Kim, Kwang-Mo;Shim, Sang-Ro;Shim, Kug-Bo;Park, Joo-Saeng;Kim, Wun-Sub;Kim, Byoung-Nam;Yeo, Hwanmyeong
Journal of the Korean Wood Science and Technology
/
v.37
no.3
/
pp.184-191
/
2009
In the southern part of the Korean Peninsula including Jeju-island, the production amount of domestic cedar has increased gradually. However, their low qualities, expected to be caused by the low density and frequent knots, have restricted their practical utilization as the high value-added products. In this study, it is aimed to look for the new uses of domestic cedar and to examine the applicability for lamination lumbers of structural glued laminated timber (glulam). Above all, machine stress ratings for individual sawn lumbers confirmed that modulus of elasticity (MOE) of cedar lumber was lower than that of other common softwood species in Korea. On the other hand, cedar lumbers have enough stiffness to manufacture the structural glulam in accordance with Korean Industrial Standard (KS). The bonding strength and durability also met the KS limitation. Nevertheless, from the result of bending tests for cedar glulam, it was shown that the modulus of elasticity (MOE) did not meet the KS limitation. Therefore, it was concluded that additional researches were needed for reinforcing the stiffness of cedar glulam.
The goal of this study was to find the optimum lamina size from red pine (Pinus densiflora) and Japanese cedar (Cryptomeria japonica) logs for the cross laminated timber (CLT) production. From visual inspection of the logs from two species, red pine log showed a larger knot and warp compared to the Japanese cedar. Different cross-sectional sizes of lamina ($110mm{\times}30mm$, $110mm{\times}40mm$, $110mm{\times}50mm$, $50mm{\times}30mm$, $30mm{\times}30mm$) from two species were analyzed for yield and grade. Regardless of the species, the optimized cross sectional size for maximizing the yield was $110mm{\times}30mm$. In grading for the different size laminas from Japanese cedar and red pine, a higher percentage of the first and second grade was found from the $110mm{\times}30mm$ lamina cut.
Kim, Kwang-Mo;Park, Jung-Hwan;Park, Byoung-Soo;Son, Dong-Won;Park, Joo-Saeng;Kim, Wun-Sub;Kim, Byoung-Nam;Shim, Sang-Ro
Journal of the Korean Wood Science and Technology
/
v.37
no.4
/
pp.330-339
/
2009
The material properties of Cedar (Cryptomeria japonica) were evaluated according to heat treatment conditions. The special focus was made on the color control of cedar wood by heat treatment. The difference of color between sapwood and heartwood could be reduced by heat treatment at a temperature above $170^{\circ}C$. Long heating time was more effective in reducing the difference. The Equilibrium Moisture Content (EMC) of heat-treated wood was as low as 50 percent. The result obviously indicates that heat-treated wood is more dimensionally stable in the change of moisture condition than the control. The heat-treated wood was also effective in increasing the durability against wood rotting fungi. However, more study is required to develop heat treatment as an environmentally-friendly technology for wood preservation without chemical. The mechanical properties of heat-treated wood showed relatively higher performance than the control in general. Meanwhile the dramatic decrease in impact bending stress due to the loss of ductility may limit uses of heat-treated wood in certain cases. There were no significant changes in microscopic structure which may cause changes in mechanical properties. Further study on the chemical analysis of heat-treated wood is needed to scrutinize the causes of changes of material properties.
Research on the rapid and accurate prediction of physical properties of wood using near-infrared (NIR) spectroscopy has attracted recent attention. In this study, partial least squares analysis was performed between NIR spectra and air-dried specific gravity of five domestic conifer species including larch (Larix kaempferi), Korean pine (Pinus koraiensis), red pine (Pinus densiflora), cedar (Cryptomeria japonica), and cypress (Chamaecyparis obtusa). Fifty different lumbers per species were purchased from the five National Forestry Cooperative Federations of Korea. The air-dried specific gravity of 100 knot- and defect-free specimens of each species was determined by NIR spectroscopy in the range of 680-2500 nm. Spectral data preprocessing including standard normal variate, detrend and forward first derivative (gap size = 8, smoothing = 8) were applied to all the NIR spectra of the specimens. Partial least squares analysis including cross-validation (five groups) was performed with the air-dried specific gravity and NIR spectra. When the performance of the regression model was expressed as $R^2$ (coefficient of determination) and root mean square error of calibration (RMSEC), $R^2$ and RMSEC were 0.63 and 0.027 for larch, 0.68 and 0.033 for Korean pine, 0.62 and 0.033 for red pine, 0.76 and 0.022 for cedar, and 0.79 and 0.027 for cypress, respectively. For the calibration model, which contained all species in this study, the $R^2$ was 0.75 and the RMSEC was 0.37.
Kim, Kwang-Mo;Park, Jung-Hwan;Park, Byoung-Soo;Son, Dong-Won;Park, Joo-Saeng;Kim, Wun-Sub;Kim, Byoung-Nam;Shim, Sang-Ro
Journal of the Korean Wood Science and Technology
/
v.38
no.1
/
pp.17-26
/
2010
Recently, yellow poplar (Liriodendron tulipifera L.) is getting attention in Korea due to the fast growing and high yield and quality of lumber. But, it is thought that the color difference between heartwood and sapwood may restrict the practical use of it. This study was aimed to enhance the value of yellow poplar lumber by the color control using high temperature heat-treatment, which had been tried for domestic cedar (Kim et al., 2009). The material properties including surface color of yellow poplar lumber were evaluated according to heat treatment conditions. The difference of color between sapwood and heartwood could be reduced by heat treatment at a temperature about $200^{\circ}C$. Long heating time was more effective in reducing the difference. The Equilibrium Moisture Content (EMC) of heat-treated wood was as low as 50 percent of the control. The result obviously indicates that heat-treated wood is more dimensionally stable in the change of moisture condition. The durability against wood rotting fungi also increased by the heat-treated, but it was not so effective as the case of cedar. The changes of mechanical properties of heat-treated yellow poplar were very similar to that of heat-treated cedar. In order to develop new use of heat-treated yellow poplar, the changes of mechanical properties should be considered. There were no significant changes in microscopic structure which may cause changes in mechanical properties. Further study of heat-treated wood is needed to scrutinize the causes of changes of material properties.
To evaluate the natural decay durability of valuable domestic softwoods which are used for preservative treatment in our country, we carried out decay test by European standard method. Of all test wood species, Japanese larch (Larix leptolepis) showed slightly high natural decay durability compared to other 4 wood species, Japanese red pine (Pinus densiflora), pitch pine (Pinus rigida), Japanese cedar (Cryptomeria japonica), and scots pine (Pinus sylvestris). However, all of evaluated domestic softwood species in this study caused high weight losses over about 30% in heartwood by test fungus, Poria placenta. We can hardly expect a good natural decay durability from these softwood species. According to the classification of the natural durability of European standard (EN 350-1), they are classified into "Not durable" or "Slightly durable". Therefore, if using these softwoods as exterior materials, we must do preservative treatment to ensure durability.
Park, Se-Yeong;Kim, Jong-Chan;Kim, Jong-Hwa;Yang, Sang-Yun;Kwon, Ohkyung;Yeo, Hwanmyeong;Cho, Kyu-Chae;Choi, In-Gyu
Journal of the Korean Wood Science and Technology
/
v.45
no.2
/
pp.202-212
/
2017
This study was to establish the interrelation between chemical compositions and near infrared (NIR) spectra for the classification on distinguishability of domestic gymnosperms. Traditional wet chemistry methods and infrared spectral analyses were performed. In chemical compositions of five softwood species including larch (Larix kaempferi), red pine (Pinus densiflora), Korean pine (Pinus koraiensis), cypress (Chamaecyparis obtusa), and cedar (Cryptomeria japonica), their extractives and lignin contents provided the major information for distinction between the wood species. However, depending on the production region and purchasing time of woods, chemical compositions were different even though in same species. Especially, red pine harvested from Naju showed the highest extractive content about 16.3%, whereas that from Donghae showed about 5.0%. These results were expected due to different environmental conditions such as sunshine amount, nutrients and moisture contents, and these phenomena were also observed in other species. As a result of the principal component analysis (PCA) using NIR between five species (total 19 samples), the samples were divided into three groups in the score plot based on principal component (PC) 1 and principal component (PC) 2; group 1) red pine and Korean pine, group 2) larch, and group 3) cypress and cedar. Based on the chemical composition results, it was concluded that extractive content was highly relevant to wood classification by NIR analysis.
This paper examines the classification of five coniferous species, including larch (Larix kaempferi), red pine (Pinus densiflora), Korean pine (Pinus koraiensis), cedar (Cryptomeria japonica), and cypress (Chamaecyparis obtusa), using near-infrared (NIR) spectra. Fifty lumber samples were collected for each species. After air-drying the lumber, the NIR spectra (wavelength = 780-2500 nm) were acquired on the wide face of the lumber samples. Soft independent modeling of class analogy (SIMCA) was performed to classify the five species using their NIR spectra. Three types of spectra (raw, standard normal variated, and Savitzky-Golay $2^{nd}$ derivative) were used to compare the classification reliability of the SIMCA models. The SIMCA model based on Savitzky-Golay $2^{nd}$ derivatives preprocessing was determined as the best classification model in this study. The accuracy, minimum precision, and minimum recall of the best model (PCA models using Savitzky-Golay $2^{nd}$ derivative preprocessed spectra) were evaluated as 73.00%, 98.54% (Korean pine), and 67.50% (Korean pine), respectively.
This study was carried out to investigate a radial distribution of moisture contents (MCs) within a log cross section (LC) during oven-drying of 3 mm-thick circumferential slices cut from several domestic softwoods LCs.For Korean red pine, drying rate of sapwood slices during oven-drying represented much higher values than that of heartwood slices, and so sapwood with higher green MC early reached below fiber saturation point (FSP) rather than heartwood did. However, this distribution of moistures did not last for long duration. For Japanese larch, green MC of sapwood was approximately three times higher than that of heartwood. This similar distribution in MC was lasted until about 20% average MC. The MC was around uniform throughout the sapwood of Ginkgo when green and during oven-drying, although it was somewhat fluctuated. For Japanese cedar, the heartwood with so low moistures around FSP would begin to shrink from the beginning stage of drying, but the sapwood above hygroscopic MC prevents the heartwood from shrinking, and consequently, the heartwood or the transition wood goes into tension stress. The results for Japanese cypress showed that the green MCs of the sapwoods were much lower than those for heartwoods, and then this trend was continued until about 20% in average MC. For Chinese thuja, the green MCs of sapwoods were about 2 times as high as those of heartwood, but this along the radial gradient in MC rapidly became gentle during oven-drying.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.