In this study, the shrinkage properties of concrete with the high-performance shrinkage admixture and the crack reinforcing materials applied to the high-flatness flooring of hypermarkets, outlets and warehouses was evaluated. The concrete with the popular shrinkage admixture is significantly reduced compared to the plain concrete without shrinkage admixture for the dry shrinkage deformation, and the difference of shrinkage ratio between the concretes has been shown to increase with increasing age.
In general, the shrinkage occurring in the floor mortar is large the influence by the dry shrinkage. In order to reduce the cracks occurring in the floor mortar, studies of physical methods are often performed, but these methods is difficult to prevent cracking of the floor mortar essentially. Therefore, in this study, the dry shrinkage properties of floor mortar of gypsum and red clay type using alpha-hemihydrate gypsum had been evaluated. The experimental variables were cement mortar(CM), gypsum mortar(GM), red-clay mortar(RM), the evaluation items was conducted experiment to evaluate the setting time, the compressive strength, drying shrinkage cracks, the dry shrinkage. As a result, it was confirmed that condensation time of GM is shorter that that of CM, and GM satisfied the compressive strength of the floor mortar standard. Also shrinkage deformation of GM reduced more than the CM.
Taking high geothermal tunnels as background, the deformation of concrete for shotcrete use was studied by simulating hot-humid and hot-dry environments in a laboratory. The research is made up by two parts, one is the influence of two kinds of high geothermal environments on the deformation of shotcrete, and the other is the shrinkage inhibited effect of fiber materials (steel fibers, polypropylene fibers, and the mixture of both) on the concrete in hot-dry environments. The research results show that: (1) in hot and humid environments, wet expansion and thermal expansion happened on concrete, but the deformation is smooth throughout the whole curing age. (2) In hot and dry environments, the concrete suffers from shrinkage. The deformation obeys linear relationship with the natural logarithm of curing age in the first 28 days, and it becomes stable after the $28^{th}$ day. (3) The shrinkage of concrete in a hot and dry environment can be inhibited by adding fiber materials especially steel fibers, and it also obeys linear relationship with the natural logarithm of curing age before it becomes stable. However, compared with no-fiber condition, it takes 14 days, half of 28 days, to make the shrinkage become stable, and the shrinkage ratio of concrete at 180-day age decreases by 63.2% as well. (4) According to submicroscopic and microscopic analysis, there is great bond strength at the interface between steel fiber and concrete. The fiber meshes are formed in concrete by disorderly distributed fibers, which not only can effectively restrain the shrinkage, but also prevent the micro and macro cracks from extending.
콘크리트의 크리프와 건조수축에 의한 장기변형의 일부가 구속되는 합성단면에 대해 콘크리트에 발생되는 잔류응력과 이로 인한 콘크리트 단면에 선압축력의 손실을 계산하기 위해 콘크리트 장기변형의 구속계수가 유도되었으며, 선압축력의 손실률을 계산하기 위한 식을 제안하였다. 제안된 구속계수는 재령수정 유효탄성계수가 적용된 환산단면특성으로부터 계산되며, 복잡한 형태의 합성단면에 대해서도 쉽게 적용될 수 있다. 기존 설계기준에서 콘크리트의 장기변형과 관련된 조항을 검토하기 위해서 도로설계편람의 일반 합성단면에 대해 이 구속계수와 선압축력의 손실 계산식이 적용되었다. 부정정력과 신축이음량의 계산에 적용되는 건조수축변형률 $150 ~ 200$\times$10^{-6}$ 은 장기변형의 구속정도가 적은 경우에 과소 계산될 수 있으며, 잔류응력의 계산에 는 적용되는 $180$\times$10^{-6}$ 은 비정상적으로 작은 값이다. 이 논문에서 적용된 PSC 합성단면에 대한 도로교 설계기준의 손실률 16.3%는 ACI 209에 대해서는 안전측으로 계산되었으나 Eurocode 2에 대해서는 안전을 보장할 수 없었다. 강합성 단면의 콘크리트 바닥판에 일반 보강철근의 긴장에 의해 선압축력이 도입되면 철근비의 증가로 긴장에 의한 경우보다 상당히 큰 손실이 발생되었으며, 강재거더의 구속에 의해 긴장된 보강재 선인장력의 손실은 감소한 반면에, 콘크리트 선압축력의 손실은 증가하였다.
본 연구에서는 바닥 모르타르에 발생하는 균열을 방지하기 위해, 팽창성이 있는 재료인 알파반수석고를 활용한 비소성결합재 기반 바닥 모르타르의 경화특성 및 건조수축 특성을 평가하고, 건설현장에 적용하여 외기환경에 노출된 조건에서 바닥 모르타르의 수축변형 거동 및 균열 발생여부를 검토하였다. 그 결과, 슬래그계 바닥 모르타르의 경우 시멘트계 모르타르에 비해 초결 및 종결시간이 급격히 단축되었고 압축강도는 관련기준을 만족하는 것으로 확인되었으며, 초기에 팽창 변형 이후의 수축변형 거동은 시멘트계 모르타르와 유사한 경향을 나타내었다. 슬래그계 바닥 모르타르의 현장 적용 결과 균열이 발생하지 않았으며, 외기환경 조건에 의한 변형률의 차이가 크지 않아 시멘트계 바닥 모르타르에 비해 치수안정성이 큰 것으로 판단된다.
지속적으로 증가하고 있는 이산화탄소 배출량을 저감시키기 위한 국제사회의 노력과 더불어 건설업계, 특히 시멘트 산업에서 알칼리 활성화제를 첨가한 알칼리 활성 슬래그를 활용하고자 하는 연구가 다수 수행되고 있다. 연구결과로 알칼리 활성 슬래그 모르타르의 고강도화 가능성이 밝혀지면서 초고층 구조물에 대한 적용가능성이 검토되고 있다. 그러나 초고층 구조물의 부재로 사용되기 위해서는 시간의 존 변형 거동에 관한 연구가 중요함에도 불구하고 굉장히 미흡한 실정이다. 따라서 본 연구에서는 OPC와 AAS를 이용한 콘크리트 시험체를 제작하여 크리프와 건조수축을 측정하고 도출된 결과값을 ACI 209R-92, CEB-FIP(1990)의 예측모델을 이용한 비선형 회귀분석을 통해 시간의존 변형 특성을 분석하였다. 각각의 열분석 및 SEM촬영을 통해 변형 발생 메카니즘을 규명하고자 하였다.
Two dinnerware porcelain bodies involving partial replacement of feldspar and kaoline by about 35wt% domestic GYUNGJU-pottery stone were developed and their properties such as shrinkage, porosity, firing range, linear thermal expansion, pyroplastic deformation, degree of whiteness and mechanical strength were compared with those of a traditional clay-flint-feldspar body. The experimental results showed that one of the clay-flint-feldspar-pottery stone body with 1% ZnO addition had the firing range of 115$0^{\circ}C$~121$0^{\circ}C$, whereas the traditional body had the firing range of 12$25^{\circ}C$~129$0^{\circ}C$. The linear drying shrinkage and linear dry-to-fired shrinkage of all bodies were 2.5~4.5% and 15~18%, respectively. And the major crystalline phases of sintered bodies were $\alpha$-quartz and secondary mullite surrounded by glassy phases. The modulus of rutpture of sintered bodies was ranged from 860 to 870kg/$\textrm{cm}^2$, and the microhardness of sintered bodies was 680 kg/$\textrm{cm}^2$.
In this study, creep deformation characteristics of high strength concrete under dry curing conditions were investigated. It was confirmed that the creep coefficient decreases as the compressive strength of concrete increases. In addition, a modified proposal for calculating the ultimate creep factor of the ACI 209 model can be derived using the measured values.
Long-term behavior of reinforced clayey soil by model tests were performed to investigate the effect of reinforcement during loads and under static loads. In order to determine proper contents by weight of monofilament polypropylene fiber and calcium carbonate, the drying shrinkage and compressive strength tests had been conducted before model tests. Model tests were run on a clayey soil mixed with or without reinforcement and test specimen in test apparatus was placed in air dry for 7days before load application. In the case of fiber reinforced soil, the horizontal strain was lower than others during loads because the presence of fibers increased the soil's resistance to deformation. All of reinforced clayey soil, horizontal strain decreased as the water content decrease under static loads.
순환잔골재의 고부가가치 활용촉진 및 이를 사용한 콘크리트구조물의 건조수축에 대한 내구성을 확보하기 위한 배합설계자료로 제시하고자 천연잔골재에 대한 고품질 순환잔골재의 대체율별 굳지 않은 콘크리트 성상 및 경화성상 그리고 건조수축특성등을 실험 실증적으로 검증하였다. 그 결과 고품질 순환잔골재를 사용한 콘크리트의 슬럼프, 공기량, 압축강도 및 인장강도는 대체율에 관계없이 유사한 수준을 보였으나, 구속 및 비구속상태에서의 건조수축특성은 큰 차이를 요였다. 구속 및 비구속상태에서 건조수축에 의한 변형량은 고품질 순환잔골재 대제율 30%까지는 천연잔골재만을 사용한 경우에 비해 오히려 건조수축에 대한 저항성이 우수한 것으로 나타났으며, 구조체 콘크리트용 잔골재로 고품질 순환잔골재를 30%까지 대체 사용하는 것이 유효하다는 것을 검증할 수 있었다. 반면, 고품질 순환잔골재 대체율이 50% 이상인 경우에는 천연잔골재만을 사용한 경우에 비해 구속 및 비구상태에서의 건조수축 저항성이 저하되는 것으로 나타났으며, 특히 고품질 순환잔골재 대체율 100%의 경우에는 건조수축에 의한 변형량이 다른 시험체에 비해 급격히 증가되어 구속상태에서 건조수축에 의한 균열발생 시점이 단축되는 것을 확인할 수 있었다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.