Effects of Mineral Admixture on the Paste Fluidity and Mortar Strength Development of High Chloride Cement (염소 고함유시멘트의 페이스트 유동성과 모르타르 강도발현성에 미치는 무기질 혼화재의 영향)

  • Jeong, Chan-Il;Park, Soo-Kyung;Lee, Eui-Hak;Lee, Kyung-Hee
    • Journal of the Korean Ceramic Society
    • /
    • v.44 no.1 s.296
    • /
    • pp.43-51
    • /
    • 2007
  • Fluidity, setting time, hydration heat, bond water ratio, compressive strength, SEM and BET of OPC were measured by adding 1.0 wt% KCl and replacing 20 wt% mineral admixture in order to examine effects of blast furnace slag (BFS), limestone powder (LSP), and fly ash (FA) on fluidity and strength development of the cement contained much chloride. In general, the cement contained much chloride was high in heat of hydration, short in its setting time, low in its fluidity and low in its strength at 28 days due to the rapid hydration in its initial stage. As a result of the experiment, it has been demonstrated that fluidity became improved but the compressive strength at 28 days was decreased as replaced LSP to the cement contained much chloride. the fluidity and compressive strength at 28 days was improved as replaced BFS, the initial compressive strength development was improved due to the activation of initial reaction by KCl. Fluidity, initial compressive strength and late compressive strength at 28 days of cement contained much chloride replaced 5 wt% LSP and 15 wt% BFS concurrently was better than OPC, but the hydration heat was lower.

Analysis of Rheological Properties of Cement Paste with Binder Type and Composition Ratio (결합재 타입 및 구성비 변화에 따른 시멘트 페이스트의 레올로지 특성 분석)

  • Jeon, Sung IL;Nam, Jeong Hee;Lee, Moon Sup;Nho, Jae Myun
    • International Journal of Highway Engineering
    • /
    • v.19 no.5
    • /
    • pp.77-88
    • /
    • 2017
  • PURPOSES : It is necessary to clarify the rheological properties of cement paste as a basic research in the development of mechanistic concrete mix design. The rheological properties of cement paste with different binder types, mix propositions, and with/without high range water reducers have been analyzed. METHODS : In this study, ordinary Portland cement, fly-ash, blast furnace slag, silica fume, and limestone powder were used as binders. The range of water-binder ratio was 0.3-0.5, and a total of 30 different mixes have been tested. The slump flow test, V-funnel test, and Dynamic Shear Rheometer (DSR) test were performed to analyze the rheological properties of cement paste. RESULTS : As a result of the slump flow test, it was found that the composition ratio of the binder contents greatly affected the paste flow when the high range water reducers were added. The results of V-funnel test showed that when the water-binder ratio was decreased without high range water reducers, the binder composition ratio had a large effect on the passing time of the V-funnel tester, but with high range water reducers the impact of the binder composition ratio was decreased. The slump flow and V-funnel have a certain relationship with the rheological factors (yield stress and plastic viscosity), but the correlation was not significant. Finally, we proposed the M-value considering the density and specific surface area of the binder. The correlation between rheological factors and M-value were better demonstrated than experimental values, but there is still a limit to predict the rheological factor in general mix design. CONCLUSIONS :In this study, the rheological properties of cement paste were analyzed. The binder type, composition ratio of binder, and with/without high range water reducers have combined to provide the complex effects on the rheological properties of cement paste. The correlation between the proposed M-value and rheological factor was found to be better than experimental results, but needs to be improved in the future.

Evaluation on Mechanical and Mixing Properties of Ultra-high Strength Concrete with fck=150MPa (150MPa 초고강도 콘크리트의 배합 및 재료역학특성 평가 연구)

  • Kang, Hoon;Ahn, Jong-Mun;Shin, Sung-Woo
    • Journal of the Korea Institute of Building Construction
    • /
    • v.10 no.3
    • /
    • pp.113-120
    • /
    • 2010
  • Ultra-High Strength Concrete (UHSC) demands a clear presentation of its mechanical properties, as distinct from normal strength concrete, and an evaluation of the serviceability of high-rise buildings that use ultra-high strength concrete. Ultra-high strength concrete fck=150MPa was manufactured with pre-mix cement, and an experimental study was conducted to evaluate the mixing properties and compressive strength, with the major variables being unit cement contents, water-binder ratio, and type of pre-mix cement. The test result showed that 150MPa concrete requires about 6~7 minutes of mixing time until each of the materials (ordinary Portland cement, silica fume, blast-furnace slag powder and anhydrite) are sufficiently revitalized. The slump flow of fresh concrete was shown to be about 700~800mm with the proper viscosity. The average value of concrete compressive strength was shown to be about 70% in 7 days, 85% in 14 days, and 95% in 28 days, for 56 days of concrete material age.

A Study on the Quality Properties of Alkali-activated cement free Mortar using Industrial by-products (산업부산물을 사용한 알칼리 활성 무시멘트 모르타르의 품질특성에 관한 연구)

  • Kwon, Yong-Hun;Kwon, Yeong-Ho;Lee, Dong-Gyu
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.1 no.1
    • /
    • pp.58-66
    • /
    • 2013
  • This study investigated quality properties of alkali activated cement free mortar using industrial by-product such as cement kiln dust(CKD), silica fume(SF) and quartz sand powder(SP) to compare with previous research about blast furnace slag(BS) and fly ash(FA). The results were as following. All materials were effective to increase compressive strength, however they showed different tendency on flowability. CKD and SP increased flowability, but on the other hand SF did not because it's blain was great difference with other materials. Flowability and compressive strength were related with grading distributions of binders because CKD, SP and SF which had small particle size filled up BS and FA. Application of industrial by-products with various grading distributions could be effective for the high early strength and flowability of alkali activated cement free mortar using BS.

An Experimental Study on the Ready-Mixed Concrete Manufacture Performance of Ultra-High Strength Concrete using the Crushed Sand (부순모래를 사용한 초고강도 콘크리트의 레미콘 제조성능에 관한 실험적 연구)

  • Rho, Hyoung-Nam;Lim, Hyon-Ung;Choi, Se-Jin;Lee, Seong-Yeon;Lee, Sang-Soo;Song, Ha-Youg
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2007.04a
    • /
    • pp.25-28
    • /
    • 2007
  • In this study we measured the changes according to time respectively on the basis of 0, 30, 60 and 90 minutes, taking into consideration the decline in fluidity of concrete according to elapsed time to analyze manufacturing capability of batcher plant according to elapsed time of ready-mixed concrete manufactured in batcher plant, and offer basic data for mixture design of ultra-high strength concrete. The proportion of water-binder was 23.55, water content was 160kg/m3, proportion of replacement of crushed sand was 0, 20 and 40% at 3 level, and we applied to the same condition of triaxial component using blast furnace slag powder and silica fume as admixture. And to meet the demand of certain fluidity, we measured respectively on property before and after hardening of ultra-high strength concrete using superplasticizer. As a result of experiment, before hardening of ultra-high strength concrete showed the best fluidity in conditions of crushed sand replacement rates of 20% and superplasticizer composition of 1.95%, but it appeared that fluidity drops as time goes by in the same composition condition. And it appeared that when it comes to hardened, the changes of compression strength according to elapsed time by crushed sand replacement rates were within 1MPa. Therefore, it turned out that the difference of strength according to elapsed time was low and compression strength of 280dys in composition mentioned above appeared highly as 88MPa.

  • PDF

Properties on the Freeze-Thaw of Concrete Subjected to Seawater Attack (해수의 영향을 받은 콘크리트의 동결융해 특성)

  • Park, Kwang-Pil;Kim, Seong-Soo;Lee, Seung-Tae;Kim, Jong-Pil;Jung, Ho-Seop
    • Journal of the Korea Concrete Institute
    • /
    • v.23 no.1
    • /
    • pp.23-30
    • /
    • 2011
  • In this study, deterioration degrees of concrete were investigated at laboratory under seawater attack and cycling freeze-thaw, which are major durability performance deterioration factors of concrete. Deteriorations of mixed concrete using Portland & blended cement were examined by instrumental analysis of changes in relative dynamic modulus of elasticity and compressive strength. After 520 cycles of freeze-thaw, relative dynamic modulus of elasticity and compressive strength of concrete mixed with normal Portland and LHC over 75% showed relatively low resistance of approximately 44% of those values of SRC. Concrete replaced with 50% fine powder of blast furnace slag showed the most excellent freeze-thaw resistance among the tested blended cement concrete.

Evaluation of Rainwater Storage Block Using Recycled Aggregate By-product (순환골재 공정부산물을 활용한 빗물저류블록의 성능평가)

  • Kim, Ho-Kyu;Kim, Young-Ahn;Choi, Seung-Yong;Cho, Young-Keun
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.6 no.3
    • /
    • pp.167-173
    • /
    • 2018
  • In general, calcium is required for the reaction of blast furnace slag fine powder and fly ash. The by-products generated during the process of producing recycled aggregates have different calcium contents depending on the crushing stage and the possibility of using the process by-product as a concrete mixture is also different. In this study, the effect of the calcium content of the by-products on the compressive strength was investigated and the block was fabricated by using this. To utilize the by-products as an admixture, the calcium content was analyzed and the bending strength and surface temperature were measured according to the shape of the water storage block. As a result of this study, the possibility of making a block using recycled aggregate by-products was verified and arch type block was constructed to secure storage capacity and bending strength. Also, the surface temperature of the water storage block was reduced by $9^{\circ}C$ or more than that of the general permeable block.

A Study on the Cementitious Materials as Carbon Capture Materials-Micro-Structure Change by Carbonation Curing (시멘트계 재료의 탄소포집 건설재료로 활용연구 - 탄산화 양생에 의한 미세구조 변화)

  • Moon, Eun-Jin;Kim, Sang Jun;Park, Hong Gi;Choi, Young Cheol
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.22 no.6
    • /
    • pp.123-129
    • /
    • 2018
  • Recently, there has been a growing interest in the study of treatment of $CO_2$ generated by industrial activities and resource recycling of industrial byproducts. The aim of this study is to investigate the applicability of industrial byproducts that can be used as concrete mixed materials by carbonation curing. For this purpose, the physical and chemical changes of the pastes with research cement(RC), blast furnace slag powder (GGBFS) and circulating fluidized bed combustion ashes (CFBC) were evaluated by carbonation curing. XRD and SEM analyzes were performed to investigate micro-structural changes. As a result, it was confirmed that calcium carbonate, which is a reaction product produced by carbonation curing, filled the space inside the paste and formed a dense micro-structure. Also, as the $CO_2$ curing time increased, it was confirmed that calcium carbonate crystals were grown together to form a dense micro-structure.

The Diffusion Property of Chloride Ion into Concrete by Electrically Accelerated Method (전기적인 촉진시험에 의한 콘크리트의 염화물이온 확산특성)

  • Bae, Ju-Seong;Park, Gook-Joon
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.14 no.3
    • /
    • pp.138-143
    • /
    • 2010
  • Recently, as many big marine concrete structures increase, it is necessary that chloride ion diffusion coefficient of concrete shall be evaluated but it will take a long time to evaluate chloride ion diffusion coefficient of concrete. Accordingly, many test methods are suggested to evaluate chloride ion diffusion coefficient in a short period time by the promotion in electro chemical ways but the systematic study for this is insufficient. Therefore, this study evaluates chloride ion penetration and diffusion features by three representative electric promotion tests targeting for three different cements whose ingredients are different and analyzes the correlationship between them. As a result, diffusion features of chloride ion varied according to the cement ingredients and three ingredients cement in which blast furnace slag powder and fly ash are mixed in constant ratio, which shows the most excellent cement diffusion properties. For diffusion properties of chloride ion, the correlationship between test methods are good.

Characteristics of Carbon Capture by the Accelerated Carbonation Method of Circulating Fluidized Bed Combustion Ash (순환 유동층 보일러 애시의 촉진탄산화에 의한 탄소포집 특성)

  • Choi, Young-Cheol;Yoo, Sung-Won
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.25 no.5
    • /
    • pp.165-172
    • /
    • 2021
  • The purpose of this study is to investigate the carbon capture capacity of various inorganic materials. For this purpose, the change in property of ordinary Portland cement (OPC), blast furnace slag fine powder (GGBS), and circulating fluidized bed boiler ash (CFBC) due to carbonation were analyzed. Carbonation curing was performed on all specimens through the accelerated carbonation experiment, and the amount of carbon capture was quantitatively analyzed by thermogravimetric analysis according to the age of carbonation. From the results, it is confirmed that the carbon capture capacity was shown in all specimens. The carbon capture amount was shown in the order of CFBC, OPC, and GGBS. The 28-day carbon capture of CFBC, OPC, and GGBS was 3.9%, 1.3%, and 9.4%, respectively. Carbon capture reaction occurred rapidly at the beginning of carbonation, and occurred slowly with increasing age. SEM image analysis revealed that an additional product generated by carbonation curing in all specimens was calcium carbonate.