• Title/Summary/Keyword: cure step

Search Result 59, Processing Time 0.019 seconds

A multi Step Cure Process to Prevent Residual Bubbles in LED Encapsulation Silicone Resin (LED Encapsulation 실리콘의 기포잔류방지를 위한 Step 경화공정 연구)

  • Song, M.J.;Kim, H.K.;Yoon, G.S.;Kim, K.H.
    • Transactions of Materials Processing
    • /
    • v.21 no.2
    • /
    • pp.101-106
    • /
    • 2012
  • Generally, rapid cure reaction of LED encapsulation silicone resin causes serious defects in cured resin products such as warpage, residual bubbles, and reduced wettablility. In order to prevent residual bubbles in silicone resin, the step cure process was examined in the present paper. Three kinds of step cure processes were applied, and bubble-free phenomenon was observed. Most of the bubbles were removed under $70^{\circ}C$, the minimum temperature for activating cure reaction. In addition, degree of cure(DOC) and temperature distribution were predicted by using FEM analysis of heat transfer. It was concluded that maintaining cure temperature which provide a DOC under 0.5~0.6 effectively reduces residual bubbles.

Cure and Heat Transfer Analysis in LED Silicone Lens using a Dynamic Cure Kinetics Method (승온 반응속도식을 이용한 LED용 실리콘 렌즈의 경화 및 열전달해석)

  • Song, M.J.;Kim, K.H.;Hong, S.K.;Park, J.Y.;Lee, J.W.;Yoon, G. S.
    • Transactions of Materials Processing
    • /
    • v.24 no.2
    • /
    • pp.101-106
    • /
    • 2015
  • Recently, silicone is being used for LED chip lens due to its good thermal stability and optical transmittance. In order to predict residual stresses, which cause optical birefringence and mechanical warpage of silicone, a finite element analysis was conducted for the curing of silicone during molding. For the analysis of the curing process, a dynamic cure kinetics model was derived based on the results of a differential scanning calorimetry (DSC) testing and applied to the material properties for finite element analysis. Finite element simulation results showed that a step cure cycle reduced abrupt reaction heat and showed a decrease in the residual stresses.

The Study of Curing Day Reduction by Step Curing of HTPB/AP Propellant (HTPB/AP계열의 고체 추진제의 Step 경화 방법을 통한 경화일(기간) 단축)

  • Kim, Kahee;Park, Jung-Ho;Choi, Sunghan
    • Journal of the Korean Society of Propulsion Engineers
    • /
    • v.24 no.6
    • /
    • pp.101-107
    • /
    • 2020
  • In this paper, step-curing, which includes the change of curing temperature on the curing process, was applied to reduce curing day of HTPB/AP based propellant. This study targets the improvement of productivity of HTPB/AP based solid rocket motor. Comparison of mechanical properties of propellant resulted in the change of normal curing condition (60℃, 5 days) to step-curing condition (60℃, 1 day / 65℃, 3 days). Post-cure test was conducted to determine the impact on the shelf life of the solid rocket motor. The aging characteristics of propellants were analyzed by measuring mechanical properties and thermal expansion factor. To step-cured propellant, accelerated aging test was performed for 12 weeks, followed by tensile test. Sm(bar) and Em(%) were higher than 8 bar and 40% each, showing excellent mechanical properties.

Effect of Die Attach Film Composition for 1 Step Cure Characteristics and Thermomechanical Properties (다이접착필름의 조성물이 1단계 경화특성과 열기계적 물성에 미치는 영향에 관한 연구)

  • Sung, Choonghyun
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.21 no.12
    • /
    • pp.261-267
    • /
    • 2020
  • The demand for faster, lighter, and thinner portable electronic devices has brought about a change in semiconductor packaging technology. In response, a stacked chip-scale package(SCSP) is used widely in the assembly industry. One of the key materials for SCSP is a die-attach film (DAF). Excellent flowability is needed for DAF for successful die attachment without voids. For DAF with high flowability, two-step curing is often required to reduce a cure crack, but one-step curing is needed to reduce the processing time. In this study, DAF composition was categorized into three groups: cure (epoxy resins), soft (rubbers), hard (phenoxy resin, silica) component. The effect of the composition on a cure crack was examined when one-step curing was applied. The die-attach void and flowability were also assessed. The cure crack decreased as the amount of hard components decreased. Die-attach voids also decreased as the amount of hard components decreased. Moreover, the decrease in cure component became important when the amount of hard component was small. The flowability was evaluated using high-temperature storage modulus and bleed-out. A decrease in the amount of hard components was critical for the low storage modulus at 100℃. An increase in cure component and a decrease in hard component were important for the high bleed-out at 120℃(BL-120).

A Study on the Vulcanization System and Two-Step Foaming Properties for Natural Rubber Foam (천연고무의 가황시스템 및 성형공정에 따른 2단 발포 특성 연구)

  • Sunhee Lee;Ye-Eun Park;Dikshita Chowdhury
    • Textile Coloration and Finishing
    • /
    • v.35 no.4
    • /
    • pp.246-255
    • /
    • 2023
  • In this study, we investigated for natural rubber foam to replace petrochemical-based neoprene foam. Experiments were conducted on vulcanization system and 2-step foaming process of natural rubber. The vulcanization system were EV(Efficient Vulcanization Cure), Semi-EV(Semi-Efficient Vulcanization Cure) and CV(Conventional Vulcanization Cure). In the 2-step foaming process, first molding temperature was 140℃, times were 15, 20, 25, and 30minutes, and the second molding temperature was 160℃, the times 5, 10, 15, and 20minutes. The cure and viscosity characterization were evaluated by oscillating disc rheometer (ODR) and mooney viscosmeter. Various mechanical characteristics, including hardness, tensile strength, elongation at the point of rupture, and tear strength, were quantified. Subsequently, an assessment of alterations in these mechanical attributes was conducted post-immersion in a NaCl solution. In addition degree of volume change was measured after immersing the NR foam in NaCl solution and the low-temperature permanent compression set was evaluated at 4℃. And expansion ratio and shrinkage ratio of NR foam were evaluated for 28 days. As a result the EV vulcanization system showed the least change in physical properties before and after salt water immersion, and the lowest shrinkage ratio for 28 days. In addition it was confirmed that the 2-step foaming optimum condition differed depending on the appropriate vulcanization condition.

Dynamic Optimization of o Tire Curing Process for Product Quality (제품품질을 위한 타이어 가황공정의 동적 최적화)

  • Han, In-Su;Kang, Sung-Ju;Chung, Chang-Bock
    • Elastomers and Composites
    • /
    • v.34 no.4
    • /
    • pp.321-331
    • /
    • 1999
  • The curing process is the final step in tire manufacturing whereby a green tire built from layers of rubber compounds is formed to the desired shape and the compounds are converted to a strong, elastic materials to meet tire performance needs under elevated pressure and temperature in a press. A numerical optimization procedure was developed to improve product quality in a tire curing process. First, a dynamic constrained optimization problem was formulated to determine the optimal condition of the supplied cure media during a curing process. The objective function is subject to an equality constraint representing the process model that describes the heat transfer and cures kinetic phenomena in a cure press and is subject to inequality constraints representing temperature limits imposed on cure media. Then, the optimization problem was solved to determine optimal condition of the supplied cure media for a tire using the complex algorithm along with a finite element model solver.

  • PDF

Cure Cycle for Thick Glass/Polyester Composites (두꺼운 유리섬유/폴리에스터 복합재료를 위한 경화 사이클)

  • 김형근;오제훈;이대길
    • Composites Research
    • /
    • v.14 no.2
    • /
    • pp.33-42
    • /
    • 2001
  • The cure kinetic equation fur 52-glass/polyester prepreg composites was established through DSC (differential scanning calorimetry). Using the established kinetic equation, the temperature distribution of the thick composite was calculated considering the change of heat transfer resistance due to resin impregnation of bleeder plies used. In order to reduce the overheat during cure of thick glass fiber composites, the cure cycle was modified by introducing the cooling and reheating steps. Then the thick glass composites were cured both by the conventional cycle without any cooling or reheating step and the modified cure cycle. The mechanical properties of the thick composites cured by the both cycles were tested by the short beam shear test and the Barcol hardness test, and then their results were compared.

  • PDF

EFFECT OF INTERMEDIATE RESIN HYDROPHILICITY ON BOND STRENGTH OF SINGLE STEP ADHESIVE (중간레진의 친수성이 상아질 접착에 미치는 영향)

  • Kim, Yong-Sung;Park, Sang-Hyuk;Choi, Gi-Woon;Choi, Kyoung-Kyu
    • Restorative Dentistry and Endodontics
    • /
    • v.32 no.5
    • /
    • pp.445-458
    • /
    • 2007
  • The purpose of this study was to evaluate the bond strength of a new Single step system with different curing mode composites, and to evaluate the effect of the intermediate resins which have different hydrophilicity on bonding ability by means of the micro shear bond testing and TEM examination for the adhesive interface. The adhesive used in this study was an experimental single step system (Bisco Inc., Schaumburg IL). Experimental groups were produced by using six kinds of intermediate resin having different hydrophilicity that was hydrophilic, hydrophobic and most hydrophobic resin and as filled or not after applying adhesive. Each experimental group was further divided into two subgroups whether the adhesive was light cured or not. Dual cured composite (Bis Core, Bisco Ltd., Schaumburg, IL) was placed on the adhesive layer as light cure or self cure mode. The results or bond strength were statistically analyzed using one way ANOVA and multiple comparisons are made using Tukey's test at ${\alpha}\;<\;0.05$ level. The results of this study were as follows ; 1. The application of intermediate resin did not increase the bond strength for light cured composite. 2. The bond strength of an experimental adhesive with self cured composite was significantly increased by the application of intermediate resin layer. 3. The bond strength of adhesive was irrespective of the cure or not of itself before intermediate resin layer applied. 4. As applied hydrophilic resin layer was, the initial bond strength was higher than both hydrophobic and most hydrophobic one used but there was no significance. Using a single step adhesive with dual/self cured composite, the incompatibility between both of them should be solved by the application of intermediate hydrophobic resin to reduce the adhesive permeability. However, Single step adhesive can be used in the light cured composite restoration without any decrease of the initial bond strength.

Effect of 1,3-Diphenyl-guanidine (DPG) Mixing Step on the Properties of SSBR-silica Compounds

  • Lim, Seok-Hwan;Lee, Sangdae;Lee, Noori;Ahn, Byeong Kyu;Park, Nam;Kim, Wonho
    • Elastomers and Composites
    • /
    • v.51 no.2
    • /
    • pp.81-92
    • /
    • 2016
  • 1,3-Diphenylguanidine (DPG) is commonly used as a secondary accelerator which not only acts as booster of cure but also activating silanization reaction. The aim of this study is to increase the interaction between silica and rubber by using DPG. In this study, mixing was proceeded in two steps. The T-1 compound is mixed DPG with silica and silane coupling agent in the kneader at high temperature which is named as $1^{st}$ mixing step. T-3 compound is mixed DPG with curatives in the two-roll mill at low temperature which is named as $2^{nd}$ mixing step. The T-2 compound is mixed a half of DPG in $1^{st}$ mixing step and the remainder is mixed in $2^{nd}$ mixing step. Total DPG content was equal for all compounds. When DPG is mixed with silica, silane coupling agent during the $1^{st}$ mixing step, a decrease in cure rate and an increase in scorch time can be seen. This indicates that DPG is adsorbed on the surface of silica. during rubber processing. However, bound rubber content is increased and dynamic properties are improved. These results are due to the highly accelerated silanization reaction. However, there are no significant difference in 100%, 300% modulus.

Effects of Reactive Compatibilizers on the Morphology and Properties of Natural Rubber/SiO2 Composites

  • Lee, Min Young;Park, Jin Young;Song, Ki Chan;Kim, Su Kyung
    • Elastomers and Composites
    • /
    • v.51 no.2
    • /
    • pp.106-112
    • /
    • 2016
  • Maleimidopropyltriethoxysilane grafted natural rubber (MISNR) was prepared by reaction of maleic anhydride grafted natural rubber and 3-aminopropyl triethoxysilane. MISNR was used as the compatibilizer of natural rubber/silica composites. The composites were prepared by two-step mixing procedures. The final mixtures were cured with optimum cure condition, which was established by a rheometer. Effects of the amounts of compatibilizer in the composites on the cure characteristics, morphology, thermal stability, and physical and mechanical behaviors were investigated. The composites having MISNR had shown cure characteristics and physical and mechanical properties superior to those without MISNR. Silica particles in the former appeared to be more uniform and reduced in size compared with the latter. The effects of the types of silica were also evaluated.