Lee, Yu Jun;Lee, Su Bin;Jung, Jae Young;Lee, Dam Hee;Cho, Ur Ryong
Elastomers and Composites
/
제51권2호
/
pp.93-98
/
2016
The composites of EVA/EPDM including aluminum trioxide (ATH) as a fire retardant were manufactured for the purpose of improving low temperature property and flame resistance in the rubbery materials. The ratio of EVA to EPDM didn't affect the flame resistance of the rubber composites. The addition of ATH resulted in increase of the flame resistance. In the evaluation of the cold resistance, the increasing EPDM content showed enhancement of cold resistance in the composites due to increasing low Tg EPDM. It was found out that tensile strengths of the composites showed a maximum value at 100 phr of ATH by reinforcing effect, but a minimum value at 200 phr of ATH owing to slippage between the flame retardant by the external stress. In the measurement of solvent resistance in tetrahydrofuran, the increasing ATH content yielded enhancement of solvent resistance by reducing swelling of the composite, and increasing EPDM content also resulted from increase of the solvent resistance by reduction of polarizability as well as increase of crosslink in the composites.
건축 재료로 사용되는 목재의 내화성능에 관한 기존 연구들은 목재에 난연 또는 방염 처리하였을 경우 연소특성을 확인하는 것에 집중되어 졌다. 본 논문에서는 화염에 노출된 목재의 열분해와 밀접한 관련이 있는 내부 온도 변화를 확인하기 위하여 건축용 구조재로 널리 사용되는 미송(Douglas-fir)에 방염액 및 방염도료를 처리 후 표준 가열 온도 곡선에 따라 수평가열로에서 가열실험을 실시하였다. 실험결과 방염액을 처리하였을 때 목재내부의 열확산이 현저히 감소하는 것을 확인할 수 있었으며 방염도료를 처리한 시료의 경우 고온에 노출 되었을 때 도막이 박리되어 방염효과를 기대할 수 없었다. 따라서 두꺼운 목재에 방염효과를 높이기 위해서는 목재표면에 도막을 형성시키는 방염도료보다는 목재내부로 침투하는 방염액을 사용하는 것이 방화효과가 클 것으로 판단된다.
Conventional flame retardant cable using PVC or CR materials generate considerable amount of toxic and acidic gas (HCI etc.) together with excessive black smoke during a fire. The newly developed halogen free materials have dissolved the problem of halogen acid gases. This paer describes the development of this power cable insulation and sheath, using halogen free materals.
To improve flame retardation of poly(ethylene terephthalate) (PET) against burning, resorcinol bis(diphenyl phosphate) (RDP), phosphorous containing flame retardant, was incorporated into PET backbone by radical reaction pathway. Radical endcapping of PET with RDP was confirmed by spectroscopic and thermal analysis. From 400 MHz $^{31}P$ solid state FT-NMR spectrum of PET with RDP (PET-RDP), phosphorus spectra peak in RDP was found at ca. -10 ppm. Furthermore, P-C bond stretching vibration peaks were found ca. $530cm^{-1}$ in FT-IR spectrums of PET-RDP. These results indicated that RDP can be chemically bound at the ends of PET by radical addition method. Thermal characteristics of pure PET (pPET) and PET-RDP were measured and evaluated by TGA thermal analysis. There was not significant changes in thermal characteristics of PET-RDP compared to that of pPET.
Kim, Chowon;Lee, Jinwoo;Yoon, Hyejeong;Suhr, Jonghwan
Composites Research
/
제35권5호
/
pp.359-364
/
2022
Polymers are inherently vulnerable to flame, which limits their application to various high-tech industries. In addition, environmental regulations restrict the use of halogen-based flame retardants which has best flame-retardant effect. There are inorganic flame retardants and phosphorous flame retardants as representative non-halogen-based flame retardants. However, high content of flame retardants is required to impart high flame retardancy of the polymers, and this leads to a decrease in mechanical properties. In this research, a new approach for inorganic flame retardant-based polymer composites with high mechanical properties and flame retardancy was suggested. Inorganic flame retardants called as magnesium oxysulfate whisker (MOSw) were used in this research. MOSw can extinguish fire by releasing water and non-combustible gases when exposed to flame. In addition, they have reinforcing effect when added into the polymer with its high aspect ratio. Expandable graphite (EG) was used as a flame-retardant supplement by helping to form a more dense char layer. Through this research, it is expected that it can be applied to various industries requiring flame retardancy such as automobile, and architecture by replacing halogen-based flame polymer composites.
Wood is a construction material that has the advantages of carbon dioxide storage ability, noise reflection, and eco-friendliness. In order to use wood for a long time, you must use wood-specific paint, which is called oil stain. Oil stain improves water resistance and moisture resistance, but has the disadvantage of being weak against fire. This is because the oil contained in the oil stain causes a chemical reaction, and this chemical reaction causes the oil stain to spontaneously ignite, igniting nearby combustible materials and causing frequent fires. To improve this, in this study, different flame retardants were mixed and added to oil stain to produce functional oil stain. In addition, we would like to apply it to wood to check glow time and carbonization area. As a result of the experiment, it shows the best performance when mixed at 30(15 + 15)(%) and added to oil stain. The remaining burn time is satisfied from 10% for all samples, and the carbonized area is satisfied when it is 30%.
향상된 특성을 갖는 환경친화적인 복합재료의 개발은 고분자재료의 미래에 있어 필수적이며, 부분적으로 또는 완전히 재생가능한 기지재 또는 보강재에 단지 몇 %의 첨가제를 첨가함으로써 쉽게 제작할 수 있다. 본 연구에서는 마닐라삼 섬유를 보강재로, 비닐에스터를 기지재로 사용하였으며, VARTM 공정을 이용하여 복합재료를 제조하였다. 또한 마닐라삼 섬유의 알칼리표면처리를 수행하고, APP, HNT를 난연제를 첨가함으로써 기계적 물성과 난연 물성을 향상시키고자 하였다. 실험을 통하여 표면처리가 천연섬유의 친수성을 감소시키고 소수성인 기지재와의 계면접착력을 향상시켰으며, 이는 개발된 복합재료의 기계적 물성 향상을 이끌었다. 유사하게, 복합재료의 난연성도 난연제의 함량이 증가함에 따라 크게 향상되는 결과를 얻을 수 있었다.
내화재료는 건축물에서 화재사고로부터 화염을 차단하기 위해 사용된다. 본 연구에서는 실리콘 고무에 무기계 난연제인 aluminium trihydroxide(ATH, $Al(OH)_3$)와 magnesium dihydroxide(MDH, $Mg(OH)_2$)를 첨가한 복합체를 기계적 교반으로 제조한 후 내화성능향상에 관한 연구를 진행하였다. 내화재료의 열 특성분석을 위해 TGA를 사용하였고, rheometer를 이용해 유변학적 분석을 하였다. 내화특성을 분석하기 위해 gas torch를 이용하였다. 본 연구를 통하여 ATH와 MDH가 첨가되면 실리콘 고무의 내화성능이 향상됨을 알 수 있었다.
Garcia, Harkaitz;Cuadrado, Jesus;Biezma, Maria V.;Calderon, Inigo
Structural Engineering and Mechanics
/
제78권1호
/
pp.67-75
/
2021
This work studies the behaviour of a steel portal frame selection under fire exposure, considering both span lengths and fire exposure times as variables. Such structures combine carbon steel (S275), fireproof micro-alloyed steel (FR), and coatings of intumescent paint with variable thicknesses, improving thereby the flame retardant behaviour of the steel structure. Thus, the main contribution of this study is the optimization of the portal frames by combining both steels, analysing the resulting costs influence on the final dimensions. Besides, the topological optimization of each steel component within the structure is also defined, in accordance with the following variables: weather conditions, span, paint thickness, and cost of steel. The results mainly confirmed that using both FR and S275 grades with intumescent painting is the Pareto optimum when considering performance, feasibility and costs of such portal frames widely used for industrial facilities.
본 연구는 주택이나 창고 등의 건축용 합성 단열재의 연소특성을 분석한 것으로 콘칼로리미터 및 SEM을 활용해 난연 스티로폼, 일반 스티로폼, 우레탄, 석고보드 등 4종의 재료별 연소특성을 실험 및 분석하였다. 시험결과 각 재료별 착화특성으로는 상기 단열재에 대한 착화시간(TTI)은 27 s~43 s로 나타났으며, 이중 난연 스티로폼은 TTI이 가장 낮은 27 s에 착화되었다가 28 s에 소멸됨을 보였다. 또한 각 재료들의 최대열방출율(peak HRR)과 평균열방출율(mean HRR)의 크기는 우레탄>석고보드>난연 스티로폼>일반 스티로폼으로 나타났으며, 총열방출량(Total Heat Release Rate, THR)은 우레탄>난연 스티로폼>일반 스티로폼>석고보드 순으로 나타났다. 또한 총연기방출량(Total smoke release, $m^2/m^2$)은 난연 스티로폼에서 가장 많은 $30.798m^2/m^2$을 보였다. 일반 스티로폼의 CO 방출농도는 0.275 kg/kg, $CO_2$ 방출농도는 12.807 kg/kg값이 나타났다. 잔유물은 위 4가지 재료 중 석고보드에서 가장 많은 0.029 g을 보였다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.