The hydraulic structure of the hydroelectric power plant such as aqueduct tunnels and the drainage canal became old. Therefore, because the concrete surface of the aqueduct tunnel has received severe damage by wear-out and the crack etc the repair is demanded. This research examined the applicability of the repair mortar which mixed the fly ash and an artificial aggregate by using the very high early strength cement. As a result, good Quality repair mortar which satisfied the demand performance more than self-flow 270mm and compressive strength $50N/mm^2$ (age of 28days) adjusting of water cement ratio by using the MTX cement be able to be manufactured.
본 연구에서는 SBFC의 기본 성능을 분석하고, 페이스트 및 모르터에서의 공학적 특성을 검토하여, 향후 경제적인 조강콘크리트 개발을 위한 방안으로 활용하고자 하였다. 실험결과 SBFC의 우수한 조기강도 발현 성능을 확인 할 수 있었고, 유동성을 고려했을 때 OPC와 SBFC와의 적정 혼입율을 도출하여 사용하는 것이 바람직 할 것으로 판단된다.
The purpose of this research is to seek properties of flowing light-weight aggregate concrete and possibility of application. The experimental analysis results by using light-weight aggregate and industrial waste such flyash, furnace slag are as follow. 1) The research shows that flowing light-weight aggregate concrete of slump 23~27cm, slump flow 58~69 cm is possible, but material segregation is appeared above slump 26.5cm and slump flow 65 cm. 2) If mixing ratio of flyash is increase, strength deterioration is about 25 % in early age. It showed that effectiveness of long time strength improvement because strength manifestation ratio is above 95% in a long term. 3) This research showed possibility of substitution of blast furnace slag because strength deterioration by using mixing of furnace slag was appeared small deterioration range as below 10 %. 4) Each experimental compressive strength ratios were 77 %(1st week), 86 %(2nd week), 109 %(8th week), 115 %(13th week), 125 % (26th week) on the basis of 28 days. If mixing ratio of flyash is increase, long term strength increase ratio is improved.
In this study, prediction of later-age compressive strength of ultra-high strength concrete, based on the accelerated strength of concrete cured in 80℃ warm water was investigated. As a result, the nature of ultra-high strength concrete showed a rapid early strength enhancement, compressive strength using warm water method of 80℃ at 2days is same compressive at 28days using standard curing.
This study is intended to investigate the properties of early strength development by application of TEA to the field. According to the results, when TEA is added, fluidity is almost same to base concrete, and increases upto aimed slump after field flowing. Setting time does not differ in the case of base and TEA, but retarded after flowing. The time when compressive strength gains 5 MPa, which side form can be removed, is 23 hours, and so the removal time is shortened by I hours in comparison with plain concrete. But compressive strength is almost same to that of plain concrete at 28 days. The rebound value of P type schmidt hammer show similar tendency to compressive strength, and the rebound value of structure is higher than that of standard curing specimen due to heat capacity effect and drying by the air outside. Therefore, it is thought that if the rebound value of P type schmidt hammer is controled. by about 26 in consideration of open air environment, it is very effective to determine the removal time of side forms.
This study is intended to investigate the properties of early strength development by application of TEA to the field. According to the results, when TEA is added, fluidity is almost same to base concrete, and increases upto aimed slump after field flowing. Setting time does not differ in the case of base and TEA, but is retarded after flowing. The time when compressive strength gains 5 MPa, which side form can be removed, is 23 hours, and so the removal time is shortened by 1hours in comparison with plain concrete. But compressive strength is almost same to that of plain concrete at 28 days. The rebound value of P type schmidt hammer show similar tendency to compressive strength, and the rebound value of structure is higher than that of standard curing specimen due to heat capacity effect and drying by the air outside. Therefore, it is thought that if the rebound value of P type schmidt hammer is controled. by about 26 in consideration of open air environment, it is very effective to determine the removal time of side forms.
In this study, the experiment was carried out to investigate and analyze the influence of fineness of blast furnace slag powder on the properties of high strength concrete. The main experimental variables were water/binder ratio 27.5, 31.5, 35.5(%) water content $165kg/m^3$ and mineral admixtures such as blast furnace slag powder. Even in a case where the ratio of blast furnace slag powder is 70%, using a fineness of 8000 grade afforded a higher strength development than using a plain concrete, which indicates the potential of high utilization in the future. Although it has been pointed out that the concrete using blast furnace slag powder has a problem of yielding relatively low rate of strength development in the early age, it is demonstrated that this can be resolved by using a powder with fineness greater than 6000 grade. It is considered necessary that powder fineness should be upgraded for the applications such as high performance concrete to be used in high strength required areas by considering hydration heat control and early strength requirements in the future.
The advantages of blast-furnace slag concrete may include lower hydration heating velocity, restraint on concrete temperature increase, long-age strength improvement due to latent hydraulic reaction, improved water tightness, and repulsion to chemical erosion. These advantages contribute to the high quality of the blast-furnace slag concrete. However, the blast-furnace slag concrete has its limitations as well. These disadvantages may include retarded setting and elongated retention of mold due to the weak strength of early-age. Nevertheless, much research is currently under way to improve the aforementioned issues. To improve activity of blast furnace slag powder, alkaline irritants has been used. In this study, we analyze effect on activity fineness and rate of substitution of Alkali Activator toward activity.
In this study, study about fly ash and blast-furnace slag used as substitutive materials for cement, and the influence on the neutralization of high flow concrete durability with these substitutive materials was performed and analyzed. The results are as follows 1) Aggregate segregation was partially improved with the progress of the admixture input at the mix proportion above slump flow 65 cm 2) Compressive strength with the progress of the increasement of fly ash input was decreased in early age, but decrease range was improved in long term age. Also, in case of blast-furnace, similar or improved compressive strength was appeared. 3) The neutralization depth with fly ash input was noticeably increased. But blast-furnace slag was effective to prevent. 4) In this experiment, high powder content was advantageously affected on preventive effect of the neutralization, and the relationship between the compressive strength and the neutralization depth was inversely proportional.
Purpose: The purpose of the study is to evaluate the clinical outcomes of acute achilles tendon rupture patients treated by early mobilization after operative repair. Materials and Methods: In this retrospective study, 12 patients of acute Achilles tendon rupture were surgically treated from May 2001 to November 2002, with follow-up period of at least 6 months. There were 10 men and 2 women, and mean age was 35.9 year. The repair method was single Krackow suture technique. Two to three weeks after the operation, early ROM with removable ankle-foot orthosis(AFO) was started. We used Amer-Lindholm scale for the clinical evaluation and analyzed patient's satisfaction and subjective strength deficit. Results: We had 11 excellent results(92%), and 1 good results(8%). One-leg heel raising was possible in all patients. All the patients returned to the preinjury occupations and 7 patients(58%) reached the preoperative level of sports activities. There was no significant difference in ankle ROM and ankle plantar flexion isokinetic strength compared to contralateral side. There was, no reruptures. Conclusion: Early mobilization proved to be a well tolerated, safe, and effective means for the compliant patient.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.