증가할수록 한계산소지수 및 탄화층 생성량이 증가하여 난연성이 향상되었으나 연기 밀도는 오히려 증가하는 결과를 나타내었다.
3-(Hydroxyphenyl phosphinyl) propanoic acid (HPPA) has been one of the most commonly used durable flame retardant agents for polyethylene terephthalate (PET) for many years. We intended to explore the application of HPPA to cellulose fabrics as formaldehyde-free phosphorus based flame retardants (FRs) through green chemistry process. The flame retardancy of the flame-retardant treated cellulose fabrics were characterized by using inductively coupled plasma spectroscopy (ICP) and limiting oxygen index (LOI). Structural changes of the treated cellulose fabrics were carried out by thermogravimetric analysis (TGA) and Fourier transform infrared (FT-IR) spectroscopy. To enhance the flame retardancy of HPPA treated cellulose fibers, glycerol polyglycidyl ether (GPE), a crosslinking agent was employed. Both HPPA and GPE treated cotton fabric imparted an LOI value over 26.
The study was conducted to find out suitable flame proofing on silk fabrics and to examine closely the flame retardancy effect and the physical properties changes of the silk, which was dyed by natural dyes and synthetic dyes, treated with agent (Diphenylbutylamidophosphate (DPBAP)). The results of the study were as follows: 1) Silk could be treated with DPBAP easily soluble in water by means of simple Pad-Dry-Cure. 2) The add-on of silk fabrics dyed by natural dyes was more than that of silk fabrics dyed by synthetic dyes. 3) The silk fabrics dyed by india ink among natural dyes has more flame retardancy effect in before treating with flame proofing agent than in after treating with it. 4) The physical properties (stiffness and tensile strength) of the silk fabrics treated with flame retardancy agent were little changed.
This study analyzed the physical properties and flame retardancy of Tencel FR/Cotton complex knit fabrics in order to satisfy two aspects of eco-friendliness and functionality. The flame retardant (FR) treatment of complex knit fabrics was applied by a pad-dry-cure method for additional functionality. Tensile strength, extension, bursting strength, LOI, and flame retardancy were measured by the KS (Korean Standard) K manual. The hand value knit fabrics were measured by KES-FB system. Subsequently, tensile strength and extension of wale and tensile strength of course increased in tandem with the Tencel FR yarn content. Tencel FR/Cotton complex knit fabrics were suitable for summer-weight and for baby clothes through the KES-FB system measurements. The bursting strength of Tencel FR/Cotton complex knit fabrics decreased as the contents of the Tencel FR increased; in addition, LOI increased as the contents of Tencel FR increased. This was due to the Tencel FR flame resistance function; however, the tensile strength decreased. The optimum fiber content of Tencel FR/cotton content was 1:1. The optimum conditions of flame retardant treatment were a treatment temperature $130^{\circ}C$ and the concentration of finishing agent and assistance binder (AR4260) was 35% and 1%, respectively.
The flame-retardant coatings were prepared by blending the synthesized triphosphorus modified polyester in the previous paper and hexamethylene diisocyanate-trimer and curing it at room temperature. The characterization of the films of the prepared coatings was performed. It was confirmed that no deterioration of physical properties of PU coatings was observed with the increasing phenylphosphonic acid (PPA) contents. Flame retardancy was tested by a $45^{\circ}$ Meckel burner method and LOI method. With the $45^{\circ}$ Meckel burner method, CATBTP-20C and CATBTP-30C that contain 20 wt% and 30 wt% of PPA, flame retarding component, respectively, showed the first grade flame retardancy with $2.8{\sim}3.9\;cm$ of char length ; and, with LOI method, they exhibited a good flame retardancy as a range of $30{\sim}32%$ of combustion values.
The flame retardancy by the addition of clay was evaluated to present as the fundamental data to decrease the fire hazard of polymers and life losses. The flame retardancy was examined to increase flame retardancy and to decrease smoke yield of epoxy by the addition of clay such as montmorillonite. For this study, the experiments of flame retardancy were conducted as follows : the measurement of the limiting oxygen index(LOI), char yield, and smoke density. As MMT concentration increased, epoxy/MMT composite increased LOI and char yield with the decreased smoke density.
This study was performed to test the flame retardancy of zelkova sarrata-based materials by the treatment of ammonium salts. Zelkova sarrata plate was soaked by the treatment with three 20 wt% ammonium salt solutions consisting ammonium chloride (AMSL), monoammonium phosphate (MAPP), and diammonium phosphate (DAPP), respectively, at the room temperature. After the drying specimen treated with chemicals, combustion properties were examined by the cone calorimeter (ISO 5660-1). When the ammonium salts were used as the retardant for zelkova sarrata, the flame retardancy improved due to the treated ammonium salts in the virgin zelkova sarrata. However the specimen shows increasing CO over virgin zelkova sarrata and It is supposed that toxicities depend on extents. Also, the specimen with ammonium salts showed the higher total smoke release (TSR) than that of virgin plate. Of specimens treated with ammonium salts the ammonium chloride handled the test side was considered a improved inhibitory effect of combustion.
4종의 판상형 목재제품의 방염제 도포량과 침지시간에 따른 방염성능을 분석하기 위하여 소방청의 방염성능기준에 따라 목재제품의 탄화길이와 탄화면적을 측정하였다. 잣나무 합판, 낙엽송 합판, 편백 판재, 타공처리된 자작나무 합판에 자체 개발된 방염제를 각각 300, 500 g/㎡씩 도포하고 방염처리되지 않은 시험편과 비교하였다. 일반적으로 방염제의 도포량이 증가함에 따라 탄화길이와 탄화면적이 감소하여 방염성능이 증가하는 경향을 나타냈으나, 낙엽송 합판을 제외하고 탄화길이와 탄화면적의 감소량이 크지 않았다. 타공처리된 자작나무 합판의 침지시간에 따른 방염성능은 60분의 침지시간까지 양의 상관관계를 나타냈으나, 그 이후 점차 완만해지는 경향을 보였다. 방염제의 도포량과 침지시간에 따른 목재제품의 방염성능은 추후 방염성능 기준에 맞는 불연·준불연 목재의 생산을 위한 기초자료로 이용될 것으로 기대된다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.