비소성 시멘트 모르타르의 작업성 및 강도 개선을 위한 페로니켈슬래그 골재의 적용방안 (Application of Ferronickel Slag Aggregate to Improve Workability and Strength of Non-Sintered Cement Mortar)

  • 장경수;나형원;형원길
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2023년도 봄 학술논문 발표대회
    • /
    • pp.309-310
    • /
    • 2023
  • Slag and ash generally have a higher powder degree than portland cement, so workability may deteriorate under the same unit quantity condition, and strength and durability decrease when the unit quantity is increased. At this time, if an aggregate having a low water absorption and an appropriate particle size is used to recover the loss of strength, it can contribute to reducing the unit quantity of the binder. Therefore, for the purpose of improving the workability and strength of non-sintered cement mortar using slag and ash, ferro nikel slag whose particle size was adjusted was used as an aggregate and its applicability was identified. In this experimental condition, it was confirmed that non-sintered cement mortar tends to improve workability and secure strength when ferro nikel slag having various particle size distributions is used as an aggregate. This can be analyzed as the effect of ferro nikel slag material properties including glassy properties and mixing conditions with a wide particle size distribution.

  • PDF

수산물 가공 폐슬러지를 이용한 인산염인 제거 (Removal of Phosphate by Using Wasted Sludge of Seafood Processing Factory)

  • 최봉종;이승목;김근한
    • 한국환경보건학회지
    • /
    • 제25권3호
    • /
    • pp.23-28
    • /
    • 1999
  • Phosphate removal through adsorbent, such as activated alumina, powdered aluminum oxide, flyash, blasted furnace slag and other materials, is commonly and widely practiced. The purpose of this study was to improve the removal efficiency of phosphorus in waste sludge earned at seafood processing factories. To investigate the utility and the feasibility of this sludge disposal process, experiment was carried out with a batch process. As a result, phosphate removal appears to increase with increasing adsorbent does, but shows no changes at an adsorbent does over 5g/l. With increasing ratios of initial phosphate concentration to adsorbent does, the amount of removed phosphate is increased while phosphate removal(%) is decreased. Wasted sludge, treated with zinc chloride chemically, represented a better efficiency than the untreated activated sludge and zinc chloride itself, when they reacted with phosphate solution.

  • PDF

혼합된 나트륨계열 활성화제에 의한 고로슬래그 기반 모르타르의 강도발현 특성 (Strength Development of Blended Sodium Alkali-Activated Ground Granulated Blast-Furnace Slag (GGBS) Mortar)

  • 김건우;김병조;양근혁;송진규
    • 콘크리트학회논문집
    • /
    • 제24권2호
    • /
    • pp.137-145
    • /
    • 2012
  • 이 연구는 수산화나트륨과 탄산나트륨이 혼합된 알칼리 활성화제에 의한 고로슬래그 모르타르의 강도발현 특성을 파악하기 위한 연구이다. 주요 변수는 활성화제의 첨가량, 물-바인더비(W/B) 그리고 골재-바인더비(S/A)이다. 활성화제의 첨가량에 따른 강도 특성을 수산화나트륨 3%, 4% 및 탄산나트륨 4%~8%까지 조절하여 측정하였다. 물-바인더비는 0.45~0.60까지 그리고 골재-바이더비는 2.05~2.85의 범위 내에서 변화하며 측정하였다. 원재료의 주요 성분 및 수산화나트륨, 탄산나트륨에 포함된 산화나트륨($Na_2O$) 양에 따라 조합된 알칼리 품질계수($Q_A$)를 산정하고, 이를 적용하여 알칼리 활성 모르타르의 28일 압축강도 예측식을 제안하였다. 각 변수에 따른 시험값과 제안된 예측식을 통한 결과값은 오차범위 5% 이내의 범위에서 만족하는 것으로 나타났다.