  • In DNA microarray produced by DNA-deposition technology, DNA-immobilization and -hybridization yields on a solid support are most important factors for its accuracy and sensitivity. We have developed a dendrimeric support using silylated aldehyde slides and polyamidoamine (PAMAM) dendrimers. An oligonucleotide array was prepared through a crosslinking between the dendrimeric support and an oligonucleotide. Both DNAimmobilization and -hybridization yields on the solid support increased by the modification with the dendrimers. The increase of the immobilization and hybridization efficiency seems to result from a threedimensional arrangement of the attached oligonucleotide. Therefore, our dendrimeric support may provide a simple and efficient solution to the preparation of DNA microarrays with high-density DNA-deposition and high hybridization efficiency.

Study on Property Modification with Polymer Compositions in the Manufacture of Compounds for Cable Sheath

  • Li, Xiang Xu;Lee, Sang Bong;Cho, Ur Ryong
    • Elastomers and Composites
    • /
    • 제54권3호
    • /
    • pp.220-224
    • /
    • 2019
  • Herein, three polymer compounds were manufactured using three polymer combination methods, ethylene-vinyl acetate/ethylene-propylene-diene-copolymer (EPDM), ethylene-vinyl acetate (EVA)/polyethylene-A (PE-A; density: 0.870), and ethylene-vinyl acetate (EVA)/polyethylene-B (PE-B; density: 0.885), for making cable sheath for use in the shipping industry. In this study, EVA, EPDM, PE-A, and PE-B were used as matrix polymers, and EVA-grafted maleic anhydride was used as a coupling agent for compounding with various compounds such as a fire retardant, cross-linking agent, filler, and other additives, besides the plasticizer. ${\Delta}T$, Mooney viscosity, and tensile strength increased in order of EPDM < PE-A < PE-B, the probable reason is due to the different crosslinking effect. The three compounds showed similar results for fire resistance and aging resistance after compounding process, but they showed excellent cold resistance owing to the non-polarity of the polymers and sufficient plasticizer content.

모르타르 강도 증진을 위한 고분자 흡수제의 역유화 중합 (Inverse Emulsion Polymerization of Water Absorbent Polymer for Strength Enhancement of Mortars)

  • 황기섭;정명근;장석수;정용욱;이승한;하기룡
    • 폴리머
    • /
    • 제34권5호
    • /
    • pp.434-441
    • /
    • 2010
  • 콘크리트 제조 시 사용되는 잉여수를 흡수하기 위하여 흡수성의 sodium polyacrylate(PAANa)를 역유화중합법으로 제조하였다. 연속상은 paraffin liquid를 사용하였으며 acrylic acid(AA)는 NaOH로 중화시켜 사용하였다. 가교제는 N,N'-methylene bisacrylamide(MBA)를 사용하였고 첨가량을 다르게 하여 중합을 실시하였다. 중합된 PAANa들의 입자크기 분석을 실시하고 이들이 탈이온수, 시멘트 포화수용액 및 $Ca(OH)_2$ 수용액에서의 팽윤비를 측정하였다. $Ca^{2+}$ 이온과 PAANa의 상호작용을 관찰하기 위하여 FTIR spectroscopy 분석을 실시하였다. 중합된 PAANa를 포틀랜드 시멘트에 1 wt% 혼합 후 시멘트 모르타르 공시체의 압축강도와 휨강도를 측정한 결과, AA에 대하여 0.15 mol%의 MBA를 첨가하여 중합한 PAANa를 첨가하여 제조한 PAANa-시멘트가 일반 포틀랜드 시멘트와 비교하여 압축강도 약 30% 및 휨강도 약 10%가 각각 증가함을 확인하였다.

Modification of polyamide reverse osmosis membranes seeking for better resistance to oxidizing agents

  • Silva, Lucinda F.;Michel, Ricardo C.;Borges, Cristiano P.
    • Membrane and Water Treatment
    • /
    • 제3권3호
    • /
    • pp.169-179
    • /
    • 2012
  • One of the major limitations in the use of commercial aromatic polyamide thin film composite (TFC) reverse osmosis (RO) membranes is to maintain high performance over a long period of operation, due to the sensitivity of polyamide (PA) skin layer to oxidizing agents, such as chlorine, even at very low concentrations in feed water. This article reports surface modification of a commercial TFC RO membrane (BW30-Dow Filmtec) by covering it with a thin film of poly(vinyl alcohol) (PVA) crosslinked with glutaraldehyde (GA) to improve its resistance to chlorine. Crosslinking reaction was carried out at 25 and $40^{\circ}C$ by using PVA 1.0 wt.% solutions at different GA/PVA mass ratio, namely 0.0022, 0.0043 and 0.013. Water swelling measurements indicated a maximum crosslinking density for PVA films prepared at $40^{\circ}C$ and GA/PVA 0.0043. ATR-FTIR and TGA analysis confirmed the reaction between GA and PVA. SEM images of the original and modified membranes were used to evaluate the surface coating. Chlorine resistance of original and modified membranes was evaluated by exposing it to an oxidant solution (NaClO 300 mg/L, NaCl 2,000 mg/L, pH 9.5) and measuring water permeability and salt rejection during more than 100 h period. The surface modification effectively was demonstrated by increasing the chlorine resistance of PA commercial membrane from 1,000 ppm.h to more than 15.000 ppm.h.

Comparison of Pervaporation and Vapor Permeation Separation Processes for MTBE-methanol System

  • Kim, Youn-Kook;Lee, Keun-Bok;Rhim, Ji-Won
    • Korean Membrane Journal
    • /
    • 제2권1호
    • /
    • pp.36-47
    • /
    • 2000
  • This paper deals with the separation of MTBE-methanol mixtures using crosslinked Poly(vinyl alcohol)(PVA) membranes with sulfur-succinic acid(SSA) as a crosslinking agent by pervaporation and vapor permeation technique. The operating temperatures, methanol concentration in feed mixtures, and SSA concentrations in PVA membranes were varied to investigate the separation performance of PVA/SSA membranes and the optimum separation characteristics by pervaporation and vapor permeation. And also, for PVA/SSA membranes, the swelling measurements were carried out to study the transport phenomena. The swelling measurements were carried out for pure MTBE and methanol, and MTBE/methanol=90/10, 80/20 mixtures using PVA/SSA membranes with varying SSA compositions. There are two factors of the membrane network and the hydrogen bonding. In pervaporation separation was also carried out for MTBE/methanol=90/10, 80/20 mixtures at various temperatures. The sulfuric acid group in SSA took an important role in the membrane performance. The crosslinking effect might be over the hydrogen bonding effect due to the sulfuric acid group at 3 and 5% SSA membranes, and this two factors act vice versa on 7% SSA membrane. In this case, the 5% SSA membrane shows the highest separation factor of 2,095 with the flux of 12.79g/㎡$.$hr for MTBE/methanol=80/20 mixtures at 30$^{\circ}C$ which this mixtures show near the azeotopic composition. Compared to pervaporation, vapor permeation showed less flux and similar separation factor. In this case, the flux decreased significantly because of compact structure and the effect of hydrogen bonding. In vapor permeation, density or concentration of methanol in vaporous feed is lower than that of methanol in liquid feed, as a result, the hydrogen bonding portion between the solvent and the hydroxyl group in PVA is reduced in vapor permeation. In this case, the 7% SSA membranes shows the highest separation factor of 2,187 with the flux of 4.84g/㎡$.$hr for MTBE/methanol=80/20 mixtures at 30$^{\circ}C$.

  • PDF

Ethylene Vinyl Acetate / Styrene Vinyl Isoprene Styrene Triblock Copolymer 블렌드의 발포특성 (Foaming Characteristics of Ethylene Vinyl Acetate/Styrene Vinyl Isoprene Styrene Triblock Copolymer Blend)

  • 허재영;김진태;윤정식;유종선;김원호
    • Elastomers and Composites
    • /
    • 제35권2호
    • /
    • pp.106-114
    • /
    • 2000
  • 상온에서의 충격 흡수특성과 compression set 특성을 향상시키기 위하여 ethylene vinyl acetate copolymer (EVA)와 styrene vinyl isoprene styrene triblock copolymer (SVIS)를 블렌드하여 발포체를 제조하였다. 발포제 및 EVA/SVIS 블렌드비가 발포배율 및 기계적 물성에 미치는 영향을 조사하였다. SVIS 함량이 증가함에 따라 블렌드의 점도는 증가하였고 가교 속도는 감소하였으며, 발포배율은 감소하여 비중은 증가하였다. 발포제 함량 증가, 즉 발포배율 증가에 따른 반발탄성은 변화가 없는 반면에, SVIS 함량 증가에 따라 발포체의 상온에서의 tan ${\delta}$ 값은 증가하였으며 따라서 반발 탄성은 감소함을 알 수 있었다. EVA/SVIS 블렌드 발포체에서 SVIS 함량 증가에 따라 가교밀도와 비중이 증가하므로 compression set 값도 낮은 값을 나타내었다.

  • PDF

HIPE 중합에 의한 미세기공 발포체의 모폴로지 및 물성: 유화계 조성의 영향 (Morphology and Properties of Microcellular foams by High Infernal Phase Emulsion Polymerization: Effect of Emulsion Compositions)

  • 정한균;지수진;이성재
    • 폴리머
    • /
    • 제26권6호
    • /
    • pp.759-766
    • /
    • 2002
  • 스티렌과 물이 주된 원료로 구성된 혼합물을 high internal Phase emulsion (HIP보) 중합을 통하여 균일한 구형의 등방성 구조로 이루어진 저밀도의 열린 구조 미세기공 발포체를 제조하였고, 물, 가교결합제인 divinylbenzene, 사슬이동제인 dodecane의 함량 변화 등의 중합조건이 미세기공발포체의 기공 크기 및 물성에 미치는 영향을 조사하였다. 제조한 HIPE 발포체의 미세구조 모폴로지를 확인하기 위하여 SEM 사진으로 관찰하였고 기계적 물성을 평가하기 위하여 압축시험으로 압축 탄성률을 측정하였다. 연구 결과 오일 상에 수용액 상을 주입할 때 한 방울씩 연속적으로 주입하는 연속투여 방식의 경우가 한번에 주입하는 일괄투여 방식의 경우보다 균일하고 안정한 발포체를 제조하는데 효과적이었다. 교반속도와 계면활성제는 기공 크기와 계면의 window 크기에 상당한 영향을 끼쳤다. 사슬이동제의 첨가는 기공 크기를 증가시켰지만 window 크기는 오히려 감소시켰다. 발포체의 압축 탄성률은 가교결합제의 함량이 증가할수록, 사슬이동제의 함량이 감소할수록 증가하였다.

천연(天然)고무의 Damping Property에 관(關)한 연구(硏究) (A study on the Damping Properties of NR Vulcanizates.)

  • 최재운;백남철
    • Elastomers and Composites
    • /
    • 제20권3호
    • /
    • pp.189-204
    • /
    • 1985
  • The purpose of this study is to examine the dynamic properties, especially the damping and fatigue properites, of NR vulcanizates and to find out the vulcanizate which can be used as damping materials in industry. The results of this study can be summarized as follows: 1. In the ODR test, the S-2 vulcanizate was the fastest one in terms of having reached to optimum cure times($t_{90}$) and, with the same formula, when 50phr of HAF carbon black loaded, the shortest optimum cure times has shown. 2. The S - 2 vulcanizate was the best than the others in the physical properties. In aging properties, however, the E - 1 vulcanizate appeared to be better than the other vulcanizates. 3. The results of the RDS test for the NR vulcanization system under the condition of 0.1% strain amplitude and 1 Hz frequency showed no connection between Tg and the the nature of the crosslinking system, but 50phr loading of HAF carbon black increased Tg. The damping values of vulcanizates in the elastic region showed a strong relations the damping values and the crosslinking system. The S - 2 vulcanizate with higher crosslink density had lower damping values than other vulcanizates, and furthermore, the SH - 2 vulcanizates with 50phr loading of HAF carbon black increased the damping values. 4. The Goodrich Flexometer test showed that the heat buildup for the gum NR vulcanizates was less than for those which contained 50phr of HAF carbon black. In particular, the fatigue life of the vulcanizate with lower damping values appeared to be longer than that of the vulcanizates with higher damping values. In the fatigue test, the increasment of the loading or the temperature, applied to the vulcanizates, appeared to be shorten their fatigue life.

  • PDF

Comparison of Pervaporation and Vapor Permeation Separation Processes for MTBE-methanol System

  • 김연국;이근복;임지원
    • 멤브레인
    • /
    • 제2권1호
    • /
    • pp.36-36
    • /
    • 1992
  • This paper deals with the separation of MTBE-methanol mixtures using crosslinked Poly(vinyl alcohol)(PVA) membranes with sulfur-succinic acid(SSA) as a crosslinking agent by pervaporation and vapor permeation technique. The operating temperatures, methanol concentration in feed mixtures, and SSA concentrations in PVA membranes were varied to investigate the separation performance of PVA/SSA membranes and the optimum separation characteristics by pervaporation and vapor permeation. And also, for PVA/SSA membranes, the swelling measurements were carried out to study the transport phenomena. The swelling measurements were carried out for pure MTBE and methanol, and MTBE/methanol=90/10, 80/20 mixtures using PVA/SSA membranes with varying SSA compositions. There are two factors of the membrane network and the hydrogen bonding. In pervaporation separation was also carried out for MTBE/methanol=90/10, 80/20 mixtures at various temperatures. The sulfuric acid group in SSA took an important role in the membrane performance. The crosslinking effect might be over the hydrogen bonding effect due to the sulfuric acid group at 3 and 5% SSA membranes, and this two factors act vice versa on 7% SSA membrane. In this case, the 5% SSA membrane shows the highest separation factor of 2,095 with the flux of 12.79g/㎡·hr for MTBE/methanol=80/20 mixtures at 30℃ which this mixtures show near the azeotopic composition. Compared to pervaporation, vapor permeation showed less flux and similar separation factor. In this case, the flux decreased significantly because of compact structure and the effect of hydrogen bonding. In vapor permeation, density or concentration of methanol in vaporous feed is lower than that of methanol in liquid feed, as a result, the hydrogen bonding portion between the solvent and the hydroxyl group in PVA is reduced in vapor permeation. In this case, the 7% SSA membranes shows the highest separation factor of 2,187 with the flux of 4.84g/㎡·hr for MTBE/methanol=80/20 mixtures at 30℃.

저밀도 폴리에틸렌의 방사선 조사에 따른 전기 트리 특성 변화 (Radiation Effects on Electrical Treeing Characteristics of Low Density Polyethylene)

  • 이청;신희경;김기엽;박수길;류부형
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1999년도 하계학술대회 논문집 D
    • /
    • pp.1992-1994
    • /
    • 1999
  • Dicumyl peroxide (DCP) is used for crosslinking agent in general. And the correlation between polyethylene and DCP is significant in particular radiation environment. On this paper, The effects on $Co^{60}{\gamma}$-ray irradiation of polyethylene doped dicumyl peroxide(DCP) were investigated. We experimented on electrical properties as following; electrical tree inception and growing type for applying AC step voltage, AC breakdown strength, volume resistivity, capacitance and dissipation factor at high frequency as increasing dosage. Also, chemical analysis was performed TGA, gel content.