Journal of the Microelectronics and Packaging Society
/
v.22
no.2
/
pp.33-39
/
2015
$BaTiO_3$ is typical ferromagnetic materials with dielectric constant of above 200. $BaTiO_3$ nanoparticles applications are available for multiple purposes such as nanocapacitors, ferroelectric random access memories, and so on. Applications are is diverse from the dispersion of nanoparticles depending on the route of synthesis. In this study, $BaTiO_3$ nanoparticles were synthesized by two different methods such as oxalate method and sol-gel process (ambient condition sol method). Particle size and dispersion condition were studied according to the preparation method and capping agent. Poly vinyl pyrrolidone (PVP) was used as a capping agent in oxalate method and tetrabutylammonium hydroxide (TBAH) used as a capping agent in sol-gel process each. Cubic crystal structure of $BaTiO_3$ phase could be confirmed by X-ray diffraction analysis. Fourier transform-infrared spectroscopy was employed for the confirmation of the capping agent and $BaTiO_3$ nanoparticles. The particle size and distribution analysis was also performed by particles size analyzer and scanning electron microscope.
As electromagnetic waves are affected by electrical conductivity or permittivity, they are widely used to evaluate geotechnical characteristics. In this study, a probe for measuring electromagnetic waves using a time domain reflectometry is manufactured to evaluate heavy metal concentration in saline water. In the experiments, a copper is used as a heavy metal, and a probe is demonstrated with the concentration of copper. Solutions were set for 8 different copper concentration (0, 0.01, 0.05, 0.1, 0.5, 1, 5, 10 mg/L) in saline water with 3% salinity. The probe is coated by electrical insulating materials such as epoxy, top-coat, varnish, acrylic paint, heat-shrinkage tube to measure electromagnetic waves in saline water. The measured signals are compared according to coating material. As results, for probes coated with acrylic paint and heat-shrinkage tube, signal variation is not detected. For epoxy, top-coat, and varnish coated probes, the voltage decreases with an increase of copper concentration. Probes coated by epoxy at once and top coat can estimate under 5 mg/L of copper concentration and the probe coated by epoxy twice can estimate over 5 mg/L of copper concentration. This study shows that the probe using the time domain reflectometry can be used to evaluate the concentration of heavy metal in saline water by coating the probe with insulating material.
Journal of the Korea Institute of Information and Communication Engineering
/
v.21
no.4
/
pp.679-687
/
2017
In this paper, a microstrip-fed triple-band monopole antenna with DGS (Defected Ground Structure) for WLAN/WiMAX applications was proposed. The proposed antenna is based on a microstrip-fed structure, and composed of two strip lines and DGS structure and then designed in order to get triple band characteristics. We carried out simulation about parameters. Adjusted the position and length of the two strips and three slits, we get the optimized parameters. The proposed antenna is fabricated on an FR-4 substrate of which the dielectric constant is 4.4, and its overall size is $34mm(W_1){\times}34mm(L_1){\times}1.6mm(t)$, and its proposed antenna size is $17.0mm(W_6){\times}30.75mm(L_3+L_4+L_9)$. From the fabricated and measured results, return loss of the proposed antenna satisfied return loss -10dB bandwidth 360 MHz (2.335~2.695 GHz), 645 MHz (3.37~4.015 GHz) and 1,770 MHz (5.14~6.91 GHz). And measured results of gain and radiation patterns characteristics displayed for operating bands.
Pb(Ni$\_$1/3/Nb$\_$2/3/)O$_3$-PbZrO$_3$-PbTiO$_3$ thick films were screen-printed on platinized alumina substrates and fired at 800-1000$^{\circ}C$. Two kinds of powders with different particle size were prepared by attrition and ball milling methods. Effects of particle size of starting material on the microstructure and electrical properties of the thick films were investigated. Average particle size of attrition milled-powder (0.44 ${\mu}$m) was much smaller than that of ball milled-powder (2.87 ${\mu}$m). Average grain size of the thick film prepared from attrition-milled powder was smaller than that of the thick film prepared from ball-milled powder at the sintering temperature of 800$^{\circ}C$. However, the difference in average particle size became smaller with increasing the sintering temperature. Thick films prepared from attrition-milled powders showed more uniform and denser microstructures at all firing temperatures. Thick films prepared from attrition-milled powders had better electrical properties at the firing temperature above 900$^{\circ}C$ than thick films prepared from ball-milled powders. Dielectric constant, remanent polarization and coercive field of the thick film prepared from attrition-milled powders and fired at 900$^{\circ}C$ were 559, 16.3 ${\mu}$C/cm$^2$, and 51.3 kV/cm, respectively.
Journal of the Institute of Electronics Engineers of Korea SD
/
v.40
no.9
/
pp.631-637
/
2003
We have evaluated structural and electric, ferroelectric properties of PZT(30/70) thick film prepared by using 1,3-propanediol based sol-gel method on Pt/Ti/SiO$_2$/Si substrates. Rapid thermal annealing (RTA) is used to reduce the thermal stress and final furnace annealing is processed at $650^{\circ}C$. As the results of SEM analysis, we find that we get 350 nm in thickness for one coating and 1 $\mu$m for three times of coating. In the results of C-D analysis at 1 kHz, dielectric constant ($\varepsilon$$_{r}$) and dissipation factor were 886 and 0.03, respectively. C-V curve is shaped as a symmetrical butterfly. Leakage current density at 200 kV/cm is 1.23${\times}$10$^{-5}$ A/cm$^2$ and in the results of hysteresis loops measured at 150 kV/cm, the remnant polarization (P$_{r}$) and the coercive field (E$_{c}$) are 33.8 $\mu$C/cm$^2$ and 56.9 kV/cm, respectively. PZT(30/70) thick film exhibits relatively good ferroelectric, electric properties.s..
Journal of the Institute of Electronics Engineers of Korea SD
/
v.41
no.6
/
pp.9-15
/
2004
PZT(30/70) thick film was fabricated by using 1,3 propanediol-based sol-gel method. Prepared film of pyroelectric property was investigated by Dynamic method of modulation frequency dependence. Pyroelectric coefficient was obtained about $5.0{\times}10^{-8}\;C/cm^2{\cdot}K$. The figure of merits for voltage responsively and specific detectivity were $3.4{\times}10^{-11}\;C{\cdot}cm/J$ and $5.9{\times}10^{-9}\;C{\cdot}cm/J$, respectively, because of relative high-dielectric constant and high-pyroelectric coefficient. Voltage responsively was increased at low modulation frequency and it was decreased at high modulation frequency. Voltage responsively was maximum 1.84 V/W at 10Hz. As Johnson noise is dominant, Noise voltage was increased nearly proportional to $f^{-1/2}$. Noise equivalent power and specific detectivity were $2.83{\times}10^{-7}\;W/Hz^{1/2}$ and 3.13{\times}10^5\;cm{\cdot}Hz^{1/2}/W$ the same frequency at 80Hz, respectively.
The Journal of Korean Institute of Electromagnetic Engineering and Science
/
v.23
no.6
/
pp.723-730
/
2012
The radar cross section(RCS) of a trihedral corner reflector(TCR) should be accurately computed when it is used as an external calibration target for a satellite synthetic aperture radar(SAR) calibration campaign. This paper presents the RCS analysis on a trihedral corner reflector which is installed on a calibration site, using the wave reflection from the rough surface and the wave diffraction from the TCR edges. The results in this paper show quantitatively the effect of the front surface on the RCS of a TCR. The difference of the RCS between a TCR in air and a TCR on a ground surface is computed by including the interaction term which consists of the edge diffraction from the TCR edges and the surface reflection from the front rough surface. The reflection coefficient of a randomly rough surface is a function of the surface roughness and dielectric constant of the surface. The RCS of $10{\lambda}$ size TCR on a ground is 0.46 dB higher than TCR in air at 9.65 GHz, and this can reach at maximum 1.55 dB depending on a surface condition and TCR size. The effect of the front surface on the RCS of a TCR increases, as the surface roughness decreases, the soil moisture increases, and the size of TCR in wavelength decreases.
p-Phenylenediamine dihydroperchlorate, $C_6H_4N_2H_4{\cdot}2HC1O_4$, crystallizes in space group $P\={1}$ with $a=4.79{\pm}0.02,\;b=9.03{\pm}0.02,\;c=7.12{\pm}0.03{\AA},\;{\alpha}=109.4{\pm}0.2,\;{\beta}=79.6{\pm}0.2,\;r=104.6{\pm}0.2^{\circ},\;Z=1$. The structure has been solved by the Patterson and Fourier methods. The refinement by block-diagonal least-squares cycles gives R = 0.13 for 387 observed reflexions collected on equi-inclination Weissenberg photographs with CuK${\alpha}$ radiation. There are two different types of five hydrogen bonds. The first type consists of one trifurcated N${\cdot}{\cdot}{\cdot}$O hydrogen bond and the second of two normal N${\cdot}{\cdot}{\cdot}$O hydrogen bonds, both of which exist between the amino group and the perchlorate, groups. A p-phenylenediamine group is approximately planar within an experimental error and bonded to twelve perchlorates: ten perchlorates forming hydrogen bonds and two being contacted with the van der Waals forces. A perchlorate group is surrounded by six p-phenylenediamines and four perchlorates; among the six p-phenylenediamines, five of them are hydrogen-bonded, and the rest contacted with the van der Waals force.ce anaysis of our samples and investigated the variarions in the values of parameters obtained through fitting the theoretical impedance to the experimental impedance. The characters of the dielectric constant and the impedance showed abnormal variations for the 0.2 at K-doped NSBN ceramics, which we were able to interpret in terms of the variations in the number A-site vacancies with the K doping ratio. From these results, A-site vacancies are thought to be space charges that influence the ferroelectric properties of NSBN ceramics.
Journal of the Microelectronics and Packaging Society
/
v.15
no.1
/
pp.19-25
/
2008
In this paper, the front end module (FEM) was proposed for 2.4GHz WLAN band by LTCC multilayer application. The FEM was composed of power amplifier IC, switch IC, and LTCC module. LTCC module consists of output matching circuit and lowpass filter as Tx part, bandpass filter as Rx part. Design of output matching circuit for LTCC was used matching parameter from output matching circuit based on lumped circuit on the PCB board. The dielectric constant of LTCC substrate is 9. The substrate was composed of total 26 layers with each 30um thickness. Ag paste was used for the internal pattern as the conductor material. The size of the module is $4.5mm{\times}3.2mm{\times}1.4mm$. The fabricated FEM showed the gain of 21dB, ACPR of less than -31dBc first side lobe and Less than -59dBc second side lobe and the output power of 23Bm at P1dB.
Proceedings of the Korean Vacuum Society Conference
/
1999.07a
/
pp.58-58
/
1999
The diamond films which can be applied to SOD (silicon-on-diamond) structure were deposited on Si(100) substrate using CO/H2 CH4/H2 source gases by microwave plasma chemical vapor deposition(MPCVD), and SOD structure have been fabricated by poly-silicon film deposited on the diamond/Si(100) structure y low pressure chemical vapor deposition(LPCVD). The phase of the diamond film, surface morpholog, and diamond/Si(100) interface were confirmed by X-ray diffraction(XRD), scanning electron microscopy(SEM), atomic force microscopy(AFM), and Raman spectroscopy. The dielectric constant, leakage current and resistivity as a function of temperature in films are investigated by C-V and I-V characteristics and four-point probe method. The high quality diamond films without amorphous carbon and non-diamond elements were formed on a Si(100), which could be obtained by CO/H2 and CH4/H2 concentration ratio of 15.3% and 1.5%, respectively. The (111) plane of diamond films was preferentially grown on the Si(100) substrate. The grain size of the films deposited by CO/H2 are gradually increased from 26nm to 36 nm as deposition times increased. The well developed cubo-octahedron 100 structure nd triangle shape 111 are mixed together and make smooth and even film surface. The surface roughness of the diamond films deposited by under the condition of CO/H2 and CH4/H2 concentration ratio of 15.3% and 1.5% were 1.86nm and 3.7 nm, respectively, and the diamond/Si(100) interface was uniform resistivity of the films deposited by CO/H2 concentration ratio of 15.3% are obtained 5.3, 1$\times$10-9 A/cm, 1 MV/cm2, and 7.2$\times$106 $\Omega$cm, respectively. In the case of the films deposited by CH4/H2 resistivity are 5.8, 1$\times$10-9 A/cm, 1 MV/cm, and 8.5$\times$106 $\Omega$cm, respectively. In this study, it is known that the diamond films deposited by using CO/H2 gas mixture as a carbon source are better thane these of CH4/H2 one.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.