• 제목/요약/키워드: electrical melting

검색결과 400건 처리시간 0.024초

출탕유도전극을 이용한 용융물의 출탕방법 및 특성에 대한 연구 (A Study on the Properties and Methods of Electrode System for Tapping of Melts)

  • 문영표;최장영
    • 전기학회논문지
    • /
    • 제65권3호
    • /
    • pp.499-503
    • /
    • 2016
  • For safety and economy reasons, hazardous waste including radioactive waste is desired to be converted into stable waste forms with a maximum volume reduction. High temperature melting technology using a plasma torch system can effectively treat even the non-flammable waste as desired. By far, one of the most difficult process for melting the non-flammable waste is a tapping of melts because the melting point of a residual slag in the tapping hole is high and because the viscosity of the melt increases sharply when tapping out. In case of a stationary furnace with a slant tapping port on the side of furnace, a certain amount of melts is left in the tapping hole after tapping out. Because of this, at every end of a melting cycle, the tapping hole needs to be opened by tapping device. The developed tapping device of melts based on both a guide electrode and auxiliary electrode is adequate for the application to discharge of melts except that the consumption of the guide electrode is somewhat faster than expected. Melt is collected in the water cooled vessel.

전자선 조사된 저밀도 폴리에틸렌 박막의 체적고유저항 특성 (Volume Resistivity Characteristics of Low Density Polyethylene film irradiated with Electron Beam)

  • 조돈찬;조경순;이수원;김왕곤;홍진웅
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1996년도 추계학술대회 논문집 학회본부
    • /
    • pp.193-195
    • /
    • 1996
  • Low-density polyethylene(LDPE ; thickness 100[${\mu}m$] as a experimental specimen is irradiated with electron beam by using electron beam accelerator, and as an experimental specimen, the nonirradiated specimen and the specimen irradiated with electron beam is produced according to the classification of dose. From the analysis of DSC, the crystalline melting point of the specimen irradiated with electron beam is lower than that of virgin specimen. It is confirmed thai the volume resistivity is increased from the temperature over $50[^{\circ}C]{\sim}60[^{\circ}C]$ to the crystalline melting point because of the defects of solid structure and the formation of many trap centers by means of electron beam irradiation, but decreased in the temperature over the crystalline melting point because of the melt of crystalline.

  • PDF

용융온도와 유지시간이 용융법으로 제작한 고온초전도체의 임계특성에 미치는 영향 (The Effects of Melting Temperature and Holding Time on Critical Characteristics of HTSC Fabricated by Melting Method)

  • 임성훈;한태희;박경국;임성우;조동언;한병성
    • 한국전기전자재료학회논문지
    • /
    • 제11권2호
    • /
    • pp.154-161
    • /
    • 1998
  • The effects of melting temperature and holding time on the critical current density($J_c$) of $YBa_2Cu_3O_x$ based superconducting bulk fabricated by MPMG process were investigated. The amount of the formed $Y_2BaCuO_5$ phases increased with the melting temperature. However, the value of critical current density was highest at 1120 $^{\circ}C$. With this proper melting temperature, the effect of holding time on the critical characteristics was also investigated. In the case of Ag addition, the volume of the formed $Y_2BaCuO_5$ phase when the amount of Ag addition was 10 wt% and 20 wt% was observed to be highest at 20 minute and 40 minute respectively. But in the specimen without Ag, volume of $Y_2BaCuO_5$ phase increased as the holding time increased. The proper melting temperature and the holding time obtained were 1120 $^{\circ}C$ and 20 minute. The long holding time was not effective for the $J_c$ improvement as well as the formation of $Y_2BaCuO_5$.

  • PDF

Study on Properties of Ag and PbO Doped $YBa_2Cu_3O_x$

  • Son, Dea-Wha;Fan, Zhanguo
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 하계학술대회 논문집 Vol.4 No.1
    • /
    • pp.593-596
    • /
    • 2003
  • A proposed way to prepare $YBa_2Cu_3O_y$ wires or tapes is that Ag is used as substrate and melting point of $YBa_2Cu_3O_y$ is decreased to lower than the melting point of silver ($961\;^{\circ}C$). Therefore after the deposition of $YBa_2Cu_3O_y$ film on Ag substrate, the heat treatment can be carried out below the Ag melting point. Silver (Ag) and Lead oxide(PbO) were selected to be additives for $YBa_2Cu_3O_y$. Different Ag and PbO contents were added in $YBa_2Cu_3O_y$, the melting points of which were measured by DTA. In order to guarantee that the superconductivity of $YBa_2Cu_3O_y$ was not reduced after Ag and PbO added into $YBa_2Cu_3O_y$, their superconductivities were measured. It is proved that as additives, both Ag and PbO can reduce the melting point of $YBa_2Cu_3O_y$. For Ag doped $YBa_2Cu_3O_y$, $T_c$ is about 93K and ${\Delta}Tc$ is $2{\sim}3K$. For PbO doped $YBa_2Cu_3O_y$, $T_c$ is $88K{\sim}92K$ and ${\Delta}T_c$ is $11{\sim}12K$. When 10 wt% of Ag and 10 wt% PbO were added in $YBa_2Cu_3O_y$, the melting point of the mixture of $YBa_2Cu_3O_y$ (80 wt%), Ag (10 wt%) and PbO (l0 wt%) is $943^{\circ}C$. The transition temperatures ($T_c$) of the sample is 91.8 K.

  • PDF

존멜팅법으로 제조한 (YNdSm)-Ba-Cu-O계 고온복합초전도체의 미세구조 및 전기적 특성 (Microstructure and Electrical Properties of (YNdSm)-Ba-Cu-O High Tc Composite Superconductors by Zone Melting Process)

  • 김소정;이상헌
    • 한국전기전자재료학회논문지
    • /
    • 제29권2호
    • /
    • pp.110-113
    • /
    • 2016
  • (YNdSm)-Ba-Cu-O system high Tc composite superconductors were directionally grown by zone melting process, having large temperature gradient, in air atmosphere. Cylindrical green rods of $(YNdSm)_{1.8}Ba_{2.4}Cu_{3.4}O_x$ [(YNS)1.8]composite oxides by CIP (cold isostatic pressing) method using rubber mold were fabricated. The microstructure and superconducting properties were investigated by XRD, TEM and SQUID magnetometer. The size of nonsuperconducting $(YNdSm)_2BaCuO_5$ inclusions of the melt-textured (YNS)1.8 sample with $CeO_2$ additive were remarkably reduced and uniformly distributed within the superconducting (YNS)1.8 matrix. (YNS)1.8 samples, with / without $CeO_2$ additive, showed an onset $T_c{\geq}90K$ and sharp superconducting transition. The critical current density $J_c$ value of the (YNdSm)1.8 superconductor with $CeO_2$ additive were 840 A, $1.2{\times}104A/cm^2$ in 77 K, 0 Tesla by direct current transport method.

전기저항선용 Fe-xCr합금의 미세조직에 미치는 Al 및 Ti첨가의 영향 (Effects of Al and Ti Additons on Microstructure in Fe-xCrAlloy for Electrical Resistance Wire.)

  • 최수정;박수동;이희웅;김봉서
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 하계학술대회 논문집
    • /
    • pp.108-110
    • /
    • 2000
  • The aim of this paper is to investigate the effect of Al and Ti on microstructure of Fe-Cr-Al alloy systems for applying electrical resistance wires of electrical furnace. From the preliminary study, the amount of recovered addition elements increased in the case of both vacuum and Ar-atmosphere melting than that in the case of air-atmosphere melting. Also, optimum Cr content for good performance at high temperature was approximately 24wt% from the observation of microstucture. The precipitates of Fe-Cr, Al-Cr and Al phases were observed, adding Al and Ti. Especially, Sharp rectangular shapes of precipitates were observed with increasing amount of Ti.

  • PDF

열처리 조건에 따른 Bi-2212 초전도 튜브의 특성 (Characteristics of Bi-2212 Superconductor Tube Depending on Heat-treatment Conditions)

  • 박용민;장건익
    • 한국전기전자재료학회논문지
    • /
    • 제14권7호
    • /
    • pp.606-610
    • /
    • 2001
  • Bi-2212 HTS tube was fabricated by centrifugal forming and partial melting processes. Bi-2212 bulk tube has been optimized to achieve smooth surface and uniform thickness. The slurry was prepared in the mixing ratio of 10:1 between Bi-2212 powder and binder and initially charged into the rotating mold under the speed of 300~450 rpm. Heat-treatment was performed at the temperature ranges of 860~89$0^{\circ}C$ in air for partial melting. the HTS tube fabricated by centrifugal forming process at 89$0^{\circ}C$ under the rotating speed of 450 rpm was highly densified and the plate-like grains with more than 20${\mu}{\textrm}{m}$ were well oriented along the rotating axis. The measured Tc and J$_{c}$ at 10K on specimen heat treated at 89$0^{\circ}C$ was around 85 K and 1,200 A/$\textrm{cm}^2$ respectively.y.

  • PDF

NdBCO 벌크 HTS 초전도 특성 (Superconducting Properties of NdBCO Bulk HTS)

  • 소대화;이영매;번점국
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 추계학술대회 논문집 Vol.15
    • /
    • pp.91-94
    • /
    • 2002
  • The conditions of zone-melting method such as a sample travel speed in a furnace, content of Nd422, control of melting temperature, and heat-treatment with/without Ar gas for $NdBa_{2}Cu_{3}O_{7-\delta}$ superconductor was optimized, As a results, a $NdBa_{2}Cu_{3}O_{7-\delta}$ sample with a surface area of $25mm^{2}$ showed a good superconducting properties when its travel speed was 6 mm/h, The improvement of superconductivity added with 10~20 wt% of Nd422 phase increasing pinning effect was also shown. The critical current density, $J_{c}$ was remarkable affected by the condition of heat-treatment temperature of $NdBa_{2}Cu_{3}O_{7-\delta}$superconductor with/without Ar ambient gas.

  • PDF

전기로 대전류 케이블 고장진단 알고리즘 개발 (Development of a Fault Diagnosis Algorithm on a High Current Cable of Arc Furnace)

  • 김상우;장유진
    • 대한전기학회논문지:시스템및제어부문D
    • /
    • 제55권3호
    • /
    • pp.115-118
    • /
    • 2006
  • In the steel industry, a steel melting electric arc furnace is used to produce both carbon and alloy steels. Steel scrap which is charged into the furnace is heated by means of electric arc between graphite electrodes and the scrap. In this melting process, current is supplied to the furnace through HCC(high current cable) which connect the furnace and transformer. Four HCCs are assigned to each phase in our system to divide the current. Since a sudden cable breaking result in the shutdown of melting process, an aging detection of HCC is very important for both an improvement of productivity and cost reduction. In this paper, the aging of the HCC is estimated by using the current ratio between four HCCs.

melting법에 의해 La이 첨가된 Bi-Te계 가압 소결체의 열전특성

  • 양준혁;김봉서;도환수;오민욱;박수동;이희웅;배동식
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 추계학술대회 논문집
    • /
    • pp.143-143
    • /
    • 2007
  • Bi-Te계 화합물은 상온영역($250^{\circ}C$이하)에서 열전특성이 우수하여, 냉각용 및 발전용 열전소자 재료로 사용되고 있다. 앞선 연구에서 MA법에 의한 La이 치환된 Bi-Te 진공가압 소결체의 열전특성이 $Bi_2Te_3$와 비교하여 향상된 값을 나타내었다. 본 연구에서는 Bi와 Te을 각각 0.01wt%, 0.02wt% La으로 미량 치환하여 melting법으로 제조한 분말을 $420^{\circ}C$, 200MPa로 가압 소결하였다. 가압 소결체의 열전특성은 Seebeck계수, 전기전도도. 열전도도를 측정하여 성능지수를 계산하였고 Bi-Te, (Bi-La)-Te, Bi-(Te-La)의 열전특성을 비교 분석하였다.

  • PDF