• Title/Summary/Keyword: compacted materials

Search Result 182, Processing Time 0.032 seconds

Mechanical Evaluation of Compacted Granular Materials Considering Particle Size Distribution (입도분포를 고려한 다짐된 지반재료의 역학적 거동 평가)

  • Park, Hyung-Min;Park, Hyun-Su;Park, Seong-Wan
    • Journal of the Korean Geotechnical Society
    • /
    • v.32 no.1
    • /
    • pp.45-53
    • /
    • 2016
  • Generally, conventional transport infrastructures consist of compacted granular materials. Their stiffness and response greatly depend on the particle sizes and distributions, and application of loading on the surface over a foundation may induce deformation in both the surface and the underlying foundations. Therefore, a better understanding of the deformation characteristics on granular materials and the prediction are needed. For this reason, an attempt to evaluate and predict deformation of coarse materials based on the discrete element method is presented in this paper. An algorithm for particle distribution curve analysis was formulated and incorporated into the discrete element program. The results show that the discrete element model with particle distribution curve is suitable for estimating stress deformation in a pre-peak response. Unlike conventional uniform or random particle distribution, the response can be obtained by the use of the proper model and approach.

Analysis of the Change in Microstructures of Nano Copper Powders During the Hydrogen Reduction using X-ray Diffraction Patterns and Transmission Electron Microscope, and the Mechanical Property of Compacted Powders (X-선 회절 패턴 측정과 투과 전자 현미경을 이용한 구리 나노분말의 수소 환원 처리 시 발생하는 미세조직 변화 및 치밀화 시편의 물성 분석)

  • Ahn, Dong-Hyun;Lee, Dong Jun;Kim, Wooyeol;Park, Lee Ju;Kim, Hyoung Seop
    • Journal of Powder Materials
    • /
    • v.21 no.3
    • /
    • pp.207-214
    • /
    • 2014
  • In this study, nano-scale copper powders were reduction treated in a hydrogen atmosphere at the relatively high temperature of $350^{\circ}C$ in order to eliminate surface oxide layers, which are the main obstacles for fabricating a nano/ultrafine grained bulk parts from the nano-scale powders. The changes in composition and microstructure before and after the hydrogen reduction treatment were evaluated by analyzing X-ray diffraction (XRD) line profile patterns using the convolutional multiple whole profile (CMWP) procedure. In order to confirm the result from the XRD line profile analysis, transmitted electron microscope observations were performed on the specimen of the hydrogen reduction treated powders fabricated using a focused ion beam process. A quasi-statically compacted specimen from the nano-scale powders was produced and Vickers micro-hardness was measured to verify the potential of the powders as the basis for a bulk nano/ultrafine grained material. Although the bonding between particles and the growth in size of the particles occurred, crystallites retained their nano-scale size evaluated using the XRD results. The hardness results demonstrate the usefulness of the powders for a nano/ultrafine grained material, once a good consolidation of powders is achieved.

Control of Grain Refinement and Anisotropy of NdFeB Alloy Powder by Severe Plastic Deformation Fabricated by the Gas Atomization Process (가스분무로 제조된 NdFeB 합금분말의 강소성변형을 통한 결정립 미세화 및 이방성 제어)

  • Cho, J.Y.;Park, S.M.;Hussain, J.;Song, M.S.;Kim, T.S.
    • Transactions of Materials Processing
    • /
    • v.31 no.3
    • /
    • pp.124-128
    • /
    • 2022
  • NdFeB magnets have been positioned as the core materials in advanced technologies such as MRI (magnetic resonance imaging), FA (factory automation system), robot, motors, and so on based on the highest magnetic properties. To effectively improve the refined microstructure, the plastic deformation has been known as the good alternatives by the recrystallization. However, it has been regarded as being impossible because of the few slip systems in the RE-Fe-B magnets at room temperature. The purpose of this study was to investigate the possibility of control of grain refinement and magnetic anisotropy of NdFeB alloy powder by the severe plastic deformation. The NdFeB magnet powder was fabricated by gas atomization process, and the powder was pre-compacted at high temperature. The pre-compacted billets were deformed by HPT (high pressure torsion), and then the deformed billets were observed microstructure and magnetic properties. After the HPT process at room temperature, the grain size decreased with increasing because of the melted Nd-rich phase, and the anisotropy of Nd2Fe14B phase was formed after the HPT process.

Compacted expansive elastic silt and tyre powder waste

  • Ghadr, Soheil;Mirsalehi, Sajjad;Assadi-Langroudi, Arya
    • Geomechanics and Engineering
    • /
    • v.18 no.5
    • /
    • pp.535-543
    • /
    • 2019
  • Building on/with expansive soils with no treatment brings complications. Compacted expansive soils specifically fall short in satisfying the minimum requirements for transport embankment infrastructures, requiring the adoption of hauled virgin mineral aggregates or a sustainable alternative. Use of hauled aggregates comes at a high carbon and economical cost. On average, every 9m high embankment built with quarried/hauled soils cost $12600MJ.m^{-2}$ Embodied Energy (EE). A prospect of using mixed cutting-arising expansive soils with industrial/domestic wastes can reduce the carbon cost and ease the pressure on landfills. The widespread use of recycled materials has been extensively limited due to concerns over their long-term performance, generally low shear strength and stiffness. In this contribution, hydromechanical properties of a waste tyre sand-sized rubber (a mixture of polybutadiene, polyisoprene, elastomers, and styrene-butadiene) and expansive silt is studied, allowing the short- and long-term behaviour of optimum compacted composites to be better established. The inclusion of tyre shred substantially decreased the swelling potential/pressure and modestly lowered the compression index. Silt-Tyre powder replacement lowered the bulk density, allowing construction of lighter reinforced earth structures. The shear strength and stiffness decreased on addition of tyre powder, yet the contribution of matric suction to the shear strength remained constant for tyre shred contents up to 20%. Reinforced soils adopted a ductile post-peak plastic behaviour with enhanced failure strain, offering the opportunity to build more flexible subgrades as recommended for expansive soils. Residual water content and tyre shred content are directly correlated; tyre-reinforced silt showed a greater capacity of water storage (than natural silts) and hence a sustainable solution to waterlogging and surficial flooding particularly in urban settings. Crushed fine tyre shred mixed with expansive silts/sands at 15 to 20 wt% appear to offer the maximum reduction in swelling-shrinking properties at minimum cracking, strength loss and enhanced compressibility expenses.

A Small Scale Test using the Coal Ash Placement Equipment (고유동성 채움재 타설장비를 이용한 모형시험)

  • Kim, Ju-Hyong;Cho, Sam-Deok;Ham, Tae-Gyu;Do, Jong-Nam;Chun, Byung-Sik
    • Proceedings of the Korean Geotechical Society Conference
    • /
    • 2010.03a
    • /
    • pp.1452-1457
    • /
    • 2010
  • Recently, coal ash is used as resources to make controlled low-strength material (CLSM) which a self-compacted, cementitious material used primarily as a backfill in lieu of compacted fill. Pozzolanic reaction is strongly related with self-cementation of coal ashes. However, this reaction depends on pozzolanic content in fill materials and is disappeared in 2-3 days after placement of coal ash fill. Therefore, state of coal ash fill is commonly very loose and not appropriate for foundations of structures without special treatments. In this study, a coal ash placement device was developed to place coal ashes effectively to improve density of coal ash fills. The device consists of a ribbon type mixer to obtain homogeneous materials mixture and a piston type pump for density control of fill materials. Based on several laboratory test results, more stable coal ash fill state can be obtained with controlling placement pressure.

  • PDF

Study on Wear Properties of GCV Materials with DLC Coating (GCV소재의 DLC 코팅 마모특성에 관한 연구)

  • Lee, Soo-Chul;Kim, Nam-Seok;Nam, Ki-Woo;Ahn, Seok-Hwan;Kim, Hyun-Soo
    • Journal of Ocean Engineering and Technology
    • /
    • v.24 no.6
    • /
    • pp.71-75
    • /
    • 2010
  • Although Graphite Compacted Vermicular (GCV) was first observed in 1948, the narrow range for stable foundry production precluded the high volume application of GCV to complex components such as cylinder blocks and heads until advanced process control technologies became available. This, in turn, had to await the advent of modern measurement electronics and computer processors. Following the development of foundry techniques and manufacturing solutions, primarily initiated in Europe during the 1990s, the first series production of GCV cylinder blocks began during 1999. Today, more than 40,000 GCV cylinder blocks are produced each month for OEMs, including Audi, DAF, Ford, Hundai, MAN, Mercedes, PSA, Volkswagen, and Volvo. Given that new engine programs are typically intended to support three to four vehicle generations, the chosen engine materials must satisfy current design criteria and also provide the potential for future performance upgrades without changing the overall block architecture. With at least a 75% increase in the ultimate tensile strength, a 40% increase in the elastic modulus, and approximately double the fatigue strength of either iron or aluminum, GCV is ideally suited to meet current and future of engine design and performance requirements.

Aging Characteristics of Al P/M Composites with Variation of Ceramic Contents

  • Min, Kyung-Ho;Chang, Si-Young;Kim, Deok-Soo;Kim, Ji-Soon;Kim, Young-Do
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.1065-1066
    • /
    • 2006
  • The aging behavior of sintered Al composites with various ceramic contents was investigated. 2xxx series blended powder was used as the starting powder. Ceramic contents were 0wt.% and 5wt.%. The blended powders were compacted at 250MPa. The sintering process was performed at $620^{\circ}C$ for 60min in a $N_2$ atmosphere. Each part was solution-treated at $518^{\circ}C$ for 60min and aged at $180^{\circ}C$. The Rockwell hardness at the peak aging time increased with ceramic contents. However, the peak aging time at maximum hardness was reduced with increased ceramic contents.

  • PDF

Effect of Cu and Mg on Forging Property and Mechanical Behavior of Powder Forged Al-Si-Fe Based Alloy

  • Lee, Dong-Suk;Jung, Taek-Kyun;Kim, Mok-Soon;Kim, Won-Yong
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.1000-1001
    • /
    • 2006
  • Two atomized alloy powders were pre-compacted by cold and subsequently hot forged at temperatures ranging from 653K to 845K. The addition of Cu and Mg causes a decrease in the eutectic reaction temperature of Al-10Si-5Fe-1Zr alloy from 841K to 786K and results in a decrease of flow stress at the given forging temperature. TEM observation revealed that in addition to Al-Fe based intermetallics, $Al_2Cu$ and $Al_2CuMg$ intermetallics appeared. The volume fraction of intermetallic dispersoids increased by the addition of Cu and Mg. Compressive strength of the present alloys was closely related to the volume fraction of intermetallic dispersoids.

  • PDF

Compaction Properties of Fe Powder Fabricated by Warm Compaction (온간성형법으로 제조된 Fe 분말의 성형특성)

  • Kim, Se-Hoon;Lee, Young-Jung;Lee, Jea-Sung;Kim, Young-Do
    • Journal of Powder Materials
    • /
    • v.14 no.3 s.62
    • /
    • pp.185-189
    • /
    • 2007
  • Various approaches have been proposed to increase the green density. Warm compaction method has been used for the reduction of residual stress, the improvement of magnetic properties and the higher densities. In this work, the effect of warm compaction on green density of Fe powder was investigated. After ball-milling of Fe oxide powder for 30 hours, Fe oxide powder was reduced through the hydrogen reduction process. The pure Fe powder and polymer binder were mixed by 3-D tubular mixer. And then the mixed powder was warm-compacted with various compaction pressure and binder contents. The green density of specimen was added polyvinyl binder was higher than any other specimens.

Densification Behavior of Fe-Ni Alloy Nanoparticles

  • Kim, Sang-Phil;Lee, Woo-Seok;Lee, Jae-Wook;Choi, Chul-Jin
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.531-532
    • /
    • 2006
  • The effects of compaction pressure and sintering temperature on the densification of Fe-40wt%Ni alloy nanoparticles were analyzed. The Fe-Ni nanoparticles were fabricated by an arc-discharge method and then, compacted at three different pressures and sintered at 550 to $900\;^{\circ}C$. Densification was completed at temperature as low as $600\;^{\circ}C$ and high-pressure compaction was found to enhance densification. Densification behaviors and microstructure developments have been investigated through density measurements, electron microscopies, and hardness measurements.

  • PDF