Derivation of Optimum GGBFS Replacement with Durability Design Parameters (내구성 설계 변수에 따른 최적 고로슬래그 미분말의 치환율 도출)

  • Jang, Seung-Yup;Yoon, Yong-Sik;Kwon, Seung-Jun
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.6 no.1
    • /
    • pp.36-42
    • /
    • 2018
  • GGBFS(Ground Granulated Blast Furnace Slag)-replacement is very effective for improving resistance to chloride attack and this can induce a long service life for RC(Reinforced Concrete) structures exposed to chlorides. In the work, the design parameters such as cover depth, surface chloride content, critical chloride content, and replacement ratio of GGBFS are considered, and optimum replacement ratio of GGBFS are derived with intended service life. The changes of surface chloride content and cover depth show 3.16~3.38 and 3.02~3.34 times of service life variation, which are most influencing parameters. Critical chloride content shows 1.53~1.57 times of service life variation regardless of w/b(Water to Binder) ratios. In the case of surface chloride content $18.0kg/m^3$, the most severe condition, cover depth over 70 mm and GGBFS replacement ratio over 42% are required with concrete containing w/b ratio under 0.42 for 100 years of intended service life. The condition of $13.0kg/m^3$, GGBFS replacement over 35% is required. For reasonable durability design, quantitative exterior condition and critical chloride content should be determined, and the criteria in Domestic Specification is evaluated to be conservative.

Resistance of Chloride Penetration into High Strength Concrete Containing Mineral Admixtures according to Curing Conditions (광물질혼화재 혼합 고강도콘크리트의 양생조건에 따른 염화물이온 침투저항성)

  • Moon, Han-Young;Kim, Byoung-Kwon
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.8 no.2
    • /
    • pp.185-194
    • /
    • 2004
  • In recent years, construction company makes inroads into the world construction market, and receives the order of extra-large concrete structure under marine environment in south-east asia specially. At this point of time, to enhance the quality of concrete, we research the High Strength Concrete (HSC) containing mineral admixtures. In this study, therefore, HSC with various combination of ordinary portland cement(OPC), blast-furnace slag(SG), silica fume(SF), and expansion admixture(SS) are cured 23 and $35^{\circ}C$ considering the site weather, and are cured in water for 3, 7 or 56 days respectively. Test results show that the HSC cured at $35^{\circ}C$ gains higher early-age strength but eventually gains lower later-age strength compare with the HSC cured at $23^{\circ}C$. Especially, HSC with combination of OPC+SG+SF+SS or OPC+SG+SF show very excellent resistance of chloride penetration. The permeability of HSC was therefore enhanced as because of containing the proper content of SG, SF, and SS and making dense micro-structure of HSC.

A Study of the Effect of Mineral Admixtures on the Chloride Diffusion of the Concrete Immersed in Chloride Solution (무기질 혼화재가 염수침지한 콘크리트의 염화물 확산에 미치는 영향에 관한 연구)

  • Kim Dong-Seok;Yoo Jae-Kang;Park Sang-Joon;Won Cheol;Kim Young-Jin
    • Journal of the Korea Concrete Institute
    • /
    • v.17 no.5 s.89
    • /
    • pp.679-686
    • /
    • 2005
  • The corrosion of reinforcement induced by chloride ingress is the main deterioration cause of coastal reinforced concrete structures. In this paper, an experimental study was executed to investigate the effect of the kinds and replacement ratios of mineral admixtures (fly-ash, ground granulated blast-furnace slag silica fume and meta-kaolin), W/B and curing time on chloride diffusion of concrete by long-time immersion test in chloride solution. According to the result, the use of mineral admixtures was effective in improving the resistant to chloride ingress. The chloride penetration depth and diffusion coefficient were decreased as replacement ratios of mineral admixture were increased. The kind and replacement ratio of the mineral admixture are more important than the W/B in reducing the chloride diffusion of concrete. Chloride binding capacity of mineral admixture, which was sequenced in the order of MK

The Properties of Underwater-Hardening Epoxy Mortar Used the Rapidly Cooled Steel Slag (RCSS) (급냉 제강슬래그를 사용한 수중 경화형 에폭시 모르타르의 특성)

  • Kim, Jin-Man;Kwak, Eun-Gu;Bae, Kee-Sun
    • Journal of the Korea Concrete Institute
    • /
    • v.19 no.5
    • /
    • pp.549-555
    • /
    • 2007
  • Although blast furnace slag has been widely used in concrete as a cementitious admixture or aggregate for many years, the slowly cooled steel slag is not used in concrete but mainly in road. Its use in concrete operates problem such as the lack of volume stability due to high free CaO content, which can be potentially hazardous in concrete. However, the rapidly cooled steel slag by atomization has a low free CaO content, a high density, and a spherical shape, so it is expected to use in concrete so much. This paper is to understand the probability that the rapid cooled steel slag can replace the silica sand used as aggregate in the epoxy mortar. We did the experimental study on the properties of the epoxy mortar having various replacement proportion of rapidly cooled steel slag. This study shown that increasing content of the rapidly cooled steel slag in epoxy mortar lead to increase largely the passing time of nozzle by O-lot, compressive strength and flexural strength. However except the flow is almost same level. So we understand that the rapidly cooled steel slag has positive effect on increasing of properties in epoxy mortar.

Assessment of Bond Characteristics between New and Old Concrete in Various Mixtures and Joint Conditions (배합 및 접합면 처리에 따른 신·구 콘크리트의 부착특성 평가)

  • Cho, Byeong-Du;Kim, Sang-Hyun;Jeon, Se-Jin
    • Journal of the Korea Concrete Institute
    • /
    • v.26 no.4
    • /
    • pp.507-515
    • /
    • 2014
  • Although the construction joints of a concrete structure are properly treated with some measures, leakage has frequently occurred. A series of tests on the bond characteristics between new and old concrete were carried out in this study, assuming that the leakage at the construction joints has certain relationship with the bond of concrete. To assess the bond characteristics under various conditions, a number of specimens were made that have an interface between new and old concrete and bond strength, flexural strength and splitting tensile strength were measured. Main test variables are type and amount of mineral admixtures, treatment method of the interface and type of waterstops. In addition, the effects of placing interval between the concrete and of the age of the strength tests were investigated. The test results showed a slightly increased bond strength when applying mineral admixtures, which can be attributed to the interface filled with the calcium silicate hydrate that is formed by pozzolanic reaction. On the other hand, the bond strength was higher when the interface was treated rough and dry, and the roughness of a waterstop affected the bond capacity of the waterstop. Also, an assessment is required that considers the type of strength test because the bond strength varied according to the test methods.

Flexural Behavior of Hwangtoh Concrete Beams with Recycled PET Fiber (재생 PET섬유가 혼입된 황토 콘크리트 보의 휨 거동)

  • Kim, Sung-Bae;Nam, Jin-Won;Yi, Na-Hyun;Kim, Jang-Jay-Ho;Choi, Hong-Shik
    • Journal of the Korea Concrete Institute
    • /
    • v.20 no.5
    • /
    • pp.619-626
    • /
    • 2008
  • There have been numerous studies to develop eco-friendly concrete. The attempt to reduce the amount of cement usage is suggested as one of the solutions for eco-friendly concrete. To reduce the amount of cement usage, the pozzolan-reaction materials such as ground granulated blast furnace slag, fly ash, and meta kaolin are widely used as the mineral admixture. Hwangtoh which deposited broadly in Korea is a well known eco-friendly material and the activated Hwangtoh with pozzolan-reaction can be practically used as a mineral admixture of concrete. Meanwhile, PET fiber made of recycled PET bottle is a type of recycled material, which can be used to control micro cracks in concrete. But the study about concrete mixed with recycled PET fiber is insufficient and the research of Hwangtoh concrete mixed with PET fiber is urgently needed presently. In this study, experiment and analysis flexural behavior of Hwangtoh concrete blended with recycled PET fiber are carried out. The results are discussed in detail.

Development and performance verification of induced drainage method for leakage treatment in existing underground structures (운영중인 지하구조물 누수처리를 위한 유도배수공법 개발 및 성능 검증)

  • Kim, Dong-Gyou;Yim, Min-Jin
    • Journal of Korean Tunnelling and Underground Space Association
    • /
    • v.19 no.3
    • /
    • pp.533-549
    • /
    • 2017
  • In this study, drainage systems were proposed to drain the leakage of groundwater in the existing underground concrete structures. The system consists of drainage board, wire mesh, fixed nail, and mortar with mineral. In order to increase constructability, the drainage board and wire mesh were attached on the surface of cement concrete using the air nailer and fixed nail. The mortar with 30% of blast furnace slag was sprayed on the drainage board and wire mesh using the spray mortar equipment. The field test construction was carried out in a conventional concrete lining tunnel and concrete retaining wall for performance verification of the drainage system in the field. There was no problem with performance degradation in the drainage system for three years after construction. The bond strength tests were performed on the sprayed mortar at 14 days and about 3 years after field test construction. In case of attaching the wire mesh on the drainage board, the bond strengths of the sprayed mortar were 1.04 MPa at 14 days and 1.46 MPa about 3 years. In case of the drainage board without the wire mesh, the bond strengths of the sprayed mortar were 1.13 MPa at 14 days and 0.89 MPa, less than 1 MPa of bond strength criteria, about 3 years.

Evaluation on Feasibility of Industrial By-products for Development of Mono-Layer Landfill Cover System (산업부산물을 이용한 단층형 매립지 복토시스템 개발을 위한 적용 타당성 평가)

  • Kim, Soon-Oh;Kim, Pil-Joo;Yu, Chan
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.30 no.11
    • /
    • pp.1075-1086
    • /
    • 2008
  • In order to investigate the applicability and suitability of the industrial by-products to apply mono-layer cover system for non-sanitary landfill sites, 6 different industrial by-products, such as construction waste, bottom ash, gypsum, blast furnace and steel manufacture slags, and stone powder sludge, were evaluated. Various physicochemical and hydrodynamic properties of the industrial byproducts were investigated. The environmental safety was monitored using batch and long-term leaching tests as well. In addition, the flexibility of plants was observed by cultivating them in the industrial by-products. The results for physicochemical properties indicate that most of the materials considered appeared to be suitable for landfill cover. Particularly, the concentration levels of hazardous elements regulated by the Korean Law for Waste Management did not exceed the regulatory limits in all target materials. In addition, the concentrations of regulated elements for the Korean Soil Conservation Law were examined below the regulatory limits in most of materials considered, except for the stone powder sludge. The results of batch and long-term experiments showed bottom ash and construction waste were the most suitable materials for landfill cover among the industrial by-products considered. The results of plant studies indicate that the bottom ash among industrial by-products considered was most effective in developing vegetation on landfill site, showing fast germination and large growth index. At the final covering system made of mixture of soil and bottom ash, the optimum application rate of farmyard manure was observed to be 40-50 Mg/ha.

A Study on the Effective Length Factor for Steel Plate-Concrete Structures using Cementless Concrete (무시멘트 콘크리트를 활용한 강판콘크리트 구조의 유효좌굴길이 계수 분석에 관한 연구)

  • Han, Myoung-Hwan;Choi, Byong-Jeong
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.19 no.5
    • /
    • pp.661-671
    • /
    • 2018
  • Domestic studies on steel plate concrete structures have focused on nuclear structures with high strength. In this study, the SC structure was applied to the general structure, and the SC structure that is advantageous in terms of safety and construction was limited to a special structure. As a basic study for applying SC, this paper proposes basic design information of a SC structure applying cement concrete to plan the structure, which is suitable for eco - friendliness by replacing concrete cement, an important factor in a SC structure, with blast furnace slag. This study examined the compression characteristics and the effective length factor under central compression load. To calculate the effective length factor, the Euler column theory was applied without applying plate theory. The effective length factor was calculated from the yield strength of the steel plate, buckling of the steel plate, and the point at which the concrete was broken. In addition, this study examined whether the maximum compressive strength meets the national and international reference equations with the slenderness ratio (B/t) as a parameter. By analyzing the buckling of the specimen by applying the column theory and selecting the strain of the measured steel plate, the effective length factor was analyzed and compared with the value presented in the reference equation.

Optimum Mix Proportion and Characteristics of the Combined Self Compacting Concrete according to Cement Types (시멘트 종류에 따른 병용계 자기충전 콘크리트의 최적배합비와 특성)

  • Kwon, Yeong-Ho
    • Journal of the Korea Concrete Institute
    • /
    • v.21 no.1
    • /
    • pp.55-64
    • /
    • 2009
  • This study is aimed to derive the optimum mix proportion of the combined self compacting concrete according to cement types (blast-furnace slag cement and belite cement) and to propose the basic data to field construction work after evaluating the quality properties. Specially, lime stone powder (LSP) as binder and viscosity agent are used in the combined self compacting concrete because slurry wall of an underground LNG storage tank should be kept stability of quality during concrete working. Replacement ratio of LSP is determined by confined water ratio test and main design factors including fine aggregate ratio ($S_r$), coarse aggregate ratio ($G_v$) and water-cement ratio (W/C) are selected. Also, quality properties including setting time, bleeding content, shortening depth and hydration heat on the optimum mix proportion of the combined self compacting concrete according to cement type are compared and analyzed. As test results, the optimum mix proportion of the combined self compacting concrete according to cement type is as followings. 1) Slag cement type-replacement ratio of LSP 13.5%, $S_r$ 47% and W/C 41%. 2) Belite cement type-replacement ratio of LSP 42.7%, Sr 43% and W/C 51%. But optimum coarse aggregate ratio is 53% regardless of cement types. Also, as test results regarding setting time, bleeding content, shortening depth and hydration heat of the combined self compacting concrete by cement type, belite cement type is most stable in the quality properties and is to apply the actual construction work.