F.R.P specimens were made by mixture CM(chopped mat) 450-104 matrix & RC(roving clothes)570-100 Roving, the mixture ratio Resin: hardener (92:8) for tensile test. It was also made of plates by hand lay-up method and was been cured for 24 hours and then was cut tensile specimens in accordance with ASTM D638 Type 3. Knowing exact behavior of bonded area's stress and strain when the tensile test was going on, the test specimens were made of 2 plies laminae of F.R.P in each for supporting cut part in middle of specimen length. And in middle part also were covered of F.R.P plies of 1/2, 2/3 length of specimen in each as well. Also we consider shear stress in adhered area. This study reveals that as plys length is more longer, rupture stress grows remarkably larger.
Composite-to-aluminum joins were tested to get failure loads and modes for three types of joins; adhesive bonding, bolt fastening, and adhesive-bolt hybrid joining. Film type adhesive FM73 and paste type adhesive Cytec EA9394S were used for aluminum and composite bonding to make a double-lap joint. A digital microscope camcorder was used to monitor the failure initiation and propagation. It was found that the hybrid joining is an effective method to strengthen the joint when the mechanical fastening is stronger than the bonding as in the case of using the paste type adhesive. On the contrary, when the strength of the bolted joint is lower than the strength of the bonded joint as in the joint with the film type adhesive, the bolt joining contribute little to the hybrid joint strength.
The co-cured joint has been widely used in joining process of composite structures due to its simple and easy manufacturing process. In this paper, the effect of stacking sequence of the carbon epoxy prepreg, bonding length and thickness of the aluminum plate on the static tensile load capability of the co-cured aluminum-composite double lap joint were experimentally investigated. From experimental results, the optimum EA ratios with respect to stacking sequence and bonding length of the co-cured joint were obtained, which may be useful for the joining of hybrid structures.
Adhesive-bonded joints are widely used in the industry. Recently, applications of adhesive bonding joints have been increased extensively in automobile and aircraft industry. The strength of adhesive joints is influenced by the surface roughness, adhesive shape, stress distribution, and etc. However, the magnitude of the influence has not yet been clarified because of the complexity of the phenomena. In this study, as the fundamental research of adhesive bonding joints, the effects of adhesive shape and loading speed on bonding strength properties and durability of aluminum to polycarbonate single-lap joints were studied. To evaluate the effect of adhesive shape, several modified shapes were used, and loading speeds were varied from 0.05 to 5 mm/min. As a result, the load-displacement distribution was shown a brittle fracture tendency. The trigonal edged single lap and bevelled lap joints showed the higher strength than the plain single lap, trigonal single lap, joggle lap and double lap joints in same adhesive area. The fractures of trigonal single lap and trigonal edged single lap joints that had the higher strength level were shown as the mixture type of the cohesive and interfacial-failure, mostly joggle lap joints that had the lower strength level were shown as the adhesive-failure.
복합재료 적층판 기계적 체결부 표준시험(ASTM D5961) 결과에 대하여 이론적 강도 계산 및 유한요소 해석결과를 비교한다. 응력집중계수를 산출하기 위하여 ASM Handbook의 금속 및 복합재료에 대한 산출식을 이용하여 실험 결과값과 비교한다. 형상학적 인자들과 체결방식(단일/이중 겹칩)에 따른 체결강도의 차이도 비교한다. 유한요소 해석에 있어, 복합재료 적층판의 기계적 체결부의 효율적인 유한요소 모델을 찾기 위해 몇 가지 유한요소 모델들과 실험 결과들을 비교한다.
구조물 설계에 복합재료-금속 접착제 결합 조인트의 개발 및 사용을 제한하는 가장 큰 요인은 접착 조인트의 하중지지 능력 예측을 위한 접착 계면의 강도 평가 방법의 부재이다. 본 연구에서는 복합재료-탄소강의 접착 강도를 계면 모서리에서의 응력강도계수와 파괴 인성 값으로 평가하였다. 구체적으로 동시 경화 성형법으로 제작된 복합재료-탄소강 양면 겹치기 접착조인트의 하중지지 능력을 파괴 역학적 분석 방법을 통하여 결정하였다. 이종재료 계면 모서리 첨단의 응력 특이성과 그 지수를 제시하고 최종적으로 응력강도계수와 실험을 통한 계면의 파괴인성 값을 획득하였다. 서로 다른 접합 길이를 갖는 조인트의 하중지지 능력 비교를 통하여 양면 겹치기 접착 조인트의 파괴 인성치와 혼합 모드에서의 균열 진전 기준을 $K_1-K_{11}$ 평면 내에 도시하였다.
소경각재를 이용한 소경각재 적층목을 기둥-보 목조건축 구조재로 이용하기 위해선 장대재 제작이 가능하여야 한다. 본 연구에서는 낙엽송 소경각재의 종접합 성능평가를 실시하였다. 시험편들은 종접합 방법에 따라 6가지 형상으로 제작하였으며 인장 및 휨 강도시험으로 종접합성능을 검토하였다. 종접합 접합부의 인장시험에서 Lap 시험편의 인장강도는 Double Lap 시험편보다 양호하였으며, Scarf 시험편의 인장강도는 Hooked scarf 시험편보다 양호하였다. Rod 시험편의 인장강도는 3.6 MPa로 가장 양호하였다. 종접합 접합부의 휨 시험결과 봉형 GFRP를 삽입 접착한 시험편들은 평균 29 MPa의 휨 파괴계수가 측정되었으며, 타 접합부 시험편들은 11 MPa 이하의 휨 파괴계수 값이 관찰되었다. 봉형 GFRP (Glass Fiber Reinforced Plastic)를 삽입 접착한 시험편들은 인성파괴가 관찰되었고 나머지 시험편들은 취성파괴가 발생하였다. Rod + Lap 시험편의 평균 휨 파괴계수가 30.5 MPa로 종접합한 시험편 중 가장 양호한 성능을 발휘하였다. Rod + Lap 시험편의 휨 강도는 종접합하지 않은 대조군 시험편 휨 파괴계수의 66%에 해당되었다. 낙엽송 소경각재 종접합 방법으로 봉형 GFRP 삽입 접착이 가장 유효한 강도를 나타내는 것을 확인하였다.
We jointed Bi(Pb)-Sr-Ca-Cu-O multifilament tapes and evaluated their electrical and mechanical properties. In order to improve connectivity of multifilaments, one or two single-filament tape was inserted between two multifilament tapes. The critical current ratio(CCR) and n-value of the jointed tapes were evaluated as a function of uniaxial pressure. It was observed that critical current ratio and n-value were 24.8-29.0% and 2.5-2.8 for MM lap-jointed tape. On the other hand, the corresponding values were improved to 24.7-53.9% and 3.1-4.2 for MSM jointed tape, and 63.4-76.0% and 3.4-5.1 for double MS:vr lap-jointed tape, respectively. The highest electrical properties of double MSM lap-jointed tape are considered to be owing to the presence of single core, causing better interconnections of multifilaments between the two tapes. The mechanical property of jointed tape was evaluated and correlated to the microstructural evolution. The strength of jointed tapes was 44-64% less than that of the unjoined tape. The strain tolerance of jointed tape was also reduced compared to that of the unjoined tape. These lower mechanical properties of jointed tape are probably due to the induced nonuniform microstructure such as the existence of cracks and Ag-intrusion in the joined region.
한국초전도학회 1999년도 High Temperature Superconductivity Vol.IX
/
pp.373-377
/
1999
HTS magnet operated at 20${\sim}$40 K was fabricated using three pieces of 100 m Bi-2223 high temperature superconductors fabricated by powder-in-tube process. It was composed of 6 double pancakes with 75 ID. and 113 OD. connected by lab splice. Coil I$_c$ of each DP.(double pancake) obtained for a 140 turn, fabricated using react and wind procedure was 6${\sim}$8 A at 77 K, self field. The maximum field was measured 0.06 T at lop = 5 A, 77 K. The joint resistance due to lap splice of HTS tapes affect badly to operate HTS magnet with persistent current mode, total effective magnet resistance included lap splice was 55 ${\mu}$${\omega}$ at 77 K.
The strength of aluminum 7075 and carbon composite hybrid joints was studied for adhesive, bolt, and the adhesive-bolt combined joints. Several hybrid joint specimens were tested to get the failure load and modes for three types of the joints. Adhesive Cytec EA9394S was used for aluminum and carbon bonding. Failure load of the adhesive-bolt combined joint was 94 % of the sum of the failure load of the separately bonded and bolted joints. Hybrid joint also showed more stable failure behavior than the simple adhesive or bolted joint.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.